DE494747C DESCH87621D DESC087621D DE494747C DE 494747 C DE494747 C DE 494747C DE SCH87621 D DESCH87621 D DE SCH87621D DE SC087621 D DESC087621 D DE SC087621D DE 494747 C DE494747 C DE 494747C
Authority
DE
Germany
Prior art keywords
lower leg
pin
leg
pushed out
clamping plate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
DESCH87621D
Other languages
German (de)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to DESCH87621D priority Critical patent/DE494747C/en
Application granted granted Critical
Publication of DE494747C publication Critical patent/DE494747C/en
Expired legal-status Critical Current

Links

Classifications

    • BPERFORMING OPERATIONS; TRANSPORTING
    • B21MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL
    • B21KMAKING FORGED OR PRESSED METAL PRODUCTS, e.g. HORSE-SHOES, RIVETS, BOLTS OR WHEELS
    • B21K7/00Making railway appurtenances; Making vehicle parts
    • B21K7/02Making railway appurtenances; Making vehicle parts parts for permanent way
    • B21K7/08Making railway appurtenances; Making vehicle parts parts for permanent way base plates for rails, e.g. chairs

Landscapes

  • Engineering & Computer Science (AREA)
  • Mechanical Engineering (AREA)
  • Railway Tracks (AREA)

Description

Herstellung von Federklemmplatten Es sind Schienenbefestigungen mittels federnder Klemmplatten bekannt geworden, bei denen die Klemmplatte aus zwei in einem Abstande übereinanderliegenden Schenkeln besteht, deren unterer auf der Schwellendecke ruht und mittels eines Zapfens den Schienenfuß seitlich abstützt, während der obere Schenkel den Schienenfuß übergreift und federnd auf die Schwellendecke preßt.Manufacture of spring clamping plates There are rail fastenings by means of resilient clamping plates become known in which the clamping plate consists of two in one There are spaced legs on top of each other, the lower one on the sleeper ceiling rests and supports the rail foot laterally by means of a pin, while the upper Leg engages over the rail foot and presses it resiliently onto the sleeper ceiling.

11Zit Rücksicht darauf, daß die die Schwellendecke berührende Fläche des Schenkels auf der Schwellendecke aufliegen muß, bereitet die Ausbildung des Zapfens, der eine geringere Breite als die Klemmplatte aufweist, Schwierigkeiten, i wenn die Klemmplatte, wie es allein Wirtschaftlieh ist, im Walzverfahren hergestellt werden soll. Es müßte bei diesem Verfahren der Zapfen in Form einer Rippe mitgewalzt werden, worauf im weiteren Fertiggang dann der überflüssige Werkstoff rechts und links von dem stehenbleibenden Zapfen zu entfernen wäre. Die Entfernung durch Spanabheben oder Stangen ist unwirtschaftlich.11Because of the fact that the surface touching the threshold cover of the leg must rest on the sleeper ceiling, prepares the training of the Pin, which has a smaller width than the clamping plate, difficulties i if the clamping plate, as it is only economical, is manufactured by rolling shall be. With this method, the pin would have to be rolled in the form of a rib whereupon the superfluous material on the right and to the left of the remaining peg would have to be removed. The removal by chip removal or rods are uneconomical.

Um nun diesem Übelstande abzuhelfen und um die Platte ohne Ansatz für den Zapfen walzen zu können, hat manbereits vorgeschlagen, den Zapfen dadurch herzustellen, daß er aus der Klemmplatte herausgedrückt wird. Hierbei geschah das Herausdrücken des Zapfens derart, daß an dieser Stelle kein Zusammcnhang des .herausgedrückten Zapfens an dem am Schraubenloch anliegenden Teil mit dem Werkstoff des unteren Schenkels verblieb, wodurch eine be- , deutende, zu häufigen Rissen Anlaß gebende Schwächung der Klemmplatte entstand.In order to remedy this inconvenience and the plate without approach To be able to roll for the pin, it has already been proposed to use the pin to produce that it is pushed out of the clamping plate. This is where it happened Push out the pin in such a way that at this point there is no connection between the Pin on the part resting on the screw hole with the material of the lower leg remained, as a result of which a significant weakening giving rise to frequent cracks the clamping plate was created.

Gemäß der Erfindung soll nun eine Klemmplatte geschaffen werden. bei der ebenfalls ein Profilstab im glatten Zustande gewalzt und hiernach der Zapfen aus dem unteren Schenkel herausgepreßt wird, jedoch nur so weit, als es für das Abstützen des Schienenfußes erforderlich ist und nur so weit, daß noch ein Zusammenhang des Zapfens mit dem Schenkel der Klemmplatte verbleibt, so daß eine wesentliche Schwächung der Platte an dieser Stelle verhindert wird.According to the invention, a clamping plate is now to be created. at which also rolled a profile bar in the smooth state and then the pin is squeezed out of the lower leg, but only as far as it is for the Support of the rail foot is necessary and only so far that there is still a connection of the pin remains with the leg of the clamping plate, so that a substantial Weakening of the plate at this point is prevented.

In der Zeichnung ist der Erfindungsgedanke veranschaulicht.The idea of the invention is illustrated in the drawing.

Es wird zunächst in bekannter Weise ein Walzstab mit einem der Abb. i oder 2 entsprechenden Querschnitt gewalzt, worauf Stücke abgeteilt werden, die der Breite der Klemmplatte entsprechen. In diese. Stücke werden alsdann ebenfalls in bekannter Weise die Schraubenlöcher a und b nacheinander (Abb. i) oder gleichzeitig (Abb. 2) eingestanzt. Hierauf wird durch einen entsprechend gestalteten Stempel der Zapfen c aus dem unteren Schenkel d herausgedrückt (Abb. 3), und zwar erfindungsgemäß nur so weit, daß ein Zusammenhang des herausgepreßten Zapfens mit dem Schenkel verbleibt. Hierauf wird in bekannter Weise der Schenkel g der Klemmplatte herumgeklappt, so daß nach Anziehen der Schraube h die Klemmplattenform gemäß Abb. 4 entsteht, bei der der Schenkel g den Schienenfuß fest auf die Schwellendecke f aufpreßt, während sich der lierausgepreßtc: Zapfen c gegen die Wandung des Loches e der Schwellendecke f legt und hierdurch durch den unteren Schenkel d der Schienenfuß seitlich abgestützt wird.It is first rolled in a known manner, a roll bar with a cross-section corresponding to Fig. I or 2, whereupon pieces are divided which correspond to the width of the clamping plate. In these. Pieces are then also punched in the known manner, the screw holes a and b one after the other (Fig. I) or simultaneously (Fig. 2). Then the pin c is pushed out of the lower leg d by a correspondingly designed punch (Fig. 3), according to the invention only so far that a connection between the pressed-out pin and the leg remains. Then the leg g of the clamping plate is folded around in a known manner, so that after tightening the screw h the clamping plate shape is created according to Fig. 4, in which the leg g presses the rail foot firmly onto the sleeper ceiling f, while the lierausgeschreßtc: pin c against the Wall of the hole e of the sleeper ceiling f places and thereby the rail foot is laterally supported by the lower leg d.

Soll der Zapfen länger ausfallen oder mit dem am Schraubenloch anliegenden Teil eine weitere Verstärkung erfahren, so kann der untere Schenkel dadurch eine weitere Verstärkung erfahren, daß er mit einer angewalzten Verstärkungsrippe i (Abb. g) versehen wird, wodurch weiterhin eine Verstärkung der Klemmplatte an der Biegestelle erzielt wird.Should the pin be longer or with the one resting on the screw hole Part of the experience is further strengthened, so the lower leg can become a experience further reinforcement that it is equipped with a rolled-on reinforcing rib i (Fig. g) is provided, which further reinforces the clamping plate at the bending point is achieved.

Claims (1)

PATEN TANSPRÜCIHE: i. Verfahren zur Herstellung von Federklemmplatten mit zwei in einem Abstande übereinanderliegenden Schenkeln, deren unterer auf der Schwellendecke ruht und den Schienenfuß seitlich abstützt, während der obere Schenkel den Schienenfuß übergreift und federnd auf die Unterlage preßt, wobei ein zur Anlage am Schraubenloch dienender Zapfen durch Herausdrücken aus dem unteren Schenkel der Klemmplatte gebildet wird, dadurch gekennzeichnet, daß das Herausdrücken des Werkstoffes aus dem unteren Schenkel nur so weit erfolgt, daß der herausgedrückte Zapfen an dem am Schraubenloch anliegenden Teil mit dem Werkstoff des unteren Schenkels in festem Zusammenhang bleibt. a. Walzstab von stumpfwinkligem Profil zur Ausführung des Verfahrens nach Anspruch i, dadurch gekennzeichnet, daß der Walzstab im Walzvorgang auf der Oberseite des unteren Schenkels an der Abbiegungsstelle mit einer durchgehenden Verstärkung(i) versehen ist. PATENT CLAIMS: i. Process for the production of spring clamping plates with two legs lying one above the other at a distance, the lower leg of which rests on the sleeper ceiling and supports the rail foot laterally, while the upper leg engages over the rail foot and presses it resiliently onto the base, whereby a pin serving to rest on the screw hole is pushed out the lower leg of the clamping plate is formed, characterized in that the material is pushed out of the lower leg only so far that the pushed out pin remains firmly connected to the part resting on the screw hole with the material of the lower leg. a. Rolling bar of obtuse-angled profile for carrying out the method according to claim i, characterized in that the rolling bar is provided with a continuous reinforcement (i) in the rolling process on the upper side of the lower leg at the point of bend.
DESCH87621D 1928-09-08 1928-09-08 Manufacture of spring clamps Expired DE494747C (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
DESCH87621D DE494747C (en) 1928-09-08 1928-09-08 Manufacture of spring clamps

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
DESCH87621D DE494747C (en) 1928-09-08 1928-09-08 Manufacture of spring clamps

Publications (1)

Publication Number Publication Date
DE494747C true DE494747C (en) 1930-03-29

Family

ID=7443735

Family Applications (1)

Application Number Title Priority Date Filing Date
DESCH87621D Expired DE494747C (en) 1928-09-08 1928-09-08 Manufacture of spring clamps

Country Status (1)

Country Link
DE (1) DE494747C (en)

Similar Documents

Publication Publication Date Title
DE494747C (en) Manufacture of spring clamps
DE2166915C3 (en) Combined tension and needle clip
DE663205C (en) Removable base for the legs of door posts made of profile iron in routes
DE2307993A1 (en) CHABLON FRAME FOR SCREEN PRINTING
DE674667C (en) Rail butt connection by means of longitudinal strips reaching over the rail feet
DE946347C (en) Elastic clamping plate for rail fastening
DE579128C (en) Press die to restore the bar provided on clamping plates for the railway superstructure on both sides of the journal
DE502035C (en) Cap shoe consisting of two parts that can be moved against each other
DE662939C (en) Bar and clamping claw for a rail fastening
DE527828C (en) Method for converting a hook plate
CH430615A (en) Guide device that can be slipped onto the support rod of a heald frame
DE943223C (en) Flexible route expansion
DE597907C (en) Method for making holes with reinforced edges in iron sleepers
DE479987C (en) Compensating rail joint with bridging tongue
DE457936C (en) Manufacture of rail shims
CH137685A (en) Process for the production of rail clamping plates which hold the rail foot down resiliently and which are supported against the sleeper screw hole by means of pins.
DE540606C (en) Process for the production of iron sleepers and production boards
CH178151A (en) Rail clamp to prevent rail wandering.
AT106116B (en) Accounting facility.
DE404962C (en) Two-part rail support plate
DE360574C (en) Device for fastening rails on sleepers
DE449348C (en) Repairing worn hook plates and the associated clamping plates for railroad tracks
DE516383C (en) Clamping device for releasable fastening of printing plates on a support block within a locking frame
DE508213C (en) Manufacture of screw holes in rail pads for wooden sleepers
DE647177C (en) Process for the production of iron railway sleepers with rail guide ribs