DE441751C - Procedure for eliminating the increase in exclusion in printing forms - Google Patents
Procedure for eliminating the increase in exclusion in printing formsInfo
- Publication number
- DE441751C DE441751C DEE34379D DEE0034379D DE441751C DE 441751 C DE441751 C DE 441751C DE E34379 D DEE34379 D DE E34379D DE E0034379 D DEE0034379 D DE E0034379D DE 441751 C DE441751 C DE 441751C
- Authority
- DE
- Germany
- Prior art keywords
- exclusion
- procedure
- eliminating
- powder
- increase
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Verfahren zur Beseitigung des Steigens des Ausschlusses in Druckformen. Das Steigen des Ausschlusses in der Druckform während des Druckens, das das Schmitzen des Papiers zur Folge hat, ist eine noch immer in der Druckerei regelmäßig vorkommende Erscheinung.Procedure for eliminating the increase in exclusion in printing forms. The increase in exclusion in the printing form during printing, the smear of the paper, is still a regular occurrence in the print shop Appearance.
In vielen Fällen ist dieser Übelstand der Verwendung beschädigten oder ungleichförmigen (nicht winkelrechten) Materials zuzuschreiben; auch kann die Ursache sein, daß die Form nicht sachverständig geschlossen wird oder auch das häufige Zurichten unter der Form.In many cases, this drawback is corrupt of use or attributable to irregular (non-angular) material; also can The cause may be that the form is not closed properly or the frequent one Trimming under the form.
Aber auch das Zittern der Karren, das Ziehen der Form durch atmosphärische Wechselungen, die Fettigkeit der Lettern, Staubteilchen, allerlei Faktoren und bisweilen Kleinigkeiten, auf welche man nicht immer gefaßt sein kann, können das Steigen des Ausschlusses veranlassen.But also the trembling of the carts, the dragging of the form through atmospheric Changes, the greasiness of the letters, dust particles, all sorts of factors and sometimes Little things, which one cannot always be prepared for, can cause the rise of the Cause exclusion.
Da es, namentlich bei größeren Formen, meistens zu zeitraubend ist, allen möglichen Ursachen nachzugehen, begnügt man sich in der Praxis öfters damit, daß man versucht, dem Steigen, da wo es stellenweise vorkommt oder wo sich eine Neigung dazu zeigt, während des Druckens zu begegnen.Since it is usually too time-consuming, especially with larger forms, to investigate all possible causes, one is often content in practice with that one tries to climb where it occurs in places or where there is a Shows tendency to encounter during printing.
Nach einem bekannten Verfahren macht man dazu mit der Spitze einer Ahle in die Seiten des Ausschlusses Grübchen und Ritze, um eine rauhe Oberfläche mit großem Reibungswiderstand zu bekommen.According to a well-known method, this is done with the tip of a Awl into the sides of the exclusion dimples and cracks to get a rough surface with great frictional resistance.
Dies ist eine ziemlich primitive Methode und, da sie die Lettern der Gefahr der Beschädigung aussetzt, ist sie auch nicht einwandfrei.This is a fairly primitive method and, since it uses the letters of the If there is a risk of damage, it is also not flawless.
Eine andere bekannte Methode besteht darin, daß Gummistreifen, die sogenannten »Wunderregletten« zwischen dem Ausschluß und den Lettern angebracht werden.Another known method is that rubber strips that so-called "miracle rules" attached between the exclusion and the letters will.
Es hat sich in der Praxis gezeigt, daß auch diese elastischen Streifen das Steigen nicht verhüten können.It has been shown in practice that these elastic strips cannot prevent the climb.
Außerdem sind die beiden obenerwähnten Methoden ziemlich umständlich und nehmen dadurch recht viel Zeit in Anspruch.In addition, the two methods mentioned above are quite cumbersome and therefore take up a lot of time.
Durch die Erfindung wird dem Übel in einfacher und wirksamer Weise abgeholfen. Dazu wird nach der Erfindung auf den Stellen, wo der Ausschluß steigt oder die Neigung dazu zeigt, zwischen Ausschluß und Letter, erforderlichenfalls auch zwischen Ausschluß und Ausschluß, etwas Pulver angebracht, das den Reibungswiderstand zwischen den anstoßenden Flächen beträchtlich erhöht.The invention alleviates the evil in a simple and effective manner remedied. For this purpose, according to the invention, on the places where the exclusion increases or the tendency to, between exclusion and letter, if necessary also between exclusion and exclusion, some powder is attached to reduce the frictional resistance considerably increased between the abutting surfaces.
Das Pulver wird am besten angebracht, indem man es auf die betreffende Stelle spritzt; das Pulver selbst kann z. B. aus Magnesia, Harz, fein gemahlenem Bimsstein, Schmirgel oder aus einer Mischung zweier oder mehr dieser Stoffe bestehen.The powder is best attached by putting it on the subject Spot splashes; the powder itself can e.g. B. from magnesia, resin, finely ground Made of pumice stone, emery or a mixture of two or more of these substances.
Wenn irgendwo der Ausschluß steigt oder die Neigung dazu zeigt, so verfährt man folgendermaßen: tie Form wird aufgeschlossen, und der Ausschluß wird hinuntergedrückt. Sodann wird mit der Spitze der- Ahle ein wenig Raum zwischen dein Ausschluß und der Letter gemacht, und das Pulver wird- in den Raum gespritzt. Das kann z. B. mittels eines einfachen Apparats geschehen, der mit einer Eau-de-Colggne-Spritze Ähnlichkeit hat, oder auch mit einem, dessen Gummiball das Pulver enthält.If somewhere the exclusion increases or shows the tendency to do so, so proceed as follows: tie form is open-minded, and the Exclusion is pushed down. Then the point of the awl is a little Space is made between your exclusion and the letter, and the powder is put into the Sprayed space. This can be B. done by means of a simple apparatus with resembles an Eau-de-Colggne syringe, or one with a rubber ball the powder contains.
Als allgemeine Regel gilt, daß mehr Pulver angewendet werden muß, je größer der steigende Ausschluß ist. Das richtige Maß lernt man bald durch Erfahrung.As a general rule, more powder must be used the greater the increasing exclusion. One soon learns the right amount through experience.
Mit einem Pinsel wird das überflüssige Pulver entfernt, wonach die Form wieder geschlossen werden kann. ' Das Verfahren nach der Erfindung ist also sehr einfach, und es hat sich im praktischen Gebrauch bewährt.The excess powder is removed with a brush, after which the Form can be closed again. 'The method according to the invention is therefore very simple, and it has proven itself in practical use.
Claims (1)