DE3774580D1 - Verfahren zum hartloeten von korrosionsbestaendigen duennwandigen rohren aus nickel-basis-legierungen an rostfreie stahlbauteile. - Google Patents
Verfahren zum hartloeten von korrosionsbestaendigen duennwandigen rohren aus nickel-basis-legierungen an rostfreie stahlbauteile.Info
- Publication number
- DE3774580D1 DE3774580D1 DE8787905338T DE3774580T DE3774580D1 DE 3774580 D1 DE3774580 D1 DE 3774580D1 DE 8787905338 T DE8787905338 T DE 8787905338T DE 3774580 T DE3774580 T DE 3774580T DE 3774580 D1 DE3774580 D1 DE 3774580D1
- Authority
- DE
- Germany
- Prior art keywords
- nickel
- hard
- stainless steel
- based alloys
- steel components
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K35/00—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting
- B23K35/22—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by the composition or nature of the material
- B23K35/24—Selection of soldering or welding materials proper
- B23K35/30—Selection of soldering or welding materials proper with the principal constituent melting at less than 1550 degrees C
- B23K35/3013—Au as the principal constituent
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K1/00—Soldering, e.g. brazing, or unsoldering
- B23K1/14—Soldering, e.g. brazing, or unsoldering specially adapted for soldering seams
- B23K1/18—Soldering, e.g. brazing, or unsoldering specially adapted for soldering seams circumferential seams, e.g. of shells
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K1/00—Soldering, e.g. brazing, or unsoldering
- B23K1/19—Soldering, e.g. brazing, or unsoldering taking account of the properties of the materials to be soldered
Landscapes
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Chemical & Material Sciences (AREA)
- Materials Engineering (AREA)
- Heat Treatment Of Articles (AREA)
- Ceramic Products (AREA)
- Physical Or Chemical Processes And Apparatus (AREA)
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US06/888,544 US4726508A (en) | 1986-07-21 | 1986-07-21 | Method of brazing corrosion resistant nickel-based thin-walled tubing to stainless steel base members |
PCT/US1987/001726 WO1988000509A1 (en) | 1986-07-21 | 1987-07-17 | Method of brazing corrosion resistant nickel-based thin-walled tubing to stainless steel base members |
Publications (1)
Publication Number | Publication Date |
---|---|
DE3774580D1 true DE3774580D1 (de) | 1991-12-19 |
Family
ID=25393361
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
DE8787905338T Expired - Lifetime DE3774580D1 (de) | 1986-07-21 | 1987-07-17 | Verfahren zum hartloeten von korrosionsbestaendigen duennwandigen rohren aus nickel-basis-legierungen an rostfreie stahlbauteile. |
Country Status (7)
Country | Link |
---|---|
US (1) | US4726508A (de) |
EP (1) | EP0316353B1 (de) |
JP (1) | JPH02501718A (de) |
AU (1) | AU592223B2 (de) |
BR (1) | BR8707753A (de) |
DE (1) | DE3774580D1 (de) |
WO (1) | WO1988000509A1 (de) |
Families Citing this family (11)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US5423221A (en) * | 1986-02-11 | 1995-06-13 | Abb K-Flow Inc. | Mass flow measuring device |
US5073208A (en) * | 1989-09-14 | 1991-12-17 | K-Flow Corporation | Method for cryogenic treatment of Coriolis mass flow meter structures |
US5344717A (en) * | 1993-01-25 | 1994-09-06 | Micro Motion, Incorporated | Method of brazing and apparatus |
US5598968A (en) * | 1995-11-21 | 1997-02-04 | General Electric Company | Method for preventing recrystallization after cold working a superalloy article |
US6513392B1 (en) | 1998-12-08 | 2003-02-04 | Emerson Electric Co. | Coriolis mass flow controller |
US6748813B1 (en) | 1998-12-08 | 2004-06-15 | Emerson Electric Company | Coriolis mass flow controller |
US20020000404A1 (en) * | 2000-03-17 | 2002-01-03 | Michael Mutsakis | Filtration element for severe service applications |
CN1187159C (zh) * | 2000-04-28 | 2005-02-02 | 艾略特涡轮机械公司 | 钎焊方法和由此制得的制品 |
US6863995B2 (en) * | 2003-05-16 | 2005-03-08 | Praxair S.T. Technology, Inc. | Method for brazing components using a Ni-Au-P ternary brazing alloy, the assembly so produced and the ternary alloy |
CN101920367A (zh) * | 2010-07-27 | 2010-12-22 | 中国科学院等离子体物理研究所 | 一种钼管与不锈钢中空件的焊接工艺 |
US9765416B2 (en) * | 2015-06-24 | 2017-09-19 | Ati Properties Llc | Alloy melting and refining method |
Family Cites Families (12)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB740474A (en) * | 1953-03-17 | 1955-11-16 | Chicago Bridge & Iron Co | Improvements in or relating to the cladding of metal plates |
NL277271A (de) * | 1961-04-17 | |||
US3577233A (en) * | 1968-09-10 | 1971-05-04 | Western Gold & Platinum Co | High temperature brazing alloys |
JPS496470A (de) * | 1972-05-09 | 1974-01-21 | ||
US4274908A (en) * | 1978-08-15 | 1981-06-23 | United Technologies Corporation | Cyanide free solution and process for removing gold-nickel braze |
KR850001248B1 (ko) * | 1979-09-20 | 1985-08-26 | 웨스팅하우스 일렉트릭 코오포레이숀 | 원자로의 계기기둥의 경납땜 보수방법 |
JPS5847267B2 (ja) * | 1980-11-18 | 1983-10-21 | 株式会社東芝 | 電子管の真空容器 |
US4405391A (en) * | 1981-01-14 | 1983-09-20 | Allied Corporation | Homogeneous, ductile nickel-palladium brazing foils |
GB2092692B (en) * | 1981-02-05 | 1984-05-02 | Flowdrilling Uk Ltd | Improvements in pipe joints |
JPS5821093A (ja) * | 1981-07-29 | 1983-02-07 | 川崎重工業株式会社 | 耐蝕二重管 |
US4604328A (en) * | 1982-09-24 | 1986-08-05 | Gte Products Corporation | Ductile brazing alloy containing reactive metals and precious metals |
US4508257A (en) * | 1983-02-28 | 1985-04-02 | Allied Corporation | Method of brazing with nickel based alloy |
-
1986
- 1986-07-21 US US06/888,544 patent/US4726508A/en not_active Expired - Lifetime
-
1987
- 1987-07-17 EP EP87905338A patent/EP0316353B1/de not_active Expired
- 1987-07-17 DE DE8787905338T patent/DE3774580D1/de not_active Expired - Lifetime
- 1987-07-17 AU AU78016/87A patent/AU592223B2/en not_active Expired
- 1987-07-17 BR BR8707753A patent/BR8707753A/pt not_active IP Right Cessation
- 1987-07-17 WO PCT/US1987/001726 patent/WO1988000509A1/en active IP Right Grant
- 1987-07-17 JP JP62504801A patent/JPH02501718A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
AU7801687A (en) | 1988-02-10 |
EP0316353A1 (de) | 1989-05-24 |
BR8707753A (pt) | 1989-08-15 |
EP0316353B1 (de) | 1991-11-13 |
WO1988000509A1 (en) | 1988-01-28 |
JPH02501718A (ja) | 1990-06-14 |
JPH0372382B2 (de) | 1991-11-18 |
US4726508A (en) | 1988-02-23 |
AU592223B2 (en) | 1990-01-04 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
DE3786007D1 (de) | Verfahren zum trennen eines einzelnen bestandteils von seiner fluessigen loesung. | |
DE3584701D1 (de) | Verfahren zur anzeige eines bildes. | |
DE3877229D1 (de) | Verfahren zum entfernen von nox aus fluidstroemen. | |
DE3783593D1 (de) | Verfahren zum betreiben eines analysiergeraets. | |
DE3871877D1 (de) | Verfahren zum anbringen eines orthodontischen hilfsstuecks. | |
ATA411284A (de) | Verfahren zum schmieden von superlegierungen auf nickelbasis sowie ein gegenstand aus einer superlegierung auf nickelbasis mit verbesserter schmiedbarkeit | |
DE3786447D1 (de) | Verfahren der ortungsdaten in bogenschweissen. | |
NL191762B (nl) | Werkwijze en mengsel ter verwijdering van aluminide bekleding van nikkel superlegeringen. | |
DE3686638D1 (de) | Verfahren zur herstellung von titan-nickel-legierungen. | |
DE3483651D1 (de) | Verfahren zur lokalisierung von gegenstaenden eines sachregisters. | |
ATA392184A (de) | Gegenstand aus einer austenitischen, nichtrostenden stahl-legierung | |
DE3679617D1 (de) | Elektrolytische niederschlaege aus palladium und einer palladium enthaltenden legierung und verfahren zu ihrer herstellung. | |
ATA80288A (de) | Verfahren zum herstellen von rohren aus nichteisenmetall | |
DE3881923D1 (de) | Verfahren zur herstellung von beschichteten metallrohre. | |
DE3484637D1 (de) | Verfahren zur umwandlung eines eingangsbitstromes. | |
DE3774580D1 (de) | Verfahren zum hartloeten von korrosionsbestaendigen duennwandigen rohren aus nickel-basis-legierungen an rostfreie stahlbauteile. | |
DE3674951D1 (de) | Thermoplastisches verfahren zum verringern des durchmessers eines metallischen rohrs. | |
DK165791C (da) | Middel til inhibering af metalkorrosion i vandfoerende systemer, kompleks omfattende et aminophosphionsyrederivat og manganion samt fremgangsmaade til inhibering af metalkorrosion i vandfoerende systemer | |
DE3763492D1 (de) | Verfahren zur entfernung von metallcarbonylen aus gasfoermigen stroemen. | |
DE3485171D1 (de) | Verfahren zum anzeigen eines bildes. | |
AT380769B (de) | Verfahren zur behandlung von zu verkaufendem gemuese | |
DE3584563D1 (de) | Verfahren zur ausfuehrung eines loesungskonzentrationsprozesses. | |
DE3769879D1 (de) | Verfahren zur rueckgewinnung von metallen. | |
DE3861651D1 (de) | Verfahren zur wiedergewinnung von platingruppenmetallen. | |
DE3777237D1 (de) | Verfahren zum nachweis von metallen. |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
8364 | No opposition during term of opposition |