CS270805B3 - Cement mixture with increased watertightness - Google Patents
Cement mixture with increased watertightnessInfo
- Publication number
- CS270805B3 CS270805B3 CS516587A CS516587A CS270805B3 CS 270805 B3 CS270805 B3 CS 270805B3 CS 516587 A CS516587 A CS 516587A CS 516587 A CS516587 A CS 516587A CS 270805 B3 CS270805 B3 CS 270805B3
- Authority
- CS
- Czechoslovakia
- Prior art keywords
- mix
- cement
- cement waterproof
- cement mixture
- mass parts
- Prior art date
Links
- 239000004568 cement Substances 0.000 title abstract 5
- 239000000203 mixture Substances 0.000 title abstract 4
- 239000010426 asphalt Substances 0.000 abstract 1
- 230000007797 corrosion Effects 0.000 abstract 1
- 238000005260 corrosion Methods 0.000 abstract 1
- 230000000694 effects Effects 0.000 abstract 1
- 239000004816 latex Substances 0.000 abstract 1
- 229920000126 latex Polymers 0.000 abstract 1
- 230000000246 remedial effect Effects 0.000 abstract 1
- 230000008439 repair process Effects 0.000 abstract 1
- 239000000126 substance Substances 0.000 abstract 1
- 239000002351 wastewater Substances 0.000 abstract 1
Landscapes
- Road Paving Structures (AREA)
- Building Environments (AREA)
- Compositions Of Macromolecular Compounds (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| CS516587A CS270805B3 (en) | 1978-12-01 | 1987-07-08 | Cement mixture with increased watertightness |
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| CS791478A CS204397B1 (en) | 1978-12-01 | 1978-12-01 | Cement mixture with increased water-tightness |
| CS516587A CS270805B3 (en) | 1978-12-01 | 1987-07-08 | Cement mixture with increased watertightness |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| CS516587A1 CS516587A1 (en) | 1989-12-13 |
| CS270805B3 true CS270805B3 (en) | 1990-08-14 |
Family
ID=25746121
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| CS516587A CS270805B3 (en) | 1978-12-01 | 1987-07-08 | Cement mixture with increased watertightness |
Country Status (1)
| Country | Link |
|---|---|
| CS (1) | CS270805B3 (cs) |
-
1987
- 1987-07-08 CS CS516587A patent/CS270805B3/cs unknown
Also Published As
| Publication number | Publication date |
|---|---|
| CS516587A1 (en) | 1989-12-13 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| ATE167174T1 (de) | Gebrauchsfertige, aushärtende fugenzusammensetzung | |
| DK336185D0 (da) | Hydraulisk cement | |
| DE3170748D1 (en) | Colouring agent | |
| NO172255C (no) | Fremgangsmaate ved innblanding av tilsetningsstoffer i en stoepemasse samt tilsetning til bruk ved fremgangsmaaten | |
| CS270805B3 (en) | Cement mixture with increased watertightness | |
| ATE74579T1 (de) | Selbstnivellierende moertelmischung. | |
| ATE42265T1 (de) | Verwendung einer betonmischung bzw. zementmoertelmischung zur herstellung von abwasser-bauwerken und verfahren zur herstellung einer solchen mischung. | |
| KR890017193A (ko) | 소성경량골재의 제조방법 | |
| GB1550003A (en) | Lightweight aggregates | |
| KR890000368A (ko) | 황토흙을 이용한 벽돌의 제조방법 | |
| KR860002433A (ko) | 내수성 경량벽돌의 제법 | |
| GB899962A (en) | Improvements in mortar and grouting or pointing compositions | |
| KR830007990A (ko) | 콘크리트를 양생하는 방법 | |
| KR840008792A (ko) | 폐비닐(합성수지) 열처리용액과 연탄재 및 토사석 혼합제품 제조방법 | |
| US1506193A (en) | Waterproofing composition for walls | |
| KR850001059A (ko) | 시멘트 미장벽돌의 제법 | |
| KR880011039A (ko) | 황토 흙을 이용한 벽돌의 제조방법 | |
| KR850005388A (ko) | 아스팔트를 이용한 석재타일의 제법 | |
| GB373609A (en) | Improvements in damp-proofing and waterproofing walls | |
| KR830008951A (ko) | 토공 벽돌 제조방법 | |
| KR880007190A (ko) | 시멘트와 아스팔트의 교반법 | |
| KR880002969A (ko) | 시멘트 방수 혼화제의 제조방법 | |
| KR860001769A (ko) | 유리판 이면에 첨착물을 부착하는 방법 | |
| KR890009718A (ko) | 플로팅(floating) 플로어(floor)의 퍼얼라이트(perlite) 공법 | |
| BG51866A1 (en) | Ground coat mixtrure |