CS237448B1 - Mixture of raw materials for cement production - Google Patents
Mixture of raw materials for cement production Download PDFInfo
- Publication number
- CS237448B1 CS237448B1 CS817295A CS729581A CS237448B1 CS 237448 B1 CS237448 B1 CS 237448B1 CS 817295 A CS817295 A CS 817295A CS 729581 A CS729581 A CS 729581A CS 237448 B1 CS237448 B1 CS 237448B1
- Authority
- CS
- Czechoslovakia
- Prior art keywords
- mixture
- component
- raw materials
- cement production
- coal
- Prior art date
Description
1
UsoópeTeHse othochtcz k npoMunuieHHOCTH CTpouTejihHuxMSTepaaiOB, b zacTHOCTH, k HH3KOTeMnepaTypHoft cozeBoňTexzojiorzz npoB3£oj[CTBa ueMeHTa. M3BecTHa capteBaz cmbcb jyw nojiyHezzn neMeHTHoroXJGIHKepa, BKJUJqaBIUaH H3BeCTHHKOBH®, rjHHHCTHlt, ΚρβΜΗβ-3eMconepxamzS z xeje3zcraft κομποηθητη (I).
Haztíojiee 0λη3κο8 k Η3θόρβτβΗΗΒ no τβχΗζηβοκοδ cym-hoctk z flocrzraeMOMy pe3yju»TaTy hbjlh6tch cHpbeBaz CMecb,BKJIBqaBGjaH H3BeCTHZKOBHÍI, ΓΛΗΗΖΟΤΗΖ, ΧβΛβ3ΖΟΤΗϋ ΚΟΜΠΟ—HGHTH, 40-70% ΤΒβρΛΟΓΟ ΤΟΠΛΖΒβ Z 10-12% ΧΠΟρΗΟΤΟΓΟ KaJIB-UXS (2).
HejiocTaTKaMz z3B6Cthhx τβΧΗζζβοκζχ pemeHzft zbjudt-?,£ HZ3K8A CKOpOCTB Z ΗβΠΟΛΗΟΤβ ΟΓΟρβΗΗΗ ΤΟΠΛΗΒβ, ΗΗ3ΚΗβΕρ0Π330πΖΤβΛΒΗ00ΤΙ. ΠβΠΗ Ζ .ΓΖΑΡβΤβΠΗΟΗΗβΗ βΚΤΖΒΗΟΟΤΒsjízHKspa. ί-ΘΛΒ Ζ3ΟόρβΤβΗΖΗ - γΒβΛΖΗβΗΗβ CKOpOCTH Η ΠΟΛΗΟΤΗCropaHHZ ΤΟΠΛΗΒβ, nOBHIfleHZe πρ0Η3Β0ΛΗΤβΛΒΗ00ΤΗ nezz ΗračpaTauzoHHoit θκτηβηοοτη KJizHKepa. ΠΟΟΤβΒΛβΗΗΗΗ ϋβΛΒ ΛΟΟΤΖΓββΤΟΗ ΤβΜ, ΖΤΟ ΟΗρΒβΒβΗCMeCB jyiH ΠΟΛγΉβΗΗΛ ΙΧΘΜΘΗΤΗΟΓΟ ΚΛΖΗΚβρβ, COCTOZman Η3KSBeCTHKKOBOrO, rjIHHHCTOrO, ΚβΛβ3ΗΟΤΟΓΟ ΚΟΜΠΟΗβΗΤΟΒ,xjiqpzcToro Kajunzz z yrjiH, οοΛβρχζτ yzasaHme κομποηθη-τη b cjiejiyímeM οοοτηοιπθηηη, uacc.%: 237448 2 rJIHHHCTHfi ΚΟΜΠΟΗβΗΤ 20-22/3 xe;ie3HCTíríí ΚΟΜΠΟΗβΗΤ 2,0-3,0 xjopHCTuft Kaumuft 3,5-4,5 yrojn. 3,0-6,0 H3BQCTHKKOBNÍt ΚΟΜΠΟΗβΗΤ ΟΟΤΟΒΗΟβ ΠρΗΜβρ. ΓΟΤΟΒΗΤ ΟΗρΒβΒΗβ ΟΜΘΟΗ, ΟΟΟΤβΒΗ KOTOpHX ΠρβΑ'CTaBJíeHH β Taójume I.
Taójuma I ΚΟΜΠΟΗβΗΤΗ OoAepxaHHe κομποηθητοβ bMacc.% CMeCHX, I Π m iy IÍ3BeCTHHKOBHft 70,5 69,0 67,5 66,0 Γληηηοτηζ 20 21 22 23 Zejie3HCTHfl 2 2,5 3 1,5 KaJILUHi XJlOpHCTHft 3,5 4 4,5 7 7rojn> 4 3,5 3 2,5
CwecH rpaHyjrapy»T h otízuraazr Ha araoMepanHOHHoft ycTa-εοΒκβ c coraHHeM Haa cjioeM MaTepzajia ra3a.
Pe3yjiLTara ΗοπΗτβΗκδ πρβποτβΒΛβΗΗ b Tatíjnme 2. 237448
Tadjuma 2
XapaKTepucTHKa KJMHKepa
Bafi íKajib- man CMeci : naa :npOH3- cr CaO ΠρβΛβΛ :0cTaTOHHoe : cko- : BOJÍM- CBOÓ. npOHHOC- : cojiepxaHHe :pocTB :τβΛΒ— Ta npa :yrjiepojxa τοπ- :cnexa- :hoctb cacaTHH, :jIMBa B ΚΛΒΗ- :hhh, :ycTa- aepe3 28 :xepe, % IKM/MIIH • ÍHOBKH :t/m^ cyTOK 9Krc/cbr • • • :nac • • Πθ H3O— όρβτβ- HHB I 13,6 0,51 1,98 1,61 449 0,27 Π 13,8 0,52 2,01 1,60 460 0,30 0 13,7 0,52 2,10 1,70 456 0,31 iy π,o 0,43 2,50 2,50 350 0,61 no προ- TOTHny 10,5 0,41 3,67 3,1 320 0,90 IÍCnOJIL3OBaHHe COCTaBa CUpbeBOft CM6CZ ΠΟ Η300ρβΤΘΗΗΚ) ΠΟ3-3ο-ΐΗβτ ysejaraiTt προη3βολητθλι>ηοοτβ KOHBeftepHOft pemeTKH,noEHCHTB KanecTBO luniHKepa a CTeneHB acnojissoBaHan TBep—αΌΓο TomizBa.
KflCTOamee Η3Ο0ρβΤβΗΗβ BXOOTT B KOMIineKC ΤβΧΗΟΛΟΠί—qecKJix peineHaft, KOTopue odecnenaBaDT pa3padoTKy ΗΗ3κοτεΜ·nepaTypnoS TexHOJioraa nojiyHeHaa neMeHTHoro KJiHHKepa. 237448 - 4 - ΦΟΡΜΖΤΙΔ Η30ΕΡΕΤΕΗΗΗ
GapteBaH CMect jvlh nojiyqeHHH neMeHTHoro κΛΠΗκβρβ,.cocTOHmaa H3 Η3βθοτηηκοβογο, χβΛβ3Η0Τ0Γ0 κομποηθητοβ,xjiopHCToro KaJiLUHH h yrjLH, OTjnraaiomajicji τβΜ, hto c nejitsyBejuneHHH οκοροοτΗ η ποληοτη cropaHHH τοπληββ, ποβηπιθ-HHH npOH3BOAHTeJIBHOCTH ΠΘΗΗ H riUpaTaUHOHHOÉ aKTHBHOCTHKJiHHKepa, OHa coAepoT yKa3aHHne κομποηθητη b cJiejtysmeM οοοτηοιπθηηη, Mace. %: ΓΛΗΗΗΟΤΚί! ΚΟΜΠΟΗβΗΤ 20,0-22,0
XeJie3HCTHÍt ΚΟΜΠΟΗβΗΤ 2,0-3,0 xjiopHCTuň Kajiioalt 3,5-4,5 yroJiB 3,0-6,0 E3B6CTHHK0BHŽ ΚΟΜΠΟΗβΗΤ ΟΟΤΘΛΒΗΟβ ECTOTHÍIKH ΗΗφορΜβΠΗΗ, ΠρΗΗΗΤΗβ BO ΒΗΗΜβΗΗβ ΠρΗ3κοπβρτΗ3β: 1. D.M.EyTT h Apyrne "XnMunecKaH τθχηολογηη BHxymstxMaTepnajioB", M., Ba eman mKOJia, 1980, c. 120. 2. ΑΒΤοροκοβ CBímeTejiBCTBO CCCP J6 30I3I5, C04B 7/44,1967 (προτοτππ). 237448 5 AHHOTAUHfl
HacTOHniee Η3οΰρβτβΗΗβ othochtch k προΜϋΐιυιβΗΗοοτΗcTpoKTejihHHX MaTepHajiob , b HacTHOcTH, κ HH3KOTeMnepa-TypHofl οολθβοΛ TexHOJioro προη3βολοτβθ newieHTa.
CypseBan CMech jyiH πολ^ήθηηη neMeHTHoro KJiHHKepa,cocToamaa H3 H3BecTKOBoro, γληηηοτογο , xejte3acToro kom-ΠΟΗβΗΤΟΒ, JUIOpHCTOrO KaJIBUHH H yrJLH, ΟΤΛΗΗβΕΠΙβΗΟΗ T6M,Ήτο ona cojiepxHT yKa3aHHué κομποηβητη b cjiejtynneM coot- HOineHHH, Mace.#: rJIHHHCTHÍi ΚΟΜΠΟΗβΗΤ 20,0-22,0 xejie3HCTHft κομποηθητ 2,0-3,0 xjiopHCTUfl KaJiBiíuft 3,5-4,5 yroni 3,0-6,0 Z3BeCTKOBUfl ΚΟΜΠΟΗβΗΤ ΟΟΤβΛΒΗΟβ 237448
Severografia, n. p., MOST
Cena 2,40 Kčs
Claims (1)
- 237448 6 Ρ δ E D U £ T VYNALEZU Surovinové směs pro výrobu cementéřského slínku, skládající sa z vápencového, žele-zí tého komponentu, chloridu vápenatého a uhlí, se vyznačuje tím, že s cílem zvýženírychlosti a úplnosti shoření paliva, zvýšení produktivity pece a hydratační aktivityslínku, obsahuje uvedené komponenty v těchto váhových poměrech, %i Komponent hlinitý 20,0 až 22,0 Komponent železitý 2,0 až 3,0 Chlorid vápenatý 3,5 až 4,5 Uhlí 3,0 až 6,0 Komponent vápencový zbytek Uznáno vynálezem na základě výsledků expertizy, provedené Státním výborem pro vy-nálezy a objevy SSSR, Uoskva, SU.