CS225396B1 - Cleanning of the lining of the nose and collar of the converter - Google Patents
Cleanning of the lining of the nose and collar of the converter Download PDFInfo
- Publication number
- CS225396B1 CS225396B1 CS477782A CS477782A CS225396B1 CS 225396 B1 CS225396 B1 CS 225396B1 CS 477782 A CS477782 A CS 477782A CS 477782 A CS477782 A CS 477782A CS 225396 B1 CS225396 B1 CS 225396B1
- Authority
- CS
- Czechoslovakia
- Prior art keywords
- lining
- collar
- rod
- deposit
- converter
- Prior art date
Description
Doposud se čistí konvertory od nánosu kovu či strusky různými mechanickými prostředky, např. zbíjecími kladivy nebo opalováním hořákem či proudem kyslíku. Nevýhodou těchto způsobů je poměrně nízký výkon, značná pracnost a relativně vysoká energetická náročnost. Rovněž je nevýhodou to, že někdy dochází k poškození vyzdívky hrdla či límce konvertoru.So far, converters have been cleaned of metal or slag deposits by various mechanical means, such as hammers or by burning with a burner or oxygen stream. The disadvantages of these methods are relatively low power, considerable labor and relatively high energy consumption. It is also a disadvantage that sometimes the lining of the converter collar or neck is damaged.
Uvedené nedostatky se odstraní způsobem čistění vyzdívky hrdla a límce konvertoru podle vynálezu, Jehož podstata spočívá v tom, že nános výhozu se odtavuje paprskem plazmy plazmového hořáku stabilizovaného plynem, případně kapalinou, přičemž nános se polarizuje pomocnou tyčí, kterou se přivádí kyslík, jenž vytvoří v nánosu roztavenou oblast, do které se tyč zanoří, přívod kyslíku se pak přeruší a po zatuhnutí tyče v nánosu se tyč napojí ke zdroji plazmového hořáku.These drawbacks are eliminated by the method of cleaning the lining of the neck and collar of the converter according to the invention, characterized in that the deposition of the ejection is melted by a plasma jet of a plasma torch stabilized by a gas or liquid. The oxygen supply is then interrupted and, after the rod has solidified in the deposit, the rod is connected to the plasma torch source.
Výhodou způsobu podle vynálezu je poměrně malá pracnost a vysoký výkon čistění, přičemž nehrozí nebezpečí poškození vyzdívky. Také je výhodou to, že přes poměrně značný instalovaný příkon je způsob energeticky méně náročný a to z důvodu kratšího času čistění.The advantages of the method according to the invention are relatively low labor and high cleaning performance, without the risk of damaging the lining. It is also an advantage that, despite the relatively large installed power input, the method is less energy intensive due to the shorter cleaning time.
Pro objasnění způsobu čistění vyzdívky hrdla a límce konvertoru se uvádí příklad, kdy pro čistění nánosu výhozu byl použit plazmový hořák o výkonu 0,9 MW stabilizovaný argonem. Pomocná tyč, která byla svým koncem zatavena do nánosu výhozu, byla spojena vodivě s anodou plazmového hořáku, čímž došlo k polarizaci nánosu výhozu. Výtok plazmy byl tak usměrněn do nánosu. Spotřeba plazmového hořáku činila 0,7 GJ na tunu odtaveného materiálu, což bylo dvakrát méně než u stávajících kyslíko-propanových hořáků.To illustrate the method of cleaning the neck lining and converter collar, an example is given where a 0.9 MW plasma torch stabilized with argon has been used to clean the ejection deposit. The auxiliary rod, which was sealed into the ejection deposit at its end, was connected conductively to the plasma torch anode, thereby polarizing the ejection deposit. The plasma discharge was thus directed into the deposition. The plasma torch consumption was 0.7 GJ per tonne of molten material, which was twice as low as the existing oxy-propane torches.
Claims (1)