CS207249B1 - Method of making the pattern for making the plates with the surface connections by the photographic way - Google Patents

Method of making the pattern for making the plates with the surface connections by the photographic way Download PDF

Info

Publication number
CS207249B1
CS207249B1 CS806679A CS806679A CS207249B1 CS 207249 B1 CS207249 B1 CS 207249B1 CS 806679 A CS806679 A CS 806679A CS 806679 A CS806679 A CS 806679A CS 207249 B1 CS207249 B1 CS 207249B1
Authority
CS
Czechoslovakia
Prior art keywords
water
carrier
printed circuit
silver
developing
Prior art date
Application number
CS806679A
Other languages
Czech (cs)
Inventor
Milan Zapalka
Original Assignee
Milan Zapalka
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Milan Zapalka filed Critical Milan Zapalka
Priority to CS806679A priority Critical patent/CS207249B1/en
Publication of CS207249B1 publication Critical patent/CS207249B1/en

Description

(54) Způsob zhotovení předlohy pro výrobu desek s plošnými spoji fotografickou cestou(54) A method of making a pattern for manufacturing printed circuit boards by photographic means

Vynález se týká způsobu zhotovení předlohy pro výrobu desek s plošnými spoji fotografickou cestou snímáním zákresu plošných spojů.The invention relates to a method of making a pattern for producing printed circuit boards by photographic means by scanning a printed circuit diagram.

Předlohy pro výrobu desek s plošnými spoji se tam, kde nejsou k dispozici fotohlavy a kreslící stoly řízené počítači zhotovují fotografickou cestou na fotografickou emulsí opatřené světlopropustné nosiče tvořené zpravidla plochým filmem. U tohoto postupu se vyhotovený zákres plošných spojů oreprodukuje velkoplošnou fotografickou kamerou v měřítku 1:1 na plochý fotografický film. Po fotochemickém zpracování se negativní obraz zákresu plošných spojů vytvořený na daném nosiči překopíruje na další nosič tohoto druhu. Na něm se dalším fotografickým zpracováním získá positivní obraz zákresu, a takto získaná předloha teprve slouží pro vlastní výrobu desky s plošnými spoji. Nevýhodou tohoto způsobu zhotovení předmětné předlohy je velká spotřeba plochého filmu a vznik chyb, jako nedodržení rozměrů či přerušení čáry vlivem nečistot, při kopírování.The printed circuit board designs are made photographic on photographic emulsion coated light-transmissive carriers, generally flat film, where there are no photo heads and computer-controlled drawing tables. In this procedure, the printed circuit board is produced or produced by a large-scale photographic camera at a 1: 1 scale to produce a flat photographic film. After photochemical processing, the negative printed circuit board image formed on the carrier is copied to another carrier of this kind. On it there is obtained a further photographic processing of the positive image of the drawing, and the thus obtained template is only used for the actual production of the printed circuit board. The disadvantage of this method of making the original document is the high consumption of the flat film and the occurrence of errors such as failure to observe the dimensions or line breaks due to impurities during copying.

Tyto nevýhody jsou odstraněny u způsobu zhotovení předlohy podle vynálezu, jehož podstata i spočívá v tom, že po vyvolání fotograficky získaného latentního obrazu zákresu plošných spojů na světlopropustném nosiči opatřeném fotografickou halogenstříbrnou emulsí a po odstranění produktů vyvolávání a vyvolávací lázně z nosiče praním se na : nosiči vyredukované stříbro zoxiduje a sloučeniny vzniklé zoxidováním stříbra se praním ve vodě odstraní, načež se zbytek oxidační lázně odstraní v čistící lázni a produkty čistění se odstraní praním ve vodě, poté se provede vyjasnění čar a zvýšení kontrastu obrazu ponořením nosiče do roztoku i převádějící halogenidy stříbra na komplex rozpustný ve vodě, a vyjasňovací kapalina a vzniklá sloučenina stříbra se odstraní praním, načež se fotografická emulse nosiče osvětlí, vyvolá a praním ve vodě se odstraní produkty vyvolávání a zbytky vývojky a nosič se usuší.These drawbacks are eliminated by the method of making the present invention, which is based on the fact that after developing a photographically obtained latent image of a printed circuit board on a light-transmissive carrier provided with a photographic halogen silver emulsion and after removing the developing products and developing bath from the carrier, the reduced silver oxidizes and the silver oxidation compounds are removed by washing in water, the remainder of the oxidation bath is removed in a cleaning bath and the cleaning products are removed by washing in water, then lines are clarified and image contrast is enhanced by dipping the carrier into silver i the water-soluble complex, and the clarifying liquid and the resulting silver compound are removed by washing, whereupon the photographic emulsion of the carrier is illuminated, developed and washed with water to remove developing products and developer residues, and the support is dried.

Zhotovováním předloh pro výrobu desek s plošnými spoji způsobem podle vynálezu se ušetří padesát procent fotografického materiálu. Kromě toho vzniká předloha pouze v jediném sledu i operací, takže vyloučením kopírování je odstraněna i možnost vzniku chyb k nímž při této operaci docházelo. Oproti dosavadním způsobům zhotovování předloh fotografickou cestou je předmětný způsob i méně nákladný, neboť přináší úspory jak na materiálu, tak i na pracnosti.The production of printed circuit boards by the method of the invention saves fifty percent of the photographic material. In addition, the original is created in only one sequence and operation, so eliminating copying eliminates the possibility of errors that occurred during the operation. Compared to the existing methods of making originals by photographic means, the method is also less expensive, since it brings savings in both material and labor.

Příklad provádění způsobu zhotovení předlohy pro výrobu desek s plošnými spoji podle vynálezu:An example of a method of making a pattern for manufacturing printed circuit boards according to the invention:

Fotograficky získaný obraz zákresu plošných spojů na fotografickou emulsí opatřeném nosiči ve formě plochého filmu se vyvolá v kontrastní,A photographically obtained image of a printed circuit board on a photographic emulsion provided with a flat film carrier is developed in a contrasting,

207 249 důrazně pracující metolhydrochinonové vývojce o alkalitě pH = 10 až 11. Osvědčila se vývojka) s označením MH-28 v ředění 1:4, teplá 20 °C, kterou se vyvolává 5 minut.207 249 vigorously working metholhydroquinone developers with an alkalinity of pH = 10-11. A developer with the designation MH-28 at a dilution of 1: 4, warm 20 ° C, was developed for 5 minutes.

Poté se praním v tekoucí vodě teplé 15 až 18 °C po dobu 5 minut odstraní z nosiče produkty vyvolávání a vyvolávací lázně.Thereafter, the developing products and the developing bath are removed from the carrier by washing in running water at 15-18 ° C for 5 minutes.

Na nosiči vyredukované stříbro se zoxiduje v roztoku dvojchromanu draselného upraveného kyselinou sírovou na pH = 2 až 5. Sloučeniny vzniklé zoxidováním stříbra se odstraní praním v proudící vodě teplé 15 až 18 °C po dobu 5 minut.The carrier-reduced silver is oxidized in a solution of potassium dichromate treated with sulfuric acid to pH = 2-5.

Zbytek oxidační lázně se odstraní v čistící lázni tvořené 2 % roztokem dvojsiřiěitanu alkalického kovu nebo 1 až 5 % roztokem siřičitanu alkalického kovu, nejlépe 5 % roztokem bezvodého siřičitanu sodného. Produkty čistění se odstraní praním v proudící vodě 15 až 18 °C teplé po dobu 5 minut.The remainder of the oxidation bath is removed in a purification bath consisting of a 2% alkali metal bisulfite solution or a 1-5% alkali metal sulfite solution, preferably a 5% anhydrous sodium sulfite solution. The purification products are removed by washing in 15 to 18 ° C running water for 5 minutes.

Pak se provede vyjasnění Čar a zvýšení kontrastu obrazu ponořením nosiče na 5 až 60 sekund do roztoku převádějícího halogenidy stříbra na komplex rozpustný ve vodě. S výhodou lze použít 20 % roztoku thiosíranu sodného. Vzniklá komplexní sloučenina stříbra se odstraní praním po dobu 5 minut v proudící vodě teplé 15 až 18 °C.The lines are then clarified and the image contrast enhanced by immersing the carrier for 5 to 60 seconds in a solution converting the silver halides to a water-soluble complex. Preferably, a 20% sodium thiosulfate solution may be used. The resulting complex silver compound is removed by washing for 5 minutes in flowing water at 15-18 ° C.

Claims (1)

PŘEDMĚTSUBJECT Způsob zhotovení předlohy pro výrobu desek s plošnými spoji fotografickou cestou snímáním zákresu plošných spojů, vyznačující se tím, že po vyvolání fotograficky získaného latentního zákresu plošných spojů na světlopropustném nosiči opatřeném fotografickou halogenstříbmou emulsí a po odstranění produktů vyvolávání a vyvolávací lázně z nosiče praním, se na nosiči vyredukované stříbro zoxiduje a sloučeniny vzniklé zoxidováním stříbra se praním ve vodě odstraní, načež se zbytekA method for producing a printed circuit board photographically by scanning a printed circuit board, characterized in that after developing a photographically obtained latent printed circuit board on a light-transmissive carrier with a photographic halogen silver emulsion and after removing the developing products and developing bath from the carrier, the reduced silver is oxidized and the compounds formed by the oxidation of silver are removed by washing in water, whereupon the residue Nato se fotografická emulse nosiče osvětluje pod hladinou vody žárovkou o příkonu 40 až 500 W po dobu 20 až 180 sekund ze vzdálenosti 0,3 až 2 m od povrchu nosiče. Osvětlený halogenid stříbra se vyvolá v kontrastně pracující vývojce.Thereafter, the photographic emulsion of the carrier is illuminated under a water surface with a 40 to 500 W lamp for 20 to 180 seconds from a distance of 0.3 to 2 m from the carrier surface. Illuminated silver halide is developed in a contrasting developer. Poté se produkty vyvolávání a zbytky vývojky odstraní praním po dobu 30 minut v proudící vodě 15 až 18 °C teplé, načež se nosič opláchne ve vodě s přídavkem smáčedla(l až lOmlna 1 litr vody).Thereafter, the developing products and developer residues are removed by washing for 30 minutes in a flowing water of 15 to 18 ° C warm, then the carrier is rinsed in water with the addition of a wetting agent (1 to 10 ml per liter of water). Postup se ukončí usušením nosiče v bezprašném prostředí za teploty až 35 °C.The process is terminated by drying the support in a dust-free environment at a temperature of up to 35 ° C. Takto vyrobená předloha desky s plošnými spoji má dostatečné krytí (optickou hustotu Dm.v = 2 a více), i jasná světla (Do kolem 0,06).The produced artwork printed boards having sufficient opacity (optical density D m. V = 2 or more), and bright light (D of about 0.06). V případě, že pomocí takto získané předlohy bude zhotovován velký počet desek s plošnými spoji, je výhodné po skončení posledního praní fotografickou emulsi utvrdit v roztoku tvrdidla, s výhodou 0,5 až 2 % vodného roztoku formaldehydu.In the event that a large number of printed circuit boards are produced using the pattern thus obtained, it is advantageous to cure the photographic emulsion in the hardener solution, preferably 0.5 to 2% aqueous formaldehyde solution, after the last wash. Žádoucích výsledků při výrobě předlohy se dosahuje zejména tím, že ustalovače (thiosíranu sodného) se použije v jiném sledu než při normálním inversním vyvolávání.Desirable results in the manufacture of the template are achieved in particular by using the fixative (sodium thiosulfate) in a sequence other than that of normal inversion development. VYNÁLEZU oxidační lázně odstraní v čistící lázni a produkty čistění se odstraní praním ve vodě, poté se provede vyjasnění čar a zvýšení kontrastu obrazu ponořením nosiče do roztoku převádějícího halogenidy stříbra na komplex rozpustný ve vodě, a vyjasňovací kapalina a vzniklá sloučenina stříbra se odstraní praním, načež se fotografická emulse nosiče osvětlí, vyvolá a praním ve vodě se odstraní produkty vyvolávání a zbytky vývojky a nosič se usuší.SUMMARY OF THE INVENTION The oxidation baths are removed in a cleaning bath and the cleaning products are removed by washing with water, then clarifying lines and enhancing image contrast by immersing the carrier in a solution converting the silver halide to a water-soluble complex, and clearing liquid and silver compound formed therefrom. the photographic emulsion of the carrier is illuminated, developed and washed with water to remove developing products and developer residues and dried.
CS806679A 1979-11-23 1979-11-23 Method of making the pattern for making the plates with the surface connections by the photographic way CS207249B1 (en)