CN85202400U - Chromium plating cyclinder jacket with thin stell pipe - Google Patents

Chromium plating cyclinder jacket with thin stell pipe Download PDF

Info

Publication number
CN85202400U
CN85202400U CN 85202400 CN85202400U CN85202400U CN 85202400 U CN85202400 U CN 85202400U CN 85202400 CN85202400 CN 85202400 CN 85202400 U CN85202400 U CN 85202400U CN 85202400 U CN85202400 U CN 85202400U
Authority
CN
China
Prior art keywords
chromium plating
chromium
reticulate pattern
thin
bearing structure
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN 85202400
Other languages
Chinese (zh)
Inventor
徐宏镕
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Family has litigation
First worldwide family litigation filed litigation Critical https://patents.darts-ip.com/?family=4798216&utm_source=google_patent&utm_medium=platform_link&utm_campaign=public_patent_search&patent=CN85202400(U) "Global patent litigation dataset” by Darts-ip is licensed under a Creative Commons Attribution 4.0 International License.
Application filed by Individual filed Critical Individual
Priority to CN 85202400 priority Critical patent/CN85202400U/en
Publication of CN85202400U publication Critical patent/CN85202400U/en
Withdrawn legal-status Critical Current

Abstract

The utility model relates to a steel pipe thin wall chromium plating cylinder sleeve which is processed and molded by soft steel seamless steel pipes. The utility model is characterized in that the inner surface of the utility model is processed in an improved spongy chromium plating method and is provided with a chromium plating layer of a deep reticulate pattern groove oil storing structure, the thickness of the chromium plating layer is between 0.04 mm and 0.09 mm, and the depth of the chromium plating layer reticulate pattern groove oil storing structure is equal to from 40% to 100% of the thickness of the chromium plating layer. The utility model has the advantages of easy fabrication, short periodicity, long service life, raw material saving, good oil storing structure and abrasion resistance.

Description

Chromium plating cyclinder jacket with thin stell pipe
The utility model relates to a kind of key part on the cylinder, and steel pipe thin-walled chromium plating cylinder liner is applicable on the cylinder of automobile, tractor engine and uses.
Cast iron or cast-iron alloy cylinder sleeve that tratitional technology is produced, its wall thickness, in course of working, utilization rate of raw materials is low, brings volume big to existing tractor and motor car engine, and power is put forward not high consequence.
Be to improve engine power, energy saving consumption and saving material prolongs motor working life.Increase the power team product, the good thin-wall cylinder casing of development wear-resisting property is paid attention to by people day by day.
Because cylinder sleeve is hidden position work at the heart of starting a machine, high temperature, poor lubrication, serious wear, therefore seeking suitable surface treatment also is the center that people were studied to obtain good oil-bearing structure raising cylinder sleeve wear-resisting property.
Britain, Japan also have producer to prepare mild steel thin-walled steel bushing at present, but their general steel plate formings that adopts, utilization rate of raw materials is low, and the surperficial chromium coating reticulate pattern groove oil-bearing structure degree of depth is controlled to be about 30~35% of chromium coating thickness, their wear-resisting propertys are poor, and the life-span is short
This practical purpose provides a kind of steel pipe thin-walled steel bushing with new internal surface oil-bearing structure, so that improve the working life of wear-resisting property and prolongation cylinder sleeve.
For this reason, the utility model is designed a kind of steel pipe thin-wall cylinder casing with new internal surface oil-bearing structure, it is characterized in that its internal surface has the chromium coating of dark reticulate pattern groove oil-bearing structure, chromium coating thickness is 0.04~0.09 millimeter, and the degree of depth of chromium coating reticulate pattern groove oil-bearing structure is 40%~100% of a chromium coating thickness.The cylinder body of this cylinder sleeve is that the mild steel seamless steel pipe is processed into, and makes easily, saves material, and is with short production cycle; Because its oil-bearing structure is good, and good lubricating condition can be provided in cylinder, cylinder sleeve is prolonged working life widely but also can gives full play to the due superior function of thin-wall cylinder casing.
Furthermore bright in conjunction with the accompanying drawings by the following examples the utility model.
Fig. 1 is a steel pipe thin-wall cylinder casing shape assumption diagram.
Fig. 2 is the crystalline phase analysis chart of reticulate pattern oil-bearing structure surface distributed on the inner surface of cylinder liner chromium coating.。
Fig. 3 is a cylinder sleeve tangent plane crystalline phase analysis chart.
1~1.5 millimeter chromium plating cylinder liner of steel pipe thin-walled cylinder body (1) is to adopt No. 20 mild steel seamless steel pipes through the cold-drawn or the machine shaping of exerting pressure, this manufacturing fraction, and work simplification to the utilization rate of raw materials height, can reach about 80%.Inner surface treatment is to adopt following improved spongy chromium plating method to carry out;
Electrolyte prescription:
Chromic anhydride (Cro 3) 230~250 grams per liters, sulfuric acid (H 2So 4)
1.8~24 grams per liters, chromic anhydride/sulfuric acid (Cro 3/ H 2So 4) 100/0.85~10.9, trivalent chromium is controlled in 3~5 grams per liters; 58~60 ℃ ± 1 ℃ of chromium plating temperature, 40~50 amperes/decimeter of current densities 2, 28~40 amperes/decimeter of porosity current densities (anodic souring) 2, 4~6 minutes porosity time.
Chromium coating (2) online groove groove oil-bearing structure (3) directly forms in chrome-plating process, 0.04~0.09 millimeter of chromium coating (2) thickness, and reticulate pattern groove oil-bearing structure (3) degree of depth is 40~100% of a chromium coating thickness.
All changes and improvements that do not break away from inner characteristic of the present utility model should belong within the claim scope of the present utility model.

Claims (4)

1, relates to a kind of thin-walled chromium plating cylinder liner of engine part, it is characterized in that its internal surface has the chromium coating of dark reticulate pattern oil-bearing structure.
2, according to the described thin-walled chromium plating of claim 1 cylinder liner, dark reticulate pattern groove oil-bearing structure is characterised in that chromium coating thickness is 0.04~0.09 millimeter, and the chromium coating reticulate pattern groove oil-bearing structure degree of depth is 40~100% of a chromium coating thickness.
3, the thin wall cylinder cover of asking according to claim 1, the cylinder body that it is characterized in that cylinder sleeve are that seamless steel pipe is processed into.
4, according to the described thin wall cylinder cover of claim 1, it is characterized in that the improved spongy chromium plating method processing of internal surface, this method is: electrolyte prescription: chromic anhydride (Cro 3) 230~250 grams per liters, sulfuric acid (H 2So 4) 1.8~2.4 grams per liters, chromic anhydride/sulfuric acid 100/0.85~0.9, trivalent chromium are controlled in 3~5 grams per liters; 5860 ° ± 1 ℃ of chromium plating temperature; 40~50 amperes/decimeter of current densities 2, 28~40 amperes/decimeter of porosity current densities (anodic souring) 24~6 minutes porosity time.
CN 85202400 1985-06-18 1985-06-18 Chromium plating cyclinder jacket with thin stell pipe Withdrawn CN85202400U (en)