CN2931651Y - Double non-corrodible steel plastic-free clad plate - Google Patents

Double non-corrodible steel plastic-free clad plate Download PDF

Info

Publication number
CN2931651Y
CN2931651Y CN 200620044596 CN200620044596U CN2931651Y CN 2931651 Y CN2931651 Y CN 2931651Y CN 200620044596 CN200620044596 CN 200620044596 CN 200620044596 U CN200620044596 U CN 200620044596U CN 2931651 Y CN2931651 Y CN 2931651Y
Authority
CN
China
Prior art keywords
stainless steel
clad plate
plate
double
steel plastic
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 200620044596
Other languages
Chinese (zh)
Inventor
郭鹿
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANGHAI HUAYUAN COMPOSITE MATERIAL CO Ltd
Shanghai Huayuan New Composite Materials Co Ltd
Original Assignee
SHANGHAI HUAYUAN COMPOSITE MATERIAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANGHAI HUAYUAN COMPOSITE MATERIAL CO Ltd filed Critical SHANGHAI HUAYUAN COMPOSITE MATERIAL CO Ltd
Priority to CN 200620044596 priority Critical patent/CN2931651Y/en
Application granted granted Critical
Publication of CN2931651Y publication Critical patent/CN2931651Y/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

A non-plastic clad plate with double stainless steel sheets for decoration and fitment of construction material comprises two layers of stainless steel plates which are combined and compressed together through a high-intensity adhesive film. Compared with the single stainless steel plate, the plate has the advantages that the double one which ensures the same intensity can save a lot of stainless steel material and facilitates the processing easiness and simpleness in the actual construction process.

Description

Two stainless steels do not have plastic clad plate
Technical field
The utility model relates to building and ornament materials, and particularly a kind of pair of stainless steel do not have plastic clad plate.
Background technology
Since the aluminum composite plate invention sixties in 20th century, in building material industry, obtained extensive use.But aluminum composite plate relies on top finishing to paint often fights and gets color, still lacks the colorful and luxurious property that is shown decoration by the metal true qualities.The domestic and international just people of corrosion resistant plate are necessary its research and development always in order to the common used material of decoration.
Summary of the invention
The purpose of this utility model is to provide a kind of pair of stainless steel not have plastic clad plate, adopt two stainless coil of strips of suitable thickness, be composited, make product have the corrosion resistant plate true qualities with the high strength bonding material membrane, be rich in ornamental and durability, make that the surface of decorating, fitting up is graceful more.
For reaching above-mentioned purpose, of the present utility model pair of stainless steel do not have plastic clad plate, is composited with splicing membrance strong intensity by two top layer corrosion resistant plates up and down.
The utility model has the advantages that: compare with single corrosion resistant plate, two stainless steels do not have plastic clad plate and are guaranteeing to have saved the stainless steel of a large amount of preciousnesses under the situation of same intensity, make that again processing and fabricating became extremely simple and convenient when product used at the scene.
Description of drawings
Fig. 1 is a structural representation of the present utility model.
Label declaration in the accompanying drawing
1, the bonding film of 3-corrosion resistant plate 2-
The specific embodiment
The utility model is described in further detail below in conjunction with accompanying drawing.
See also shown in Figure 1ly, the utility model adopts suitable thickness, the stainless-steel roll material (being corrosion resistant plate 1,3) of hardness to be composited with splicing membrance strong intensity 2.Adopt the stainless-steel roll material can realize continuous production, cut into various different sizes more as required, can reduce production costs greatly.

Claims (1)

1, a kind of pair of stainless steel do not have plastic clad plate, it is characterized in that:
Be compositely suppressed to form with splicing membrance strong intensity by upper and lower two top layer corrosion resistant plates.
CN 200620044596 2006-08-07 2006-08-07 Double non-corrodible steel plastic-free clad plate Expired - Fee Related CN2931651Y (en)