CN2849914Y - 铜包铝纳米云母漆包线 - Google Patents
铜包铝纳米云母漆包线 Download PDFInfo
- Publication number
- CN2849914Y CN2849914Y CN 200520052699 CN200520052699U CN2849914Y CN 2849914 Y CN2849914 Y CN 2849914Y CN 200520052699 CN200520052699 CN 200520052699 CN 200520052699 U CN200520052699 U CN 200520052699U CN 2849914 Y CN2849914 Y CN 2849914Y
- Authority
- CN
- China
- Prior art keywords
- copper
- covered
- enamel
- wire
- aluminium
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种铜包铝纳米云母漆包线,包括铝芯(1)和包覆在铝芯(1)上的铜层(2),在所述的铜层(2)外表面涂覆有一层纳米云母绝缘漆(3)。本实用新型是一种绝缘层薄、绝缘性能强、耐高温、耐高压和防水、防油、抗电晕等性能高且结构简单、制造方便、性能可靠的铜包铝纳米云母漆包线。
Description
技术领域
本实用新型涉及一种铜包铝双金属导线,特别是涉及一种铜包铝纳米云母漆包线。
背景技术
目前,人们已经研制出多种复合导线,用以解决铜导线的贵重、铝导线的导电不良以及铜资源日趋匮乏的问题,如铜包钢、铜包铝复合导线。如公告号为“CN 2348466Y”的中国专利公开了一种铜包铝双金属导体,其主要结构是由铝芯和包覆在铝芯上的铜层构成。它用大部份低价格的铝金属替代高价格的铜金属,节约了大量的铜资源,在传递方面,由于导体的集肤效应,性能上则相差很小。但铜包铝双金属导体的缺点是具有绝缘层较厚、不耐高温、不耐高压,防水、防油、抗电晕等性能差。
实用新型内容
本实用新型所要解决的技术问题是提供一种绝缘层薄、绝缘性能强、耐高温、耐高压和防水、防油、抗电晕等性能高的铜包铝纳米云母漆包线。
为了解决上述技术问题,本实用新型采用的技术方案是:在铝芯上的包覆有铜层,在铜层外表面涂覆有一层纳米云母绝缘漆。
采用上述技术方案的铜包铝纳米云母漆包线,由于铜包铝纳米云母漆包线是以铜包铝双金属线作导体,又采用了高科技纳米材料纳米云母绝缘漆作绝缘漆,用作高性能电机、电器绕组线,具有高科技、低成本的新材料特点,它用大部份低价格的铝金属替代高价格的铜金属,节约了大量的铜资源,加之,铜包铝的密度是纯铜的1/2.45,因而可以大幅度减轻线材单位长度的重量,更有利于我国电机、变压器,乃至IT信息产业等客户单位方便使用和降低成本。它采用高科技纳米云母绝缘漆作绝缘材料,具有绝缘层超薄、超强、耐高温、耐高压和防水、防油、抗电晕等高性能优势。
综上所述,本实用新型是一种绝缘层薄、绝缘性能强、耐高温、耐高压和防水、防油、抗电晕等性能高且结构简单、制造方便、性能可靠的铜包铝纳米云母漆包线。
附图说明
附图是本实用新型结构示意图。
具体实施方式
参见附图,在铝芯1上的包覆有铜层2,在铜层2外表面涂覆有一层纳米云母绝缘漆3。
由于导体的“集肤效应”——即:高频电流主要集中在导体的表面层即铜层2传输。虽然铜包铝的直流电阻率相当于铜的1.55倍,但作用于电机、变压器运行中的交流电阻率则趋近于纯铜线。特别是在高频信号传递方面,由于导体的集肤效应,性能上则相差很小。因此,铜包铝纳米云母漆包线不但能实现以铝代铜,降低成本,提高效益之目的;又能够发挥高科技纳米技术和提升产品等级,并促进产品更新换代之优势;本实用新型采用铜包铝双金属作导体线芯,兼具铜的导电性好、强度高和铝的密度小、重量轻等优点;又采用高科技纳米云母绝缘漆3作绝缘材料,具有绝缘层超薄、超强、附着力好和耐高温、耐高压,防水、防油、抗电晕等高品质性能;既可用作高性能电机、电器绕组线,亦可用作高频信号传输方面作编转线圈绕组线。
本实用新型的主要技术指标对比参见下表:
主要技术指标对比
铜包铝线芯的物理和机械性能对照 | 铜包铝纳米云母导线产品性能对照 | ||||
铜包铝与纯铜线 | 铜包铝CopperVolume | 纯铜线Copperwire | 铜包铝纳米云母漆包线企业标准与220聚酰亚胺漆包扁线国家标准对比 | 企业标准Q/BABF003-2005Q/TLNMFC-0.13/250 | 国家标准QB/T7095.5-1995QYB-2/220 |
铜层体积比Copper involume(%) | 13-17 | 100 | 导体尺寸mm | 等同国家标准 | 等同企业标准 |
铜层质量比Copper inmass(%) | 37 | 100 | 漆膜厚度δ.mm | δ=0.13(±15%) | 0.11<δ≤0.16 |
与纯铜线的长度比LengthComparison | 2.45∶1 | 1∶1 | 最大外径mm/max | 等同国家标准 | 等同企业标准 |
密度Density(g/cm3) | 3.63 | 8.89 | 直流电阻Ω/mR20=P20/Smin | P20=1/37.37Ω.mm2/m=0.02676 | |
抗拉强度(Mpa)Elingation | 95-135 | 215-265 | 伸长率% | 圆线≥25扁线≥15 | |
伸长率(%)Elongation | ≥15 | ≥20 | 回弹角 | ≤5° | |
最大直流电阻率Mgx.DCresistivityΩ.mm2/m(20℃) | 0.02676 | 0.017241 | 耐溶剂 | 等同国家标准 | 等同企业标准 |
最小相对导电率MinConductivity(%IACS) | 65 | 100 | 刮漆 | 等同国家标准 | 等同企业标准 |
最大交流电阻率 | 最小击穿电压(室温下V) | 6000V | 2000V | ||
最小相对导电率MinConductivity(%IACS) | 耐温等级 | 250级 | 220级 | ||
注:软化击穿与热冲击只考核漆包圆线,不考核漆包扁线。 |
Claims (1)
- 一种铜包铝纳米云母漆包线,包括铝芯(1)和包覆在铝芯(1)上的铜层(2),其特征是:在所述的铜层(2)外表面涂覆有一层纳米云母绝缘漆(3)。