CN2810793Y - 一种轧钢用堆焊复合导卫板 - Google Patents

一种轧钢用堆焊复合导卫板 Download PDF

Info

Publication number
CN2810793Y
CN2810793Y CN 200520128846 CN200520128846U CN2810793Y CN 2810793 Y CN2810793 Y CN 2810793Y CN 200520128846 CN200520128846 CN 200520128846 CN 200520128846 U CN200520128846 U CN 200520128846U CN 2810793 Y CN2810793 Y CN 2810793Y
Authority
CN
China
Prior art keywords
welding
foreplate
built
working face
steel
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 200520128846
Other languages
English (en)
Inventor
完卫国
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Maanshan Iron and Steel Co Ltd
Original Assignee
Maanshan Iron and Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Maanshan Iron and Steel Co Ltd filed Critical Maanshan Iron and Steel Co Ltd
Priority to CN 200520128846 priority Critical patent/CN2810793Y/zh
Application granted granted Critical
Publication of CN2810793Y publication Critical patent/CN2810793Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

轧钢用堆焊复合导卫板,包括钢基体板,钢基体板工作面堆焊合金层,特点是钢基体板背面堆焊矫正变形堆焊层。工作面堆焊合金层,耐热、耐磨,可以延长导卫板的使用寿命,背面堆焊矫正变形堆焊层,可以矫正钢基体板因堆焊合金时产生的严重变形,尺寸精度高;容易制造,成品率高,可以制造基体板刚度小,工作面堆焊层面积大,厚度大的导卫板。

Description

一种轧钢用堆焊复合导卫板
技术领域
本实用新型涉及一种轧钢用导卫板,尤其是一种堆焊复合导卫板。
背景技术
在轧钢用导卫板的工作面上堆焊耐热、耐磨的合金层能有效地延长导卫板的使用寿命。现用的堆焊复合导卫板由导卫板基体和堆焊合金层两部分构成。中国专利ZL91221901.7公开了一种复合导卫板,它在冲击韧性好的铸钢基体上用高温耐磨焊条堆焊成工作面层,具有良好的耐磨性和抗冲击性。中国专利ZL94206064.4,一种轧机用导卫板,该导卫板由碳钢基体和与钢材接触的合金堆焊层构成。上述的导卫板均为两层焊接而成,堆焊后因熔敷金属凝固时的收缩而产生较大的变形,如一种20mm厚的导卫板,即使在工作面上手工电弧堆焊一层1-2mm厚的堆焊层,也会使其产生严重的变形而不能使用,这种堆焊变形是一般方法难以矫正的。因而要求堆焊复合导卫板的基体刚度好、堆焊层的面积和厚度不宜过大(不利于提高耐磨性)且导卫板的装配精度要求不高。这使堆焊复合导卫板的应用范围和使用效果受到了严重影响。
发明内容
为了克服现有技术存在的缺陷,本实用新型提供的是一种轧钢用堆焊复合导卫板,利用导卫板背面矫正变形堆焊层来矫正工作面堆焊合金时产生的焊接变形,从而保证了导卫板的尺寸精度,解决了堆焊合金时导卫板产生变形问题。
本实用新型的轧钢用堆焊复合导卫板,包括钢基体板、钢基体板工作面堆焊合金层,特点是钢基体板背面堆焊矫正变形堆焊层。工作面上的堆焊合金层,耐热、耐磨,可以延长导卫板的使用寿命。背面堆焊矫正变形堆焊层,可以矫正钢基体板因堆焊合金层时产生的严重变形。
与背景技术相比,导卫板焊接变形小,尺寸精度高;容易制作,提高成品率,可以制造基体板刚度小,工作面堆焊层面积大,堆焊厚度大的导卫板,扩大导卫板的应用范围。
附图说明
下面结合附图对本实用新型作进一步说明。
图1:一种轧钢用堆焊复合导卫板结构示意图。
图2:轧钢用堆焊复合导卫板俯视图。
具体实施方式
由附图可以看出,轧钢用堆焊复合导卫板由钢质基体板1、堆焊在钢质基体板1两侧面的工作面堆焊合金层2和背面矫正变形堆焊层3构成。其实施方式是在专门制造或使用后磨损的导卫板钢基体板1工作面上,用耐热、耐磨电焊条堆焊合金层2。在钢基体板1的背面,用普通的电焊条堆焊矫正变形堆焊层。可以先焊接一面,再焊另一面,也可以两面交替进行堆焊。焊接后,加工掉焊层尺寸余量,即可安装使用。

Claims (1)

1、一种轧钢用堆焊复合导卫板,包括钢基体板(1)、工作面堆焊合金层(2),其特征在于钢基体板(1)背面堆焊矫正变形堆焊层(3)。
CN 200520128846 2005-08-10 2005-10-26 一种轧钢用堆焊复合导卫板 Expired - Fee Related CN2810793Y (zh)