CN2789271Y - 侧出料推钢式加热炉复合结构出钢槽 - Google Patents
侧出料推钢式加热炉复合结构出钢槽 Download PDFInfo
- Publication number
- CN2789271Y CN2789271Y CN 200520017165 CN200520017165U CN2789271Y CN 2789271 Y CN2789271 Y CN 2789271Y CN 200520017165 CN200520017165 CN 200520017165 CN 200520017165 U CN200520017165 U CN 200520017165U CN 2789271 Y CN2789271 Y CN 2789271Y
- Authority
- CN
- China
- Prior art keywords
- plate
- composite structure
- tapping
- cooled plate
- water cooled
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种侧出料推钢式加热炉复合结构出钢槽,它由铸铁水冷板和至少一块铸钢半热板组成,水冷板呈矩形,在水冷板的板体内均布设置着沿水冷板的长度方向延伸的水冷管,半热板安装在水冷板的板面上。不仅使用寿命能得到极大的延长,而且非常易于检修,检修时间短。
Description
技术领域
本实用新型涉及一种钢铁厂侧出料推钢式加热炉用的出钢槽,特别是侧出料推钢式加热炉复合结构出钢槽。
背景技术
目前,对于侧出料推钢式加热炉使用的出钢槽,其结构形式大致可分为两类:一类为水冷或汽化冷却的铸铁出钢槽,水冷铸铁出钢槽使用寿命长,但有对钢坯吸热过多,影响钢坯轧制温度的缺点;另一类是目前使用最广泛的用耐火材料制品砌筑的出钢槽,耐火材料制品主要有电容莫来石砖和浇注料制平台砖等,以年产40万吨轧钢厂加热炉为例,耐火材料砌筑的出钢槽如使用电容莫来石砖,使用寿命只有6-8个月,使用浇注料制平台砖的使用寿命只有10-11个月。在检修时必须使加热炉的炉温从1250℃降至100℃才能进行检修施工,检修后再升温至1250℃。整个检修过程所用时间不少于48小时,施工复杂,施工条件恶劣,检修所用时间太长。
实用新型内容
本实用新型的目的在于提供一种侧出料推钢式加热炉复合结构出钢槽,不仅对钢坯的轧制温度影响小,出钢槽的使用寿命能得到极大的延长,而且非常易于检修,检修时间短。
本实用新型的目的是这样实现的:一种侧出料推钢式加热炉复合结构出钢槽,它由铸铁水冷板和至少一块铸钢半热板组成,水冷板呈矩形,在水冷板的板体内均布设置着沿水冷板的长度方向延伸的水冷管,半热板安装在水冷板的板面上。
本实用新型出钢槽分为上、下两层,下层为铸铁水冷板,在生产时向其水冷管内通入循环冷却水;半热板直接安装在水冷板上,其下表面与水冷板接触传热,使半热板在一定的温度范围内工作,不至于超温损坏,半热板上表面为出钢时与钢坯的直接摩擦面,这样钢坯不与水冷板直接接触,因而对钢坯的轧制温度影响小。本实用新型与传统的由耐火材料砌筑的出钢槽相比,耐磨性能更强,抗冲击、耐剥落性能更好。当半热板磨损严重需要更换时,只需利用热出钢机将半热板推出即可更换。本实用新型复合结构出钢槽与现在应用最广泛的耐火材料砌筑出钢槽相比,使用寿命延长了一倍,而直接建造费用相当。在相同使用条件下对比,如使用耐火材料砌筑出钢槽,检修一次至少停产48小时,检修人员进入加热炉内工作条件艰苦、劳动强度大、费时费力。但采用复合结构出钢槽,检修时不需停炉降温,检修人员全部在炉外操作,施工简单、条件好,一次检修所用时间不超过3个小时,所用时间随时可以穿插在其它停机时间内完成,不影响轧钢厂产量和作业率。
附图说明
下面将结合附图对本实用新型作进一步说明。
图1为本实用新型的俯视结构示意图;
图2为本实用新型的侧视结构示意图。
具体实施方式
一种侧出料推钢式加热炉复合结构出钢槽,如图1、图2所示,它由铸铁水冷板2和至少一块铸钢半热板3组成,水冷板2呈矩形,在水冷板2的板体内均布设置着沿水冷板2的长度方向延伸的水冷管1,水冷管1为厚皮无缝钢管。半热板3安装在水冷板2的板面上,半热板3的宽度和水冷板2的宽度相匹配。铸铁水冷板2为灰口铸铁水冷板(如灰口铁HT150)或耐热铸铁水冷板。为了防止半热板3在工作时发生变形,在半热板3的板体上均布设置着透孔4,透孔4的形状为长圆形、圆形或椭圆形。半热板3的厚度为60-70mm,最好为65mm。半热板的材质为ZGCr30Ni14Nre。本实用新型结构简单,制造容易,使用寿命长,检修维护时间短。
Claims (4)
1、一种侧出料推钢式加热炉复合结构出钢槽,其特征是:它由铸铁水冷板(2)和至少一块铸钢半热板(3)组成,水冷板(2)呈矩形,在水冷板(2)的板体内均布设置着沿水冷板(2)的长度方向延伸的水冷管(1),半热板(3)安装在水冷板(2)的板面上。
2、根据权利要求1所述的侧出料推钢式加热炉复合结构出钢槽,其特征是:铸铁水冷板(2)为灰口铸铁水冷板或耐热铸铁水冷板。
3、根据权利要求1所述的侧出料推钢式加热炉复合结构出钢槽,其特征是:在半热板(3)的板体上均布设置着透孔(4),透孔(4)的形状为长圆形、圆形或椭圆形。
4、根据权利要求1所述的侧出料推钢式加热炉复合结构出钢槽,其特征是:半热板(3)的厚度为60-70mm。