CN2343953Y - Toughened glass chopping board - Google Patents
Toughened glass chopping board Download PDFInfo
- Publication number
- CN2343953Y CN2343953Y CN 98243234 CN98243234U CN2343953Y CN 2343953 Y CN2343953 Y CN 2343953Y CN 98243234 CN98243234 CN 98243234 CN 98243234 U CN98243234 U CN 98243234U CN 2343953 Y CN2343953 Y CN 2343953Y
- Authority
- CN
- China
- Prior art keywords
- safety glass
- toughened glass
- chopping board
- chopping block
- lower floor
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model provides a toughened glass chopping board which is characterized in that the upper layer of the chopping board is provided with a piece toughened glass, the middle layer is provided with an adhesive layer, and the lower layer is provided with a backing board. The utility model has the advantages of sanitary use without leaving food, easy cleaning without damage, long service life, etc.
Description
The utility model relates to improved chopping block, and particularly a kind of safety glass chopping block is suitable for that family cuts the dish, meat cutting uses.
As everyone knows, chopping block is mainly made with solid timber, and its advantage is low price, makes easily, and food is not produced adverse effect.But not enough is that hardness is not high, is easy to generate tool marks, and the food that remains on the chopping block is difficult to remove, and can influence food hygiene by the evil endophytic bacteria.In addition, time one length also can be gone rotten rotten, and service life is not long.Though, there is a kind of chopping block made from nontoxic engineering plastics to come out in recent years, because its hardness is not high enough, there is the problem of Wood chopping block equally.
The purpose of this utility model is to provide a kind of hardness height, is not easy residual food, is easy to cleaning, uses the safety glass chopping block of health and long service life.
Above-mentioned task realizes by this way: the upper strata of this chopping block is a safety glass, and the middle level is an adhesive-layer, and lower floor is a backing plate.
The purpose of this utility model also can take following measure to realize:
Upper surface at upper strata safety glass is provided with ridge design, to increase friction, reduces the slip of food, helps the carrying out of cutting the dish.
The backing plate of lower floor can adopt plastic plate or plastic plate, but preferably adopts polyvinyl chloride (PVC) thin plate with uneven glue, so that directly be close to the bottom surface of safety glass, simplifies manufacture craft.
In the bottom surface of backing plate four colloid supporting plush coppers can be set, make this chopping block can be placed on the table top reposefully and anti-sliding stop.
Safety glass is not that simple glass is made through Quenching Treatment, has very high hardness, and is easy to wear and under normal operating position, is difficult to bump ring and damaged, and in addition, its smooth surface is not stayed residual thing and smell, is not easy the evil endophytic bacteria, easily cleaning.Therefore, the utlity model has the use health, the advantage of not fragile and long service life.
Below in conjunction with accompanying drawing structure of the present utility model is further described.
Fig. 1 is the cutaway view of a kind of concrete structure of the utility model.
As shown in Figure 1, upper strata 1 is to make with safety glass, and the surface is provided with concavo-convex embossing thereon.This safety glass is suitable with 4-6 millimeter thickness, and its decorative pattern can directly be made in glass manufacturing process.The backing plate of the adhesive-layer in middle level 2 and lower floor 3 can directly adopt the polychlorostyrene second combustion (PVC) of band adhesive sticker to make, and is close to the bottom surface on upper strata 1 then.Four colloids are propped up plush copper 4 and can be used silica gel to make, and just can in four angles that are bonded at the lower floor bottom surface with viscose glue.
The utility model is suitable for family to be used.
Claims (4)
1, a kind of safety glass chopping block is characterized in that upper strata (1) is safety glass, and middle level (2) are adhesive-layer, and lower floor (3) is a backing plate.
2, chopping block according to claim 1 is characterized in that the surface of (1) safety glass on the upper strata is provided with ridge design.
3, brill plate according to claim 1, the backing plate that it is characterized in that lower floor (3) are with polyvinyl chloride (PVC) thin plate with uneven glue.
4, brill plate according to claim 1 is characterized in that also being provided with on the bottom surface of lower floor (3) four colloids supporting plush coppers (4).