CN217149013U - Scratch-proof and deformation-proof batten for chemical toughening of glass - Google Patents

Scratch-proof and deformation-proof batten for chemical toughening of glass Download PDF

Info

Publication number
CN217149013U
CN217149013U CN202123394571.2U CN202123394571U CN217149013U CN 217149013 U CN217149013 U CN 217149013U CN 202123394571 U CN202123394571 U CN 202123394571U CN 217149013 U CN217149013 U CN 217149013U
Authority
CN
China
Prior art keywords
glass
bolt
sets
group
limiting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN202123394571.2U
Other languages
Chinese (zh)
Inventor
彭海丰
魏书强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dongguan Longqing Xiangrui Photoelectric Technology Co ltd
Original Assignee
Dongguan Longqing Xiangrui Photoelectric Technology Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dongguan Longqing Xiangrui Photoelectric Technology Co ltd filed Critical Dongguan Longqing Xiangrui Photoelectric Technology Co ltd
Priority to CN202123394571.2U priority Critical patent/CN217149013U/en
Application granted granted Critical
Publication of CN217149013U publication Critical patent/CN217149013U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses a fish tail, deformation layering are prevented to glass chemical tempering, concretely relates to glass protection technical field, including two mounting panels, be equipped with two sets of glass subassemblies between two mounting panels, two sets of glass subassembly intervals set up, and every group glass subassembly top all is equipped with the layering tool, a plurality of locating holes have all been run through and have been seted up to layering tool bottom both sides, and every group glass subassembly all includes a plurality of glass pieces, and even interval sets up between a plurality of glass pieces, the locating hole is corresponding from top to bottom with the position of glass piece, and every group glass subassembly outside all is equipped with first locating component, and every group glass subassembly bottom all is equipped with second locating component. The utility model discloses a align the position of locating hole on the layering tool with the glass piece, make the glass piece at the in-process of chemistry high temperature tempering, can reduce the glass piece and warp, avoid the glass piece to warp the adjacent glass piece of touching fish tail to reach the effect at tempering production process reduction defective rate.

Description

Scratch-proof and deformation-proof batten for chemical toughening of glass
Technical Field
The utility model relates to a glass protection technical field, the more specifically fish tail, deformation layering are prevented in glass chemical tempering that says so.
Background
The strength of glass lenses is generally strengthened by chemical tempering. The chemical tempering process can be generally divided into three stages, firstly, preheating the glass lens, then immersing the glass lens into a high-temperature chemical agent for chemical tempering, and finally cooling the glass lens, wherein the steps are as follows: the glass is put into a chemical tempering furnace filled with potassium nitrate solution, so that the glass substrate is soaked in the potassium nitrate solution, and the Na + ions with lower molecular weight in the glass are replaced by the K + ions with higher molecular weight in the potassium nitrate solution at the high temperature of 400-500 ℃, thereby improving the rigidity of the glass substrate.
The condition that the glass deforms and softens to scratch adjacent glass can occur in the high-temperature tempering process of the existing glass, and further the processing success rate of glass tempering can be influenced, so that scratch and deformation preventing battens for chemical tempering of the glass are needed.
Disclosure of Invention
In order to overcome the above-mentioned defect of prior art, the utility model provides a fish tail, deformation layering are prevented in glass chemical tempering aligns through the position with the locating hole on the layering tool and glass piece, makes glass piece at the in-process of chemical high temperature tempering, can reduce glass piece deformation, avoids glass piece to warp the adjacent glass piece of touching fish tail to reach the effect that reduces the defective rate at tempering production process, with the problem that appears in solving above-mentioned background art.
In order to achieve the above object, the utility model provides a following technical scheme: the utility model provides a fish tail, deformation layering are prevented in glass chemical tempering, includes two mounting panels, is equipped with two sets of glass subassemblies between two mounting panels, and two sets of glass subassemblies interval set up, and every group glass subassembly top all is equipped with the layering tool, layering tool bottom both sides all run through and have seted up a plurality of locating holes, and every group glass subassembly all includes a plurality of glass pieces, and even interval sets up between a plurality of glass pieces, the locating hole is corresponding from top to bottom with the position of glass piece, and every group glass subassembly outside all is equipped with first locating component, and every group glass subassembly bottom all is equipped with second locating component.
In a preferred embodiment, the first positioning assembly comprises two limiting plates, the two limiting plates are arranged on two sides of the glass assembly, one side, close to the glass sheet, of each of the two limiting plates is provided with a plurality of limiting grooves in a penetrating mode, the plurality of limiting grooves correspond to the plurality of glass sheets in the left and right directions respectively, through the arrangement of the plurality of limiting grooves in the two limiting plates, the two sides of the glass sheet can be limited and fixed, and therefore the glass sheet can be prevented from being deformed and scratched.
In a preferred embodiment, the fixed plate that is equipped with in mounting panel top, both ends extend to two fixed plate bottoms respectively around the limiting plate, the limiting plate top is equipped with first bolt, first bolt is located the fixed plate top, first bolt bottom runs through the fixed plate and extends to the limiting plate inside, first bolt and limiting plate are threaded connection, and through the setting of first bolt, be convenient for install fixed to the limiting plate, and then be convenient for fix spacingly through the setting of spacing groove on the limiting plate to the glass piece.
In a preferred embodiment, the second positioning assembly comprises two transverse plates, the two transverse plates are located at the bottom of the glass assembly, a plurality of transverse grooves are formed in the tops of the transverse plates in a penetrating mode, the positions of the plurality of transverse grooves and the positions of the plurality of glass sheets correspond up and down, and the bottoms of the glass sheets can be limited and fixed through the arrangement of the plurality of transverse grooves in the two transverse plates.
In a preferred embodiment, two mounting plate bottom one sides that are close to all are equipped with the L board, both ends extend to two diaphragm tops respectively around the diaphragm, both ends bottom respectively with two diaphragm top fixed connection around the diaphragm, one side that two mounting plates kept away from mutually all is equipped with the second bolt, the second bolt runs through the mounting panel and extends to the L inboard portion, the second bolt is threaded connection with the L board, through the setting of second bolt, is convenient for ann changes fixedly to the L board, and then is convenient for install the diaphragm.
In a preferred embodiment, be equipped with two sets of coupling assembling between two mounting panels, two sets of coupling assembling set up about mounting panel the central axis bilateral symmetry, every group coupling assembling all includes two connecting plates, both ends are close to one side fixed connection mutually with two mounting panels respectively around two connecting plates, the interval sets up about two connecting plates, through the setting of connecting plate, be convenient for connect fixedly to two mounting panels, improve the stability and the support intensity of two mounting panels, and then can be fine support fixedly to the glass piece.
The utility model discloses a technological effect and advantage:
the utility model discloses a align the locating hole on the layering tool with the position of glass piece, make the glass piece at the in-process of chemistry high temperature tempering, can reduce the glass piece and warp, avoid the glass piece to warp the glass piece that touches the fish tail adjacent, and through the setting of a plurality of cross slots on a plurality of spacing grooves and two diaphragms on two limiting plates, can carry out spacing fixed to the both sides and the bottom of glass piece, and then can prevent that the glass piece from warping with the condition of fish tail, thereby reach the effect that reduces the defective rate at tempering production process.
Drawings
FIG. 1 is a front view of the overall structure of the present invention;
fig. 2 is a bottom view of the pressing bar fixture of the present invention;
fig. 3 is a top view of the mounting plate of the present invention;
fig. 4 is a top view of the transverse plate of the present invention;
fig. 5 is a top view of the limiting plate of the present invention.
The reference signs are: 1. mounting a plate; 2. pressing a strip jig; 3. positioning holes; 4. a glass sheet; 5. a limiting plate; 6. a limiting groove; 7. a fixing plate; 8. a first bolt; 9. a transverse plate; 10. a transverse groove; 11. an L plate; 12. a second bolt; 13. a connecting plate.
Detailed Description
The technical solutions in the embodiments of the present invention will be described clearly and completely with reference to the accompanying drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only some embodiments of the present invention, not all embodiments. Based on the embodiments in the present invention, all other embodiments obtained by a person skilled in the art without creative work belong to the protection scope of the present invention.
Referring to the attached drawings 1-5 of the specification, the scratch-proof and deformation-proof bead for chemical tempering of glass comprises two mounting plates 1, two groups of glass assemblies are arranged between the two mounting plates 1 and are arranged at intervals, a bead jig 2 is arranged at the top of each group of glass assemblies, a plurality of positioning holes 3 are formed in the two sides of the bottom end of the bead jig 2 in a penetrating manner, each group of glass assemblies comprises a plurality of glass sheets 4, the glass sheets 4 are arranged at uniform intervals, the positioning holes 3 correspond to the glass sheets 4 in the vertical direction, a first positioning assembly is arranged outside each group of glass assemblies, a second positioning assembly is arranged at the bottom of each group of glass assemblies, each first positioning assembly comprises two limiting plates 5, the two limiting plates 5 are arranged on the two sides of each glass assembly, and a plurality of limiting grooves 6 are formed in the two limiting plates 5 at the side close to the glass sheets 4, the plurality of limiting grooves 6 correspond to the plurality of glass sheets 4 left and right respectively, the two sides of the glass sheets 4 can be limited and fixed through the arrangement of the plurality of limiting grooves 6 on the two limiting plates 5, so that the glass sheets 4 can be prevented from being deformed and scratched, the top of the mounting plate 1 is fixedly provided with a fixing plate 7, the front end and the rear end of each limiting plate 5 respectively extend to the bottoms of the two fixing plates 7, the top of each limiting plate 5 is provided with a first bolt 8, the first bolt 8 is positioned at the top of the fixing plate 7, the bottom end of each first bolt 8 penetrates through the fixing plate 7 and extends into the limiting plate 5, the first bolts 8 and the limiting plates 5 are in threaded connection, the limiting plates 5 can be conveniently installed and fixed through the arrangement of the first bolts 8, so that the glass sheets 4 can be fixed and limited through the arrangement of the limiting grooves 6 on the limiting plates 5, the second positioning assembly comprises two transverse plates 9, two diaphragms 9 are located the glass subassembly bottom, diaphragm 9 top is run through and has been seted up a plurality of cross slots 10, and a plurality of cross slots 10 are corresponding from top to bottom with the position of a plurality of glass pieces 4, and through the setting of a plurality of cross slots 10 on two diaphragms 9, can carry out spacing fixed to the bottom of glass pieces 4, and one side that two mounting panels 1 bottoms are close to mutually all is equipped with L board 11, both ends extend to two diaphragm 9 tops respectively around diaphragm 9, diaphragm 9 around both ends bottom respectively with two diaphragm 9 top fixed connection, one side that two mounting panels 1 kept away from mutually all is equipped with second bolt 12, second bolt 12 runs through mounting panel 1 and extends to inside the L board 11, second bolt 12 is threaded connection with L board 11, through the setting of second bolt 12, is convenient for ann changes fixedly to L board 11, and then is convenient for install diaphragm 9.
The implementation scenario is specifically as follows: through the position alignment with locating hole 3 on the layering tool 2 and glass piece 4, make glass piece 4 at the in-process of chemistry high temperature tempering, can reduce glass piece 4 and warp, avoid glass piece 4 to warp touching the adjacent glass piece 4 of fish tail, and through the setting of a plurality of cross slots 10 on a plurality of spacing grooves 6 and two diaphragm 9 on two limiting plates 5, can carry out spacing fixed to the both sides and the bottom of glass piece 4, and then can prevent the condition of glass piece 4 deformation and fish tail, thereby reach the effect that reduces the defective rate at tempering production process.
Referring to description attached drawings 1 and 3, the chemical tempering of glass of this embodiment prevents fish tail, the deformation layering, be equipped with two sets of coupling assembling between two mounting panels 1, two sets of coupling assembling set up about mounting panel 1 the central axis bilateral symmetry, every group coupling assembling all includes two connecting plates 13, both ends are respectively with one side fixed connection that two mounting panels 1 are close to mutually around two connecting plates 13, two connecting plates 13 are the interval setting from top to bottom, setting through connecting plate 13, be convenient for connect fixedly to two mounting panels 1, improve the stability and the support intensity of two mounting panels 1, and then can be fine support fixedly to glass piece 4.
And finally: the above description is only for the preferred embodiment of the present invention and should not be taken as limiting the invention, and any modifications, equivalent replacements, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims (6)

1. The utility model provides a glass chemical tempering prevents fish tail, deformation layering, includes two mounting panels (1), its characterized in that: be equipped with two sets of glass unit between two mounting panels (1), two sets of glass unit interval sets up, and every group glass unit top all is equipped with layering tool (2), layering tool (2) bottom both sides all run through and have seted up a plurality of locating holes (3), and every group glass unit all includes a plurality of glass pieces (4), and even interval sets up between a plurality of glass pieces (4), locating hole (3) are corresponding from top to bottom with the position of glass piece (4), and every group glass unit outside all is equipped with first locating component, and every group glass unit bottom all is equipped with second locating component.
2. The chemical toughening scratch and deformation resistant bead for glass according to claim 1, characterized in that: the first positioning assembly comprises two limiting plates (5), the two limiting plates (5) are arranged on two sides of the glass assembly, one side, close to the glass sheets (4), of each of the two limiting plates (5) is penetrated through and provided with a plurality of limiting grooves (6), and the plurality of limiting grooves (6) correspond to the plurality of glass sheets (4) in the left-right direction respectively.
3. The chemical toughening scratch and deformation resistant bead for glass according to claim 2, characterized in that: mounting panel (1) top is fixed and is equipped with fixed plate (7), both ends extend to two fixed plate (7) bottoms respectively around limiting plate (5), limiting plate (5) top is equipped with first bolt (8), first bolt (8) are located fixed plate (7) top, first bolt (8) bottom runs through fixed plate (7) and extends to limiting plate (5) inside, first bolt (8) are threaded connection with limiting plate (5).
4. The chemical toughening scratch and deformation resistant bead for glass according to claim 1, characterized in that: the second positioning assembly comprises two transverse plates (9), the two transverse plates (9) are located at the bottom of the glass assembly, a plurality of transverse grooves (10) are formed in the top of the transverse plates (9) in a penetrating mode, and the positions of the plurality of transverse grooves (10) and the positions of the plurality of glass sheets (4) are up-down corresponding.
5. The chemical toughening scratch and deformation resistant bead for glass according to claim 4, wherein: one side that two mounting panel (1) bottom are close to mutually all is equipped with L board (11), both ends extend to two diaphragm (9) tops respectively around diaphragm (9), both ends bottom respectively with two diaphragm (9) top fixed connection around diaphragm (9), one side that two mounting panel (1) kept away from mutually all is equipped with second bolt (12), second bolt (12) run through mounting panel (1) and extend to inside L board (11), second bolt (12) are threaded connection with L board (11).
6. The chemical toughening scratch and deformation resistant bead for glass according to claim 1, characterized in that: be equipped with two sets of coupling assembling between two mounting panels (1), two sets of coupling assembling set up about mounting panel (1) the central axis bilateral symmetry, and every group coupling assembling all includes two connecting plates (13), and both ends are close to one side fixed connection mutually with two mounting panels (1) respectively around two connecting plates (13), and two connecting plates (13) are the interval setting from top to bottom.
CN202123394571.2U 2021-12-31 2021-12-31 Scratch-proof and deformation-proof batten for chemical toughening of glass Active CN217149013U (en)