CN217127327U - Simple and easy wall mounting of display screen is laminated easily and is torn easily structure of peeling off entirely - Google Patents

Simple and easy wall mounting of display screen is laminated easily and is torn easily structure of peeling off entirely Download PDF

Info

Publication number
CN217127327U
CN217127327U CN202220313319.XU CN202220313319U CN217127327U CN 217127327 U CN217127327 U CN 217127327U CN 202220313319 U CN202220313319 U CN 202220313319U CN 217127327 U CN217127327 U CN 217127327U
Authority
CN
China
Prior art keywords
upper wall
liquid medicine
elastomer
medicine layer
eva
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN202220313319.XU
Other languages
Chinese (zh)
Inventor
汤立文
叶宗和
董宇坤
尹志安
莫春鉴
丁武
马晓鑫
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhuhai Huacui Technology Co ltd
Original Assignee
Zhuhai Huacui Technology Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhuhai Huacui Technology Co ltd filed Critical Zhuhai Huacui Technology Co ltd
Priority to CN202220313319.XU priority Critical patent/CN217127327U/en
Application granted granted Critical
Publication of CN217127327U publication Critical patent/CN217127327U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses a simple and easy-to-peel structure for a display screen, which is fully attached to a wall and comprises a wall surface, a wall-attaching liquid medicine layer, an elastomer and a LED screen film; the upper wall liquid medicine layer is divided into an inner upper wall liquid medicine layer and an outer upper wall liquid medicine layer, the inner upper wall liquid medicine layer is coated on the wall surface of the area to be provided with the LED screen film in advance, and the other side of the inner upper wall liquid medicine layer is filled with an elastomer; coating the other side of the elastomer with an outer upper wall medicinal water layer with the same area and size again; the inner side surface of the LED screen film is provided with an EVA (ethylene-vinyl acetate copolymer), an elastomer or a silica gel layer, and the LED screen film is adhered to the outer upper wall liquid medicine layer through the EVA, the elastomer or the silica gel layer on the inner side surface and is bonded into a whole. This practicality utilizes the elastomer can react with last wall liquid medicine, and it is good with glass and EVA adhesion force, and the elastomer matter is soft can be along with the EVA shrink, reduces the EVA and directly attaches the shrinkage stress on glass, reaches the function of simply going up the wall.

Description

Simple and easy wall mounting of display screen is laminated easily and is torn easily structure of peeling off entirely
Technical Field
The utility model relates to a Mini LED shows that touch screen dress pastes technical field, specifically is a simple and easy wall mounting is laminated completely and is easily torn easily and shell structure on display screen.
Background
Laminated glass is a glass widely used in the field of architectural glass, which is also called safety glass. Laminated glass, as the name implies, is a glass consisting of a plurality of layers, except for the glass, which is left as an intermediate layer in the glass, in general there being three types of layers: EVA, PVB and SGP.
Among them, PVB interlayer is an interlayer material that is widely used in current architectural glass and automotive glass. The PVB interlayer has a more complicated storage process and processing mode than EVA and has higher requirements on temperature and humidity. When PVB is processed and laminated, the temperature is required to be controlled between 18 ℃ and 23 ℃, the relative humidity is controlled between 18 percent and 23 percent, the PVB keeps 0.4 percent to 0.6 percent of water content, after the process of preheating, rolling or vacuumizing, an autoclave is used for heat preservation and pressure maintaining, and the temperature of the autoclave is as follows: 120 ℃ and 130 ℃, pressure: 1.0-1.3MPa, time: 30-60 min. A PVB plant requires about 100 million. PVB has good safety, sound insulation, transparency and ultraviolet resistance, but PVB has poor water resistance and is easy to be stripped and shed when being in a humid environment for a long time.
And EVA is known as ethylene-vinyl acetate copolymer. Because of strong water resistance and corrosion resistance, the coating is widely applied to the fields of packaging films, functional greenhouse films, foaming shoe materials, hot melt adhesives, wires and cables, toys and the like. EVA is also used as an interlayer of laminated glass, has high cost performance, and compared with PVB and SGP, EVA has good fluidity and low melting temperature, and can be processed when the temperature reaches about 110 ℃. The whole set of production equipment only needs about 10 ten thousand yuan.
The EVA film has good fluidity, and can be subjected to processes such as wire clamping, wire clamping and the like in the film to manufacture beautiful decorative glass with patterns and decorative patterns. EVA has good water resistance, but has weak ultraviolet resistance, and is easy to yellow and black after being exposed to the sun for a long time, so that the EVA is mainly used for indoor partition.
For the high-performance interlayer material SGP, it is called ionic intermediate film (sentryglassplus). The high performance is embodied as follows: excellent mechanical performance and high strength. Under the same thickness, the bearing capacity of the SGP interlayer is 2 times that of PVB; the bending deflection of the SGP laminated glass is one fourth of that of PVB at the same load and thickness. Tear strength. Under the same thickness, the tearing strength of the PVB laminated film is 5 times that of PVB, and the PVB laminated film can be bonded on glass under the tearing condition, so that the whole glass cannot fall off. High stability and high resistance to moisture. The SGP laminated film is colorless and transparent, is ultraviolet-resistant, is not easy to yellow after being exposed to the sun and rain for a long time, and has the yellowing coefficient less than 1.5, while the PVB laminated film has the yellowing coefficient of 6-12. SGP is therefore a pet for ultrawhite laminated glass. Although the production process of SGP is close to PVB, the terminal price is high.
Aiming at the direct wall-mounting design of PVB developed by the existing company, the wall-mounting and dismounting actions can be easily realized by matching with the wall-mounting liquid medicine developed by the PVB. However, if the wall-mounting material is made of EVA, the EVA is very stable, and thus wall-mounting and dismounting operations cannot be realized by matching with wall-mounting chemicals. The following table one shows the thermal expansion coefficients of Glass (Glass) and plastic materials commonly used for laminated Glass, and the thermal expansion coefficients of Glass (Glass) and Glass (Glass) are higher than those of Epoxy resin (Epoxy) and Acrylic resin (Acrylic); therefore, only the symmetrical hot-pressing and laminating operation can be used, the asymmetrical simple wall mounting operation cannot be realized, and the shrinkage and the warping are easily caused by the cold pasting method in particular.
Watch 1
Material Coefficient of thermal expansion (10) -6 m/mk)
TPU 180
EVA 180
PVB 220
Silicon 590
Glass 5.9
Acrylic 81
Epoxy 45
PET 59
SUMMERY OF THE UTILITY MODEL
An object of the utility model is to provide a simple and easy wall mounting is laminated completely and is easily torn easily and shell structure, show the touch-control screen to flexible transparent miniLED, it can not hurt display screen inside lamp pearl and circuit to have to easily tear the design of easily shelling, can use the EVA of great shrinkage factor and silica gel as the protective layer of lamp pearl crowd, can reduce flexible transparent LED by a wide margin, the film thickness and the volume design of miniLED or micro LED display screen, through the EVA packaging material at glass and flexible transparent LED membrane, can use an elastic colloid as the buffering in the middle of the two, and react with last wall liquid medicine, in order to compensate the shortcoming that EVA can not simply go up the wall, in order to solve the problem that proposes among the above-mentioned background art.
In order to achieve the above purpose, the utility model provides the following technical scheme:
a simple and easy-to-peel structure with a fully-laminated upper wall for a display screen comprises a wall surface, an upper wall liquid medicine layer, an elastic body and an LED screen film; the upper wall liquid medicine layer is divided into an inner upper wall liquid medicine layer and an outer upper wall liquid medicine layer, the inner upper wall liquid medicine layer is coated on the wall surface of the area to be provided with the LED screen film in advance, and the other side of the inner upper wall liquid medicine layer is filled with an elastomer; coating the other side of the elastomer with an outer upper wall medicinal water layer with the same area and size again; the inner side surface of the LED screen film is provided with an EVA (ethylene-vinyl acetate copolymer), an elastomer or a silica gel layer, and the LED screen film is adhered to the outer upper wall medical water layer through the EVA, the elastomer or the silica gel layer on the inner side surface and is bonded into a whole.
Further, the elastomer is a soft encapsulating member made of TPU or PVB.
Furthermore, the elastic body is arranged between the inner upper wall liquid medicine layer and the outer upper wall liquid medicine layer and is bonded with the inner upper wall liquid medicine layer and the outer upper wall liquid medicine layer into a whole after the curing time.
Furthermore, the LED screen film is attached to the wall surface after the elastomer is bonded with the upper wall liquid medicine layer.
Compared with the prior art, this practical beneficial effect is:
1. the utility model provides a pair of display screen is simply gone up wall and is laminated completely and easily torn easily and shell structure uses an elastic colloid as the buffering in the middle of the EVA packaging material of glass and flexible transparent LED membrane, and it utilizes the elastomer can react with last wall liquid medicine, and is good with glass and EVA adhesion force, and the elastomer matter is soft can be along with the EVA shrink in addition, reduces the shrinkage stress of EVA direct attach on glass, reaches the function of simply going up the wall, in order to compensate the shortcoming that EVA can not simply go up the wall.
2. The utility model provides a pair of simple and easy laminating of going up wall of display screen is easily torn and is easily shelled structure, to flexible transparent Mini LED display touch screen, it has easily to tear and easily shells the design and can not hurt display screen inside lamp pearl and circuit, still can use EVA and the silica gel of great shrinkage factor as the protective layer of lamp pearl crowd, can reduce flexible transparent LED by a wide margin, film thickness and volume design between Mini LED or the Micro LED display screen, and combine transparent substrate can possess flexibility and transparent advantage simultaneously.
Drawings
FIG. 1 is a construction state diagram of the upper wall liquid medicine layer of the utility model;
FIG. 2 is a view showing a single-side construction of the elastic body of the present invention;
FIG. 3 is a view showing a double-sided construction of the elastic body according to the present invention;
FIG. 4 is a diagram of the construction state of the LED screen film of the present application;
fig. 5 is a final structure construction drawing of the present invention.
In the figure: 1. a wall surface; 2. putting on a wall liquid medicine layer; 3. an elastomer; 4. an LED screen film; 5. EVA, elastomer, or silicone layers.
Detailed Description
The technical solutions in the embodiments of the present invention will be described clearly and completely with reference to the accompanying drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only some embodiments of the present invention, not all embodiments. All other embodiments obtained by persons skilled in the art based on the embodiments in the present application without any creative work belong to the protection scope of the present application.
Referring to fig. 4-5, in an embodiment of the present invention, a simple, fully-attached, easy-to-tear and easy-to-peel structure for a display screen includes a wall surface 1, an upper wall liquid medicine layer 2, an elastic body 3, and an LED screen film 4; the upper wall liquid medicine layer 2 is divided into an inner upper wall liquid medicine layer and an outer upper wall liquid medicine layer, the inner upper wall liquid medicine layer is coated on the wall surface 1 of the area to be provided with the LED screen film 4 in advance, and the other side of the inner upper wall liquid medicine layer is filled with the elastomer 3; coating the other side of the elastomer 3 with an outer upper wall medicinal water layer with the same area; the inner side surface of the LED screen film 4 is provided with an EVA (ethylene vinyl acetate), elastomer or silica gel layer 5, the LED screen film 4 is adhered to the outer upper wall liquid medicine layer through the EVA, elastomer or silica gel layer 5 on the inner side surface and is adhered to the wall surface 1, and the LED screen film 4 is adhered to the upper wall liquid medicine layer 2 through the elastomer 3.
In the embodiment of the present invention, the elastomer 3 is a soft packaging component composed of TPU or PVB, the elastomer 3 is disposed between the inner upper wall liquid medicine layer and the outer upper wall liquid medicine layer, and is bonded with the inner upper wall liquid medicine layer and the outer upper wall liquid medicine layer into a whole after the curing time, after it utilizes the elastomer 3 to react with the upper wall liquid medicine, it is good with glass and EVA adhesion force, and the elastomer 3 is soft and can shrink along with the EVA, the elastomer or the silica gel layer 5, so as to reduce the shrinkage stress of the EVA, the elastomer or the silica gel layer 5 directly attached to the glass, and achieve the simple function of upper wall.
Referring to fig. 1-5, for better explanation of the present invention, a design principle of a simple display screen fully-adhered to a wall and easily torn and peeled structure is provided: firstly, coating a wall surface 1 of a wall with a wall-coating liquid medicine, wherein the wall-coating liquid medicine forms an inner wall-coating liquid medicine layer on the wall surface 1; then the elastomer 3 is pasted on the inner upper wall liquid medicine layer, and the other side of the elastomer 3 is coated with the upper wall liquid medicine again to form an outer upper wall liquid medicine layer; then sticking the EVA or silica gel layer 5 on the LED screen film 4 on the outer upper wall medicinal water layer; and finally, after the inner and outer upper wall liquid medicine layers are solidified, the simple wall mounting operation of the LED screen film 4 can be completed.
In summary, the following steps: the utility model provides a simple upper wall full-lamination easy-tearing and easy-peeling structure of a display screen, an elastic colloid is used as a buffer between the glass and the EVA packaging material of a flexible transparent LED film, it utilizes the fact that the elastic body 3 can react with the liquid medicine on the wall, the adhesion force with the glass and the EVA is good, and the elastic body 3 is soft and can shrink along with the EVA, so as to reduce the shrinkage stress of the EVA directly adhered to the glass, thereby achieving the function of simply mounting the wall, so as to make up the defect that EVA cannot be simply put on the wall, especially aiming at the flexible transparent Mini LED display touch screen, the design of easy tearing and peeling can not damage the lamp beads and circuits in the display screen, and EVA and silica gel with larger shrinkage rate can be used as the protective layer of the lamp bead group, the thickness and the volume design of the film between flexible transparent LED, Mini LED or Micro LED display screens can be greatly reduced, and the combination of the transparent base material can simultaneously have the advantages of flexibility and transparency.
The above description is only for the preferred embodiment of the present invention, but the scope of the present invention is not limited thereto, and any person skilled in the art should be covered by the scope of the present invention by the technical solutions and the practical concepts equivalent to or modified from the technical solutions and the practical concepts of the present invention.

Claims (4)

1. A simple and easy-to-tear and easy-to-peel structure for a display screen, which is fully attached to an upper wall, is characterized by comprising a wall surface (1), an upper wall liquid medicine layer (2), an elastic body (3) and an LED screen film (4); the upper wall liquid medicine layer (2) is divided into an inner upper wall liquid medicine layer and an outer upper wall liquid medicine layer, the inner upper wall liquid medicine layer is coated on the wall surface (1) of the area to be provided with the LED screen film (4) in advance, and the other side of the inner upper wall liquid medicine layer is filled with the elastomer (3); the other side of the elastomer (3) is coated with an outer upper wall medicinal water layer with the same area; the inner side surface of the LED screen membrane (4) is provided with an EVA (ethylene vinyl acetate), elastomer or silica gel layer (5), and the LED screen membrane (4) is attached to the outer upper wall water layer through the EVA, elastomer or silica gel layer (5) on the inner side surface and is bonded into a whole.
2. The simple and easy-to-tear and easy-to-peel structure for the display screen on the upper wall is characterized in that: the elastomer (3) is a soft packaging component made of TPU or PVB.
3. The simple and easy-to-tear and easy-to-peel structure for the display screen on the upper wall is characterized in that: the elastomer (3) is arranged between the inner upper wall liquid medicine layer and the outer upper wall liquid medicine layer and is bonded with the inner upper wall liquid medicine layer and the outer upper wall liquid medicine layer into a whole after curing time.
4. The simple and easy-to-tear and easy-to-peel structure for the display screen on the upper wall is characterized in that: the LED screen film (4) is adhered to the wall surface (1) after the elastomer (3) is adhered to the upper wall liquid medicine layer (2).
CN202220313319.XU 2022-02-16 2022-02-16 Simple and easy wall mounting of display screen is laminated easily and is torn easily structure of peeling off entirely Active CN217127327U (en)