CN216832703U - Phenolic aldehyde regeneration bakelite regeneration board - Google Patents
Phenolic aldehyde regeneration bakelite regeneration board Download PDFInfo
- Publication number
- CN216832703U CN216832703U CN202220057529.7U CN202220057529U CN216832703U CN 216832703 U CN216832703 U CN 216832703U CN 202220057529 U CN202220057529 U CN 202220057529U CN 216832703 U CN216832703 U CN 216832703U
- Authority
- CN
- China
- Prior art keywords
- regeneration
- board body
- inner chamber
- regeneration board
- regenerated
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model discloses a phenolic aldehyde regeneration bakelite regeneration board, including the regeneration board body, the inner chamber has been seted up on the surface of regeneration board body, the inside of inner chamber is provided with the strengthening layer, the top and the bottom of strengthening layer all are provided with the buffer layer that is located the inner chamber inside, one side and the surface contact of inner chamber that the strengthening layer was kept away from to the buffer layer, the top and the bottom of regeneration board body all are provided with the inoxidizing coating, the strengthening layer is including setting up the backup pad in the inner chamber inside. The utility model discloses a set up the inner chamber in the inside of regeneration board body, can reduce the whole manufacturing cost of regeneration board body, reduce material consumption, the strengthening layer can improve the bulk strength of regeneration board body, can support the inner chamber, avoid regeneration board body because of the too high fracture of bearing to appear, solved current phenolic aldehyde regeneration board structure and function comparatively single, bulk strength is relatively poor with the protecting effect, can't satisfy the problem of the user demand of the too high environment of part bearing.
Description
Technical Field
The utility model relates to a regeneration board technical field specifically is a phenolic aldehyde regeneration bakelite regeneration board.
Background
The phenolic aldehyde regeneration board has the characteristics of insulation, no static electricity generation, wear resistance, high temperature resistance and the like, becomes an insulation switch and a variable resistor of an electronic product, a mold for machinery and a jig on a production line, can be used in transformer oil and other products, but the existing phenolic aldehyde regeneration board has single structure and function, is poor in overall strength and protection effect, and cannot meet the use requirement of part of over-high bearing environments.
SUMMERY OF THE UTILITY MODEL
For solving the problem that provides in the above-mentioned background art, the utility model aims to provide a phenolic aldehyde regeneration bakelite regeneration board possesses the advantage of function pluralism, has solved current phenolic aldehyde regeneration board structure and function comparatively single, and bulk strength is relatively poor with the protecting effect, can't satisfy the problem of the user demand of the too high environment of part bearing.
In order to achieve the above object, the utility model provides a following technical scheme: a phenolic aldehyde regeneration bakelite regeneration board comprises a regeneration board body;
the inner chamber has been seted up on the surface of regeneration board body, the inside of inner chamber is provided with the strengthening layer, the top and the bottom of strengthening layer all are provided with the buffer layer that is located the inner chamber inside, the buffer layer is kept away from the one side of strengthening layer and the surface contact of inner chamber, the top and the bottom of regeneration board body all are provided with the inoxidizing coating.
As the utility model discloses it is preferred, the strengthening layer is including setting up the backup pad in inner chamber inside, the inboard fixedly connected with strengthening rib of backup pad, the quantity of strengthening rib is a plurality of and even interval arrangement.
As the utility model discloses it is preferred, the buffer layer includes the cushion of fixed connection in the backup pad outside, the outside fixedly connected with damping plate of cushion, one side of cushion and the inner wall fixed connection of inner chamber are kept away from to the damping plate.
As the utility model discloses preferred, the inoxidizing coating includes the resistant membrane of waiting of fixed connection in the regeneration board body outside, the corrosion-resistant membrane of outside fixedly connected with of resistant membrane of waiting.
As the utility model discloses it is preferred, the left side of regeneration board body is seted up flutedly, the right side of regeneration board body is provided with the arch, protruding and recess can peg graft each other.
As the utility model discloses it is preferred, the front of regeneration board body and the equal fixedly connected with closing plate in the back, the closing plate is the same with the material of regeneration board body, the top and the bottom of closing plate all with the inboard fixed connection who waits to wait the membrane.
Compared with the prior art, the beneficial effects of the utility model are as follows:
1. the utility model discloses a set up the inner chamber in the inside of regeneration board body, can reduce the whole manufacturing cost of regeneration board body, reduce material consumption, the strengthening layer can improve the bulk strength of regeneration board body, can support the inner chamber, avoid regeneration board body because of the too high fracture of bearing to appear, solved current phenolic aldehyde regeneration board structure and function comparatively single, bulk strength is relatively poor with the protecting effect, can't satisfy the problem of the user demand of the too high environment of part bearing.
2. The utility model discloses a set up backup pad and strengthening rib, can improve the bulk strength of regeneration board body, can be simultaneously vertical and horizontal synchronous support of carrying on of regeneration board body.
3. The utility model discloses a set up cushion and damping plate, can weaken outside vibrations, can effectively be connected strengthening layer and regeneration board body.
4. The utility model discloses a set up and wait membrane and corrosion-resistant membrane, can carry out the separation with external environment and regeneration board body, can reduce the injury that the environmental corrosion caused to regeneration board body.
5. The utility model discloses a set up recess and arch, can the person of facilitating the use peg graft the regeneration board body, improve the connection stability of regeneration board body.
6. The utility model discloses a set up the closing plate, can seal the inner chamber, avoid corrosive gas or liquid to get into the inside of inner chamber.
Drawings
FIG. 1 is a schematic structural view of the present invention;
FIG. 2 is a schematic view of the structure of the present invention
Fig. 3 is a schematic view of the local structure of the present invention.
In the figure: 1. a regeneration board body; 2. an inner cavity; 3. a strengthening layer; 4. a buffer layer; 5. a protective layer; 6. a support plate; 7. reinforcing ribs; 8. a rubber pad; 9. a damping plate; 10. a weatherable film; 11. a corrosion resistant film; 12. a groove; 13. a protrusion; 14. and (7) sealing the plate.
Detailed Description
The technical solutions in the embodiments of the present invention will be described clearly and completely with reference to the accompanying drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only some embodiments of the present invention, not all embodiments. Based on the embodiments in the present invention, all other embodiments obtained by a person skilled in the art without creative work belong to the protection scope of the present invention.
As shown in fig. 1 to 3, the utility model provides a phenolic aldehyde regeneration bakelite regeneration board, which comprises a regeneration board body 1;
Referring to fig. 2, the reinforcing layer 3 includes a supporting plate 6 disposed inside the inner cavity 2, reinforcing ribs 7 are fixedly connected to the inner side of the supporting plate 6, and the number of the reinforcing ribs 7 is several and are uniformly arranged at intervals.
As the utility model discloses a technical optimization scheme through setting up backup pad 6 and strengthening rib 7, can improve regeneration board body 1's bulk strength, can be simultaneously to regeneration board body 1 vertically with transversely carry out synchronous stay.
Referring to fig. 3, the buffer layer 4 includes a rubber mat 8 fixedly connected to the outer side of the supporting plate 6, a damping plate 9 is fixedly connected to the outer side of the rubber mat 8, and one side of the damping plate 9 away from the rubber mat 8 is fixedly connected to the inner wall of the inner cavity 2.
As a technical optimization scheme of the utility model, through setting up cushion 8 and damping plate 9, can weaken the outside vibrations, can effectively be connected strengthening layer 3 and regeneration board body 1.
Referring to fig. 3, the protective layer 5 includes a weather-resistant film 10 fixedly attached to the outer side of the regenerated board body 1, and a corrosion-resistant film 11 fixedly attached to the outer side of the weather-resistant film 10.
As the utility model discloses a technical optimization scheme is through setting up resistant time membrane 10 and corrosion-resistant membrane 11, can carry out the separation with external environment and regeneration board body 1, can reduce the injury that environmental corrosion caused regeneration board body 1.
Referring to fig. 1, a groove 12 is formed in the left side of the regeneration board body 1, a protrusion 13 is formed in the right side of the regeneration board body 1, and the protrusion 13 and the groove 12 can be inserted into each other.
As a technical optimization scheme of the utility model, through setting up recess 12 and arch 13, can the person of facilitating the use peg graft regeneration board body 1, improve regeneration board body 1's connection stability.
Referring to fig. 1, the front and back surfaces of the regeneration board body 1 are fixedly connected with a sealing plate 14, the material of the sealing plate 14 is the same as that of the regeneration board body 1, and the top and bottom of the sealing plate 14 are fixedly connected with the inner side of the weather-resistant film 10.
As a technical optimization scheme of the utility model, through setting up closing plate 14, can seal inner chamber 2, avoid corrosive gas or liquid to get into the inside of inner chamber 2.
The utility model discloses a theory of operation and use flow: during the use, the whole manufacturing cost of regeneration board body 1 can be reduced to the inside inner chamber 2 of regeneration board body 1, reduce material consumption, strengthening layer 3 can improve regeneration board body 1's bulk strength, can support inner chamber 2, avoid regeneration board body 1 to appear the fracture because of the bearing is too high, buffer layer 4 can weaken the extrusion and to its influence that causes, can play the effect of buffering to outside vibrations and pressure, inoxidizing coating 5 can improve regeneration board body 1's protecting effect, reduce the injury that external corrosion and friction caused regeneration board body 1.
In summary, the following steps: this phenolic aldehyde regeneration bakelite regeneration board, inside through at regeneration board body 1 sets up inner chamber 2, can reduce regeneration board body 1's whole manufacturing cost, reduce material consumption, strengthening layer 3 can improve regeneration board body 1's bulk strength, can support inner chamber 2, avoid regeneration board body 1 to appear the fracture because of the bearing is too high, it is comparatively single with the function to have solved current phenolic aldehyde regeneration board structure, bulk strength is relatively poor with the protecting effect, can't satisfy the problem of the user demand of the too high environment of part bearing.
It is noted that, herein, relational terms such as first and second, and the like may be used solely to distinguish one entity or action from another entity or action without necessarily requiring or implying any actual such relationship or order between such entities or actions. Also, the terms "comprises," "comprising," or any other variation thereof, are intended to cover a non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements does not include only those elements but may include other elements not expressly listed or inherent to such process, method, article, or apparatus.
Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that changes, modifications, substitutions and alterations can be made in these embodiments without departing from the principles and spirit of the invention, the scope of which is defined in the appended claims and their equivalents.
Claims (6)
1. A phenolic aldehyde regeneration bakelite regeneration board comprises a regeneration board body (1);
the method is characterized in that: inner chamber (2) have been seted up on the surface of regeneration board body (1), the inside of inner chamber (2) is provided with strengthening layer (3), the top and the bottom of strengthening layer (3) all are provided with buffer layer (4) that are located inner chamber (2) inside, one side that strengthening layer (3) were kept away from in buffer layer (4) and the surface contact of inner chamber (2), the top and the bottom of regeneration board body (1) all are provided with inoxidizing coating (5).
2. The phenolic regenerated bakelite regenerated board according to claim 1, characterized in that: the reinforcing layer (3) comprises a supporting plate (6) arranged in the inner cavity (2), reinforcing ribs (7) are fixedly connected to the inner side of the supporting plate (6), and the reinforcing ribs (7) are arranged in a plurality of uniform intervals.
3. The phenolic regenerated bakelite regenerated board according to claim 2, characterized in that: buffer layer (4) are including rubber mat (8) of fixed connection in backup pad (6) outside, the outside fixedly connected with damping plate (9) of rubber mat (8), the inner wall fixed connection of one side and inner chamber (2) of rubber mat (8) is kept away from in damping plate (9).
4. The phenolic regenerated bakelite regenerated board according to claim 1, characterized in that: the protective layer (5) comprises a weather-resistant film (10) fixedly connected to the outer side of the regeneration board body (1), and a corrosion-resistant film (11) is fixedly connected to the outer side of the weather-resistant film (10).
5. The phenolic regenerated bakelite regenerated board according to claim 1, characterized in that: the regeneration board is characterized in that a groove (12) is formed in the left side of the regeneration board body (1), a protrusion (13) is arranged on the right side of the regeneration board body (1), and the protrusion (13) and the groove (12) can be mutually inserted.
6. The phenolic regenerated bakelite regenerated board according to claim 4, characterized in that: the front surface and the back surface of the regeneration plate body (1) are fixedly connected with sealing plates (14), the sealing plates (14) are made of the same material as the regeneration plate body (1), and the top and the bottom of the sealing plates (14) are fixedly connected with the inner side of the weather-resistant film (10).