CN216239521U - Antibacterial plastic floor - Google Patents

Antibacterial plastic floor Download PDF

Info

Publication number
CN216239521U
CN216239521U CN202023327670.4U CN202023327670U CN216239521U CN 216239521 U CN216239521 U CN 216239521U CN 202023327670 U CN202023327670 U CN 202023327670U CN 216239521 U CN216239521 U CN 216239521U
Authority
CN
China
Prior art keywords
layer
antibacterial
wpc
base material
plastic floor
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN202023327670.4U
Other languages
Chinese (zh)
Inventor
戴会斌
章忠飞
王涛
董利杰
李猛飞
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Jingtong New Material Group Co ltd
Original Assignee
Zhejiang Jingtong New Material Group Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhejiang Jingtong New Material Group Co ltd filed Critical Zhejiang Jingtong New Material Group Co ltd
Priority to CN202023327670.4U priority Critical patent/CN216239521U/en
Application granted granted Critical
Publication of CN216239521U publication Critical patent/CN216239521U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses an antibacterial plastic floor, which comprises: a WPC substrate layer; the upper surface of WPC substrate layer still is equipped with: the first antibacterial layer is used for enabling the WPC base material layer to have an antibacterial function, the first adhesive layer is used for fixing the first antibacterial layer, the second antibacterial layer is used for enabling the WPC base material layer to have the antibacterial function, and the second adhesive layer is used for fixing the second antibacterial layer; the first antibacterial layer, the first adhesive layer, the second antibacterial layer and the second adhesive layer are arranged at one time from top to bottom; the first antibacterial layer is firmly adhered to the upper surface of the second antibacterial layer through the first adhesive layer; the second antibacterial layer is firmly adhered to the upper surface of the WPC base material layer through a second adhesive layer; the upper surface of the first antibacterial layer is also provided with a protective layer for protecting the first antibacterial layer; the protective layer is uniformly distributed on the surface layer of the first antibacterial layer. The antibacterial plastic floor has good antibacterial capability and long service life in the long-time use process.

Description

Antibacterial plastic floor
Technical Field
The utility model relates to an antibacterial plastic floor.
Background
Traditional plastic floor, such as LVT floor, SPC floor, WPC floor etc. do not have very good antibacterial ability, only decorate a layer of antibiotic drench membrane oil as the protective layer on its surface. The thickness of the antibacterial laminating oil of the floor is only about 0.02mm, and the wear resistance is insufficient, so that the floor loses the antibacterial effect shortly after being used.
SUMMERY OF THE UTILITY MODEL
The utility model provides an antibacterial plastic floor, which adopts the following technical scheme:
an antimicrobial plastic floor comprising: a WPC substrate layer; the upper surface of WPC substrate layer still is equipped with: the first antibacterial layer is used for enabling the WPC base material layer to have an antibacterial function, the first adhesive layer is used for fixing the first antibacterial layer, the second antibacterial layer is used for enabling the WPC base material layer to have the antibacterial function, and the second adhesive layer is used for fixing the second antibacterial layer; the first antibacterial layer, the first adhesive layer, the second antibacterial layer and the second adhesive layer are arranged at one time from top to bottom; the first antibacterial layer is firmly adhered to the upper surface of the second antibacterial layer through the first adhesive layer; the second antibacterial layer is firmly adhered to the upper surface of the WPC base material layer through a second adhesive layer; the upper surface of the first antibacterial layer is also provided with a protective layer for protecting the first antibacterial layer; the protective layer is uniformly distributed on the surface layer of the first antibacterial layer.
Further, the first antibacterial layer is an antibacterial laminating oil layer containing an antibacterial agent.
Furthermore, the thickness value range of the antibacterial drenching film oil layer is more than or equal to 0.05mm and less than or equal to 0.6 mm.
Further, the second antibacterial layer is an abrasion-resistant layer containing an antibacterial agent and capable of improving the scratch resistance of the floor.
Further, the thickness value range of the wear-resistant layer is greater than or equal to 0.08mm and less than or equal to 0.8 mm.
The antibacterial plastic floor has the beneficial effects that the first antibacterial layer and the second antibacterial layer are combined, so that the antibacterial capability of the floor can be effectively improved, the antibacterial time of the floor can be effectively prolonged, the floor has good antibacterial capability in the long-time use process, and the service life is long. Meanwhile, the first antibacterial layer and the second antibacterial layer are fixed through the first adhesive layer and the second adhesive layer respectively, and the structure is more stable.
Drawings
FIG. 1 is a schematic view of an antibacterial plastic floor according to the present invention;
FIG. 2 is a partially enlarged view of the antibacterial plastic floor in FIG. 1;
the plastic floor comprises an antibacterial plastic floor 10, a WPC base material layer 11, a first antibacterial layer 12, a first adhesive layer 13, a second antibacterial layer 14, a second adhesive layer 15 and a protective layer 16.
Detailed Description
The utility model is described in detail below with reference to the figures and the embodiments.
As shown in fig. 1 to 2, an antibacterial plastic floor 10 of the present invention includes: WPC substrate layer 11. The upper surface of WPC substrate layer 11 still is equipped with: a first antibacterial layer 12, a first adhesive layer 13, a second antibacterial layer 14 and a second adhesive layer 15. The first antibacterial layer 12 is used to provide the WPC base material layer 11 with an antibacterial function. The first adhesive layer 13 is used to fix the first antibacterial layer 12. The second antibacterial layer 14 is used to further improve the antibacterial function of the WPC base material layer 11. The second adhesive layer 15 is used to fix the second antibacterial layer 14. The first antibacterial layer 12, the first adhesive layer 13, the second antibacterial layer 14 and the second adhesive layer 15 are arranged at a time in a direction from top to bottom. The first antibiotic layer 12 is firmly adhered to the upper surface of the second antibiotic layer 14 by the first adhesive layer 13. The second antibacterial layer 14 is firmly adhered to the upper surface of the WPC base material layer 11 by the second adhesive layer 15. The upper surface of the first antibacterial layer 12 is also provided with a protective layer 16. The protective layer 16 serves to protect the first antibiotic layer 12. The protective layer 16 is uniformly distributed on the surface layer of the first antibacterial layer 12. The protective layer 16 may be a wax layer having a waterproof function.
Specifically, the antibacterial plastic floor 10 combines the first antibacterial layer 12 and the second antibacterial layer 14, so that the antibacterial ability of the floor can be effectively improved, and the antibacterial time of the floor can be effectively prolonged, so that the floor has good antibacterial ability and long service life in a long-time use process. Meanwhile, the first antibacterial layer 12 and the second antibacterial layer 14 are fixed through the first adhesive layer 13 and the second adhesive layer 15 respectively, so that the structure is more stable.
In a specific embodiment, the first antibacterial layer 12 is an antibacterial oil-coated layer containing an antibacterial agent. The antibacterial drenching film oil layer is directly sprayed, and the processing technology is simple.
In a specific embodiment, the thickness of the antibacterial laminated oil layer ranges from 0.05mm or more to 0.6mm or less. The thickness value of the antibacterial drenching film oil layer is set in such a way that the antibacterial performance of the antibacterial drenching film oil layer can be guaranteed.
As a specific embodiment, the second antibacterial layer 14 is an abrasion resistant layer containing an antibacterial agent capable of improving scratch resistance of the floor. The wear-resistant layer improves the antibacterial property and the wear resistance of the floor.
In a specific embodiment, the wear resistant layer has a thickness value ranging from 0.08mm or more to 0.8mm or less. The thickness value of the wear-resistant layer is set, so that the floor can be guaranteed to have enough wear resistance while the antibacterial property is guaranteed.
The foregoing illustrates and describes the principles, general features, and advantages of the present invention. It should be understood by those skilled in the art that the above embodiments do not limit the present invention in any way, and all technical solutions obtained by using equivalent alternatives or equivalent variations fall within the scope of the present invention.

Claims (5)

1. An antimicrobial plastic floor comprising: a WPC substrate layer; the WPC base material layer is characterized in that the upper surface of the WPC base material layer is further provided with: the first antibacterial layer is used for enabling the WPC base material layer to have an antibacterial function, the first adhesive layer is used for fixing the first antibacterial layer, the second antibacterial layer is used for enabling the WPC base material layer to have an antibacterial function, and the second adhesive layer is used for fixing the second antibacterial layer; the first antibacterial layer, the first adhesive layer, the second antibacterial layer and the second adhesive layer are arranged at one time along the direction from top to bottom; the first antibacterial layer is firmly adhered to the upper surface of the second antibacterial layer through the first adhesive layer; the second antibacterial layer is firmly adhered to the upper surface of the WPC base material layer through the second adhesive layer; the upper surface of the first antibacterial layer is also provided with a protective layer for protecting the first antibacterial layer; the protective layer is uniformly distributed on the surface layer of the first antibacterial layer.
2. The antibacterial plastic floor according to claim 1,
the first antibacterial layer is an antibacterial drenching film oil layer.
3. The antimicrobial plastic floor according to claim 2,
the thickness value range of the antibacterial laminating oil layer is more than or equal to 0.05mm and less than or equal to 0.6 mm.
4. The antibacterial plastic floor according to claim 1,
the second antibacterial layer is a wear-resistant layer capable of improving the scratch resistance of the floor.
5. The antibacterial plastic floor according to claim 4,
the thickness value range of the wear-resistant layer is more than or equal to 0.08mm and less than or equal to 0.8 mm.
CN202023327670.4U 2020-12-31 2020-12-31 Antibacterial plastic floor Active CN216239521U (en)