CN214089287U - Self-luminous pavement structure manufactured based on cold-mixed asphalt process - Google Patents
Self-luminous pavement structure manufactured based on cold-mixed asphalt process Download PDFInfo
- Publication number
- CN214089287U CN214089287U CN202022432227.7U CN202022432227U CN214089287U CN 214089287 U CN214089287 U CN 214089287U CN 202022432227 U CN202022432227 U CN 202022432227U CN 214089287 U CN214089287 U CN 214089287U
- Authority
- CN
- China
- Prior art keywords
- luminous
- layer
- cold
- self
- plain soil
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model discloses a self-luminous road surface structure based on pitch technology is made to cold mix, mix pitch and luminous particle surface course, concrete cushion, rubble bed course and plain soil tamp layer including colored cold mix, colored cold mix pitch and luminous particle surface course coating are in the top layer at concrete cushion surface course, the concrete cushion lay rubble bed course top, the rubble bed course is laid on the plain soil tamp layer, the plain soil tamp layer is located the bottom for the plane of playing basic support. The utility model discloses can reduce the use of main equipment, reduce the fuel consume, the work progress is simpler, material utilization is higher.
Description
Technical Field
The utility model relates to a road construction technical field, concretely relates to self-luminous pavement structure based on pitch technology is made to cold mixing.
Background
In recent years, with the continuous development of urban road traffic, the requirements of people on safety warning, landscape humanistic characteristics and the like of the road surface are continuously improved, so that the research on the special road surface paving material is increasingly deep; the requirements of environmental protection and tourism are considered, and the self-luminous road is introduced into the construction engineering of modern road construction. Asphalt is mostly adopted as a pavement material for highway pavements, but because the asphalt is a thermoplastic material, the asphalt pavement material is usually subjected to a hot mixing mode in the construction process, but the hot mixing mode is complex in construction process, large-scale equipment is required, a large amount of fuel is consumed, the construction process is influenced by weather, the process matching requirement is strict, the material utilization rate is low, and the waste is serious, so that the research on the self-luminous road manufactured based on the cold-mix asphalt process is particularly important.
SUMMERY OF THE UTILITY MODEL
The utility model discloses a solve the problem that proposes in the above-mentioned technical background, provide a self-luminous road surface structure based on pitch technology is made to cold mixing, reduce the use of main equipment, reduce the fuel consume, the work progress is simpler, material utilization is higher.
The utility model adopts the following technical scheme:
a self-luminous pavement structure manufactured based on a cold-mixed asphalt process comprises a colorful cold-mixed asphalt and luminous particle surface layer, a concrete cushion layer, a gravel cushion layer and a plain soil ramming stone layer, the colorful cold-mixed asphalt and the luminous particle surface layer are coated on the surface of the concrete cushion layer and are positioned on the outermost layer, the concrete cushion is paved above the gravel cushion, the gravel cushion is paved on the plain soil rammed rock layer, the plain soil rammed stone layer is a plane for supporting a foundation and is positioned at the bottommost layer, the thickness of the colorful cold-mixed asphalt and luminous particle surface layer is 30MM, acrylic light-storing luminous stones are added into the surface layers of the colored cold-mixed asphalt and the luminous particles, the particle diameter of the acrylic light-storing luminous stones is 5-8MM, the optional colors comprise blue green, yellow green and sky blue, the thickness of the gravel cushion layer is 200MM, and the specification is reasonable gradation of Q2, 4 and 6 cm.
As the utility model relates to a preferred technical scheme of self-luminous road surface structure based on cold mix pitch technology is made, the thickness of concrete cushion is 100 MM.
As the utility model relates to a preferred technical scheme of self-luminous road surface structure based on cold mix pitch technology is made, plain soil tamp layer is layering tamp state, and heavy compactedness is more than or equal to 93%.
The utility model has the advantages that:
the utility model discloses a self-luminous road is made to the mode of cold mix pitch technology, reduce the fuel consumption, do not receive the influence of weather in the work progress, reduce the use of main equipment, compare with traditional pitch construction scheme, the work progress is simple, material utilization increases, the energy saving, add ya keli light storage type night light stone on road surface structure surface, absorb energy daytime, give off the energy evening, need not set up the light source illumination in addition on the road, have illumination and ornamental effect concurrently, accord with the requirement of environmental protection.
Drawings
Fig. 1 is a schematic structural view of a self-luminous pavement structure manufactured based on a cold-mix asphalt process of the present invention; the symbols in the drawings illustrate that: 1 colorful cold-mixed asphalt and luminous particle surface layer, 2 concrete cushion layer, 3 broken stone cushion layer and 4 plain soil rammed rock layer.
Detailed Description
The invention will now be described in further detail with reference to the accompanying drawings.
As shown in fig. 1, a self-luminous road surface structure based on cold mix asphalt technology is made, including colored cold mix asphalt and luminous particle surface course 1, concrete cushion 2, rubble bed course 3 and plain soil tamp layer 4, colored cold mix asphalt and luminous particle surface course 1 coating are in the top layer on concrete cushion 2 surface, concrete cushion 2 paves rubble bed course 3 top, rubble bed course 3 paves on plain soil tamp layer 4, plain soil tamp layer 4 is the plane of foundation support, is located the bottom layer, colored cold mix asphalt is 30MM with the thickness of luminous particle surface course 1, the ya keli light type night light stone has been added in colored cold mix asphalt and the luminous particle surface course 1, the particle diameter of ya keli light type night light stone is 5-8MM, and optional colour has blue-green, yellow-green and sky blue, the thickness of rubble bed course 3 is 200MM, the specification is Q2, 4, 6cm reasonable gradation. Specifically, in this embodiment, the cold asphalt mixing process adopts a conventional process technology known to those skilled in the art, and the improvement point of the present invention does not relate to a specific manufacturing method of the cold asphalt mixing process, and therefore, the detailed description of the specific manufacturing method of the cold asphalt mixing process is omitted.
Specifically, in the present invention, the thickness of the concrete pad 2 is 100 MM.
The utility model discloses in, plain soil tamp layer 4 is the layering tamp state, and heavy compactedness is more than or equal to 93%.
Finally, it should be noted that: these embodiments are merely illustrative of the present invention and do not limit the scope of the invention. In addition, other variations and modifications will be apparent to persons skilled in the art based on the foregoing description. And are neither required nor exhaustive of all embodiments. And obvious changes and modifications may be made without departing from the scope of the present invention.
Claims (3)
1. The utility model provides a self-luminous road surface structure based on cold mix pitch technology is made, includes colored cold mix pitch and luminous particle surface course (1), concrete cushion (2), rubble bed course (3) and plain soil tamped stone layer (4), its characterized in that: colored cold mix pitch and luminous particle surface course (1) coating are on concrete cushion (2) surface, are in the top layer, concrete cushion (2) are laid rubble cushion (3) top, rubble cushion (3) are laid on the plain soil tamp layer, plain soil tamp layer (4) are the plane of basic support, are located the bottom, the thickness of colored cold mix pitch and luminous particle surface course (1) is 30MM, inferior gram force light-storing type night light stone has been added in colored cold mix pitch and luminous particle surface course (1), the particle diameter of inferior gram force light-storing type night light stone is 5-8MM, and optional colour has blue-green, yellow green and sky blue, the thickness of rubble cushion (3) is 200MM, and the specification is Q2, 4, 6cm reasonable gradation.
2. The self-luminous pavement structure manufactured based on the cold-mix asphalt process as claimed in claim 1, wherein: the thickness of the concrete cushion layer (2) is 100 MM.
3. The self-luminous pavement structure manufactured based on the cold-mix asphalt process as claimed in claim 1, wherein: the plain soil rammed rock layer (4) is in a layered rammed state, and the heavy-duty compaction degree is more than or equal to 93%.