CN213345317U - Anti-cracking ceramic marmite structure - Google Patents
Anti-cracking ceramic marmite structure Download PDFInfo
- Publication number
- CN213345317U CN213345317U CN202021853891.2U CN202021853891U CN213345317U CN 213345317 U CN213345317 U CN 213345317U CN 202021853891 U CN202021853891 U CN 202021853891U CN 213345317 U CN213345317 U CN 213345317U
- Authority
- CN
- China
- Prior art keywords
- pot body
- pot
- pot cover
- marmite
- handle
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model relates to a marmite technical field, and disclose a crack control type pottery marmite structure, solved the relatively poor problem of present marmite crack control effect, it includes the pot body, pot body lower extreme circumference is connected with the arch, and pot body upper portion both sides all are connected with the handle, and pot body upper end is connected with the pot lid, and pot lid upper end middle part is connected with the handle, and the pot lid lower extreme is close to the edge and has seted up the ring channel, and pot body upper end corresponds ring channel department and has seted up the arcwall face, the utility model discloses, through the arch that sets up at the bottom of the pot body, when making the pot body place after heating, can hang in the air, avoid directly contacting with the mesa to avoid cold and hot direct contact, make its even heat dissipation; through the iron ring and the connecting rib which are arranged inside the pot body, the strength of the whole structure can be improved, and the anti-cracking effect is further achieved.
Description
Technical Field
The utility model belongs to the technical field of the marmite, specifically be a crack control type pottery marmite structure.
Background
Earthen pot is a kind of cooking utensil. The traditional earthenware pot is made of ceramic products compounded by quartz, feldspar, clay and other raw materials which are difficult to transfer heat, and is fired at high temperature, and has the characteristics of air permeability, adsorbability, uniform heat transfer, slow heat dissipation and the like.
Traditional marmite anti-cracking effect is relatively poor, and after the heating use, the bottom is usually required to be separated from the table top by tools such as a wooden frame and the like, so that direct contact is avoided, and the phenomenon of shrinkage cracking caused by cold and hot contact is avoided.
Disclosure of Invention
To the above situation, for overcoming prior art's defect, the utility model provides a crack control type ceramic marmite structure, the effectual relatively poor problem of present marmite crack control effect of having solved.
In order to achieve the above object, the utility model provides a following technical scheme: the utility model provides an anti-cracking ceramic marmite structure, includes the pot body, arch, lifting lug, pot cover, handle, ring channel, arcwall face, argil layer, iron ring, splice bar and exhaust hole, pot body lower extreme circumferential connection has the arch, and pot body upper portion both sides all are connected with the lifting lug, and pot body upper end is connected with the pot cover, and pot cover upper end middle part is connected with the handle, and the pot cover lower extreme is close to the edge and has seted up the ring channel, and pot body upper end corresponds ring channel department and has seted up the arcwall face, and the pot body and pot cover all include argil layer, iron ring and splice bar, and argil layer inside evenly is connected with.
Preferably, the lower ends of the protrusions are arranged in a hemispherical structure, the number of the protrusions is six, and the six protrusions are annularly distributed at the lower end of the pot body.
Preferably, the lifting lug and the pot body are arranged in an integrated structure, and the lifting handle and the pot cover are arranged in an integrated structure.
Preferably, one side of the upper end of the pot cover is provided with an exhaust hole convenient for air outlet.
Preferably, the inner diameter of the lower part of the pot body is smaller than that of the upper part of the pot body.
Preferably, the outer edge of the lifting lug is provided with a fillet.
Compared with the prior art, the beneficial effects of the utility model are that:
(1) the utility model can suspend in the air when the pot body is placed after being heated through the bulge arranged at the bottom of the pot body, thereby avoiding direct contact with the table-board, avoiding direct contact of cold and heat, enabling the pot body to radiate heat evenly and cool slowly, and avoiding the shrinkage cracking phenomenon;
(2) the iron ring and the connecting ribs are arranged inside the pot body, so that the strength of the integral structure can be improved, and the anti-cracking effect is further achieved.
Drawings
The accompanying drawings are included to provide a further understanding of the invention, and are incorporated in and constitute a part of this specification, illustrate embodiments of the invention, and together with the description serve to explain the invention and not to limit the invention.
In the drawings:
FIG. 1 is a schematic structural view of the present invention;
fig. 2 is a front view of the present invention;
fig. 3 is a cross-sectional view of the present invention;
fig. 4 is an enlarged schematic view of a in fig. 3 according to the present invention;
in the figure: 1. a pan body; 2. a protrusion; 3. lifting the ears; 4. a pot cover; 5. a handle; 6. an annular groove; 7. an arc-shaped surface; 8. a layer of clay; 9. an iron ring; 10. connecting ribs; 11. and (4) exhausting holes.
Detailed Description
The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only some embodiments of the present invention, not all embodiments; based on the embodiments in the present invention, all other embodiments obtained by a person skilled in the art without creative work belong to the protection scope of the present invention.
In the first embodiment, as shown in fig. 1, fig. 2, fig. 3 and fig. 4, the present invention comprises a pot body 1, a protrusion 2, a lifting lug 3, a pot cover 4, a lifting handle 5, a ring groove 6, an arc surface 7, a clay layer 8, an iron ring 9, a connecting rib 10 and an exhaust hole 11, wherein the lower end of the pot body 1 is circumferentially connected with the protrusion 2 for supporting the pot body 1, the lifting lug 3 is connected to both sides of the upper part of the pot body 1 for lifting the pot body 1, the pot cover 4 is connected to the upper end of the pot body 1, the lifting handle 5 is connected to the middle part of the upper end of the pot cover 4 for lifting the pot cover 4, the ring groove 6 is arranged at the lower end of the pot cover 4 near the edge, the arc surface 7 is arranged at the upper end of the pot body 1 corresponding to the ring groove 6, so that the pot cover 4 is in good contact with the pot body 1, the pot body 1 and the pot, for increased structural strength.
Embodiment two, on the basis of embodiment one, 2 lower extremes of arch are the hemisphere structure setting, and 2 quantity of arch are six, and six 2 ring distributions in the 1 lower extreme of pot body are convenient for avoid when the pot body 1 is placed wearing and tearing with the contact surface.
In the third embodiment, on the basis of the first embodiment, the lifting lug 3 and the pot body 1 are integrally arranged, and the lifting handle 5 and the pot cover 4 are integrally arranged.
In the fourth embodiment, on the basis of the first embodiment, an exhaust hole 11 for facilitating air outlet is formed in one side of the upper end of the pot cover 4.
Fifth embodiment, on the basis of the first embodiment, the inner diameter of the lower part of the pot body 1 is smaller than that of the upper part of the pot body 1.
Sixth embodiment, on the basis of first embodiment, handle 3 outside edges and seted up the fillet, conveniently avoid edges and corners to damage hand when mentioning pot body 1.
The working principle is as follows: when using, remove the pot body 1 through lifting lug 3 and cook food on the flame source, after food is cooked, shift out the flame source with the pot body 1 through lifting lug 3, arrange the pot body 1 in on placing the mesa, because the protruding 2 setting in its bottom, make the pot body 1 when placing, can be unsettled, avoid with mesa direct contact, thereby avoid cold and hot direct contact, make its even heat dissipation, slow cooling, in order to avoid the shrinkage crack, in addition, at the inside iron ring 9 and the splice bar 10 that set up of the pot body 1, can improve overall structure intensity, further play the crack control effect.
It is noted that, herein, relational terms such as first and second, and the like may be used solely to distinguish one entity or action from another entity or action without necessarily requiring or implying any actual such relationship or order between such entities or actions. Also, the terms "comprises," "comprising," or any other variation thereof, are intended to cover a non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements does not include only those elements but may include other elements not expressly listed or inherent to such process, method, article, or apparatus.
Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that changes, modifications, substitutions and alterations can be made in these embodiments without departing from the principles and spirit of the invention, the scope of which is defined in the appended claims and their equivalents.
Claims (6)
1. The utility model provides an anti-cracking ceramic marmite structure, includes the pot body (1), arch (2), carries ear (3), pot cover (4), handle (5), ring channel (6), arcwall face (7), argil layer (8), iron ring (9), splice bar (10) and exhaust hole (11), its characterized in that: the pot body (1) lower extreme circumferential connection has arch (2), the pot body (1) upper portion both sides all are connected with lifting lug (3), pot body (1) upper end is connected with pot cover (4), pot cover (4) upper end middle part is connected with handle (5), pot cover (4) lower extreme is close to the edge and has seted up ring channel (6), arcwall face (7) have been seted up to corresponding ring channel (6) department in the pot body (1) upper end, the pot body (1) and pot cover (4) all include argil layer (8), iron ring (9) and splice bar (10), argil layer (8) inside evenly connected with iron ring (9), iron ring (9) outside evenly connected with splice bar (10).
2. The anti-cracking ceramic casserole structure as claimed in claim 1, wherein: the lower end of each protrusion (2) is arranged in a hemispherical structure, the number of the protrusions (2) is six, and the six protrusions (2) are annularly distributed at the lower end of the pot body (1).
3. The anti-cracking ceramic casserole structure as claimed in claim 1, wherein: the lifting lug (3) and the pot body (1) are arranged in an integrated structure, and the lifting handle (5) and the pot cover (4) are arranged in an integrated structure.
4. The anti-cracking ceramic casserole structure as claimed in claim 1, wherein: an exhaust hole (11) convenient for air outlet is formed in one side of the upper end of the pot cover (4).
5. The anti-cracking ceramic casserole structure as claimed in claim 1, wherein: the inner diameter of the lower part of the pot body (1) is smaller than that of the upper part of the pot body (1).
6. The anti-cracking ceramic casserole structure as claimed in claim 1, wherein: the outer edge of the lifting lug (3) is provided with a fillet.