CN2101535U - Hydrocooling metal die set - Google Patents
Hydrocooling metal die set Download PDFInfo
- Publication number
- CN2101535U CN2101535U CN 91209403 CN91209403U CN2101535U CN 2101535 U CN2101535 U CN 2101535U CN 91209403 CN91209403 CN 91209403 CN 91209403 U CN91209403 U CN 91209403U CN 2101535 U CN2101535 U CN 2101535U
- Authority
- CN
- China
- Prior art keywords
- water
- mould
- die
- pipeline
- metal die
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The utility model provides a water cooling metal die formed by that a common metal die body is provided with fluid or the pipeline of a water cooling system whose cooling media are oil, air or water. The cooling media flowing in the pipeline carry away heat and accelerate the cooling of the metal die, which can increase productivity and product quality and prolong the service life. The water cooling metal die can also be used for replicating dies, can lower die cost and shorten the die making period.
Description
The utility model relates to the metal die technical field.
In the modern industry production process, metal die is widely used in blank processing such as casting, forging, metal punching and powder metallurgy as a kind of instrument, and the processing and forming aspect of nonmetallic materials such as plastics, rubber, pottery, glass, utilize a metal die can obtain many identical parts, can fully show the power of production in enormous quantities.But metal die in use easily is heated, and as adopting the nature condensation, the time is longer, can influence the raising of productivity ratio and product quality, and can shorten the life-span of mould, makes mould cause damage.In addition, the manufacturing cycle of metal die is long, and die cost is high, and mould damages the general not reproducible of producer that uses in back, has a strong impact on production.Therefore with regard to die industry, reducing die manufacturing cost, shortening delivery date and the mould of reproducible mould is provided is a very severe problem.
The purpose of this utility model provides novel water-cooled metal mould and boosts productivity and product quality, prolongs die life, and the further purpose of the utility model provides the mould that can be used for copy mold and reduces die manufacturing cost and shorten delivery date.
The purpose of this utility model is achieved through the following technical solutions.
The water-cooled metal mould is to be provided with the pipeline of fluid or water cooling system and to constitute in the type body of common metal mould.Therefore, the method that the water-cooled metal mould can utilize cooling medium fluxion straps in above-mentioned pipeline such as oil, air or water to walk heat is accelerated the cooling of metal die, by adjusting to the fluid temperature (F.T.) that enters pipeline and flow size etc., the cooling velocity that can obtain to suit, owing to adopt water cooling comparatively convenient and cheap, therefore, suggestion makes water as cooling medium, and the user can select other cooling medium for use because of special requirement.
The utility model technical scheme preferably is that the pipeline of fluid or water cooling system and the type body casting of water-cooled metal mould connect as one, above-mentioned pipeline can manufacture and design shaping in advance as required, with metal die while casting, be convenient to manufacture the water-cooled metal mould then.
The better technical scheme of the utility model is that the water inlet of the pipeline of fluid or water cooling system is positioned at the bottom of water-cooled metal mould type body and delivery port is positioned at top.
The water-cooled metal mould that can be used for copy mold of the present utility model has a metal die to be made of levorotation chamber frame, right die cavity frame and apperance plate, and their type body inside is provided with the pipeline of fluid or water cooling system respectively.Owing to adopt water-cooled metal mould cast method, when therefore duplicating other mould with this mould, can directly cast out and have the higher mould of cavity dimension precision, only need simple processing polishing, just can come into operation, can finish the production of metal die in enormous quantities fast, can solve the difficulty of using producer with it, for die industry reduces production costs, delivery provides new approach fast again.
The better design that can be used for the water-cooled metal mould of copy mold is, the water inlet of the pipeline of fluid or water cooling system is all in the bottom of this water-cooled metal mould, and delivery port is positioned at the top of water-cooled metal mould.
Adopt water-cooled metal mould described in the utility model, the foundry trial that black and non-ferrous metal such as casting pig, spheroidal graphite cast-iron, aluminium, copper, albronze, copper lead glass alloy etc. are carried out shows, it can improve work efficiency greatly, casting quality further improves, than superior, for casting industry provides new mould with sand mold and common metal mold casting; The water-cooled metal mould of reproducible mould uses producer and quick, the large quantities of copy mold of die industry, reduction mould production cost for solving, shortens delivery date, and new approach is provided.Its major advantage is: (1) casting dimension is accurate, any surface finish, and allowance is little or do not process; (2) casting quality improves, in the water-cooled metal mould molten metal of cast solidify in order that principle is solidified and evenly cooling accelerate, make the refinement of foundry goods crystalline structure, compact structure, no shrinkage porosite pore, 1 of raising mechanical performance is more than the trade mark; (3) productivity ratio height, water-cooled has been accelerated casting solidification, can pour into a mould immediately behind the removing from mould again, when not only having saved the moulder, and is easy to realize mechanization pile line operation; (4) the water-cooled metal mould has cooling medium to take away the heat of mould inside, and its life-span is prolonged; (5) can realize exchanging permanent mold casting, mould has been broken the water-cooled metal mould massive duplication of the enough reproducible moulds of energy; (6) can reduce the production cost of metal die significantly; (7) reproducible water-cooled metal mould not only can be used for smart casting common metal mould, and is particularly suitable for smart casting water-cooled metal mould.
With reference to the accompanying drawings the utility model is described in further detail.
Fig. 1 cast pipe pincers pincers handle body water-cooled metal mould schematic diagram
Fig. 2 be Fig. 1 mould part profile die cavity right view on the left side
Fig. 3 casts at random pulling shaft device water-cooled metal mould and cuts open and show schematic diagram
Fig. 4 be Fig. 3 mould part profile die cavity right view on the left side
Fig. 5 is the water-cooled metal mould schematic diagram of the reproducible mould of smart casting pipe vice pincers handle body water-cooled metal mould
Fig. 6 is the right die cavity frame of a Fig. 5 mould left view
Fig. 7 is Fig. 5 mould left side apperance schematic diagram
Fig. 8 is the smart casting of the water-cooled metal mould Follower Tong Holder of Pipe Pliers forge die schematic diagram of reproducible mould
Fig. 9 is the right die cavity frame left view of Fig. 8 mould
Figure 10 is Fig. 8 mould left side apperance schematic diagram
Figure 11 is that the B-B of Figure 10 cuts open and shows schematic diagram
Fig. 1~11st, four specific embodiments of the present utility model, wherein the identical person of each figure part name to mark mark identical.First embodiment shown in Fig. 1~2 is the water-cooled metal mould of cast pipe pincers pincers handle body, be shaped on running gate system 2, water cooling pipeline 3 in the water-cooled metal mould 1 of present embodiment in advance, part profile 4 on the left side and part profile 5 on the right side, the water inlet 6 of water cooling system pipeline 3 is in the bottom of mould type body 7, and delivery port 8 is on the top of mould type body 7.Before the cast, should be at working surface spary high-temperature coatings such as die cavity 9 and sprue gates 10, spary once after, can use continuously, placing core 11 then, just can pour into a mould behind the mould assembly, the malleable cast iron molten metal is poured into the die cavity 9 through ingate 12 from cast gate 10, the fetch boiling water gauge tap of cooling system, cooling water is entered the water cooling pipeline 3 from water inlet 6, behind the heat in the absorption mould type body 7, discharge from delivery port 8 again, by adjusting to coolant-temperature gage and flow, can control the cooling velocity of mould 1, treat will cast after molten metal solidifies fully good pipe vice pincers handle body 13 and take out, mould 1 can be poured into a mould again immediately again, the water-cooled metal mould can shorten foundry goods annealing time 30%, helps the mechanization direct casting.Second embodiment shown in Fig. 3~4 casts the water-cooled metal mould of pulling shaft device 14 at random, be shaped on running gate system 2 in advance in the water-cooled metal mould 1 of present embodiment, water cooling pipeline 3, part profile 4 on the left side and part profile 5 on the right side, the water inlet 6 of water cooling system pipeline 3 is in the bottom of mould type body 7, and delivery port is on the top of mould type body 7, cast is a spheroidal graphite cast-iron with molten metal, in order to pour into a mould a plurality of devices of pulling shaft at random 14 simultaneously, set up runner gate 15, the device of the pulling shaft at random processing rear surface light that casts out is as steel part.The 3rd embodiment shown in Fig. 5~8 is a kind of water-cooled metal mould 16 of reproducible mould, it is used for smart casting pipe vice pincers handle body water-cooled metal mould 1, mould 16 is by levorotation chamber frame 17, right die cavity frame 18 and apperance plate 19 constitute, their type body 7 inside are provided with the pipeline 20 of water cooling system respectively, the water inlet 6 of the pipeline 20 of water cooling system lays respectively at the bottom of mould 16 various bodies, and delivery port 8 lays respectively at top.In order to cast out the water cooling system of water-cooled mould, before cast, pre-formed good water cooling pipeline 3 should be put into levorotation chamber frame 17 and right die cavity frame 18 respectively and by locating hole 21 location, and then be carried out the water-cooled cast and directly cast out the higher pipe vice pincers handle body water-cooled metal mould casting mold of cavity dimension precision.The 4th embodiment shown in Fig. 8~11 is the water-cooled metal mould 16 of the reproducible mould of smart casting Follower Tong Holder of Pipe Pliers forge die 22, because of forge die does not need water cooling system, does not put into water cooling pipeline 3 when therefore casting, and increasing in addition has rising head 23.After adopting mould 16 directly to cast out Follower Tong Holder of Pipe Pliers forge die 22, a simply processing polishing just can be come into operation, and has significantly reduced the die cost spending, and mould has been broken and can oneself have been cast again, can realize exchanging permanent type technology.
Claims (2)
1, water-cooled metal mould, one metal die is arranged, be provided with the pipeline (3) of fluid or water cooling system in the type body (7) of metal die, the pipeline (3) that it is characterized in that fluid or water cooling system is to manufacture and design the casting of moulding and water-cooled metal mould (1) in advance as required to connect as one.
2,, it is characterized in that the water inlet (6) of the pipeline (3) of fluid or water cooling system is positioned at the bottom of the type body (7) of water-cooled metal mould (1), and delivery port (8) is positioned at the top of type body (7) according to the described water-cooled metal mould of claim 1.