CN208993260U - A kind of halftone reducing silk-screen material leakage - Google Patents

A kind of halftone reducing silk-screen material leakage Download PDF

Info

Publication number
CN208993260U
CN208993260U CN201821519902.6U CN201821519902U CN208993260U CN 208993260 U CN208993260 U CN 208993260U CN 201821519902 U CN201821519902 U CN 201821519902U CN 208993260 U CN208993260 U CN 208993260U
Authority
CN
China
Prior art keywords
silk
ink layer
screen
halftone
photoresists
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201821519902.6U
Other languages
Chinese (zh)
Inventor
张忠涛
彭超
彭乐平
周卫华
余楚强
孟祥龙
吕尊滨
陶科屹
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hunan Fly Special Electronic Technology Co Ltd
Original Assignee
Hunan Fly Special Electronic Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hunan Fly Special Electronic Technology Co Ltd filed Critical Hunan Fly Special Electronic Technology Co Ltd
Priority to CN201821519902.6U priority Critical patent/CN208993260U/en
Application granted granted Critical
Publication of CN208993260U publication Critical patent/CN208993260U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses a kind of halftones of reduction silk-screen material leakage in screen printing technique field, including silk screen gauze, screen plate aluminum frame, lower ink layer and upper photoresists ink layer, screen plate aluminum frame is fixedly installed at the end positions of silk screen gauze upper surface, silk lace gauze cloth lower surface is provided with lower ink layer, the blanking mesh A of silk-screen blanking is provided on the lower ink layer, silk screen gauze upper surface applies and is covered with photoresists ink layer, corresponds to blanking mesh A on the upper photoresists ink layer and is provided with blanking mesh B.The utility model is designed reasonably, by the coating photoresists ink layer in the upper surface of halftone, a possibility that the big and small pin hole in the lower ink layer of halftone can be filled, therefore considerably reduce silk-screen material leakage.

Description

A kind of halftone reducing silk-screen material leakage
Technical field
The utility model discloses a kind of halftones for reducing silk-screen material leakage, specially screen printing technique field.
Background technique
Silk-screen printing originates from China earliest, away from modern existing more than 2,000 years history, as screen printing technique is continuous Develop perfect, has become indispensable a part in human lives, silk-screen printing has of large quantities, cheap, color Bright-coloured, long shelf-life, the advantages such as fast of delivering goods, are approved by more and more industries, are widely used.
Very high to environmental requirement during screen printing, halftone, the film, exposure stage surface have dust impurity that can lead The bad generation of pin hole is caused, although can carry out halftone inspection before silk-screen, time-consuming, and the tiny pin hole in part is due to light, angle A problem that degree problem, which is difficult to be checked completely, to be come's, and when silk-screen will lead to material leakage, leakage solvent generation.For this purpose, we mention The halftone for having gone out a kind of reduction silk-screen material leakage comes into operation, to solve the above problems.
Utility model content
The purpose of this utility model is to provide a kind of halftones for reducing silk-screen material leakage, to solve to mention in above-mentioned background technique Out the problem of.
To achieve the above object, the utility model provides the following technical solutions: a kind of halftone reducing silk-screen material leakage, including Silk screen gauze, screen plate aluminum frame, lower ink layer and upper photoresists ink layer are fixed at the end positions of silk screen gauze upper surface It is provided with screen plate aluminum frame, silk lace gauze cloth lower surface is provided with lower ink layer, is provided with silk-screen blanking on the lower ink layer Blanking mesh A, silk screen gauze upper surface apply be covered with photoresists ink layer, correspond to blanking on the upper photoresists ink layer Mesh A is provided with blanking mesh B.
Preferably, photopolymer layer is pasted on the silk screen gauze.
Preferably, the silk screen gauze is made of stainless steel or nylon or polyester material.
Preferably, the lower ink layer and upper photoresists ink layer are UV photosensitive resin layer.
Compared with prior art, the utility model has the beneficial effects that passing through the coating photoresists in the upper surface of halftone Ink layer can fill the big and small pin hole in the lower ink layer of halftone, thus considerably reduce silk-screen material leakage can Energy property can effectively reduce halftone inspection, net mending time-consuming and pin hole missing inspection bring material leakage risk, and present apparatus structural strength Height, wearability is strong, and surface smoothness is higher, and printing stability is high.
Detailed description of the invention
Fig. 1 is the structural schematic diagram of the utility model.
In figure: 1- silk screen gauze;2- screen plate aluminum frame;Ink layer under 3-;The upper photoresists ink layer of 4-;5- blanking mesh A;6- Blanking mesh B;7- photopolymer layer.
Specific embodiment
The following will be combined with the drawings in the embodiments of the present invention, carries out the technical scheme in the embodiment of the utility model Clearly and completely describe, it is clear that the described embodiments are only a part of the embodiments of the utility model, rather than whole Embodiment.Based on the embodiments of the present invention, those of ordinary skill in the art are without making creative work Every other embodiment obtained, fall within the protection scope of the utility model.
Referring to Fig. 1, the utility model provides a kind of technical solution: a kind of halftone reducing silk-screen material leakage, including silk screen Gauze 1, screen plate aluminum frame 2, lower ink layer 3 and upper photoresists ink layer 4 are consolidated at the end positions of 1 upper surface of silk screen gauze Surely it is provided with screen plate aluminum frame 2,1 lower surface of silk screen gauze is provided with lower ink layer 3, is provided with silk on the lower ink layer 3 The blanking mesh A5 of blanking is printed, 1 upper surface of silk screen gauze applies and is covered with photoresists ink layer 4, the upper photoresists ink layer 4 Upper corresponding blanking mesh A5 is provided with blanking mesh B6, is pasted with photopolymer layer 7 on the silk screen gauze 1, improves silk The flatness on 1 surface of grenadine cloth, the silk screen gauze 1 are made of stainless steel or nylon or polyester material, improve device Structural strength, the lower ink layer 3 and upper photoresists ink layer 4 are UV photosensitive resin layer, improve the wearability of device.
Working principle: taking the halftone for cleaning up and having dried, and front and back sides binding dust rolls the ash for sticking out surface Dirt foreign matter uniformly sprays one layer of water mist at the halftone back side, then attaches the film, strikes off extra water with scraper plate, then and with dry hair Towel dries the water of screen frame and surrounding, is put into oven and dries, and ink layer 3 and uses ultraviolet light in the case where the halftone back side for having pasted the film attaches Irradiation, then rinsed with giant, it can not be washed out by giant by the capillary film of ultraviolet light by film graph shealtering Expose silk screen gauze 1, the visuals being rinsed can allow ink through on grenadine silk-screen to stock, be finally putting into oven It dries and completes to make a plate for the first time, coated photoresists 1 to 20 time with net scraper processed in the halftone front whole face dried, made for the first time at this time The pin hole generated when version can be filled up one by one by the photoresists of flowability, and halftone is then put into oven and is dried, photoresists are consolidated Change, attach figure at the halftone back side and extend out the film of 0.1mm to 3mm and with ultraviolet light, then with giant flushing will under Ink layer 3 and neighbouring photoresists are rinsed well, the film of 0.1mm to 3mm are extended out due to using figure, so that lower ink layer Photoresists in 3 and its around 0.1 to 3mm region can be flush with water, therefore not influence normal silk-screen, and other are ultraviolet The photoresists that illumination is mapped to, which then react with ultraviolet light, to be kept down, and can not be flush with water, therefore photosensitive by this part The pin hole that glue is filled up then will not material leakage again, quality examination finally is carried out to the defects of halftone material leakage in inspection net light table, it is ensured that net Version quality meets the technique requirement of silk-screen production, due to being coated with photoresists 1 to 20 time in halftone front whole face, can use sense The flowability of optical cement fills up pin hole tiny on halftone, then solidifies photoresists by way of toasting with ultraviolet light, makes It obtains in silk-screen printing process, ink or slurry can not continue to penetrate on stock or product through pin hole, perfectly solve silk The problem of printing material leakage.
While there has been shown and described that the embodiments of the present invention, for the ordinary skill in the art, It is understood that these embodiments can be carried out with a variety of variations in the case where not departing from the principles of the present invention and spirit, repaired Change, replacement and variant, the scope of the utility model is defined by the appended claims and the equivalents thereof.

Claims (4)

1. a kind of halftone for reducing silk-screen material leakage, it is characterised in that: including silk screen gauze (1), screen plate aluminum frame (2), lower ink layer (3) and upper photoresists ink layer (4), screen plate aluminum frame is fixedly installed at the end positions of silk screen gauze (1) upper surface (2), silk screen gauze (1) lower surface is provided with lower ink layer (3), is provided with silk-screen blanking on the lower ink layer (3) Blanking mesh A (5), silk screen gauze (1) upper surface apply and are covered with photoresists ink layer (4), the upper photoresists ink layer (4) Upper corresponding blanking mesh A (5) is provided with blanking mesh B (6).
2. a kind of halftone for reducing silk-screen material leakage according to claim 1, it is characterised in that: on the silk screen gauze (1) It is pasted with photopolymer layer (7).
3. a kind of halftone for reducing silk-screen material leakage according to claim 1, it is characterised in that: the silk screen gauze (1) is adopted It is made of stainless steel or nylon or polyester material.
4. it is according to claim 1 it is a kind of reduce silk-screen material leakage halftone, it is characterised in that: the lower ink layer (3) and Upper photoresists ink layer (4) is UV photosensitive resin layer.
CN201821519902.6U 2018-09-12 2018-09-12 A kind of halftone reducing silk-screen material leakage Active CN208993260U (en)