CN208517448U - A kind of main trough of blast furnace sectional repair mold - Google Patents

A kind of main trough of blast furnace sectional repair mold Download PDF

Info

Publication number
CN208517448U
CN208517448U CN201820897635.XU CN201820897635U CN208517448U CN 208517448 U CN208517448 U CN 208517448U CN 201820897635 U CN201820897635 U CN 201820897635U CN 208517448 U CN208517448 U CN 208517448U
Authority
CN
China
Prior art keywords
blast furnace
support beam
mold
main iron
reinforcing bars
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201820897635.XU
Other languages
Chinese (zh)
Inventor
张守喜
梁科
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Bengang Steel Plates Co Ltd
Original Assignee
Bengang Steel Plates Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Bengang Steel Plates Co Ltd filed Critical Bengang Steel Plates Co Ltd
Priority to CN201820897635.XU priority Critical patent/CN208517448U/en
Application granted granted Critical
Publication of CN208517448U publication Critical patent/CN208517448U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本实用新型公开一种高炉主铁沟局部修补模具,包括两块相对设置的挡料板和多根连接在两块挡料板之间的支撑横梁;支撑横梁由相互铰接的两根梁臂组成。挡料板上设置有多根加强拉筋,水平设置的加强拉筋与竖直设置的加强拉筋相互垂直。支撑横梁的两端分别连接在两块挡料板的相对设置的两根竖直设置的加强筋上。设置在上方的支撑横梁的长度大于下方的支撑横梁的长度。本实用新型用于对主铁沟因为龟裂、剥落、侵蚀等原因形成局部损坏及时进行热态修补的模具;当修补耐火浇注料硬化到足够强度后,模具即可被移除,并可重复使用;避免了因主铁沟局部破损严重未能及时修补,渣铁继续侵蚀和渗透,而导致主铁沟烧穿事故,延长主铁沟使用寿命。

The utility model discloses a local repairing mold for a main iron groove of a blast furnace, which comprises two oppositely arranged baffle plates and a plurality of support beams connected between the two baffle plates; the support beam is composed of two beam arms hinged with each other . A plurality of reinforcing bars are arranged on the baffle plate, and the horizontally arranged reinforcing bars and the vertically arranged reinforcing bars are perpendicular to each other. The two ends of the support beam are respectively connected to the two vertically arranged reinforcing ribs of the two baffle plates. The length of the upper support beam is greater than the length of the lower support beam. The utility model is used to repair the mold in a hot state in time for the local damage of the main iron groove due to cracking, peeling, erosion, etc.; when the repaired refractory castable is hardened to a sufficient strength, the mold can be removed, and can be repeated It avoids the failure to repair in time due to the serious damage of the main iron ditch, and the slag iron continues to erode and penetrate, resulting in the main iron ditch burning through accident, and prolongs the service life of the main iron ditch.

Description

A kind of main trough of blast furnace sectional repair mold
Technical field
The utility model belongs to blast furnace field more particularly to a kind of main trough of blast furnace sectional repair mold in ironmaking.
Background technique
Main trough of blast furnace is the channel that slag iron is discharged in time, and with blast furnace enlargement and strengthening smelting, iron increases out, main Iron runner use condition is increasingly harsh, and service life greatly affected the labor intensity of flushing and casting work, ton iron refractory material Consumption, or even influence the normal production of blast furnace.
Currently, well known country's large blast furnace sow, typically uses low cement combination Al2O3-SiC-C fire proofed wood Material, is formed using die casting.Since main trough of blast furnace by tapping discontinuity because being influenced, sow inner lining refractory by There is the phenomenon that low intensity and explosion, explosion, in addition slag iron is washed away and corroded, so that the main iron of blast furnace in sometimes hot and sometimes cold impact Ditch service life reduction limits sow and crosses iron, seriously restricts the normal production of blast furnace sometimes.
In addition, there are certain drops for main trough of blast furnace and iron mouth, and sow has certain gradient, because having in blast furnace There is certain pressure, therefore there is certain kinetic energy at parabolic shape when slag iron is ejected from tapping hole into sow And hydraulic coupling, the refractory material for falling position around iron spot is washed away, causes to fall and occurs dell around iron spot, master can be also burnt when serious Iron runner.
In addition, the circulation that refractory material can bear 500 DEG C ← → 1500 DEG C of temperature is made in main trough of blast furnace use process With this meeting is so that generate horizontal and longitudinal crack inside refractory material;The crackle of generation under the action of slag and molten iron along Crackle corrodes, and generates groove, accelerates damage.
In addition, sow under the action of periodical high speed molten iron, deteriorates, position is mainly the slag for storing iron phase and tapping phase There are two local excessive damage concave grooves in line position, so that slag lining damage is serious, and the damage of other positions is lighter, Sow is caused integrally to damage unbalanced.
Utility model content
The purpose of this utility model is to provide a kind of main trough of blast furnace sectional repair mold, with solve in the prior art because Sow local damage seriously fails to repair in time, slag iron continue corrode and permeate, and cause sow burn accident the problem of.
The utility model provides a kind of main trough of blast furnace sectional repair mold, the striker plate being oppositely arranged including two pieces and more Root is connected to the support beam between two pieces of striker plates;The support beam is made of two beam arms being hinged.
In the main trough of blast furnace sectional repair mold of the utility model, it is provided with more reinforcements on the striker plate and draws Muscle, horizontally disposed reinforcement lacing wire are mutually perpendicular to the reinforcement lacing wire being vertically arranged.
In the main trough of blast furnace sectional repair mold of the utility model, the both ends of the support beam are connected to two On the reinforcing rib that two be oppositely arranged piece of block striker plate are vertically arranged, and support beam both ends are located at identical height.
In the main trough of blast furnace sectional repair mold of the utility model, the length for the support beam being disposed over is greater than The length of the support beam of lower section.
In the main trough of blast furnace sectional repair mold of the utility model, the hinged of two beam arms of support beam is being constituted End is equipped with slotted hole, by adjusting bolt fastening in slotted hole.
In the main trough of blast furnace sectional repair mold of the utility model, the striker plate upper end is equipped with hoisting ring.
In the main trough of blast furnace sectional repair mold of the utility model, the repairing mold is a kind of welding for steel structure Part.
Compared with prior art, beneficial effect is the utility model:
1, it can be directlyed adopt to main trough of blast furnace local damage region after simply clearing up using tapping interval time Hot patching, baking time is short, does not influence normal tapping, achievees the purpose that quick tapping.
2, damageable zone main for main trough of blast furnace is taken planned preventative sectional repair, is avoided because of main iron Ditch local damage seriously fails to repair in time, and slag iron continues to corrode and permeate, and sow is caused to burn accident, extends sow Service life.
3, the utility model only repairs main trough of blast furnace local damage position, where where damages repairing, other Uncorroded intact part can still continue to use, and can substantially reduce refractory material cost.
4, the main trough of blast furnace repaired through the utility model, crossing iron by 100,000 tons increases to 200,000 tons;Sow work Service life extends, and is increased to 30 days by 20 days.
5, the utility model is a kind of hardware, and simple process is cheap, be may be reused.
Detailed description of the invention
Fig. 1 is a kind of schematic diagram of main trough of blast furnace sectional repair mold of the utility model;
Fig. 2 is support beam, slotted hole, adjustment bolt enlarged drawing;
Fig. 3 is a kind of use schematic diagram of main trough of blast furnace sectional repair mold of the utility model.
Specific embodiment
In order to make the purpose of the utility model, technical solutions and advantages more clearly understood, below in conjunction with attached drawing and implementation Example, the present invention will be further described in detail.It should be appreciated that specific embodiment described herein is only used to explain The utility model is not used to limit the utility model.
As shown in Figure 1, a kind of main trough of blast furnace sectional repair mold of the utility model, the gear being oppositely arranged including two pieces Flitch 1 and Duo Gen are connected to the support beam 4 between two pieces of striker plates 1;The support beam 4 is by two beam arms being hinged Composition.More reinforcement lacing wires 2, the horizontally disposed reinforcement lacing wire reinforcing lacing wire 2 and being vertically arranged are provided on the striker plate 1 2 are mutually perpendicular to.The both ends of the support beam 4 are connected to the vertical reinforcement of two be oppositely arranged piece of two pieces of striker plates 1 On muscle 2, and 4 both ends of support beam are located at identical height.1 upper end of striker plate is equipped with multiple hoisting rings 3.
As shown in Fig. 2, slotted hole 6 is equipped in the hinged end for constituting two beam arms of support beam 4, by adjusting bolt 5 It is fastened in slotted hole 6.
When it is implemented, the length for the support beam 4 being disposed over is greater than the length of the support beam 4 of lower section.Mold Whole design has up big and down small taper when, it can be achieved that extracting mold from castable refractory and smoothly demoulds.
The mold is a kind of welding for steel structure part, and wherein 1 steel plate thickness of striker plate is 8mm, reinforces lacing wire 2 and support is horizontal Beam 4 is that 70mm angle steel is made.
As shown in figure 3, when in use, firstly, simply being cleared up 7 local damage region of main trough of blast furnace, by mold It is placed on damaged location, unclamps adjustment bolt 5, the width for adjusting striker plate 1 is identical as 7 original width of sow, fastening adjustment spiral shell Bolt 5.Then, it between the residual lining 8 of striker plate 1 and castable refractory in gap, carries out pouring repairing castable refractory 9, use simultaneously 10 jolt ramming of vibrating head.After repairing castable refractory 9 hardens to sufficient intensity, mold is pulled out, after toasting 1.5h with gas burner, Can normal tapping, mold may be reused.
The above is only the preferred embodiment of the present invention, the thought being not intended to limit the utility model, it is all Within the spirit and principles of the utility model, it is practical new to should be included in this for any modification, equivalent replacement, improvement and so on Within the protection scope of type.

Claims (4)

1.一种高炉主铁沟局部修补模具,其特征在于,包括两块相对设置的挡料板和多根连接在两块挡料板之间的支撑横梁;所述支撑横梁由相互铰接的两根梁臂组成,所述挡料板上设置有多根加强拉筋,水平设置的加强拉筋与竖直设置的加强拉筋相互垂直,所述支撑横梁的两端分别连接在两块挡料板的相对设置的两根竖直设置的加强筋上,且支撑横梁两端位于相同高度,设置在上方的支撑横梁的长度大于下方的支撑横梁的长度。1. a local repair mould for the main iron groove of a blast furnace, is characterized in that, comprises two oppositely arranged baffle plates and multiple support beams connected between two baffle plates; Described support beam is made up of two mutually hinged baffles. It is composed of beams and arms, a plurality of reinforcing bars are arranged on the baffle plate, the horizontally arranged reinforcing bars and the vertically arranged reinforcing bars are perpendicular to each other, and the two ends of the supporting beam are respectively connected to the two baffles On two vertically arranged reinforcing ribs opposite to the plate, and the two ends of the support beam are located at the same height, the length of the upper support beam is greater than the length of the lower support beam. 2.如权利要求1所述的高炉主铁沟局部修补模具,其特征在于,在构成支撑横梁的两根梁臂的铰接端设有长圆孔,通过调整螺栓紧固在长圆孔内。2 . The local repairing mold for the main iron groove of a blast furnace according to claim 1 , wherein an oblong hole is provided at the hinged end of the two beam arms constituting the support beam, and is fastened in the oblong hole by adjusting bolts. 3 . 3.如权利要求1所述的高炉主铁沟局部修补模具,其特征在于,所述挡料板上端设有吊装环。3 . The local repair mold for the main iron groove of a blast furnace according to claim 1 , wherein a hoisting ring is provided at the upper end of the baffle plate. 4 . 4.如权利要求1所述的高炉主铁沟局部修补模具,其特征在于,所述修补模具是一种钢结构焊接件。4 . The local repairing mold for the main iron groove of a blast furnace according to claim 1 , wherein the repairing mold is a steel structure weldment. 5 .
CN201820897635.XU 2018-06-11 2018-06-11 A kind of main trough of blast furnace sectional repair mold Expired - Fee Related CN208517448U (en)