CN208388440U - A kind of composite bottom aluminum pot - Google Patents

A kind of composite bottom aluminum pot Download PDF

Info

Publication number
CN208388440U
CN208388440U CN201721689114.7U CN201721689114U CN208388440U CN 208388440 U CN208388440 U CN 208388440U CN 201721689114 U CN201721689114 U CN 201721689114U CN 208388440 U CN208388440 U CN 208388440U
Authority
CN
China
Prior art keywords
aluminum
pot
ring set
pot body
ring
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201721689114.7U
Other languages
Chinese (zh)
Inventor
吕挺
王建明
杜葛云
张海生
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Tianxi Kitchen Appliance Co Ltd
Original Assignee
Zhejiang Tianxi Kitchen Appliance Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhejiang Tianxi Kitchen Appliance Co Ltd filed Critical Zhejiang Tianxi Kitchen Appliance Co Ltd
Priority to CN201721689114.7U priority Critical patent/CN208388440U/en
Application granted granted Critical
Publication of CN208388440U publication Critical patent/CN208388440U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model provides a kind of composite bottom aluminum pot, belongs to cooker technical field.It solves the problems, such as the fastness, bad of existing aluminum pot.This composite bottom aluminum pot includes pot body and the multiple bottom for being compounded in pot body outer bottom, which is characterized in that multiple bottom is steel-aluminum composite material, and the multiple bottom is that the steel-aluminum composite material that will be combined with each other in advance is compounded on pot body outer bottom by being brazed or heating the mode of forging.Compared with prior art, this composite bottom aluminum pot welding procedure is simple, quality is stable, compound securely full, and processing cost is low, is suitable for volume production.

Description

A kind of composite bottom aluminum pot
Technical field
The utility model belongs to cooker technical field, is related to a kind of composite bottom aluminum pot.
Background technique
Aluminum pot answers bottom technique and is mainly brazed multiple bottom and forges and presses multiple bottom at present.The multiple bottom of soldering has plenty of multiple bottom steel disc is direct Soldering is in outer surface of pot bottom, and this bad control of method brazing temperature be easy to cause rosin joint, and compound fastness is poor.In order to improve this Kind method has plenty of and adds one layer of aluminium sheet between outer surface of pot bottom and multiple bottom steel disc, will be brazed between outer surface of pot bottom and aluminium sheet Again although soldering connection, this method make moderate progress between connection, aluminium sheet and stainless steel substrates, but cause two brazing surfaces, increase Add between the bottom of a pan and aluminium sheet, aluminium sheet and stainless steel substrates brazing flux solder coating quality and the control being mutually located on brazing surface difficult Degree and brazing temperature and the difficulty controlled on the holding time, control is bad is easy to appear the bottom of a pan and aluminium sheet, stainless steel substrates for these With the layering that falls off of aluminium sheet, and it is easy to appear the surface defects such as bulge, pad print on multiple bottom stainless steel piece surface.Soldering has vertical edge Packet bottom stainless steel piece when among aluminium sheet under the technological temperature of soldering to perimeter very little, therefore packet bottom stainless steel piece is perpendicular Be between side and pot body and the aluminium sheet of centre it is empty, be commonly called as " vacation packet bottom ", pot body will appear gap using middle stainless steel substrates periphery. Since these existing aluminum pot soldering processes are complicated, at high cost, unstable quality, volume production is not adapted to without widely being answered With.
Utility model content
The purpose of this utility model is fastness, the bad problem for existing aluminum pot, and a kind of multiple bottom proposed Aluminum pot.
The purpose of this utility model can be realized by the following technical scheme:
A kind of composite bottom aluminum pot, including pot body and the multiple bottom for being compounded in pot body outer bottom, which is characterized in that multiple bottom is steel-aluminium Composite material, the multiple bottom are that the steel-aluminum composite material that will be combined with each other in advance is answered by being brazed or heating the mode of forging It closes on pot body outer bottom.
It is offered in the pot body for processing the hole for clamping pot body and assembling handle, is additionally provided with several two-by-two in hole The ring set being mutually arranged, the ring set is in a ring and outer diameter, internal diameter are different, and outer ring is in two neighboring ring set The internal diameter of set matches with the outer diameter in inner ring ring set, and the outer diameter of outermost layer ring set and the size in hole match, each ring set Axial length is different, and the axial length in outer ring ring set is longer than the axial length in inner ring ring set, and each ring set direction is cooked a meal Have an intrinsic side alignment Overlap design, other side due to axial length be differently formed it is ladder-like.It is complete to assemble cooker After being processed at anodic oxidation, it is also necessary to assemble handle using the hole, but the bolt size on handle for inserting in the hole is not Must be just reciprocity, so joined several ring sets in hole, undersized ring set can be squeezed out according to the size of bolt, and remain Remaining inner most ring set can cover handle again just, not will lead to handle loosening.
For the steel-aluminum composite material in plate shaped, plate can cover the outer baseplane of entire pot body,
The steel-aluminum composite material is in wrap bottom by the stamping packet egative film shape holded up upwards at periphery of form of pot bottom Piece can wrap up the entire the bottom of a pan and the bottom of a pan angular position R.
The aluminum layer thickness is 1~3mm, and stainless steel layer is with a thickness of 0.3~0.6mm.
Compared with prior art, this composite bottom aluminum pot welding procedure is simple, quality is stable, compound securely full, processing cost Bottom is suitable for volume production.
Detailed description of the invention
Fig. 1 is that the packet bottom plate of the utility model answers bottom structure schematic diagram.
Fig. 2 is the packet floor diagram of steel-aluminum composite material.
Fig. 3 is the flat multiple bottom structure schematic diagram of the utility model.
Fig. 4 is the plate schematic diagram of steel-aluminum composite material.
Fig. 5 is the structural schematic diagram of pot body and ring set relative positional relationship.
In figure, 1, pot body;2, steel-aluminum composite material;3, packet bottom plate;4, plate steel-aluminum composite material;5, ring set.
Specific embodiment
It is specific embodiment of the utility model and in conjunction with attached drawing below, the technical solution of the utility model is made further Description, but the utility model is not limited to these examples.
1, firstly, selection and the steel-aluminum composite material 2 of the bottom of a pan plane corresponding size (flat of bottom visible Fig. 1 and Fig. 2), Or steel-aluminum composite material 2 is processed into (3 part of packet bottom plate of packet bottom plate 3 coincideing with its bottom of a pan size shape according to form of pot bottom It can be seen that Fig. 3 and Fig. 4), composite material aluminium layer face and 1 outer bottom of pot body are forged by soldering or heating and are compounded in the bottom of a pan plane On, the vertical edge on 3 periphery of packet bottom plate is because having aluminium layer that can firmly be compounded on the entire the bottom of a pan and the angle R, 3 plane of packet bottom plate and vertical edge It is compound full with 1 outer bottom surface of pot body, it is commonly called as " very packet bottom ".Due to using steel-aluminum composite material 2, stainless steel layer behind multiple bottom Surface essentially eliminates the defects of bulge, pad print, rosin joint, is also easy positioning for the composite plate at multiple bottom and the bottom of a pan, and only One brazing surface brazing flux solder coating quality and brazing temperature are also easy to control, this composite bottom aluminum pot simple process, cost bottom, matter Measure easily controllable, the compound fastness beauty in the bottom of a pan.
2, secondly, it is uniform in the entire outer bottom of pot body 1 including the angle R and 3 steel-aluminum composite material of packet bottom plate, 2 aluminium layer surface Aluminium base brazing flux solder is coated, packet bottom plate 3 is coincide on 1 outer bottom of pot body with positioning fixture after coating, passes through the weldering of solderer Connect or heat the entire the bottom of a pan surface for forging and packet bottom plate 3 being firmly compounded in pot body 1 including the angle R, compound full secured beauty, As a kind of composite bottom aluminum pot.
3, finally, by outside the aluminium layer surface of plate steel-aluminum composite material 42 corresponding with the bottom of a pan planar dimension and pot body 1 Bottom surface uniformly coats aluminium base brazing flux solder, is placed composite material positioning and 1 outer bottom table of pot body with locating check fixture after coating On face, is forged by Welding or heating, steel-aluminum composite material 2 is firmly compounded on the outer bottom of pot body 1, is become A kind of composite bottom aluminum pot.
As shown in figure 5, after clamping entire pot body 1 from hole and completing processing, it is also necessary to handle is assembled using the hole, but Be on handle for the bolt size that inserts in the hole may not equity just being capable of basis so joined several ring sets 5 in hole The size of bolt squeezes out undersized ring set 5, and (be shown from Fig. 5: bolt inserts in the hole from the right, then according to bolt Diameter, by the ring set 5 smaller than its diameter to the left side squeeze out.), and remaining inner most ring set 5 can cover handle just, Not will lead to handle loosening (if handle latch is smaller than the size in hole, will lead to handle and shakes in hole.), and consistency of thickness More there is planning afterwards, can preferably correspond to the model of handle.
It should be understood that in claims, specification of the utility model, all " including ... " should be understood as out The meaning of formula is put, that is, its meaning is equal to " at least containing ... ", but should not be understood as enclosed meaning, i.e. its meaning It should not be construed " only including ... ".
The specific embodiments described herein are merely examples of the spirit of the present invention.The utility model institute Belonging to those skilled in the art can make various modifications or additions to the described embodiments or using similar Mode substitute, but without departing from the spirit of the present application or beyond the scope of the appended claims.

Claims (4)

1. a kind of composite bottom aluminum pot, including pot body (1) and it is compounded in the multiple bottom of pot body (1) outer bottom, which is characterized in that multiple bottom is Steel-aluminum composite material (2), the multiple bottom are that the steel-aluminum composite material (2) that will be combined with each other in advance passes through soldering or heating The mode of forging is compounded on pot body (1) outer bottom.
2. a kind of composite bottom aluminum pot according to claim 1, which is characterized in that offered in the pot body (1) for adding Work clamps pot body (1) and assembles the hole of handle, is additionally provided with several ring sets (5) being mutually arranged two-by-two, the ring set in hole (5) in a ring and outer diameter, internal diameter are different, the internal diameter in two neighboring ring set (5) in outer ring ring set (5) in interior The outer diameter of ring set (5) matches, and the outer diameter of outermost layer ring set (5) and the size in hole match, the axial length of each ring set (5) Different, the axial length that the axial length ratio in outer ring ring set (5) is in inner ring ring set (5) is long, and each ring set (5) direction is cooked a meal Have an intrinsic side alignment Overlap design, other side due to axial length be differently formed it is ladder-like.
3. a kind of composite bottom aluminum pot according to claim 1 or 2, which is characterized in that the steel-aluminum composite material (2) is in Plate shaped, plate can cover the outer baseplane of entire pot body (1).
4. a kind of composite bottom aluminum pot according to claim 1 or 2, which is characterized in that the steel-aluminum composite material (2) is in By the stamping packet egative film shape holded up upwards at periphery of form of pot bottom, packet egative film can wrap up the entire the bottom of a pan and the bottom of a pan angular position R.
CN201721689114.7U 2017-12-07 2017-12-07 A kind of composite bottom aluminum pot Active CN208388440U (en)