CN207057811U - 钛材氩弧焊气保装置 - Google Patents

钛材氩弧焊气保装置 Download PDF

Info

Publication number
CN207057811U
CN207057811U CN201720666608.7U CN201720666608U CN207057811U CN 207057811 U CN207057811 U CN 207057811U CN 201720666608 U CN201720666608 U CN 201720666608U CN 207057811 U CN207057811 U CN 207057811U
Authority
CN
China
Prior art keywords
nozzle
ignition tip
interior
protection device
arc welding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201720666608.7U
Other languages
English (en)
Inventor
钱爱祥
许娟娟
张秋兵
刘亚飞
叶飞
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NANTONG EXCEL MACHINERY Co Ltd
Original Assignee
NANTONG EXCEL MACHINERY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NANTONG EXCEL MACHINERY Co Ltd filed Critical NANTONG EXCEL MACHINERY Co Ltd
Priority to CN201720666608.7U priority Critical patent/CN207057811U/zh
Application granted granted Critical
Publication of CN207057811U publication Critical patent/CN207057811U/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本实用新型公开了钛材氩弧焊气保装置,包括喷嘴、瓷嘴和导电嘴,所述瓷嘴通过螺纹套设在喷嘴外部,所述导电嘴的一端固定在喷嘴内部,所述喷嘴内部以导电嘴为中心设有8个呈环状排列的分流孔,喷嘴的端部为内设腔体的保护罩结构,且在端部设有2层200目的不锈钢丝网,所述导电嘴的另一端伸至喷嘴外。该装置有效隔绝了空气,气体分散更均匀,气流更稳定,起到了更好的保护作用,焊接效果很好。

Description

钛材氩弧焊气保装置
技术领域
本实用新型涉及焊接技术领域,具体是一种钛材氩弧焊气保装置。
背景技术
钛具有很强的化学活泼性,将钛置于空气中,其表面能迅速形成一层致密的氧化膜,随着温度的急剧升高,钛的活泼性也会急剧增加,并与空气中的氧发生剧烈反应,形成钛的氧化物,更高温度时,钛会吸收空气中的氢,氮等气体元素,最终使钛的塑性降低,冲击韧性急剧下降。在焊接过程中,当熔融态的钛暴露于空气中时,空气中的氧,氢,氮等元素会迅速与钛结合,形成脆性氧化物或氮化物,使焊缝金属塑性急剧下降,冲击韧性下降,严重时会发生脆断,所以,在钛材焊接时必须采用气体保护装置,以隔绝空气对焊缝金属的危害。
但是采用现有的气保装置焊出的焊缝往往颜色发蓝发灰,实际就是被严重氧化的结果,主要原因是喷嘴和瓷嘴的直径均较小,有效覆盖范围约20mm,这样,随着焊接进程的推进,当熔池尚未冷却时,气保已脱离熔池,导致熔态金属直接暴露于空气中,接收氧化反应;其次气体进入喷嘴进行分流后直达焊缝区时,气体分散不均,且气流不稳定,同样会对熔池的保护造成不好的影响。
实用新型内容
为解决上述问题,本实用新型提供一种钛材氩弧焊气保装置,有效隔绝了空气,气体分散更均匀,气流更稳定,起到了更好的保护作用,焊接效果很好。
本实用新型采用的技术方案是:钛材氩弧焊气保装置,包括喷嘴、瓷嘴和导电嘴,所述瓷嘴通过螺纹套设在喷嘴外部,所述导电嘴的一端固定在喷嘴内部,所述喷嘴内部以导电嘴为中心设有8个呈环状排列的分流孔,喷嘴的端部为内设腔体的保护罩结构,且在端部设有2层200目的不锈钢丝网,所述导电嘴的另一端伸至喷嘴外。
所述喷嘴的有效覆盖范围为60mm。
本实用新型的有益效果是:扩大喷嘴的有效覆盖范围,有效隔绝了空气;增加分流孔数量,圆孔排布更密集,同时在喷嘴的端部加设2层200目的不锈钢丝网,使气体分散更均匀,气流更稳定,起到了更好的保护作用,焊接效果很好。
附图说明
图1为本实用新型的结构示意图;
图2是图1的A-A向剖视图;
图3是瓷嘴的结构示意图;
其中:1、喷嘴,2、瓷嘴,3、导电嘴,4、分流孔,5、腔体,6、不锈钢丝网。
具体实施方式
为了加深对本实用新型的理解,下面将结合实施例和附图对本实用新型作进一步详述,该实施例仅用于解释本实用新型,并不构成对本实用新型的保护范围的限定。
如图1至图3所示,钛材氩弧焊气保装置,包括喷嘴1、瓷嘴2和导电嘴3,瓷嘴2通过螺纹套设在喷嘴1外部,导电嘴3的一端固定在喷嘴1内部,喷嘴1内部以导电嘴3为中心设有8个呈环状排列的分流孔4,喷嘴1的端部为内设腔体5的保护罩结构。增加分流用圆孔的数量,将原有的3个增至8个,圆孔排布更密集,且在喷嘴的端部设有2层200目的不锈钢丝网6,使气体分散更均匀,气流更稳定,起到了更好的保护作用;考虑到不锈钢丝网距离钨极太近,会被燃烧的可能,特地加长导电嘴,使导电嘴3的另一端伸至喷嘴1外,有效避免这一情况的发生。
该钛材氩弧焊气保装置加大了喷嘴和瓷嘴的内外径,同时也相应增加长度,使有效覆盖范围增至60mm,这样随着焊接进程的推进,前面熔池仍可在气保范围内进行冷却,有效隔绝了空气,当熔池温度降到一定时,再暴露于空气,这时空气对焊缝金属的影响已微乎其微。 评估采用该装置后的焊接效果,发现焊缝金属呈现银白色,有效杜绝了氧化,起到了更好的保护作用,焊接效果很好。

Claims (2)

1.钛材氩弧焊气保装置,其特征在于,包括喷嘴、瓷嘴和导电嘴,所述瓷嘴通过螺纹套设在喷嘴外部,所述导电嘴的一端固定在喷嘴内部,所述喷嘴内部以导电嘴为中心设有8个呈环状排列的分流孔,喷嘴的端部为内设腔体的保护罩结构,且在端部设有2层200目的不锈钢丝网,所述导电嘴的另一端伸至喷嘴外。
2.根据权利要求1所述的钛材氩弧焊气保装置,其特征在于,所述喷嘴的有效覆盖范围为60mm。
CN201720666608.7U 2017-06-09 2017-06-09 钛材氩弧焊气保装置 Active CN207057811U (zh)