CN207026471U - 防结瘤的连铸中间包水口座砖 - Google Patents
防结瘤的连铸中间包水口座砖 Download PDFInfo
- Publication number
- CN207026471U CN207026471U CN201720741260.3U CN201720741260U CN207026471U CN 207026471 U CN207026471 U CN 207026471U CN 201720741260 U CN201720741260 U CN 201720741260U CN 207026471 U CN207026471 U CN 207026471U
- Authority
- CN
- China
- Prior art keywords
- continuous casting
- brick cup
- conical bore
- intermediate inlet
- dross
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型属于炼钢厂连铸中间包水口座砖结构的改进,特别是一种防结瘤的连铸中间包水口座砖,包括在外壁上设置有装配凸台的连铸中间包水口座砖,连铸中间包水口座砖的内孔由上部的圆锥孔和连接在圆锥孔下部的圆柱孔构成,其中圆锥孔的上口直径为20cm,圆锥孔的下口直径为22cm,圆锥孔的长度为30cm,在连铸中间包水口座砖的上端面上设置着与水口砖相配合的倒圆锥形凹台。本实用新型结构合理,可以防止高熔点夹杂物在中间包水口座砖水口内壁上沉积和结瘤,保证连铸浇注的稳定性,保证连铸坯质量,提高连铸中间包使用寿命,可以降低职工劳动强度,提高工作效率,提高工作安全性。
Description
技术领域
本实用新型属于炼钢厂连铸中间包水口座砖结构的改进,特别是一种防结瘤的连铸中间包水口座砖。
背景技术
中包水口座砖的主要作用是: 支撑中包水口,是中间包钢水浇铸通道,将中间包钢水通过上水口注入结晶器,防止钢水二次氧化氮化和钢水的飞溅,可以调节钢水流动状态和注入速度,对连铸拉坯成材率和铸坯质量有决定性影响。
中包水口座砖内壁形式为直上直下圆筒状,在浇注过程中内壁容易形成高熔点夹杂物堆积,导致水口内壁集聚夹杂物,出现结瘤现象,造成连铸浇注中断,对连铸坯质量产生不利影响。
由于此种中包水口座砖的设计特点,使用过程水口座砖内壁容易形成高熔点复合夹杂物堆积,导致水口内部堵塞现象,对连铸正常浇注产生不利影响。
传统中包水口座砖存在的主要问题如下:
1、水口座砖内壁形式为直上直下圆筒状,在浇注过程中内壁容易形成高熔点夹杂物堆积,导致水口内壁出现结瘤现象,造成连铸浇注中断。
2、浇注过程中水口座砖内壁容易形成高熔点夹杂物堆积,对连铸坯质量产生不利影响。
3、影响正常的生产操作,职工劳动强度较高。
实用新型内容
本实用新型的目的在于提供一种防结瘤的连铸中间包水口座砖,其结构合理,可以防止高熔点夹杂物在中间包水口座砖水口内壁上沉积和结瘤,保证连铸浇注的稳定性,保证连铸坯质量,提高连铸中间包使用寿命,可以降低职工劳动强度,提高工作效率,提高工作安全性。
本实用新型的目的是这样实现的:一种防结瘤的连铸中间包水口座砖,包括在外壁上设置有装配凸台的连铸中间包水口座砖,连铸中间包水口座砖的内孔由上部的圆锥孔和连接在圆锥孔下部的圆柱孔构成,其中圆锥孔的上口直径为20cm,圆锥孔的下口直径为22cm,圆锥孔的长度为30cm,在连铸中间包水口座砖的上端面上设置着与水口砖相配合的倒圆锥形凹台。
主要设计内容如下:
将连铸中包水口座砖内壁设计为上小下大的喇叭口形状,正常浇注时在吹气管内通入氩气,氩气从耐火材料内部溢入上水口座砖内壁,在上水口座砖内壁形成一圈氩气膜,防止高熔点夹杂物在上水口座砖内壁的沉积和集聚,从而防止产生浇铸过程结瘤现象。
改进效果
1、新型设计的连铸中包水口座砖在水口座砖内壁形成一圈氩气膜,防止高熔点夹杂物在上水口座砖内壁的沉积和集聚,连铸浇注过程稳定性提高。
2、浇注过程中中包水口座砖内壁不容易形成高熔点夹杂物堆积,不会带入连铸坯中对连铸坯质量产生不利影响。
3、连铸生产操作稳定性提高,可以改善职工的劳动条件,降低劳动强度。
4、连铸中包使用寿命提高,降低了非正常消耗,可以降低生产成本。
本实用新型结构合理,防止了高熔点夹杂物在中间包水口座砖水口内壁上沉积和结瘤,保证了连铸浇注的稳定性,保证了连铸坯质量,提高了连铸中间包使用寿命,降低了职工劳动强度,提高了工作效率,提高了工作安全性。
附图说明
下面将结合附图对本实用新型做进一步的描述,图1为本实用新型剖视结构示意图。
具体实施方式
一种防结瘤的连铸中间包水口座砖,如图1所示,包括在外壁上设置有装配凸台2的连铸中间包水口座砖1,连铸中间包水口座砖1的内孔由上部的圆锥孔3和连接在圆锥孔3下部的圆柱孔4构成,其中圆锥孔3的上口直径为20cm,圆锥孔3的下口直径为22cm,圆锥孔3的长度为30cm,在连铸中间包水口座砖1的上端面上设置着与水口砖相配合的倒圆锥形凹台5。
Claims (1)
1.一种防结瘤的连铸中间包水口座砖,包括在外壁上设置有装配凸台(2)的连铸中间包水口座砖(1),其特征是:连铸中间包水口座砖(1)的内孔由上部的圆锥孔(3)和连接在圆锥孔(3)下部的圆柱孔(4)构成,其中圆锥孔(3)的上口直径为20cm,圆锥孔(3)的下口直径为22cm,圆锥孔(3)的长度为30cm,在连铸中间包水口座砖(1)的上端面上设置着与水口砖相配合的倒圆锥形凹台(5)。