CN206953766U - High-precision silk screen printing template - Google Patents
High-precision silk screen printing template Download PDFInfo
- Publication number
- CN206953766U CN206953766U CN201720714046.9U CN201720714046U CN206953766U CN 206953766 U CN206953766 U CN 206953766U CN 201720714046 U CN201720714046 U CN 201720714046U CN 206953766 U CN206953766 U CN 206953766U
- Authority
- CN
- China
- Prior art keywords
- steel wire
- parallel
- district
- warp
- wire
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model discloses a kind of high-precision silk screen printing template, including silk-screen half tone and Flocked fabric, the silk-screen half tone further comprises that frame, some parallel and spaced steel wire warps be parallel with some and spaced steel wire parallel, the steel wire warp and steel wire parallel are alternately knitted to form grid regions, the grid regions are covered with glued membrane, and several window regions are provided with the glued membrane;Grid regions further comprise wire jumper sub-district and non-wire jumper sub-district, and more than the second interval of steel wire parallel corresponding to non-wire jumper sub-district or steel wire warp, the window region is located in wire jumper sub-district at the first interval of the either steel wire warp of the steel wire parallel in the wire jumper sub-district.The utility model high-precision silk screen printing template effectively prevent the node between steel wire warp and steel wire parallel, greatly reduce the probability for broken string and empty print occur, and printing is uniform, and printing precision is high.
Description
Technical field
A kind of high-precision silk screen printing template is the utility model is related to, belongs to precise silk screen printing technology.
Background technology
Silk-screen printing is will to scribble photosensitive material wrist chip base light-sensitive surface to lie on work top up, by taut good wrist net
Frame is lain in chip base, be then put into screen frame it is photosensitive starch and use soft scraper plate press coatings, through dry it is abundant after throw off modeling
Tablet base, it is attached to light-sensitive surface cirri net and can be used to printing down, silk-screen half tone is just made after developed, dry.
With the development of science and technology, this green energy of solar energy is being widely used in production, life etc.
Every field.Traditional solar energy positive electrode silk screen plate is tied because the point of intersection of the warp and weft of silk screen plate has net so that
Otherwise the existing thin grid line line width limit of solar energy easily causes printing broken string or uneven, makes solar energy at 50 μm or so
The conversion efficiency of silicon cell can not obtain.
The content of the invention
The utility model purpose is to provide a kind of high-precision silk screen printing template, and the high-precision silk screen printing template is effectively kept away
The node between steel wire warp and steel wire parallel is exempted from, has greatly reduced the probability for broken string and empty print occur, printing is uniform, printing
Precision is high.
To reach above-mentioned purpose, the technical solution adopted in the utility model is:A kind of high-precision silk screen printing template, including
Silk-screen half tone and Flocked fabric, the silk-screen half tone further comprise frame, some parallel and spaced steel wire warps
Parallel with some and spaced steel wire parallel, the steel wire warp and steel wire parallel are alternately knitted to form grid regions,
The grid regions are covered with glued membrane, and several window regions are provided with the glued membrane, and the window region has steel wire parallel or steel wire warp
Line;
The grid regions further comprise wire jumper sub-district and non-wire jumper sub-district, steel wire parallel in the wire jumper sub-district or
First interval of steel wire warp is more than the second interval of the steel wire parallel or steel wire warp corresponding to non-wire jumper sub-district, the window
Mouth region is located in wire jumper sub-district, and the width of this window region is less than the width x length at corresponding first interval.
Further improved scheme is as follows in above-mentioned technical proposal:
1. in such scheme, the steel wire warp and steel wire parallel are located at the top of glued membrane.
2. in such scheme, a diameter of 10 ~ 25 μm of the steel wire warp and steel wire parallel.
3. in such scheme, the adjacent steel wire warp at intervals of 50 ~ 100 μm, the interval of the adjacent steel wire parallel
For 50 ~ 100 μm.
4. in such scheme, first at intervals of the second 2 ~ 5 times of interval in non-wire jumper sub-district in the wire jumper sub-district.
Because above-mentioned technical proposal is used, the utility model has following advantages and effect compared with prior art:
The utility model high-precision silk screen printing template, several window regions is provided with its glued membrane, the window region has
Steel wire parallel or steel wire warp, grid regions further comprise wire jumper sub-district and non-wire jumper sub-district, the steel wire in the wire jumper sub-district
Parallel either steel wire warp first interval be more than non-wire jumper sub-district corresponding to steel wire parallel or steel wire warp second between
Every the window region is located in wire jumper sub-district, and the width of this window region is less than the width x length at corresponding first interval, effectively keeps away
The node between steel wire warp and steel wire parallel is exempted from, has greatly reduced the probability for broken string and empty print occur, printing is uniform, printing
Precision is high, improves the conversion efficiency of cell piece and improves the utilization rate of cell piece anode sizing agent, reduces the consumption of silver paste.
Brief description of the drawings
Accompanying drawing 1 is the utility model high-precision silk screen printing formwork structure schematic diagram.
In the figures above:1st, wire jumper sub-district;2nd, non-wire jumper sub-district;3rd, frame;4th, steel wire warp;5th, steel wire parallel;6、
Glued membrane;7th, window region;8th, grid regions.
Embodiment
The utility model is further described with reference to embodiment:
Embodiment 1:A kind of high-precision silk screen printing template, including silk-screen half tone 1 and Flocked fabric 2, the silk-screen half tone 1 enter
One step includes that frame 3, some parallel and spaced steel wire warps 4 are parallel with some and spaced steel wire latitude
Line 5, the steel wire warp 4 and steel wire parallel 5 are alternately knitted to form grid regions 8, and the grid regions 8 are covered with glued membrane 6, the glue
Several window regions 7 are provided with film 6, the window region 7 has steel wire parallel 5 or steel wire warp 4;
The grid regions 8 further comprise wire jumper sub-district 1 and non-wire jumper sub-district 2, the steel wire parallel in the wire jumper sub-district 1
5 either steel wire warp 4 first interval be more than non-wire jumper sub-district 2 corresponding to steel wire parallel 5 or steel wire warp 4 second between
Every the window region 7 is located in wire jumper sub-district 1, and the width of this window region 7 is less than the width x length at corresponding first interval.
Above-mentioned steel wire warp 4 and steel wire parallel 5 are located at the top of glued membrane 6.
A diameter of 12 μm of above-mentioned steel wire warp 4 and steel wire parallel 5.
The adjacent steel wire warp 4 at intervals of 60 μm, the adjacent steel wire parallel 5 at intervals of 60 μm.
First at intervals of the second 3 times of interval in non-wire jumper sub-district 2 in above-mentioned wire jumper sub-district 1.
Embodiment 2:A kind of high-precision silk screen printing template, including silk-screen half tone 1 and Flocked fabric 2, the silk-screen half tone 1 enter
One step includes that frame 3, some parallel and spaced steel wire warps 4 are parallel with some and spaced steel wire latitude
Line 5, the steel wire warp 4 and steel wire parallel 5 are alternately knitted to form grid regions 8, and the grid regions 8 are covered with glued membrane 6, the glue
Several window regions 7 are provided with film 6, the window region 7 has steel wire parallel 5 or steel wire warp 4;
The grid regions 8 further comprise wire jumper sub-district 1 and non-wire jumper sub-district 2, the steel wire parallel in the wire jumper sub-district 1
5 either steel wire warp 4 first interval be more than non-wire jumper sub-district 2 corresponding to steel wire parallel 5 or steel wire warp 4 second between
Every the window region 7 is located in wire jumper sub-district 1, and the width of this window region 7 is less than the width x length at corresponding first interval.
Above-mentioned steel wire warp 4 and steel wire parallel 5 are located at the top of glued membrane 6.
A diameter of 15 μm of above-mentioned steel wire warp 4 and steel wire parallel 5.
The adjacent steel wire warp 4 at intervals of 90 μm, the adjacent steel wire parallel 5 at intervals of 90 μm.
First at intervals of the second 4 times of interval in non-wire jumper sub-district 2 in above-mentioned wire jumper sub-district 1.
During using above-mentioned high-precision silk screen printing template, several window regions are provided with its glued membrane, the window region has
Steel wire parallel or steel wire warp, grid regions further comprise wire jumper sub-district and non-wire jumper sub-district, the steel wire in the wire jumper sub-district
Parallel either steel wire warp first interval be more than non-wire jumper sub-district corresponding to steel wire parallel or steel wire warp second between
Every the window region is located in wire jumper sub-district, and the width of this window region is less than the width x length at corresponding first interval, effectively keeps away
The node between steel wire warp and steel wire parallel is exempted from, has greatly reduced the probability for broken string and empty print occur, printing is uniform, printing
Precision is high, improves the conversion efficiency of cell piece and improves the utilization rate of cell piece anode sizing agent, reduces the consumption of silver paste.
For above-described embodiment only to illustrate technical concepts and features of the present utility model, its object is to allow be familiar with technique
Personage can understand content of the present utility model and implement according to this, the scope of protection of the utility model can not be limited with this.
All equivalent change or modifications made according to the utility model Spirit Essence, should all cover the scope of protection of the utility model it
It is interior.
Claims (5)
- A kind of 1. high-precision silk screen printing template, it is characterised in that:Including frame(3), some it is parallel and spaced Steel wire warp(4)Parallel with some and spaced steel wire parallel(5), the steel wire warp(4)With steel wire parallel(5)Hand over Grid regions are knitted to form wrongly(8), the grid regions(8)It is covered with glued membrane(6), the glued membrane(6)On be provided with several window regions (7), the window region(7)With steel wire parallel(5)Or steel wire warp(4);The grid regions(8)Further comprise wire jumper sub-district(1)With non-wire jumper sub-district(2), the wire jumper sub-district(1)Interior steel wire Parallel(5)Or steel wire warp(4)First interval be more than non-wire jumper sub-district(2)Corresponding steel wire parallel(5)Or steel wire warp Line(4)Second interval, the window region(7)Positioned at wire jumper sub-district(1)It is interior, this window region(7)Width be less than corresponding the The width x length at one interval.
- 2. high-precision silk screen printing template according to claim 1, it is characterised in that:The steel wire warp(4)And steel wire Parallel(5)Positioned at glued membrane(6)Top.
- 3. high-precision silk screen printing template according to claim 1, it is characterised in that:The steel wire warp(4)And steel wire Parallel(5)A diameter of 10 ~ 25 μm.
- 4. high-precision silk screen printing template according to claim 1, it is characterised in that:The adjacent steel wire warp(4)'s At intervals of 50 ~ 100 μm, the adjacent steel wire parallel(5)At intervals of 50 ~ 100 μm.
- 5. high-precision silk screen printing template according to claim 1, it is characterised in that:The wire jumper sub-district(1)Interior first At intervals of non-wire jumper sub-district(2)Interior second 2 ~ 5 times of interval.