CN206810871U - A kind of wire-drawing die for improving steel wire exhaustion creep - Google Patents

A kind of wire-drawing die for improving steel wire exhaustion creep Download PDF

Info

Publication number
CN206810871U
CN206810871U CN201720303584.9U CN201720303584U CN206810871U CN 206810871 U CN206810871 U CN 206810871U CN 201720303584 U CN201720303584 U CN 201720303584U CN 206810871 U CN206810871 U CN 206810871U
Authority
CN
China
Prior art keywords
area
steel wire
main body
surface diameter
die main
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201720303584.9U
Other languages
Chinese (zh)
Inventor
朱君健
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Qidong Haina Special Steel Co Ltd
Original Assignee
Qidong Haina Special Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Qidong Haina Special Steel Co Ltd filed Critical Qidong Haina Special Steel Co Ltd
Priority to CN201720303584.9U priority Critical patent/CN206810871U/en
Application granted granted Critical
Publication of CN206810871U publication Critical patent/CN206810871U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses a kind of wire-drawing die for improving steel wire exhaustion creep, including die main body, die main body is cylindrical structure, inner core is provided with the center of die main body, inner core is from top to bottom successively by inlet region, lubricate area, compressional zone, sizing area and outlet area composition, the bottom surface of inlet region is identical with the upper bottom surface diameter in lubrication area, the bottom surface for lubricating area is identical with the upper bottom surface diameter of compressional zone, lubricate the bottom surface in area, the cross section of sizing area and the upper bottom surface diameter all same of outlet area, the Reduction per draft of die main body is 20 24%, the calculation formula of Reduction per draft is (1 (d/d0)2) × 100%, wherein d are the upper surface diameter of outlet area, and d0 is the upper surface diameter of compressional zone.The utility model enhances the antifatigue croop property of steel wire with the workload during reducing Production for Steel Wire and activity duration, the advantages of improving product quality and production efficiency.

Description

A kind of wire-drawing die for improving steel wire exhaustion creep
Technical field
It the utility model is related to a kind of Production for Steel Wire accessory, and in particular to a kind of wire drawing die for improving steel wire exhaustion creep Tool.
Background technology
Spring steel wire used in being engaged in the technological requirement of spring production must have very good antifatigue creep properties Can, i.e., kept after spring steel wire wound into spring in exhaustion creep experiment and routine use is carried out its good mechanical performance and Size, will not occur a problem that camber of spring, shorten because of long-term use of.
The cold-drawing process of steel wire, it is the wire drawing by steel wire from definite shape and size by the tractive force of equipment reel Pulled out in die hole, so as to produce the merchant wire of various cross dimensions, due to finished size compared with scantling diameter difference compared with Greatly, so thicker material could be drawn into thinner product by the drawing of multi-pass by being typically necessary, and per drawing together Special ratios between the outlet steel wire diameter d and entrance steel wire diameter d0 of silk mould, referred to as passage draft or shout secondary Compression ratio.In existing steel wire production process, the Reduction per draft of spring steel wire is generally 12-23% during the design of wire-drawing die , final pass compression ratio is generally no greater than 17%.But such set causes what existing drawing process was produced Spring steel wire situation bad through often there is antifatigue croop property after wound into spring.
Utility model content
The purpose of this utility model is to solve deficiency of the prior art, there is provided one kind is reduced during Production for Steel Wire Workload and the activity duration, while enhance the antifatigue croop property of steel wire, what is improved product quality and production efficiency changes The wire-drawing die of kind steel wire exhaustion creep.
Technical scheme:A kind of wire-drawing die for improving steel wire exhaustion creep described in the utility model, including die main body, Die main body is cylindrical structure, inner core is provided with the center of die main body, inner core is from top to bottom successively by inlet region, lubrication Area, compressional zone, sizing area and outlet area composition, inlet region, lubrication area, compressional zone, sizing area and outlet area are coaxial, and sizing area is Cylindrical structure, inlet region, lubrication area, compressional zone and outlet area are frustum cone structure, the bottom surface of inlet region and lubrication area it is upper Basal diameter is identical, and it is identical with the upper bottom surface diameter of compressional zone to lubricate the bottom surface in area, lubricates bottom surface, the horizontal stroke of sizing area in area Section and the upper bottom surface diameter all same of outlet area, the Reduction per draft of die main body are 20-24%, the calculating of Reduction per draft Formula is (1- (d/d0)2) × 100%, wherein d are the upper surface diameter of outlet area, and d0 is the upper surface diameter of compressional zone.
Further, the material of die main body is hard alloy or diamond.
The utility model has advantages below compared with prior art:From the passage pressure of technique source adjustment die main body 6 Shrinkage is 20-24%, and the antifatigue croop property for the steel wire produced effectively is improved, and enhances the antifatigue creep of steel wire Performance, improve product quality and production efficiency, while reduce the workload during Production for Steel Wire and activity duration.
Brief description of the drawings
Fig. 1 is sectional view of the present utility model.
Label in figure:1- inlet regions, 2- lubrications area, 3- compressional zones, 4- sizing areas, 5- outlet areas, 6- die main bodies, in 7- Core.
Embodiment
In order to deepen understanding of the present utility model, below we will the utility model is described in further detail with reference to accompanying drawing, The embodiment is only used for explaining the utility model, does not form the restriction to scope of protection of the utility model.
As Fig. 1 shows a kind of a kind of embodiment for the wire-drawing die for improving steel wire exhaustion creep of the utility model, bag Die main body 6 is included, the die main body 6 is cylindrical structure, and inner core 7, the inner core are provided with the center of the die main body 6 7 are made up of inlet region 1, lubrication area 2, compressional zone 3, sizing area 4 and outlet area 5 successively from top to bottom, the inlet region 1, lubrication Area 2, compressional zone 3, sizing area 4 and outlet area 5 are coaxial, and the sizing area 4 is cylindrical structure, the inlet region 1, lubrication area 2, is pressed Contracting area 3 and outlet area 5 are frustum cone structure, and the bottom surface of the inlet region 1 is identical with the upper bottom surface diameter in lubrication area 2, described The bottom surface in lubrication area 2 is identical with the upper bottom surface diameter of compressional zone 3, the bottom surface in the lubrication area 2, the cross section of sizing area 4 With the upper bottom surface diameter all same of outlet area 5, the Reduction per draft of the die main body 6 is 20-24%, the Reduction per draft Calculation formula be (1- (d/d0)2) × 100%, wherein d are the upper surface diameter of outlet area 5, and d0 is the upper surface of compressional zone 3 Diameter, the material of die main body 6 is hard alloy or diamond.
Inlet region 1, conveniently thread and prevent steel wire from abrading wire drawing die from Way in;Area 2 is lubricated, makes steel wire easy by it In bringing lubricant into;Compressional zone 3, the deformation process of steel wire are carried out herein, i.e., original section is reduced to required section Size;The effect of sizing area 4 is to obtain the accurate size for being drawn steel wire;Outlet area 5 is to be used to prevent steel wire from going out dipped ring Surely scratch Steel Wire Surface.
The utility model has advantages below compared with prior art:The utility model adjusts die main body from technique source 6 Reduction per draft is 20-24%, and the antifatigue croop property for the steel wire produced effectively is improved, and enhances steel wire Antifatigue croop property, improves product quality and production efficiency, while when reducing the workload during Production for Steel Wire and operation Between.
Above-mentioned embodiment, only illustrate technical concept and architectural feature of the present utility model, it is therefore intended that allow ripe Knowing the stakeholder of technique can implement according to this, but above content is not intended to limit the scope of protection of the utility model, every Any equivalent change or modification made according to Spirit Essence of the present utility model, all should fall into the scope of protection of the utility model Within.

Claims (2)

  1. A kind of 1. wire-drawing die for improving steel wire exhaustion creep, it is characterised in that:Including die main body (6), the die main body (6) be cylindrical structure, be provided with inner core (7) at the center of the die main body (6), the inner core (7) from top to bottom successively by Inlet region (1), lubrication area (2), compressional zone (3), sizing area (4) and outlet area (5) composition, the inlet region (1), lubrication area (2), coaxially, the sizing area (4) is cylindrical structure for compressional zone (3), sizing area (4) and outlet area (5), the inlet region (1), It is frustum cone structure to lubricate area (2), compressional zone (3) and outlet area (5), bottom surface and lubrication area (2) of the inlet region (1) Upper bottom surface diameter is identical, and the bottom surface of lubrication area (2) is identical with the upper bottom surface diameter of compressional zone (3), lubrication area (2) Bottom surface, the cross section of sizing area (4) and the upper bottom surface diameter all same of outlet area (5), the passage of the die main body (6) Compression ratio is 20-24%, and the calculation formula of the Reduction per draft is (1- (d/d0)2) × 100%, wherein d are outlet area (5) Upper surface diameter, d0 be compressional zone (3) upper surface diameter.
  2. A kind of 2. wire-drawing die for improving steel wire exhaustion creep according to claim 1, it is characterised in that:The mould master The material of body (6) is hard alloy or diamond.
CN201720303584.9U 2017-03-27 2017-03-27 A kind of wire-drawing die for improving steel wire exhaustion creep Active CN206810871U (en)