CN206556959U - The eight word die trials detected for bitumen ductility - Google Patents
The eight word die trials detected for bitumen ductility Download PDFInfo
- Publication number
- CN206556959U CN206556959U CN201720238514.XU CN201720238514U CN206556959U CN 206556959 U CN206556959 U CN 206556959U CN 201720238514 U CN201720238514 U CN 201720238514U CN 206556959 U CN206556959 U CN 206556959U
- Authority
- CN
- China
- Prior art keywords
- plate
- submodule
- shape
- fixed block
- bitumen ductility
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model discloses a kind of eight word die trials detected for bitumen ductility, including Contraband shape bottom plate, bottom plate is provided with alignment pin;A pair of end plate, the relative recess for being provided with a L-shaped in both sides of the opposite one end of the end plate;A pair of side plates, the relative convex portion for being provided with a L-shaped in two ends for the side that the side plate mutually deviates from, the convex portion and the structure matching of the recess, are moved towards, eight type matrix chambers of the end plate and the side plate one closing of formation with limiting the side plate;The side plate includes fixed block, and fixed block is provided with a groove, and one vertical cross-section of the groove formation is stair-stepping mortise;Side form block, including multiple submodule overlapping from top to bottom, length of the submodule along baseplate width direction increase successively from top to bottom, form the structure matching of tenon, tenon and mortise, so that the side form block is contradicted in the groove of fixed block.The utility model, which has, improves bitumen ductility detection sample preparation qualification rate, improves the beneficial effect of bitumen ductility detection efficiency.
Description
Technical field
The utility model is related to bitumen ductility detection field.More specifically, the utility model is related to a kind of for pitch
Eight word die trials of ductility detection.
Background technology
The word die trial of pitch eight is widely used in highway engineering construction experiment, construction of railway project experiment, construction site engineering
Construction test, Concrete Mixing Station experiment, building engineering quality supervision experiment, and various universities and colleges, scientific research institution, water
Sharp engineering etc. is tested, and eight word die trials coat interleaving agent using the preceding inner surface in bottom plate and two side forms, then will constitute eight words
Each part of die cavity is assembled, and is then carefully come and gone sample for several times in slowly injection mould from one end of die trial to the other end, most
Die trial is slightly higher than afterwards, test specimen cools down 30~40min at room temperature, in the Water Tank with Temp.-controlled for being subsequently placed in regulation test temperature, keep
After 30min take out, the pitch for being higher by die trial is struck off with hot scraper, bituminous sheaths is flushed with die trial face, by die trial together with bottom plate again
1~1.5h in the tank of immersion regulation test temperature, then test specimen after insulation is moved into the tank of ductility machine, take together with bottom plate
The hole of two end plates is respectively fitted on the metal column of slide plate and groove end fixed plate after lower shoe, two side plates is then removed, opens
Dynamic ductility machine is detected, because the interleaving agent being coated on two side plates can be because of Action of Gravity Field toward dirty so that two side plates
On interleaving agent be lost in, because cohesive action can usually destroy the test specimen of good heat insulation when causing to remove two side plates, and can not
Continue ductility detection experiment, the qualification rate of sample is low, remakes sample for examination, it is necessary to take considerable time and energy, examines
Survey efficiency low.
Utility model content
A purpose of the present utility model is to solve at least the above, and provides the advantage that at least will be described later.
The utility model also has a purpose to be to provide a kind of eight word die trials detected for bitumen ductility, can make two
The interleaving agent of side plate be lost in it is few, be divided to multistep to take out two side plates and reduce the bitumen samples cohesive action that is subject to during single taking-up from
And improve bitumen ductility detection sample and prepare qualification rate, improve the beneficial effect of pitch bitumen ductility detection efficiency.
Bitumen ductility detection is used for there is provided one kind according to these purposes of the present utility model and further advantage in order to realize
Eight word die trials, including:
Contraband shape bottom plate, the bottom plate is provided with alignment pin;
A pair of end plate, its relative two ends for being fastened on the bottom plate, opposite one end of the end plate is provided with class arc groove,
Two end moulds of eight type matrix chambers are formed, the other end is provided with through hole, and the both sides of the opposite one end of the end plate are provided with a L-shaped relatively
Recess;
A pair of side plates, its relative is fastened on the bottom plate is located between the end plate, and the opposite side of the side plate is set
There is the sharp portion that width is successively decreased by centre to two ends, form the side form of eight type matrix chambers, opposite side is locked with alignment pin, the side plate
The relative convex portion for being provided with a L-shaped in the two ends of the side mutually deviated from, the convex portion and the structure matching of the recess, it is described to limit
Side plate is moved towards, eight type matrix chambers of the end plate and the side plate one closing of formation;
Wherein, the side plate includes:
Fixed block, it is in cuboid, and one side and the alignment pin of the fixed block are locked, and the fixed block is provided with one
Groove, one vertical cross-section of the groove formation is stair-stepping mortise;
Side form block, it includes from top to bottom overlapping multiple submodule successively, and the submodule is along the baseplate width
The length in direction increases successively from top to bottom, forms tenon, the structure matching of the tenon and the mortise, so that the side form
Block is contradicted in the groove of the fixed block, and side of the submodule away from the fixed block is set to the corner block of isosceles
Shape.
Preferably, the submodule is spliced by two axisymmetric L like shape parts, and the L like shape part is by more
Individual L like shape plate is spliced successively, and the L like shape plate includes integrally formed long slab and short slab, and the long slab side is set to
Inclined-plane, opposite side are provided with the breach stretched into for the short slab of adjacent L like shape plate, and the inclined-plane of multiple L like shape plates forms described
Sharp portion.
Preferably, the side of the bottom plate is relative provided with two alignment pins.
Preferably, the submodule is three, and the L like shape part is spliced successively by four L like shape plates.
Preferably, the material of the bottom plate, the end plate and the side plate is copper material or stainless steel.
Preferably, the roughness of the L like shape plate outer surface is less than 0.1 μm.
Preferably, length difference of the two neighboring submodule along the baseplate width direction is more than 5mm.
The utility model at least includes following beneficial effect:
Firstth, the defect that the interleaving agent being applied on two side plates can be overcome to be lost in due to Action of Gravity Field, point multistep
Two side plates are taken out, the bitumen samples cohesion being subject to when single takes out can be reduced, to avoid sample deformation, so as to improve drip
Blue or green ductility detection sample prepares qualification rate, improves the effect of pitch bitumen ductility detection efficiency;
Secondth, the structure matching of the L-shaped convex portion on L-shaped recess and a pair of side plates in a pair of end plate, can make side plate tight
It is close to be stuck on end plate, it is to avoid during splicing eight word die trial of pitch, two side plates are moved towards, eight type matrixes for surrounding end plate and side plate
Inner cavity surface linking is more smooth, so that the bitumen ductility specimen size more standard that this eight words die trial is produced, improves inspection
Survey accuracy rate;
3rd, when liquid phase is immersion fluid for solid, the surface tension of liquid, cohesive force and adhesive force it is common
Effect enables liquid to be attached to the surface of solids, the rubber membrane of the similar tensioning of liquid surface, if liquid level is bending, it just has change
Flat trend, therefore the side form block for forming side plate is divided into multiple submodule, can each submodule side wall and up and down
Surface smear interleaving agent, interleaving agent is made up of oily substance more, is immersion fluid for submodule, can be attached to it
Surface, and when interleaving agent has the trend moved down due to Action of Gravity Field, positioned at the interleaving agent pair of submodule upper and lower surface
It has pulling force effect, so that interleaving agent rests on submodule surface, overcomes what interleaving agent was lost in due to Action of Gravity Field to lack
Fall into, reduce the cohesion between bitumen samples and submodule, contribute to the dismounting of submodule;
The 4th, stair-stepping mortise is set on fixed block, and provided with the tenon with mortise structure matching on side form block,
Side form block can be made closely to be buckled on fixed block, so that the word die trial of pitch eight splicing is even closer, firm, made using it
When making bitumen ductility detection sample, sample more standard improves Detection accuracy.
Further advantage of the present utility model, target and feature embody part by following explanation, and part will also pass through
Research of the present utility model and practice are understood by the person skilled in the art.
Brief description of the drawings
Fig. 1 is overall structure top view of the present utility model;
Fig. 2 is the structural representation of end plate;
Fig. 3 is the structural representation of side plate;
Fig. 4 is the structural representation of fixed block;
Fig. 5 is the vertical cross-section view of fixed block;
Fig. 6 is the structural representation of side form block;
Fig. 7 is the structural representation of submodule;
Fig. 8 is the structural representation of L like shape part;
Fig. 9 is the schematic diagram of L like shape plate.
Embodiment
The utility model is described in further detail below in conjunction with the accompanying drawings, to make those skilled in the art with reference to explanation
Book word can be implemented according to this.
As shown in Fig. 1~9, the utility model provides a kind of eight word die trials detected for bitumen ductility, including:
Contraband shape bottom plate 1, the bottom plate 1 is provided with alignment pin 11;
As shown in Fig. 1 and Fig. 2, a pair of end plate 2, its relative two ends for being fastened on the bottom plate 1, the end plate 2 is opposite
One end be provided with class arc groove 22, form two of eight type matrix chambers end moulds, the other end is provided with through hole 23, and the end plate 2 is opposite
One end the relative recess 21 for being provided with a L-shaped in both sides;
As shown in Fig. 1 and Fig. 3, a pair of side plates, its relative is fastened on the bottom plate 1 is located between the end plate 2, institute
State the opposite side of side plate and be provided with the sharp portion 32 that width is successively decreased by centre to two ends, form the side form of eight type matrix chambers, opposite side
Locked with alignment pin 11, as shown in Figure 3, the relative convex portion 31 for being provided with a L-shaped in two ends for the side that the side plate mutually deviates from, institute
The structure matching of convex portion 31 and the recess 21 is stated, is moved towards with limiting the side plate, the end plate 2 and the side plate are formed
Eight type matrix chambers of one closing;
Wherein, the side plate includes:
Go out as shown in Figure 4 and Figure 5, fixed block 4, it is in cuboid, one side and the alignment pin 11 of the fixed block 4
Locking, the fixed block 4 is provided with a groove 41, and one vertical cross-section of the formation of groove 41 is stair-stepping mortise;
As shown in Fig. 6~7, side form block, it includes from top to bottom overlapping multiple submodule successively, and the submodule
Length along the width of bottom plate 1 increases successively from top to bottom, forms tenon, the structure of the tenon and the mortise
Match somebody with somebody, so that the side form block is contradicted in the groove 41 of the fixed block 4, side of the submodule away from the fixed block 4
The triangle for being set to isosceles is block.
In the above-mentioned technical solutions, the first step, smear interleaving agent in submodule upper and lower surface and bottom plate 1 in advance, then will
Submodule overlaps successively, and forms the side alignment of sharp portion 32, is thusly-formed after two side form blocks, then by side form block
The side for forming tenon is extend into the groove 41 of fixed block 4, side form block is closely joined together with fixed block 4 and is formd side
Plate, splices good another block of side plate, interleaving agent is also coated in the sharp portion 32 of side plate according to the method described above, then a pair of side plates is relative
It is placed on bottom plate 1, and fixed block 4 is located at the position that alignment pin 11 is locked, a pair of end plate 2 is then placed on bottom plate relatively
On 1, and make the convex portion 31 of the corresponding L-shaped being caught on side plate of recess 21 of L-shaped on end plate 2, then by alignment pin 11 and fixed block 4
Locking, completes the splicing of eight word die trials;
Secondth, pitch is slowly injected into eight word die trials, when can remove side plate, first unlocked alignment pin 11, then will
Bottom plate 1 is removed, after the fixed plate 4 that both sides are removed successively, removes the submodule for forming side form block successively from bottom to up, completes to remove
After can carry out ductility and have detected;
Interleaving agent is made up of oily substance more, such as machine oil is immersion fluid for submodule, can be attached to
Its surface, and when interleaving agent has the trend moved down due to Action of Gravity Field, positioned at the interleaving agent of submodule upper and lower surface
There is pulling force effect to it, so that interleaving agent is rested on submodule, make up that interleaving agent is lost in due to Action of Gravity Field lacks
Fall into, reduce the cohesion between bitumen samples and submodule, contribute to the dismounting of submodule, reduce when side plate is removed and pitch is tried
The damage block of sample, can improve the qualification rate of bitumen samples making;
Side form block be divide into multiple submodule, side plate can be made to be divided into many parts and taken out respectively, lifting surface area is reduced, can
To reduce the cohesion of side plate and bitumen samples when single takes out, sample deformation can be avoided during dismounting, to improve bitumen samples
Qualification rate;
Go out as shown in Figures 2 and 3, the structure matching of the L-shaped convex portion 31 on L-shaped recess 21 and side plate on end plate 2 can
So that side plate is closely stuck on end plate 2, it is to avoid two side plates for forming eight type matrix chambers are moved towards, and surround end plate 2 and side plate
The linking of eight type matrix inner cavity surfaces it is more smooth, contribute to the bitumen ductility detection sample more standard that this eight words die trial produces,
Improve Detection accuracy.
In another technical scheme, as shown in Fig. 7~9, the submodule is spelled by two axisymmetric L like shape parts
Connect and form, the L like shape part is spliced successively by multiple L like shape plates, the L like shape plate includes integrally formed long slab 62
With short slab 61, the side of long slab 62 is set to inclined-plane 63, opposite side and is provided with for lacking that the short slab 61 of adjacent L like shape plate is stretched into
Mouthful, the inclined-plane 63 of multiple L like shape plates forms the sharp portion 32.
In the above-mentioned technical solutions, first spliced with multiple L like shape plates, the short slab 61 of L like shape plate extend into adjacent thereto
In breach on plank, and the structure of short slab 61 and breach is just matched, and can so make the long slab 62 of adjacent two blocks of L like shape plates
Closely it is stitched together, two L like shape parts is spliced according to the method described above, then by two L like shape portion axial symmetry splicings one
Rise, form a submodule, multiple submodule is all spliced according to the method described above, multiple submodule has just been obtained, tearing open
Except when, it is necessary to be removed successively to both sides from two blocks of L like shape plates of the centre of the submodule of the bottom;
Submodule is again broken down into thinner part, when can further reduce dismounting and pitch lifting surface area, and subtract
Its few cohesion with pitch, reduces bitumen samples deformation, improves the qualification rate that bitumen samples make, at the same can also increase every
Contact area from agent and side plate is bigger, and then increases the recoverable amount of the interleaving agent on side plate, and the dismounting to side plate is more favourable, can
Further to reduce the cohesion of pitch and side plate, the qualification rate that bitumen samples make is improved;
In the breach that the short slab 61 of each L like shape plate is buckled in adjacent L like shape plate, can avoid L like shape plate to
Move at eight word die trial centers, it is ensured that the size of eight type matrix chambers in eight word die trials meets standard;
In another technical scheme, as shown in Figure 1, the side of the bottom plate 1 is relative provided with two alignment pins
11.Alignment pin 11 is oppositely arranged on a side plate, the both sides of eight word die trials can be made to lock simultaneously, eight word die trials are difficult
Deformation, so as to ensure that eight type matrix chambers meet standard size.
In another technical scheme, the submodule be three, the L like shape part by four L like shape plates according to
It is secondary to be spliced.One side plate is divided into 24 pieces of L like shape plate compositions, the qualification rate that bitumen samples make has reached
More than 90%, if being further added by the quantity of L like shape plate, difficulty and the time of eight word die trials of splicing can be increased, drip can be influenceed on the contrary
The producing efficiency of blue or green sample, and L like shape plate number is more, and its section is thinner, yielding, influences the use longevity of eight word die trials
Life, increases use cost.
In another technical scheme, the material of the bottom plate 1, the end plate 2 and the side plate is for copper material or not
Rust steel matter.Due to side plate divide into multiple smaller parts, using copper material or stainless steel, it can be made not variable
Shape, extends the service life of eight word die trials.
In another technical scheme, the roughness of the L like shape plate outer surface is less than 0.1 μm.It is coarse using outer surface
It is closer that L like shape plate of the degree less than 0.1 μm can be such that it is combined when being spliced into side plate, while can also make to form eight type matrix chambers
Side mold portion is more smooth, helps to remove.
In another technical scheme, length difference of the two neighboring submodule along the width of bottom plate 1 is more than 5mm.
The stair-stepping side of side form block formation can be made, ladder width is more than 5mm, so that convenient use people force removes submodule.
Although embodiment of the present utility model is disclosed as above, it is not restricted in specification and embodiment
Listed to use, it can be applied to various suitable fields of the present utility model completely, for those skilled in the art,
Other modification is easily achieved, therefore under the universal limited without departing substantially from claim and equivalency range, this reality
Specific details is not limited to new and shown here as the legend with description.
Claims (7)
1. a kind of eight word die trials detected for bitumen ductility, it is characterised in that including:
Contraband shape bottom plate, the bottom plate is provided with alignment pin;
A pair of end plate, its relative two ends for being fastened on the bottom plate, the opposite one end of the end plate is provided with class arc groove, formed
Two end moulds of eight type matrix chambers, the other end is provided with through hole, and the both sides of the opposite one end of the end plate are relative recessed provided with a L-shaped
Portion;
A pair of side plates, its relative is fastened on the bottom plate is located between the end plate, and the opposite side of the side plate is provided with width
The sharp portion successively decreased by centre to two ends is spent, the side form of eight type matrix chambers is formed, opposite side is locked with alignment pin, and the side plate is opposite
From side the relative convex portion for being provided with a L-shaped in two ends, the convex portion and the structure matching of the recess, to limit the side plate
Move towards, eight type matrix chambers of the end plate and the side plate one closing of formation;
Wherein, the side plate includes:
Fixed block, it is in cuboid, and one side and the alignment pin of the fixed block are locked, and the fixed block is provided with a ditch
Groove, one vertical cross-section of the groove formation is stair-stepping mortise;
Side form block, it includes from top to bottom overlapping multiple submodule successively, and the submodule is along the baseplate width direction
Length increase successively from top to bottom, form tenon, the structure matching of the tenon and the mortise, so that the side form block is supported
Touch in the groove of the fixed block, the triangle that side of the submodule away from the fixed block is set to isosceles is block.
2. the eight word die trials detected as claimed in claim 1 for bitumen ductility, it is characterised in that the submodule is by two
Axisymmetric L like shape part is spliced, and the L like shape part is spliced successively by multiple L like shape plates, the L like shape plate
Including integrally formed long slab and short slab, the long slab side is set to inclined-plane, opposite side and is provided with for the short of adjacent L like shape plate
The breach that plate is stretched into, the inclined-plane of multiple L like shape plates forms the sharp portion.
3. the eight word die trials detected as claimed in claim 1 for bitumen ductility, it is characterised in that the side phase of the bottom plate
To provided with two alignment pins.
4. the eight word die trials detected as claimed in claim 2 for bitumen ductility, it is characterised in that the submodule is three
Individual, the L like shape part is spliced successively by four L like shape plates.
5. the eight word die trials detected as claimed in claim 1 for bitumen ductility, it is characterised in that the bottom plate, the end
The material of plate and the side plate is copper material or stainless steel.
6. the eight word die trials detected as claimed in claim 2 for bitumen ductility, it is characterised in that the L like shape plate appearance
The roughness in face is less than 0.1 μm.
7. the eight word die trials detected as claimed in claim 1 for bitumen ductility, it is characterised in that two neighboring submodule edge
The length difference in the baseplate width direction is more than 5mm.