CN206502772U - The composite coating film of built-in fluorescence coating - Google Patents
The composite coating film of built-in fluorescence coating Download PDFInfo
- Publication number
- CN206502772U CN206502772U CN201621443934.3U CN201621443934U CN206502772U CN 206502772 U CN206502772 U CN 206502772U CN 201621443934 U CN201621443934 U CN 201621443934U CN 206502772 U CN206502772 U CN 206502772U
- Authority
- CN
- China
- Prior art keywords
- film
- matrix
- shaped matrix
- coating
- fluorescence
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model is related to office realm, and in particular to paint film.The composite coating film of built-in fluorescence coating, including the film-shaped matrix that a high-molecular coating is made, film-shaped matrix have three layers, and the first film-shaped matrix, the second film-shaped matrix, tertiary membrane shape matrix are followed successively by from top to bottom;The fluorescence coating constituted between first film-shaped matrix and the second film-shaped matrix provided with fluorescent material;Be provided between second film-shaped matrix and tertiary membrane shape matrix is in netted web;The lower section of tertiary membrane shape matrix is provided with gum layer;The lower section of gum layer is provided with off-style paper layer.Fluorescent material built in the utility model, fluorescent material is after by the irradiation such as natural light, daylight light, ultraviolet light, luminous energy is stored, after light irradiation is stopped, slowly discharged again in the way of fluorescence, so at night or dark, remain to see luminous, duration is up to a few houres to ten a few houres, so as to illuminate composite coating film.
Description
Technical field
The utility model is related to office realm, and in particular to paint film.
Background technology
At present, many structures of common paint film are single.The single paint film of structure when in use, to evening, because membranaceous
Matrix does not light, it is difficult to observe.
Utility model content
The purpose of this utility model is to provide a kind of composite coating film of built-in fluorescence coating, with solve it is above-mentioned at least one
Technical problem.
The problem of the utility model is solved can be realized using following technical scheme:
The composite coating film of built-in fluorescence coating, including the film-shaped matrix that a high-molecular coating is made, it is characterised in that described
Film-shaped matrix has three layers, and the first film-shaped matrix, the second film-shaped matrix, tertiary membrane shape matrix are followed successively by from top to bottom;
The fluorescence coating constituted between first film-shaped matrix and second film-shaped matrix provided with fluorescent material;
Be provided between second film-shaped matrix and the tertiary membrane shape matrix is in netted web;
The lower section of the tertiary membrane shape matrix is provided with gum layer;
The lower section of the gum layer is provided with off-style paper layer.
Fluorescent material built in the utility model, fluorescent material is after by the irradiation such as natural light, daylight light, ultraviolet light, light
It can store, be discharged after light irradiation is stopped, then slowly in the way of fluorescence, so at night or dark,
Remain to see it is luminous, the duration up to a few houres to ten a few houres, so as to illuminate composite coating film.In addition, the utility model
The structure of composite coating film is also optimized, by setting web, it is possible to use web is strengthened in film-shaped matrix between molecule
Bonding strength, and then cause the composite coating film of built-in fluorescence coating when being transferred to from an object on another object, no
Easy fragmentation.
Because the purpose of this patent is to allow composite coating film to light, as long as there is fluorescent material, material, thickness to fluorescent material
Degree, arrangement mode are without too high request.
During production, Step 1: paving release liners, the glue spraying in release liners, form gum layer;Step 2: on gum layer gum
High-molecular coating is applied, tertiary membrane shape matrix is formed;Step 3: putting web on tertiary membrane shape matrix, apply high on web
Molecule coating, forms the second film-shaped matrix;Step 4, spills fluorescent material in the second film-shaped matrix, the fluorescence coating is formed, glimmering
Apply high-molecular coating on photosphere, form the first film-shaped matrix, thus be made can light, the built-in fluorescence coating that can shift is answered
Close paint film.
Fluorescent material on the fluorescence coating is in latticed arrangement, constitutes network structure.The program can effectively reduce fluorescence
The consumption of powder, can more crucially make film-shaped matrix light relatively uniform, in this case, user can not only be in light
It is quick to find luminous composite coating film in the case that line is poor, and it is also possible to the superscript text of user can be seen clearly
Word or pattern.
The crosspoint of the web and the crosspoint of the network structure are staggered.Because it is larger to intersect dot thickness,
By arrangement mode staggeredly, two crosspoints can be avoided just right, so as to effectively reduce the compound painting of built-in fluorescence coating
Expect the thickness of film, and because crosspoint is not just right, the requirement to film-shaped matrix thickness can be reduced.Therefore table can be produced
The composite coating film of face more smooth built-in fluorescence coating.
Brief description of the drawings
Fig. 1 is part-structure schematic diagram of the present utility model.
Embodiment
In order that technological means, creation characteristic, reached purpose and effect that the utility model is realized are easy to understand, under
Face, which combines to be specifically illustrating, is expanded on further the utility model.
Reference picture 1, the composite coating film of built-in fluorescence coating, including the film-shaped matrix that a high-molecular coating is made, membranaceous base
Body has three layers, and the first film-shaped matrix 1, the second film-shaped matrix 2, tertiary membrane shape matrix 3 are followed successively by from top to bottom;First film-shaped matrix
1 and second fluorescence coating 4 constituted provided with fluorescent material between film-shaped matrix 2;Between second film-shaped matrix 2 and tertiary membrane shape matrix 3
Provided with netted web 5;The lower section of tertiary membrane shape matrix 3 is provided with gum layer;The lower section of gum layer is provided with off-style paper layer.This
Fluorescent material built in utility model, fluorescent material stores luminous energy after by the irradiation such as natural light, daylight light, ultraviolet light,
Discharged after light irradiation is stopped, then slowly in the way of fluorescence, so at night or dark, remaining to see hair
Light, the duration is up to a few houres to ten a few houres, so as to illuminate composite coating film.In addition, the utility model is also optimized again
The structure of paint film is closed, by setting web 5, it is possible to use the connection that web 5 is strengthened in film-shaped matrix between molecule is strong
Degree, and then cause the composite coating film of built-in fluorescence coating 4 when being transferred to from an object on another object, it is not easy to it is broken
Split.Because the purpose of this patent is to allow composite coating film to light, as long as there is fluorescent material, to the material of fluorescent material, thickness, arrangement
Mode is without too high request.
During production, Step 1: paving release liners, the glue spraying in release liners, form gum layer;Step 2: on gum layer gum
High-molecular coating is applied, tertiary membrane shape matrix 3 is formed;Step 3: web 5 is put on tertiary membrane shape matrix 3, on web 5
High-molecular coating is applied, the second film-shaped matrix 2 is formed;Step 4, spills fluorescent material in the second film-shaped matrix 2, forms fluorescence coating 4,
High-molecular coating is applied on fluorescence coating 4, the first film-shaped matrix 1 is formed, so that the built-in fluorescence that can be lighted, can shift is made
The composite coating film of layer 4.
Fluorescent material on fluorescence coating 4 is in latticed arrangement, constitutes network structure.The program can effectively reduce fluorescent material
Consumption, can more crucially make film-shaped matrix light relatively uniform, in this case, user can not only light compared with
It is quick to find luminous composite coating film in the case of difference, and it is also possible to can see clearly the superscript word of user or
Pattern.
The crosspoint of web 5 and the crosspoint of network structure are staggered.Because it is larger to intersect dot thickness, by staggeredly
Arrangement mode, two crosspoints can be avoided just right, so as to the thickness for the composite coating film for effectively reducing built-in fluorescence coating 4
Degree, and because crosspoint is not just right, the requirement to film-shaped matrix thickness can be reduced.Therefore surface can be produced more flat
The composite coating film of sliding built-in fluorescence coating.
General principle of the present utility model and principal character and advantage of the present utility model has been shown and described above.One's own profession
The technical staff of industry is it should be appreciated that the utility model is not restricted to the described embodiments, described in above-described embodiment and specification
Simply illustrate principle of the present utility model, on the premise of the utility model spirit and scope are not departed from, the utility model is also
Various changes and modifications are had, these changes and improvements are both fallen within the range of claimed the utility model.The utility model
Claimed scope is by appended claims and its equivalent thereof.
Claims (3)
1. built in fluorescence coating composite coating film, including the film-shaped matrix that a high-molecular coating is made, it is characterised in that the film
Shape matrix has three layers, and the first film-shaped matrix, the second film-shaped matrix, tertiary membrane shape matrix are followed successively by from top to bottom;
The fluorescence coating constituted between first film-shaped matrix and second film-shaped matrix provided with fluorescent material;
Be provided between second film-shaped matrix and the tertiary membrane shape matrix is in netted web;
The lower section of the tertiary membrane shape matrix is provided with gum layer;
The lower section of the gum layer is provided with off-style paper layer.
2. the composite coating film of built-in fluorescence coating according to claim 1, it is characterised in that:Fluorescence on the fluorescence coating
Powder is in latticed arrangement, constitutes network structure.
3. the composite coating film of built-in fluorescence coating according to claim 1, it is characterised in that:The crosspoint of the web
Crosspoint with the network structure is staggered.