CN206297221U - Cover-plate glass stepped construction - Google Patents

Cover-plate glass stepped construction Download PDF

Info

Publication number
CN206297221U
CN206297221U CN201621156133.9U CN201621156133U CN206297221U CN 206297221 U CN206297221 U CN 206297221U CN 201621156133 U CN201621156133 U CN 201621156133U CN 206297221 U CN206297221 U CN 206297221U
Authority
CN
China
Prior art keywords
layer
glass substrate
cover
tack coat
stepped construction
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201621156133.9U
Other languages
Chinese (zh)
Inventor
唐根初
刘伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nanchang Ofilm Optical Technology Co ltd
OFilm Group Co Ltd
Anhui Jingzhuo Optical Display Technology Co Ltd
Original Assignee
Nanchang OFilm Optical Technology Co Ltd
Shenzhen OFilm Tech Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nanchang OFilm Optical Technology Co Ltd, Shenzhen OFilm Tech Co Ltd filed Critical Nanchang OFilm Optical Technology Co Ltd
Priority to CN201621156133.9U priority Critical patent/CN206297221U/en
Application granted granted Critical
Publication of CN206297221U publication Critical patent/CN206297221U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model is related to a kind of cover-plate glass stepped construction, a kind of cover-plate glass stepped construction, including:Glass substrate, including inner surface, the outer surface being spaced with the inner surface;Tack coat, is covered in and is provided with the inner surface of the glass substrate;Decorative layer, is formed on a surface away from the glass substrate of the tack coat;And hardened layer, it is formed on a surface away from the tack coat of the decorative layer.Decorative layer is set between hardened layer and tack coat, such as increases the black ring of camera, the hardened layer with black ring is pasted on the glass substrate by tack coat, is thusly-formed cover-plate glass stepped construction and is avoided that the visual impact that camera alignment error brings.Again or, such as character or decorative layer as icon are set between hardened layer and tack coat, can be obviously improved the display effect of character or icon, lift Consumer's Experience.

Description

Cover-plate glass stepped construction
Technical field
The utility model is related to technical field of touch control, more particularly to a kind of cover-plate glass layer applied on touch-control product Stack structure.
Background technology
At present, in the housing assembling process of camera module and the electronic product with touch controllable function, easily there is shooting The situation of the assembling position matched with camera module that the housing that head mould group deviates electronic product is reserved in advance, if occurring taking the photograph As head deviation of the alignment, consumer directly can experience from the outward appearance of electronic product, so as to reduce Consumer's Experience.
Utility model content
Based on this, it is necessary to provide a kind of cover-plate glass stepped construction that can be solved the above problems.
A kind of cover-plate glass stepped construction, including:
Glass substrate, including inner surface, the outer surface being spaced with the inner surface;
Tack coat, is covered in and is provided with the inner surface of the glass substrate;
Decorative layer, is formed on a surface away from the glass substrate of the tack coat;And
Hardened layer, is formed on a surface away from the tack coat of the decorative layer.
Wherein in one embodiment, the decorative layer is black ring, character or icon.
Wherein in one embodiment, the decorative layer is formed by silk-screen mode.
Wherein in one embodiment, when the decorative layer is black ring, the black ring is the ring junction with manhole Structure.
Wherein in one embodiment, the cover-plate glass stepped construction also includes UV texture layers, evaporation layer and base oil Layer of ink, the hardened layer, UV texture layers, evaporation layer and base ink layer are cascading.
Wherein in one embodiment, the thickness of the hardened layer is 2~5 μm.
Wherein in one embodiment, the hardened layer is UV texture layers, and the cover-plate glass stepped construction also includes steaming Coating and ink layer, the hardened layer, evaporation layer and ink layer are cascading.
Wherein in one embodiment, the thickness of the hardened layer is 10~20 μm.
Wherein in one embodiment, the thickness of the tack coat is 5~20 μm.
Wherein in one embodiment, the glass substrate has at least part of curved surface.
A kind of cover-plate glass stepped construction that the utility model is provided, at least has the advantage that:
Decorative layer is set between hardened layer and tack coat, such as increases the black ring of camera, the hardened layer with black ring passes through Tack coat is pasted on the glass substrate, is thusly-formed cover-plate glass stepped construction and is avoided that the vision that camera alignment error brings Influence, can so simplify operation so as to reduce alignment error, the yield of product be effectively improved, simultaneously because avoiding shooting The visual impact that head alignment error brings, so as to improve Consumer's Experience.Again or, such as set between hardened layer and tack coat Decorative layer as character or icon is put, the display effect of character or icon can be obviously improved, lift Consumer's Experience.
Brief description of the drawings
Fig. 1 is the cover-plate glass stepped construction schematic diagram that the utility model one is implemented to exemplify;
Fig. 2 is another cover-plate glass stepped construction schematic diagram for implementing to exemplify of the utility model;
Fig. 3 is another cover-plate glass stepped construction schematic diagram for implementing to exemplify of the utility model;
Fig. 4 is the glass basal plate structure schematic diagram that the utility model one is implemented to exemplify;
Fig. 5 is the glass substrate schematic side view that the utility model one is implemented to exemplify;
Fig. 6 is another cover-plate glass stepped construction schematic diagram for implementing to exemplify of the utility model;
Fig. 7 is the glass basal plate structure schematic diagram that the utility model one is implemented to exemplify;
Fig. 8 is the glass substrate schematic side view that the utility model one is implemented to exemplify;
Fig. 9 is the another glass basal plate structure schematic diagram for implementing to exemplify of the utility model;
Figure 10 is the another glass basal plate structure schematic diagram for implementing to exemplify of the utility model;
Figure 11 is the another glass basal plate structure schematic diagram for implementing to exemplify of the utility model;
Figure 12 is schematic side view of the curved glass panel shown in Figure 11 along W directions;
Figure 13 is schematic cross-section of the curved glass panel shown in Figure 12 along line A-A;
Figure 14 is end view schematic of the curved glass panel shown in Figure 11 along L directions;
Figure 15 is schematic cross-section of the curved glass panel shown in Figure 14 along line B-B.
Specific embodiment
To enable above-mentioned purpose of the present utility model, feature and advantage more obvious understandable, below in conjunction with the accompanying drawings to this The specific embodiment of utility model is described in detail.Elaborate many details in order to abundant in the following description Understand the utility model.But the utility model can be implemented with being much different from other manner described here, this area Technical staff can do similar improvement in the case of without prejudice to the utility model intension, therefore the utility model does not receive following public affairs The limitation of the specific implementation opened.
Unless otherwise defined, all of technologies and scientific terms used here by the article is led with technology of the present utility model is belonged to The implication that the technical staff in domain is generally understood that is identical.It is herein to be in term used in the description of the present utility model The purpose of description specific embodiment, it is not intended that in limitation the utility model.Term as used herein " and/or " include The arbitrary and all of combination of one or more related Listed Items.
A kind of cover-plate glass stepped construction that the utility model is provided is used as the electronic product with touch controllable function Display surface housing, these electronic products including but be not limited to mobile phone, camera, panel computer, terminal display etc..
Fig. 1 is the cover-plate glass stepped construction schematic diagram that the utility model one is implemented to exemplify.Refer to Fig. 1, cover plate glass Glass stepped construction includes glass substrate 10, tack coat 40, hardened layer 50 and decorative layer 30.
The cover-plate glass stepped construction also includes UV texture layers 60, is deposited with layer 70 and ink layer 80, the hardened layer 50, UV texture layers 60, evaporation layer 70 and ink layer 80 are cascading.
The glass substrate 10 has relative inner surface 101 and outer surface 102.Specific in the present embodiment, glass base Plate 10 is plate glass.Glass substrate 10 can be rendered as the shape such as rectangle, circle, square according to the electronic product applied Shape.
In the present embodiment, the inner surface 101 of glass substrate 10 is that, towards the surface inside electronic product, outer surface 102 is Towards the surface of user's viewing.In certain embodiments, can according to demands such as the antireflection of electronic product, anti-fingerprint, and The functional film layers such as antireflection film, anti-fingerprint film are set on the outer surface 102 of the glass substrate 10.Further, it is also possible to glass Glass substrate 10 carries out intensive treatment, and cured film is set on any one surface of glass substrate 10.
The tack coat 40 has stickup property, and very thin.Specific in present embodiment, tack coat 40 is optical clear (OCA, Optically Clear Adhesive) glue.Tack coat 40 is covered on the inner surface of glass substrate 10.Specific to this In implementation method, the thickness of tack coat 40 is 5~100 μm.It is furthermore preferred that the thickness of tack coat 40 is 5~20 μm.
The decorative layer 30 is formed on a surface away from the glass substrate 10 of the tack coat 40, specifically Ground, the decorative layer 30 is formed by silk-screen mode.In specific to present embodiment, the decorative layer 30 is black ring, described black Ring is the loop configuration with manhole, and the black ring is used for the visual impact for avoiding camera alignment error from bringing, and so may be used To simplify operation so as to reduce alignment error, the yield of product is effectively improved, simultaneously because avoiding camera alignment error The visual impact for bringing, so as to improve Consumer's Experience.It is appreciated that in other embodiments, the decorative layer 30 can be with It is character or icon.
The hardened layer 50 is formed on a surface away from the tack coat 40 of decorative layer 30.Specific to this implementation In mode, the thickness of hardened layer 50 is 2~20 μm.It is furthermore preferred that the thickness of hardened layer 50 is 2~5 μm, this thickness being more highly preferred to Degree can realize hardened layer fitted with glass substrate during injured it is bad it is relatively low, fit that bubble is less and the bad relatively low effect of fold Really, such that it is able to effectively improve the yield of product.
The UV texture layers 60 are transferred on the hardened layer 50 by UV.Specifically, when UV texture layers 60 are formed, can The coating UV glue on the hardened layer 50 for being formed, is then imprinted by template, UV glue is had a specific pattern, then is applied mask and consolidated Change and clean uncured UV glue, you can obtain the UV texture layers 60 being formed on hardened layer 50.In specific to present embodiment, The UV texture layers 60 region corresponding with the black ring does not imprint texture, i.e., described UV texture layers 60 do not imprint texture region and hang down The straight corresponding view field for projecting to formation on glass substrate 10 in camera light incident direction can cover the black ring Manhole.
The evaporation layer 70 is arranged on the UV texture layers 60, and evaporation layer 70 can be the film that metallic luster is for example presented Layer.Set off by the pattern of UV texture layers 60, can the unilateral observation of outer surface 102 of glass substrate 10 to different pattern and The outward appearance of color and luster, is presented metal-like, so as to be obviously improved the display effect of character or icon, lifts Consumer's Experience.
After the structures such as evaporation layer 70 are set again on the UV texture layers 60, because evaporation layer 70 is nontransparent, UV texture layers 60 It is transparent, the figure that UV texture layers 60 and evaporation layer 70 are showed still can be observed in the side of outer surface 102 of glass substrate 10 Case.
The ink layer 80 is arranged on the evaporation layer 70.Ink layer 80 and evaporation layer 70 are light tight, thus outside The side of surface 102 towards inner surface 101 direction observe when, can't see the opposite side of glass substrate 10 by ink layer 80 and steam The scene that coating 70 is blocked.
Fig. 2 is another cover-plate glass stepped construction schematic diagram for implementing to exemplify of the utility model.Refer to Fig. 2, cover plate Glass laminated structure includes glass substrate 10a, tack coat 40, hardened layer 50 and decorative layer 30.
The cover-plate glass stepped construction also include evaporation layer 70 and ink layer 80, the hardened layer 50, evaporation layer 70 and Ink layer 80 is cascading.
The glass substrate 10 has relative inner surface 101 and outer surface 102.Specific in the present embodiment, glass base Plate 10 is plate glass.Glass substrate 10 can be rendered as the shape such as rectangle, circle, square according to the electronic product applied Shape.
In the present embodiment, the inner surface 101 of glass substrate 10 is that, towards the surface inside electronic product, outer surface 102 is Towards the surface of user's viewing.In certain embodiments, can according to demands such as the antireflection of electronic product, anti-fingerprint, and The functional film layers such as antireflection film, anti-fingerprint film are set on the outer surface 102 of the glass substrate 10.Further, it is also possible to glass Glass substrate 10 carries out intensive treatment, and cured film is set on any one surface of glass substrate 10.
The tack coat 40 has stickup property, and very thin.Specific in present embodiment, tack coat 40 is optical clear (OCA, Optically Clear Adhesive) glue.Tack coat 40 is covered on the inner surface of glass substrate 10a.Specific to this In implementation method, the thickness of tack coat 40 is 5~100 μm.It is furthermore preferred that the thickness of tack coat 40 is 5~20 μm.
The decorative layer 30 is formed on a surface away from the glass substrate 10 of the tack coat 40.Specifically Ground, the decorative layer 30 is formed by silk-screen mode.In specific to present embodiment, the decorative layer 30 is black ring, described black Ring is the loop configuration with manhole, and the black ring is used for the visual impact for avoiding camera alignment error from bringing, and so may be used To simplify operation so as to reduce alignment error, the yield of product is effectively improved, simultaneously because avoiding camera alignment error The visual impact for bringing, so as to improve Consumer's Experience.It is appreciated that in other embodiments, the decorative layer 30 can be with It is character or icon.
The hardened layer 50 be formed at decorative layer 30 away from 40 1 surfaces of the tack coat.Specific to this embodiment party In formula, the hardened layer 50 is UV texture layers, is transferred on the tack coat 40 by UV.Specifically, hardened layer 50 is being formed When, can formed tack coat 40 on coating UV glue, then by template imprint, make UV glue that there is specific pattern, make UV glue With specific pattern, such as the specific pattern such as drawing pattern, CD lines or ripple glaze is set on UV glue-lines, then applies mask and consolidate Change and clean uncured UV glue, you can obtain the UV texture layers being formed on tack coat 40.In specific to present embodiment, The UV glue is both used to provide hardness support tack coat, while texture can be formed.
In specific to present embodiment, the UV texture layers 60 region corresponding with the black ring does not imprint texture, i.e. institute State UV texture layers 60 do not imprint texture region perpendicular to camera light incident direction project on glass substrate 10 formed it is right The view field answered can cover the manhole of the black ring.
Specific in present embodiment, the thickness of hardened layer 50 is 5~200 μm.Preferably, the thickness of hardened layer 50 is 10 ~50 μm.It is further preferred that the thickness of hardened layer 50 is 10~20 μm.
The evaporation layer 70 is arranged on the hardened layer 50, and evaporation layer 70 can be the film that metallic luster is for example presented Layer.Set off by the pattern of UV texture layers, can be in the unilateral observation of outer surface 102 of glass substrate 10 to different pattern and color The outward appearance in pool, is presented metal-like, so as to be obviously improved the display effect of character or icon, lifts Consumer's Experience.
After setting the structures such as evaporation layer 70 on the hardened layer 50 again, because evaporation layer 70 is nontransparent, UV texture layers are transparent, The pattern that UV texture layers and evaporation layer 70 are showed still can be observed in the side of outer surface 102 of glass substrate 10.
The ink layer 80 is arranged on the evaporation layer 70.Ink layer 80 and evaporation layer 70 are light tight, thus outside The side of surface 102 towards inner surface 101 direction observe when, can't see the opposite side of glass substrate 10 by ink layer 80 and evaporation The scene that layer 70 is blocked.
Fig. 3 is another cover-plate glass stepped construction schematic diagram for implementing to exemplify of the utility model.Refer to Fig. 3, cover plate Glass laminated structure includes glass substrate 20, tack coat 40, hardened layer 50 and decorative layer 30.
The cover-plate glass stepped construction also includes UV texture layers 60, is deposited with layer 70 and ink layer 80, the hardened layer 50, UV texture layers 60, evaporation layer 70 and ink layer 80 are cascading.
Refer to Fig. 4, the glass substrate 20 includes planar portions 21 and the relative two edges court respectively by planar portions 21 The curved face part 22 that the bending of the same side surface of planar portions 21 is extended.It is appreciated that in other embodiments, glass substrate 20 Four edges may extend away and form curved face part 22, or the one of edge of glass substrate 20 extends curved face part 22.
Also referring to Fig. 5, more specifically, the glass substrate 20 includes inner surface 201, with the interval of inner surface 201 Outer surface 202, and connect the lateral circle surface 203 of outer surface 202 and inner surface 201.The inner surface 201 refers to recessed one Face, the outer surface 202 refers to the one side of evagination.The inner surface 201 and outer surface 202 are respectively provided with zone line and edge Region.Wherein, in the present embodiment, planar portions 21 define the zone line, and curved face part 22 defines the fringe region, Ye Jiping Face 21 is located at the zone line, and curved face part 22 is located at the fringe region.In other embodiments, fringe region can also It is around the zone line, such as when four edges of glass substrate 20 extend to form curved face part 22, the mesozone Domain by fringe region around.
The inner surface 201 equally including planar portions 211 and by planar portions 211 relative two edges respectively towards a lateral bending The curved face part 221 that folding extends.Two curved face parts 221 are symmetrical arranged with respect to planar portions 211.The section of curved face part 221 is circle Arc.Two radiuses of curved face part 221 can be with equal, it is also possible to.In the present embodiment, the radius of two curved face parts 221 is equal. Two radiuses of curved face part 221 are 1~50mm, preferably 5~50mm, further preferred 5~20mm, preferred 5~10mm.Half Footpath is smaller, and circular arc camber is more precipitous, thus its outward appearance 3D stereoeffects of glass substrate 20 for being formed are stronger.
The outer surface 202 similarly include planar portions 212 and by planar portions 212 relative two edges respectively towards side The curved face part 222 that bending is extended.Wherein, the curved face part 222 of outer surface 202 and the curved face part 221 of inner surface 201 are courts The same side bends, namely is bent towards the side of inner surface 201.Two curved face parts 222 are symmetrical arranged with respect to planar portions 212. The section of curved face part 222 is circular arc.Two radiuses of curved face part 222 can be with equal, it is also possible to.In the present embodiment, two The radius of curved face part 222 is equal.Two radiuses of curved face part 222 be 1~50mm, preferably 5~50mm, further preferred 5~ 20mm, preferred 5~10mm.
Wherein, planar portions 212 are corresponding with the position of planar portions 211, and size is identical, thus when the glass substrate 20 Outer surface 202 place when in the horizontal plane, the orthographic projection in the horizontal plane of planar portions 211 and planar portions 212 is completely superposed.
More specifically, the radius of curved face part 222 and curved face part 221 is also equal.In the present embodiment, inner surface 201 and appearance The distance between face 202, namely the thickness of the glass substrate 20 is 0.2~1.0mm.Thickness one everywhere of glass substrate 20 Cause, so can preferably eliminate stress concentration, lift bulk strength.Preferably, the thickness of glass substrate 20 be 0.5~ 0.7mm。
The tangent line of the point at the place circular arc most edge of the curved face part 222 is defined as C angles, C with the angle of the planar portions 212 Angle is 0 °<C<90 °, preferably 0 °<C<45°.C angles between curved face part 221 and planar portions 211 can also have identical setting.
Further, the distance between the point at the place circular arc most edge of the curved face part 221 and described planar portions 212, The height H of i.e. described glass substrate 20 is 0.5~5mm.
In certain embodiments, the orthographic projection in the horizontal plane of the glass substrate 20 is rectangle, wherein rectangular 50~500mm, 30~300mm wide long.The curved face part 221,222 be arranged on it is rectangular length where two edges.
In embodiment shown in Fig. 3 to Fig. 5, curved face part 22 is by planar portions 21 with respect to both sides towards side bending extension Go out.In other embodiment, also can extend the curved face part 22 for forming circular arc towards side bending by four sides of planar portions 21.Relatively The radius of the curved face part 22 that both sides are extended can be with equal, it is also possible to.The radius of the curved face part 22 that adjacent both sides are extended Can be with equal, it is also possible to.Four sides are respectively formed in the embodiment of curved face part 22, and other features can join the reality shown in Fig. 3 to Fig. 5 Example setting is applied, this is not repeated.
Referring to Fig. 3, the tack coat 40 has stickup property, and very thin.Specific in present embodiment, tack coat 40 is optical clear (OCA, Optically Clear Adhesive) glue.Tack coat 40 is covered in the inner surface of glass substrate 20 On.Specific in present embodiment, the thickness of tack coat 40 is 5~100 μm.It is furthermore preferred that the thickness of tack coat 40 is 5~20 μm。
The decorative layer 30 is formed on a surface away from the glass substrate 20 of the tack coat 40.Specifically Ground, the decorative layer 30 is formed by silk-screen mode.In specific to present embodiment, the decorative layer 30 is black ring, described black Ring is the loop configuration with manhole, and the black ring is used for the visual impact for avoiding camera alignment error from bringing, and so may be used To simplify operation so as to reduce alignment error, the yield of product is effectively improved, simultaneously because avoiding camera alignment error The visual impact for bringing, so as to improve Consumer's Experience.It is appreciated that in other embodiments, the decorative layer 30 can be with It is character or icon.
The hardened layer 50 is formed on a surface away from the tack coat 40 of decorative layer 30.Specific to this implementation In mode, the thickness of hardened layer 50 is 2~20 μm.It is furthermore preferred that the thickness of hardened layer 50 is 2~5 μm, this thickness being more highly preferred to Degree can realize hardened layer fitted with glass substrate during injured it is bad it is relatively low, fit that bubble is less and the bad relatively low effect of fold Really, such that it is able to effectively improve the yield of product.
The UV texture layers 60 are transferred on the hardened layer 50 by UV.Specifically, when UV texture layers 60 are formed, can The coating UV glue on the hardened layer 50 for being formed, is then imprinted by template, UV glue is had a specific pattern, then is applied mask and consolidated Change and clean uncured UV glue, you can obtain the UV texture layers 60 being formed on hardened layer 50.In specific to present embodiment, The UV texture layers 60 region corresponding with the black ring does not imprint texture, i.e., described UV texture layers 60 do not imprint texture region The corresponding view field formed on glass substrate 20 is projected to perpendicular to camera light incident direction can cover the black ring Manhole.
The evaporation layer 70 is arranged on the UV texture layers 60, and evaporation layer 70 can be the film that metallic luster is for example presented Layer.Set off by the pattern of UV texture layers 60, can the unilateral observation of outer surface 202 of glass substrate 20 to different pattern and The outward appearance of color and luster, is presented metal-like, so as to be obviously improved the display effect of character or icon, lifts Consumer's Experience.
After the structures such as evaporation layer 70 are set again on the UV texture layers 60, because evaporation layer 70 is nontransparent, UV texture layers 60 It is transparent, the figure that UV texture layers 60 and evaporation layer 70 are showed still can be observed in the side of outer surface 202 of glass substrate 20 Case.
The ink layer 80 is arranged on the evaporation layer 70.Ink layer 80 and evaporation layer 70 are light tight, thus outside The side of surface 202 towards inner surface 201 direction observe when, can't see the opposite side of glass substrate 20 by ink layer 80 and evaporation The scene that layer 70 is blocked.
Fig. 6 is another cover-plate glass stepped construction schematic diagram for implementing to exemplify of the utility model.Refer to Fig. 6, cover plate Glass laminated structure includes glass substrate 20, tack coat 40, hardened layer 50 and decorative layer 30.
The cover-plate glass stepped construction also include evaporation layer 70 and ink layer 80, the hardened layer 50, evaporation layer 70 and Ink layer 80 is cascading.
Refer to Fig. 7, the glass substrate 20 includes planar portions 21 and the relative two edges court respectively by planar portions 21 The curved face part 22 that the bending of the same side surface of planar portions 21 is extended.It is appreciated that in other embodiments, glass substrate 20 Four edges may extend away and form curved face part 22, or the one of edge of glass substrate 20 extends curved face part 22.
Also referring to Fig. 8, more specifically, the glass substrate 20 includes inner surface 201, with the interval of inner surface 201 Outer surface 202, and connect the lateral circle surface 203 of outer surface 202 and inner surface 201.The inner surface 201 refers to recessed one Face, the outer surface 202 refers to the one side of evagination.The inner surface 201 and outer surface 202 are respectively provided with zone line and marginal zone Domain.Wherein, in the present embodiment, planar portions 21 define the zone line, and curved face part 22 defines the fringe region, namely plane Portion 21 is located at the zone line, and curved face part 22 is located at the fringe region.In other embodiments, fringe region can also be Around the zone line, such as when four edges of glass substrate 20 extend to form curved face part 22, the zone line By fringe region around.
The inner surface 201 equally including planar portions 211 and by planar portions 211 relative two edges respectively towards a lateral bending The curved face part 221 that folding extends.Two curved face parts 221 are symmetrical arranged with respect to planar portions 211.The section of curved face part 221 is circle Arc.Two radiuses of curved face part 221 can be with equal, it is also possible to.In the present embodiment, the radius of two curved face parts 221 is equal. Two radiuses of curved face part 221 are 1~50mm, preferably 5~50mm, further preferred 5~20mm, preferred 5~10mm.Half Footpath is smaller, and circular arc camber is more precipitous, thus its outward appearance 3D stereoeffects of glass substrate 20 for being formed are stronger.
The outer surface 202 similarly include planar portions 212 and by planar portions 212 relative two edges respectively towards side The curved face part 222 that bending is extended.Wherein, the curved face part 222 of outer surface 202 and the curved face part 221 of inner surface 201 are courts The same side bends, namely is bent towards the side of inner surface 201.Two curved face parts 222 are symmetrical arranged with respect to planar portions 212. The section of curved face part 222 is circular arc.Two radiuses of curved face part 222 can be with equal, it is also possible to.In the present embodiment, two The radius of curved face part 222 is equal.Two radiuses of curved face part 222 be 1~50mm, preferably 5~50mm, further preferred 5~ 20mm, preferred 5~10mm.
Wherein, planar portions 212 are corresponding with the position of planar portions 211, and size is identical, thus when the glass substrate 20 Outer surface 202 place when in the horizontal plane, the orthographic projection in the horizontal plane of planar portions 211 and planar portions 212 is completely superposed.
More specifically, the radius of curved face part 222 and curved face part 221 is also equal.In the present embodiment, inner surface 201 and appearance The distance between face 202, namely the thickness of the glass substrate 20 is 0.2~1.0mm.Thickness one everywhere of glass substrate 20 Cause, so can preferably eliminate stress concentration, lift bulk strength.Preferably, the thickness of glass substrate 20 be 0.5~ 0.7mm。
The tangent line of the point at the place circular arc most edge of the curved face part 222 is defined as C angles, C with the angle of the planar portions 212 Angle is 0 °<C<90 °, preferably 0 °<C<45°.C angles between curved face part 221 and planar portions 211 can also have identical setting.
Further, the distance between the point at the place circular arc most edge of the curved face part 221 and described planar portions 212, The height H of i.e. described glass substrate 20 is 0.5~5mm.
In certain embodiments, the orthographic projection in the horizontal plane of the glass substrate 20 is rectangle, wherein rectangular 50~500mm, 30~300mm wide long.The curved face part 221,222 be arranged on it is rectangular length where two edges.
In embodiment shown in Fig. 6 to Fig. 8, curved face part 22 is by planar portions 21 with respect to both sides towards side bending extension Go out.In other embodiment, also can extend the curved face part 22 for forming circular arc towards side bending by four sides of planar portions 21.Relatively The radius of the curved face part 22 that both sides are extended can be with equal, it is also possible to.The radius of the curved face part 22 that adjacent both sides are extended Can be with equal, it is also possible to.Four sides are respectively formed in the embodiment of curved face part 22, and other features can join the reality shown in Fig. 6 to Fig. 8 Example setting is applied, this is not repeated.
Referring to Fig. 6, the tack coat 40 has stickup property, and very thin.Specific in present embodiment, tack coat 40 is optical clear (OCA, Optically Clear Adhesive) glue.Tack coat 40 is covered in the inner surface of glass substrate 20 On.Specific in present embodiment, the thickness of tack coat 40 is 5~100 μm.It is furthermore preferred that the thickness of tack coat 40 is 5~20 μm。
The decorative layer 30 is formed on a surface away from the glass substrate 20 of the tack coat 40.Specifically Ground, the decorative layer 30 is formed by silk-screen mode.In specific to present embodiment, the decorative layer 30 is black ring, described black Ring is the loop configuration with manhole, and the black ring is used for the visual impact for avoiding camera alignment error from bringing, and so may be used To simplify operation so as to reduce alignment error, the yield of product is effectively improved, simultaneously because avoiding camera alignment error The visual impact for bringing, so as to improve Consumer's Experience.It is appreciated that in other embodiments, the decorative layer 30 can be with It is character or icon.
The hardened layer 50 is formed on a surface away from the tack coat 40 of decorative layer 30.Specific to this implementation In mode, the hardened layer 50 is UV texture layers, is transferred on the tack coat 40 by UV.Specifically, hardened layer is being formed When 50, can formed tack coat 40 on coating UV glue, then by template imprint, make UV glue that there is specific pattern, make UV Glue has specific pattern, such as the specific pattern such as drawing pattern, CD lines or ripple glaze is set on UV glue-lines, then apply mask Solidify and clean uncured UV glue, you can obtain the UV texture layers being formed on tack coat 40.In specific to present embodiment, The UV glue is both used to provide hardness support tack coat, while texture can be formed.
In specific to present embodiment, the UV texture layers 60 region corresponding with the black ring does not imprint texture, i.e. institute State UV texture layers 60 do not imprint texture region perpendicular to camera light incident direction project on glass substrate 20 formed it is right The view field answered can cover the manhole of the black ring.
Specific in present embodiment, the thickness of hardened layer 50 is 5~200 μm.Preferably, the thickness of hardened layer 50 is 10 ~50 μm.It is further preferred that the thickness of hardened layer 50 is 10~20 μm.
The evaporation layer 70 is arranged on the hardened layer 50, and evaporation layer 70 can be the film that metallic luster is for example presented Layer.Set off by the pattern of UV texture layers, can be in the unilateral observation of outer surface 202 of glass substrate 20 to different pattern and color The outward appearance in pool, is presented metal-like, so as to be obviously improved the display effect of character or icon, lifts Consumer's Experience.
After setting the structures such as evaporation layer 70 on the hardened layer 50 again, because evaporation layer 70 is nontransparent, UV texture layers are transparent, The pattern that UV texture layers and evaporation layer 70 are showed still can be observed in the side of outer surface 202 of glass substrate 20.
The ink layer 80 is arranged on the evaporation layer 70.Ink layer 80 and evaporation layer 70 are light tight, thus outside The side of surface 202 towards inner surface 201 direction observe when, can't see the opposite side of glass substrate 20 by ink layer 80 and evaporation The scene that layer 70 is blocked.
In some other embodiments, glass substrate 20 is not limited to the structure shown in Fig. 4-Fig. 8.For example, Fig. 9 and Tu It is the glass substrate of another embodiment shown in 10, it includes inner surface 201a, the outer surface 202a being spaced with inner surface 201a, And the lateral circle surface (figure is not marked) of connection outer surface 202a and inner surface 201a.
The distance between described inner surface 201a and outer surface 202a be 0.2~1.0mm, namely the glass substrate thickness It is 0.2~1.0mm to spend.
It is in symmetrically to set along central shaft 203a that the inner surface 201a has central shaft a 203a, the inner surface 201a Put.Also there is the outer surface 202a central shaft 204a, the outer surface 202a to be symmetrical set along central shaft 204a.
The inner surface 201a is bent to form the introversion of circular arc centered on the central shaft 203a of inner surface 201a to homonymy Face, the outer surface 202a is bent to form the positive camber of circular arc, institute centered on the central shaft 204a of outer surface 202a to homonymy State negative camber, the radius R of positive camber is 50~1000mm, the height H of the glass substrate is 0.5~5mm.
In certain embodiments, the negative camber, positive camber radius R it is equal, namely the thickness everywhere of glass substrate is equal It is even.Stress concentration so can be preferably eliminated, bulk strength is lifted.
The height H of the glass substrate refers to inner surface 201a two parallel sides farthest with respect to central shaft 203a The distance between plane where 205a, 206a, with the central shaft 204a of outer surface 202a.
In certain embodiments, in circular arc inner surface 201a two parallel sides 205a, 206a and the center of circle of circular arc The corresponding central angle of circular arc where the angle of line, namely inner surface 201a is represented with C, wherein 60 ° of 180 ° of < C <.Outer surface The corresponding central angle C of circular arc of 202a also meets 60 ° of 180 ° of < C <.
It is the glass substrate of another embodiment shown in Figure 11, with reference to Figure 12 and Figure 13, the glass substrate includes Inner surface 201b, the outer surface 202b being spaced with inner surface 201b, and the side of connection outer surface 202b and inner surface 201b are all Face (figure is not marked).
The distance between described inner surface 201b and outer surface 202b be 0.2~1.0mm, namely the glass substrate thickness It is 0.2~1.0mm to spend.
The inner surface 201b has a center line W1 in the direction of the width, and the outer surface 202b is in the direction of the width With a center line W2.The inner surface 201b is symmetrical along center line W1 minute surfaces.The outer surface 202b is along center line W2 minute surfaces Symmetrically.Glass substrate is placed on horizontal plane, makees orthographic projection in the horizontal plane to the glass substrate, the inner surface 201b's The center line W2 of center line W1 and outer surface 202b overlaps on the orthographic projection direction of glass substrate.
With reference to Figure 14 and Figure 15, the inner surface 201b has a center line L1, the appearance in the longitudinal direction Face 202b also has a center line L2 in the longitudinal direction.The inner surface 201b is symmetrical along center line L1 minute surfaces.The appearance Face 202b is symmetrical along center line L2 minute surfaces.Glass substrate is placed on horizontal plane, the glass substrate is made just in the horizontal plane Projection, the center line L2 of the center line L1 and outer surface 202b of the inner surface 201b is heavy on the orthographic projection direction of glass substrate Close.The orthographic projection of described center line L1, L2 is vertical with the orthographic projection of described center line W1, L2.
The inner surface 201b centered on the center line L1 of length direction to same lateral bend, the outer surface 202b also with To the same lateral bend centered on the center line L2 of length direction.The circle of the center line L1 of the length direction of the inner surface 201b Arc radius are 50~1000mm, the arc radius of the center line L2 of the length direction of the outer surface 202b also for 50~ 1000mm.In the embodiment shown in FIG., the inner surface 201b and outer surface 202b center line L1, L2 in the longitudinal direction Arc radius it is equal.
The inner surface 201b is simultaneously to the same lateral bend, the appearance also centered on the center line W1 of width Face 202b is to the same lateral bend yet centered on the center line W2 of width.The width of the inner surface 201b The arc radius of center line W1 are 50~1000mm, the arc radius of the center line W2 on the width of the outer surface 202b Also it is 50~1000mm.The arc radius of the inner surface 201b and outer surface 202b center line W1, W2 in the direction of the width It is equal.
The height of the glass substrate is 0.5~5mm.The height refers to, the central point of the outer surface 202b (namely The intersection point of the center line W2 on center line L2 and width on length direction) it is minimum extremely to the position of the inner surface 201 The distance between plane that few three points are formed.Shown in figure in embodiment, in the corner of inner surface 201b is generally aligned in the same plane, The distance between central point of plane and outer surface 202b where the height namely the corner.
In certain embodiments, the thickness everywhere of glass substrate is uniform.Stress concentration so can be preferably eliminated, is lifted Bulk strength.
In addition, the arc radius of center line W1, W2 can be equal with the arc radius of center line L1, L2, it is also possible to not phase Deng.
In certain embodiments, the circular arc of inner surface 201b and outer surface 202b center line L1, L2 in the longitudinal direction Corresponding central angle is C1, wherein 60 ° of 180 ° of < C1 <.Inner surface 201b and outer surface 202b center line in the direction of the width The corresponding central angle of circular arc of W1, W2 is C2, wherein 60 ° of 180 ° of < C2 <.
Each technical characteristic of embodiment described above can be combined arbitrarily, to make description succinct, not to above-mentioned reality Apply all possible combination of each technical characteristic in example to be all described, as long as however, the combination of these technical characteristics is not deposited In contradiction, the scope of this specification record is all considered to be.
A kind of cover-plate glass stepped construction that the utility model is provided, at least has the advantage that:
Decorative layer is set between hardened layer and tack coat, such as increases the black ring of camera, the hardened layer with black ring passes through Tack coat is pasted on the glass substrate, is thusly-formed cover-plate glass stepped construction and is avoided that the vision that camera alignment error brings Influence, can so simplify operation so as to reduce alignment error, the yield of product be effectively improved, simultaneously because avoiding shooting The visual impact that head alignment error brings, so as to improve Consumer's Experience.Again or, such as set between hardened layer and tack coat Decorative layer as character or icon is put, the display effect of character or icon can be obviously improved, lift Consumer's Experience.
Embodiment described above only expresses several embodiments of the present utility model, and its description is more specific and detailed, But therefore can not be interpreted as the limitation to the utility model the scope of the claims.It should be pointed out that common for this area For technical staff, without departing from the concept of the premise utility, various modifications and improvements can be made, these all belong to In protection domain of the present utility model.Therefore, the protection domain of the utility model patent should be determined by the appended claims.

Claims (9)

1. a kind of cover-plate glass stepped construction, it is characterised in that including:
Glass substrate, including inner surface, the outer surface being spaced with the inner surface;
Tack coat, is covered in and is provided with the inner surface of the glass substrate;
Decorative layer, is formed on a surface away from the glass substrate of the tack coat;And
Hardened layer, is formed on a surface away from the tack coat of the decorative layer.
2. cover-plate glass stepped construction according to claim 1, it is characterised in that the decorative layer is black ring.
3. cover-plate glass stepped construction according to claim 2, it is characterised in that the black ring is the ring with manhole Shape structure.
4. cover-plate glass stepped construction according to claim 1, it is characterised in that the cover-plate glass stepped construction is also wrapped UV texture layers, evaporation layer and base ink layer are included, the hardened layer, UV texture layers, evaporation layer and base ink layer are stacked gradually Set.
5. cover-plate glass stepped construction according to claim 4, it is characterised in that the thickness of the hardened layer is 2~5 μ m。
6. cover-plate glass stepped construction according to claim 1, it is characterised in that the hardened layer is UV texture layers, institute Stating cover-plate glass stepped construction also includes evaporation layer and ink layer, and the hardened layer, evaporation layer and ink layer are cascading.
7. cover-plate glass stepped construction according to claim 6, it is characterised in that the thickness of the hardened layer is 10~20 μm。
8. cover-plate glass stepped construction according to claim 1, it is characterised in that the thickness of the tack coat is 5~20 μ m。
9. the cover-plate glass stepped construction according to any one of claim 1 to 8, it is characterised in that the glass substrate tool There is at least part of curved surface.
CN201621156133.9U 2016-10-31 2016-10-31 Cover-plate glass stepped construction Active CN206297221U (en)