CN206161618U - Capability test appearance is restoreed in selfreparing coating crack - Google Patents
Capability test appearance is restoreed in selfreparing coating crack Download PDFInfo
- Publication number
- CN206161618U CN206161618U CN201621153437.XU CN201621153437U CN206161618U CN 206161618 U CN206161618 U CN 206161618U CN 201621153437 U CN201621153437 U CN 201621153437U CN 206161618 U CN206161618 U CN 206161618U
- Authority
- CN
- China
- Prior art keywords
- corrosion resistant
- resistant plate
- crack
- plate
- communicating pipe
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model discloses a capability test appearance is restoreed in selfreparing coating crack, it includes that glass pipe, cooperation set up at the first clamp plate of glass socle portion, set up communicating pipe, cooperation in glass pipe below and sets up second clamp plate and the cooperation third clamp plate that sets up mouthful department at the bottom of communicating pipe in communicating pipe department suitable for reading, a serial communication port, the end of communicating pipe is equipped with crack control unit, crack control unit includes left corrosion resistant plate, right corrosion resistant plate and is used for connecting left corrosion resistant plate and right corrosion resistant plate's adjusting screw, one side central point that left side corrosion resistant plate and right corrosion resistant plate splice each other puts and is equipped with the notch respectively. The beneficial effects of the utility model are that, in test procedure, adjusting screw on the control unit of crack, it films to make receives the pulling force to can adjust fracture width, more accord with the nature of filming and form fissured state and width size, can reach better experiment effect.
Description
Technical field
This utility model is related to coating test instrunment technical field, and in particular to self-healing coatings crack repairing performance is tested
Instrument.
Background technology
Self-healing coatings are a kind of new coatings for having an automatic healing ability, and nearly more than ten years have developed rapidly, multiple
Field is widely used.This kind of material is just widely studied at present, is developed this coating by with very high Jing
Ji value.But with developing rapidly for this new material, the test mode of self-healing coatings, method of testing, test equipment instrument
Device does not all obtain improving well and development.Cause test project all can not state well selfreparing elastomeric material from
Repairing performance, invent it is a kind of can simulate dry formed and repair state equipment be very important.
A critically important performance of self-healing coatings is exactly to test the crack self-healing time.Artificially coating entered before test
Row manufacture crack, becomes the key technology in test performance.The various states such as fracture length, the width of manufacture, can serious shadow
Ring the test result to the later stage.The reason for causing building coating layer to ftracture species is very more, mainly have base layer structure cracking, it is greasy
Sublayer cracking, base treatment is improper, coating dehydration is too fast etc., and reason causes.Coating is flexible material, and base material cracking can make coating
Film produces crack, and coating film receives pulling force in engineering, and there is certain width in the crack of film self-assembling formation(0.2~
0.5mm).Some meetings are bigger.Fracture width is accurately manufactured, stress during phenomenon simulation crack occurrence is to design this
The important references factor of class testing instrument.
Mostly manufacture crack using patterning method at present.
1st, single blade directly cuts manufacture crack:
Row are such as:The crack of 5mm length is directly cut out at test specimen center with the wallpaper knife of 0.5mm thickness, is then split at this
Sew on the certain hydraulic pressure of loading to be tested.Secondary method is easy to operate simple, and error is little;But the crack that secondary method cuts out, by
In the resilience of flexible paint itself, cause fracture width to be substantially not reaching to desired width, load during test after hydraulic pressure,
Leakage very little at crack, is unfavorable for embodying the self-repairability of coating.And be not inconsistent with the fracture width of appearance in engineering.
2nd, double blade cutting manufacture crack:
Row are such as:The crack of 5mm length is cut out at test specimen center with the wallpaper knife of two panels 0.5mm thickness is simultaneously neat, in two blades
The distance of point of a knife is 0.5mm, and the crack of 0.5mm width can be cut out on film, is then loaded on this crack certain
Hydraulic pressure is tested.The method is easy to operate simple;But the fracture width for cutting out can not be controlled accurately, and fracture width is general
0.5mm can be more than, and the width for cutting out every time is inconsistent.Load after hydraulic pressure during test, leakage is very big at crack, also unfavorable
In the self-repairability for embodying coating.And be to dig up 0.5mm*5mm sizes from painting center membrane in this crack manufacture process
Coating, so as to produce crack.The crack caused by film disappearance, carries out state and does not meet with actual engineering crackses.Survey
The accuracy of examination film self-healing properties also can heavy discount greatly.
Utility model content
For the problem that prior art is present, this utility model provides the self-healing coatings crack prosthetic of simple structure
Can tester.
The technical solution of the utility model is as follows:
Self-healing coatings crack repairing performance tester, including glass tubing, be equipped with glass bottom of the tube first press
Plate, the communicating pipe being arranged on below glass tubing, be equipped with communicating pipe place suitable for reading the second pressing plate and be equipped with connection
The 3rd pressing plate at ttom of pipe mouth, it is characterised in that the end of the communicating pipe is provided with Crack Control part, the Crack Control portion
Part includes left corrosion resistant plate, right corrosion resistant plate and the adjusting screw rod for connecting left corrosion resistant plate and right corrosion resistant plate, the left side
One side center that corrosion resistant plate and right corrosion resistant plate mutually splice is respectively equipped with notch.
Described self-healing coatings crack repairing performance tester, it is characterised in that the notch is U-type groove mouth, and a left side is not
Notch on rust steel plate is symmetrical arranged and equivalently-sized with the notch on right corrosion resistant plate.
Described self-healing coatings crack repairing performance tester, it is characterised in that the left corrosion resistant plate and the right side are stainless
The center of steel plate is respectively welded and is provided for the nut that adjusting screw rod interts installation.
Described self-healing coatings crack repairing performance tester, it is characterised in that the left corrosion resistant plate and the right side are stainless
Installing hole is respectively equipped with steel plate, and installing hole is kidney ellipsoid structure.
Described self-healing coatings crack repairing performance tester, it is characterised in that the installing hole is in left corrosion resistant plate
And two are respectively equipped with right corrosion resistant plate, and left corrosion resistant plate is symmetrical arranged with the installing hole on right corrosion resistant plate.
Described self-healing coatings crack repairing performance tester, it is characterised in that the left corrosion resistant plate is stainless with the right side
Plate size size is identical.
The beneficial effects of the utility model are, in test process, the adjusting screw rod on Crack Control part receives film
To pulling force, and fracture width can be adjusted, more meet the state and width dimensions in film self-assembling formation crack, can be reached preferably
Experiment effect.
Description of the drawings
Fig. 1 is structural representation of the present utility model;
In figure:1st, glass tubing, the 2, first pressing plate, the 3, second pressing plate, the 4, the 3rd pressing plate, 5, right corrosion resistant plate, 6, left stainless
Steel plate, 7, adjusting screw rod, 8, installing hole, 9, communicating pipe.
Specific embodiment
This utility model is described in further detail with reference to Figure of description.
As shown in figure 1, self-healing coatings crack repairing performance tester of the present utility model, including the pressure of glass tubing 1, first
Plate 2, the second pressing plate 3, the 3rd pressing plate 4, right corrosion resistant plate 5, left corrosion resistant plate 6, adjusting screw rod 7, installing hole 8 and communicating pipe 9.The
One pressing plate 2 is equipped with the bottom of glass tubing 1, is arranged on the lower section of glass tubing 1 communicating pipe 9, and the second pressing plate 3 is arranged on connection
The place suitable for reading of pipe 9, the 3rd pressing plate 4 is arranged at the base opening of communicating pipe 9, and the first pressing plate 2 is passed through between communicating pipe 9 and glass tubing 1
It is fixedly connected with the second pressing plate 3, Crack Control part is located at the base opening of communicating pipe 9 and is fixedly connected by the 3rd pressing plate 4, crack control
Part processed includes right corrosion resistant plate 5, left corrosion resistant plate 6 and adjusting screw rod 7, right corrosion resistant plate 5 and the size phase of left corrosion resistant plate 6
Together, right corrosion resistant plate 5 and the upper surface center position of left corrosion resistant plate 6 are respectively welded a nut, the interspersed peace of adjusting screw rod 7
It is mounted between two nuts, for adjusting the distance between right corrosion resistant plate 5 and left corrosion resistant plate 6, installing hole 8 is in left rustless steel
Plate 6 and right corrosion resistant plate 5 are respectively provided with two, and left corrosion resistant plate 6 is symmetrical arranged with the installing hole 8 on right corrosion resistant plate 5, peace
Dress hole 8 adopts kidney ellipsoid structure, is easy to the regulation that moves left and right of left corrosion resistant plate 6 and right corrosion resistant plate 5, left corrosion resistant plate 6 and
One side center position of the mutually splicing of right corrosion resistant plate 5 is respectively equipped with notch, and notch adopts specification for 10mm*2mmU type grooves
Mouthful, and the notch on left corrosion resistant plate 6 is symmetrical arranged with the notch on right corrosion resistant plate 5.
Test process:
It is step one, first Crack Control member align and fixed with adjusting screw rod 7, Crack Control part centre after aliging
The 10mm*2mmU type groove mouth small piece of tape of two fixes the notch for being spliced into a 10mm*4mm, in the Crack Control part back of the body
Spliced notch is filled up with the unit of plastic of 10mm*4mm*3mm in face so that Crack Control component back surface is smooth, and easily blade coating is applied
Material;
Step 2, coat by several times on Crack Control component back surface and specify proportioning mixed polymer cement waterproof paint
Test portion, makes coating layer thickness be 1.5-2.0mm, presses《Polymer cement paint》7.4.2 regulations in GB/T 23445-2009 standards
Method is conserved, is dried;
Fixed adhesive tape, carefully throws off the unit of plastic of prior landfill on step 3, removing Crack Control part, makes coating sudden and violent
Dew, with 0.5mm heavy wall paper knives the crack of long 5mm is gone out in exposed film heartcut;
Step 4, slow adjusting screw rod 7 so that left corrosion resistant plate 6 is parallel with right corrosion resistant plate 5 to be pulled open, and drives crack
The film crack of well cutting is slowly opened on control unit, and when film fracture width reaches desired value, stop the rotation adjusting screw rod
7;
Step 5, Crack Control part and communicating pipe 9 are connected and fixed on test stand, junction is close with fluid sealant
Envelope, injects in glass tubing 1(23±2)DEG C clean water, make liquid level to test specimen center height be 300mm, in process of the test
In make the height that liquid level maintains like;Infiltration situation at observation test specimen crack, records impermeable at from water filling to test specimen crack
Time;
Step 6, the test specimen after test is placed 24h under standard test conditionss, whether observation test specimen is closed at crack,
If crack closure, test passes through.
Claims (6)
1. self-healing coatings crack repairing performance tester, including glass tubing(1), be equipped with glass tubing(1)The of bottom
One pressing plate(2), be arranged on glass tubing(1)The communicating pipe of lower section(9), be equipped with communicating pipe(9)Second pressing plate at place suitable for reading
(3)And be equipped with communicating pipe(9)The 3rd pressing plate at base opening(4), it is characterised in that the communicating pipe(9)End set
There is Crack Control part, the Crack Control part includes left corrosion resistant plate(6), right corrosion resistant plate(5)And for connecting a left side not
Rust steel plate(6)With right corrosion resistant plate(5)Adjusting screw rod(7), the left corrosion resistant plate(6)And right corrosion resistant plate(5)Mutually spell
One side center for connecing is respectively equipped with notch.
2. self-healing coatings crack repairing performance tester according to claim 1, it is characterised in that the notch is U
Type groove mouth, left corrosion resistant plate(6)On notch and right corrosion resistant plate(5)On notch be symmetrical arranged and equivalently-sized.
3. self-healing coatings crack repairing performance tester according to claim 1, it is characterised in that the left rustless steel
Plate(6)And right corrosion resistant plate(5)Center be respectively welded and be provided for adjusting screw rod(7)The interspersed nut installed.
4. the self-healing coatings crack repairing performance tester according to claim 1 or 3, it is characterised in that it is described it is left not
Rust steel plate(6)And right corrosion resistant plate(5)On be respectively equipped with installing hole(8), and installing hole(8)For kidney ellipsoid structure.
5. self-healing coatings crack repairing performance tester according to claim 4, it is characterised in that the installing hole
(8)In left corrosion resistant plate(6)And right corrosion resistant plate(5)On be respectively equipped with two, and left corrosion resistant plate(6)With right corrosion resistant plate
(5)On installing hole(8)It is symmetrical arranged.
6. self-healing coatings crack repairing performance tester according to claim 1, it is characterised in that the left rustless steel
Plate(6)With right corrosion resistant plate(5)Size is identical.