CN205800391U - A kind of protecting film of band touch-control site - Google Patents
A kind of protecting film of band touch-control site Download PDFInfo
- Publication number
- CN205800391U CN205800391U CN201620572043.1U CN201620572043U CN205800391U CN 205800391 U CN205800391 U CN 205800391U CN 201620572043 U CN201620572043 U CN 201620572043U CN 205800391 U CN205800391 U CN 205800391U
- Authority
- CN
- China
- Prior art keywords
- touch
- control site
- protecting film
- control
- layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model discloses the protecting film of a kind of band touch-control site; including the scratch resistant layer set gradually from top to bottom and anti-riot layer; the lower surface of described anti-riot layer is provided with adhesive linkage and several spaced touch-control sites; described touch-control site is positioned at the zone line of described anti-riot layer, and described adhesive linkage is positioned at the surrounding of described anti-riot layer.The beneficial effects of the utility model: the application provides that a kind of centre is unsettled, the protecting film of surrounding band glue form; to avoid white edge phenomenon; and it is configured the touch-control site array in unsettled region in the middle of protecting film, it is possible to reduce the water wave that protecting film and screen contact produce prints or the phenomenon of rainbow stricture of vagina.
Description
Technical field
This utility model relates to a kind of protecting film, particularly relates to the protecting film of a kind of band touch-control site.
Background technology
Mobile phone curve tempering protecting film in the market mainly has two kinds, and a kind of is the guarantor that fit in centre, surrounding is unsettled
Cuticula, the protecting film that fit in this centre, surrounding is unsettled reduces form to ensure arcing point white edge problem, directly affects and disappear
The satisfaction of the person of expense;Another kind is middle unsettled, the protecting film of surrounding band glue form, and the contact surface of its protecting film does not processes,
Cause this protecting film that Contact-sorption after contacting with glass screen, can be produced, produce the obvious contact area of naked eyes and dynamics effect
Under water wave print or rainbow stricture of vagina, cause screen surface touch area obscure.Additionally, bump contact also will result in screen touch-control essence
Degree declines, and directly affects the user satisfaction that mobile phone protect by consumer, thus be necessary existing protecting film is improved with
Perfect.
Utility model content
The technical problems to be solved in the utility model is, for drawbacks described above of the prior art, it is provided that a kind of structure
Advantages of simple, the protecting film of band touch-control site of low cost of manufacture.
This utility model solves its technical problem and be the technical scheme is that
The protecting film of a kind of band touch-control site is provided, including the scratch resistant layer set gradually from top to bottom and anti-riot layer, described
The lower surface of anti-riot layer is provided with adhesive linkage and several spaced touch-control sites, and described touch-control site is positioned at described anti-riot
The zone line of layer, described adhesive linkage is positioned at the surrounding of described anti-riot layer.
In the protecting film of band touch-control site described in the utility model, several described touch-control sites surround site battle array
Row.
In the protecting film of band touch-control site described in the utility model, adjacent two in neighbouring or left and right are described to be touched
The spacing of control site is 1mm~3mm.
In the protecting film of band touch-control site described in the utility model, described touch-control site is for being fixed on described anti-riot layer
On column structure or cone structure, the height of described touch-control site is 0.04mm~0.08mm.
In the protecting film of band touch-control site described in the utility model, described touch-control site is cylindrical structure, described
The section radius of cylindrical structure is 0.01mm~0.03mm.
In the protecting film of band touch-control site described in the utility model, described anti-riot layer includes base material and is attached to described
The glue-line of the upper surface of base material, described glue-line conforms to the lower surface of described scratch resistant layer, and described touch-control site projection is at described base
The lower surface of material.
In the protecting film of band touch-control site described in the utility model, described scratch resistant layer is tempering film.
In sum, implement the protecting film of a kind of band touch-control site of the application, have the advantages that the application carries
Unsettled, the protecting film of surrounding band glue form for a kind of centre, to avoid white edge phenomenon, and is configured suspension area in the middle of protecting film
The touch-control site array in territory, it is possible to reduce the water wave that protecting film and screen contact produce prints or the phenomenon of rainbow stricture of vagina, additionally, due to
Reduce touch-control active area, touch accuracy can be improved, improve Consumer's Experience effect.
Accompanying drawing explanation
Below in conjunction with drawings and Examples, the utility model is described in further detail, in accompanying drawing:
Fig. 1 is the profile of the protecting film of a kind of band touch-control site that this utility model preferred embodiment provides;
Fig. 2 is the profile affixing on screen by the protecting film of the site of band touch-control shown in Fig. 1;
Fig. 3 is the structural representation affixing on screen by protecting film without touch-control site in prior art;
Fig. 4 is the structural representation affixing on screen by the protecting film of the site of band touch-control shown in Fig. 1;
Fig. 5 is the mobile phone of the protecting film being stained with the site of band touch-control shown in Fig. 1.
Detailed description of the invention
In order to make the purpose of this utility model, technical scheme and advantage clearer, below in conjunction with accompanying drawing and enforcement
Example, is further elaborated to this utility model.Should be appreciated that specific embodiment described herein is only in order to explain
This utility model, is not used to limit this utility model.
As it is shown in figure 1, this utility model provides the protecting film of a kind of band touch-control site, including setting gradually from top to bottom
Scratch resistant layer 1 and anti-riot layer 2, the lower surface of anti-riot layer 2 is provided with adhesive linkage 3 and several spaced touch-control sites 4, if
Dry touch-control site 4 is positioned at the zone line of anti-riot layer 2, and adhesive linkage 3 is positioned at the surrounding of anti-riot layer 2 and sets around touch-control site 4
Put.
The scratch resistant layer 1 of the present embodiment is tempering film, and it has the high grade of transparency and rigidity, and the surface of tempering film is enough hard, and
Scratch resistance, it is possible to the article phase mutual friction that is prevented effectively from daily life and the phenomenon being scratched.Explosion-proof layer 2 is anti-riot film, permissible
Being scattered after preventing glass fragmentation faced and damage people, explosion-proof layer 2 includes base material 22 and is attached to the glue-line of upper surface of base material 22
21, glue-line 21 conforms to the lower surface of scratch resistant layer 1, between scratch resistant layer 1 and base material 22, several touch-control sites 4 and bonding
Layer 3 is positioned at the lower surface of base material 22.
Adhesive linkage 3 is double faced adhesive tape, and it is for sticking to screen 5 by protecting film, shown in Fig. 2, when protecting film passes through
When adhesive linkage 3 sticks on screen 5, it is positioned at the touch-control site 4 in the middle of anti-riot film 2 and abuts to screen 5, make the protecting film of the application
Forming that a kind of centre is unsettled, the structure of surrounding band glue form, this centre is unsettled, the protecting film of surrounding band glue form can be effective
Avoid white edge phenomenon.
Further, be configured in the touch-control site 4 in middle unsettled region may be used for reducing anti-riot film 2 and screen 5 it
Between Contact-sorption.Fig. 3 is the schematic diagram that the protecting film without touch-control site is pasted onto on screen 5, depresses pressing of finger, by
Without any support between this kind of protecting film contact surface and screen 5, the Contact-sorption big by producing extensibility, Contact-sorption a1's
Area will be greater than 1.3mm2, thus produce obviously water wave print or rainbow stricture of vagina.Fig. 4 is the protection of the application band touch-control site
Film is pasted onto the schematic diagram on screen 5, at finger by pressure, due to the support of touch-control site 4, can eliminate anti-riot film 2 and screen 5
The interference produced during contact, makes the area of Contact-sorption a2 be not more than 1.3mm2, it is greatly reduced touch-control sensing, reaches to solve
Water wave print or the phenomenon of rainbow stricture of vagina.Additionally, due to the contact area between the protecting film 2 of the application and screen 5 is little, it is possible to reduce touch
Control active area, improves touch accuracy, thus improves Consumer's Experience effect.
In order to avoid due to the distance between adjacent two touch-control sites 4 different, and cause between protecting film and screen 5
Subregion produces water wave print or rainbow stricture of vagina, and the touch-control site 4 of the application surrounds the form of site array, has been distance, big
Little and that printing points highly is on anti-riot film 2 row and column, as shown in Figure 5.In the present embodiment, neighbouring or left and right is adjacent
The spacing of two touch-control sites 4 is 1mm~3mm, it is preferred that the spacing of adjacent two touch-control sites 4 is 1.5mm.
Touch-control site 4 can be projection at the column structure of anti-riot film 2 lower surface or cone structure, such as cylinder, circular cone
Body or prism etc., the height of touch-control site 4 is 0.04mm~0.08mm.In the present embodiment, touch-control site 4 is tied for cylinder
Structure, its height is 0.06mm, and the section radius of this cylindrical structure is 0.01mm~0.03mm.
In sum, implement the protecting film of a kind of band touch-control site of the application, have the advantages that the application carries
Unsettled, the protecting film of surrounding band glue form for a kind of centre, to avoid white edge phenomenon, and is configured suspension area in the middle of protecting film
The touch-control site array in territory, it is possible to reduce the water wave that protecting film and screen contact produce prints or the phenomenon of rainbow stricture of vagina, additionally, due to
Reduce touch-control active area, touch accuracy can be improved, improve Consumer's Experience effect.
Although this utility model is illustrated by specific embodiment, it will be appreciated by those skilled in the art that, not
In the case of departing from this utility model scope, it is also possible to this utility model is carried out various conversion and equivalent substitutes.It addition, for
Particular condition or material, can make various amendment, without deviating from scope of the present utility model to this utility model.Therefore, this reality
Be not limited to disclosed specific embodiment with novel, and should include falling in this utility model right whole
Embodiment.
Claims (7)
1. the protecting film of a band touch-control site, it is characterised in that include that the scratch resistant layer (1) set gradually from top to bottom is with anti-riot
Layer (2), the lower surface of described anti-riot layer (2) is provided with adhesive linkage (3) and several spaced touch-control sites (4), described
Touch-control site (4) is positioned at the zone line of described anti-riot layer (2), and described adhesive linkage (3) is positioned at the surrounding of described anti-riot layer (2).
The protecting film of band touch-control site the most according to claim 1, it is characterised in that several described touch-control sites (4)
Surround site array.
The protecting film of band touch-control site the most according to claim 2, it is characterised in that neighbouring or left and right adjacent two
The spacing of individual described touch-control site (4) is 1mm~3mm.
The protecting film of band touch-control site the most according to claim 2, it is characterised in that described touch-control site (4) is fixing
Column structure on described anti-riot layer (2) or cone structure, the height of described touch-control site (4) is 0.04mm~0.08mm.
The protecting film of band touch-control site the most according to claim 4, it is characterised in that described touch-control site (4) is cylinder
Body structure, the section radius of described cylindrical structure is 0.01mm~0.03mm.
The protecting film of band touch-control site the most according to claim 1, it is characterised in that described anti-riot layer (2) includes base material
(22) and be attached to the glue-line (21) of upper surface of described base material (22), described glue-line (21) conforms to described scratch resistant layer (1)
Lower surface, described touch-control site (4) projection lower surface in described base material (22).
The protecting film of band touch-control site the most according to claim 1, it is characterised in that described scratch resistant layer (1) is tempering film.