CN205726659U - Fingerprint recognition FPC reinforcement steel disc and the material strip of excessive glue can be solved - Google Patents
Fingerprint recognition FPC reinforcement steel disc and the material strip of excessive glue can be solved Download PDFInfo
- Publication number
- CN205726659U CN205726659U CN201620564924.9U CN201620564924U CN205726659U CN 205726659 U CN205726659 U CN 205726659U CN 201620564924 U CN201620564924 U CN 201620564924U CN 205726659 U CN205726659 U CN 205726659U
- Authority
- CN
- China
- Prior art keywords
- steel disc
- hot
- setting adhesive
- material strip
- reinforcement steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
This utility model discloses reinforcement steel disc and the material strip of a kind of fingerprint recognition FPC that can solve excessive glue, reinforcement steel disc includes steel disc body and hot-setting adhesive, together with hot-setting adhesive is fixedly installed with steel disc body, the outer edge of the outer edge distance steel disc body of hot hot-setting adhesive is 0.15~0.3mm, material strip includes more than material strip support part and row reinforcement steel disc described above, and reinforcement steel disc is arranged in material strip support part.Hot-setting adhesive with hot-setting adhesive kind, pressing parameter, shape of product and size etc., is recessed in reinforcement steel disc 0.15 to 0.3mm according to the overflow producing cause of glue of hot-setting adhesive by this utility model, it is possible to resolve hot-setting adhesive overflows glue and the problem that causes FPC disabler.
Description
Technical field
The open a kind of fingerprint identification device accessory of this utility model, a kind of fingerprint recognition FPC that can solve excessive glue
Reinforcement steel disc and material strip.
Background technology
Along with image scan and the development of the technology of identification, fingerprint recognition application in people live is more and more wider
General, such as: fingerprint clocking-in machine, unlocked by fingerprint etc..And the identification module in fingerprint recognition machine is normally mounted on FPC,
And this FPC is usually provided with reinforcement steel disc at the back side of fingerprint identification module installation site, for this position is carried out reinforcement, mend
Strong steel disc is typically with hot-setting adhesive and is fitted on FPC, at present, fingerprint recognition FPC in hot pressing production process, reinforcement steel
The hot-setting adhesive of sheet laminating usually there will be excessive glue phenomenon, and the glue that overflows then can cause FPC disabler, there is serious quality hidden danger.
Summary of the invention
Excessive glue is easily produced the when of for fingerprint recognition FPC hot pressing reinforcement steel disc of the prior art mentioned above
Problem, this utility model provides a kind of fingerprint recognition FPC reinforcement steel disc that can solve excessive glue and material strip, and it uses special processing
Hot-setting adhesive monolithic is arranged and is fitted on reinforcement steel disc material strip by technique, and hot-setting adhesive is recessed in reinforcement steel disc 0.15mm~0.3mm,
Hot-setting adhesive can be solved overflow the problem of glue.
This utility model solves its technical problem and the technical scheme is that a kind of fingerprint recognition FPC that can solve excessive glue
Reinforcement steel disc, reinforcement steel disc includes steel disc body and hot-setting adhesive, together with hot-setting adhesive is fixedly installed with steel disc body, thermosetting
The outer edge of the outer edge distance steel disc body of glue is 0.15~0.3mm.
A kind of reinforcement steel disc material strip, material strip includes more than material strip support part and row reinforcement steel disc described above, reinforcement
Steel disc is arranged in material strip support part.
This utility model solves the technical scheme of its technical problem employing and further comprises:
Fabrication hole is offered, outside the outer edge distance fabrication hole of the hot-setting adhesive around fabrication hole on described steel disc body
Edge is 0.15~0.3mm.
Described material strip support part is respectively provided on two sides with hole, location, and each steel disc body is provided with a location
Hole.
Described reinforcement steel disc is provided with two rows.
The wall scroll gummed paper length of described hot-setting adhesive is at 150mm.
The beneficial effects of the utility model are: this utility model overflows the producing cause of glue with hot-setting adhesive kind according to hot-setting adhesive
Class, pressing parameter, shape of product and size etc., be recessed in reinforcement steel disc 0.15 to 0.3mm by hot-setting adhesive, it is possible to resolve hot-setting adhesive overflows
Glue and the problem that causes FPC disabler.
Below in conjunction with the drawings and specific embodiments, this utility model is described further.
Accompanying drawing explanation
Fig. 1 is this utility model monolithic Facad structure schematic diagram.
Fig. 2 is this utility model monolithic structure schematic diagram.
Fig. 3 is this utility model monolithic cross-sectional view.
Fig. 4 is this utility model material-strap structure schematic diagram.
In figure, 1-steel disc body, 2-hot-setting adhesive, 3-fabrication hole, 4-material strip support part, 5-positions hole.
Detailed description of the invention
The present embodiment is this utility model preferred implementation, and other its principles all are identical with the present embodiment with basic structure
Or approximation, all within this utility model protection domain.
Refer to accompanying drawing 1, accompanying drawing 2 and accompanying drawing 3, in this utility model, reinforcement steel disc mainly includes steel disc body 1 and thermosetting
Glue 2, together with hot-setting adhesive 2 is fixedly installed with steel disc body 1, hot-setting adhesive 2 is recessed in reinforcement steel disc body 0.15~0.3mm, i.e.
The outer edge 0.15~0.3mm of the outer edge distance steel disc body 1 of hot-setting adhesive 2, it can effectively ensure reinforcement steel disc and FPC
Between bonding strength, can effectively solve again the hot-setting adhesive 2 excessive glue problem in hot pressing.In the present embodiment, at steel disc
Offer fabrication hole 3 on body 1, around fabrication hole 3, also be provided with hot-setting adhesive 2, outside the outer edge distance fabrication hole 3 of hot-setting adhesive 2
Edge is also 0.15~0.3mm.
Refer to accompanying drawing 4, this utility model protects a Seed packaged band simultaneously, and it stamps out single steel disc body 1 on steel band
Being formed, material strip includes the single steel disc body 1 of more than material strip support part 4 and a row, and in the present embodiment, steel disc body 1 sets
There are two rows, material strip support part 4 to be respectively provided on two sides with hole 5, location, each steel disc body 1 is provided with hole 5, a location.
Manufacturing process of the present utility model comprises the steps:
1, design hot-setting adhesive and reinforcement steel disc, owing to bi-material is required to design size, arrangement etc., design sequence regardless of
Successively:
A, hot-setting adhesive design: with reinforcement steel disc a size of radix, hot-setting adhesive be recessed in reinforcement steel disc body 0.15~
0.3mm;
B, reinforcement steel disc design: carry out typesetting according to reinforcement steel disc size, and during typesetting, necessary related positioning process hole 5 is together
Design typesetting, meanwhile, carries out punching mold part design according to typesetting, carries out punching mold part design according to typesetting, location
Fabrication hole 5 designs in steel band scrap area (i.e. material strip support part 4), for gummed paper location and the location of second time punching press;
2, hot-setting adhesive carries out wall scroll design with reference to reinforcement steel disc typesetting, makees with the positioning process hole 5 on reinforcement steel disc material strip
For positioning datum.In order to ensure machining accuracy, wall scroll gummed paper length uses cutting die cross cutting or five metals at about 150mm, gummed paper
Stamping die punching press production method makes;
3, use high velocity ram machine (punching speed 300 times/min of >) that steel band carries out punch process, for the first time punching press bag for the first time
Containing the positioning process hole 5 on material strip and fabrication hole 3 punch forming together on product;
4, making localization tool, localization tool uses aluminium sheet or bakelite plate material to make.Positioning needle on tool should exceed
Tool face about 3-5mm, positions the steel band after first time punching press and the wall scroll hot-setting adhesive after cross cutting for borehole jack and enters tool positioning needle,
Use flatiron pressing hot-setting adhesive after pressing, allow it be pasted on the steel band after for the first time punching press;
5, using hot press that the steel band after hot pressure hot-setting adhesive is carried out pressing, parameter during hot pressing is, air pressure 0.8Mpa, temperature
Spending 120-150 DEG C, hot pressing time is 2 seconds, and in bonding processes, pressing machine must be smooth, and homogeneous temperature just can ensure that the steel after pressing
Carry non-foaming with hot-setting adhesive, without impression and water wave.In order to reach this requirement, the making using hot press in the present embodiment need to be according to
The processing mode of precision die makes, and hot press heating board and lower force fit plate use SKD-11 structural section to make, and material is by super
Cryogenic technology processes, and hardness can reach HRC60-62 °, ground flat degree < 0.02mm, hot press heating board and lower force fit plate
Guide and use four guide pillar structures to guide, guide guide pillar and guide pin bushing uses vacuum heat processing, prevent deformation, concentricity requirement <
0.01mm.Temperature control system in the present embodiment uses 4 heat-generating pipe modes to make, it is ensured that heating board heating is uniformly.
6, the steel band after pressing hot-setting adhesive using laminating machine laminating, laminating parameter is upper glue roller 150 DEG C, lower rubber roller 140
DEG C, speed 0.3m/min;
7, the steel band after laminating hot-setting adhesive use high velocity ram machine (punching speed 300 times/min of >) carry out second time punching press, the
Use positioning process hole 5 to position during two times punch, make difform reinforcement steel disc product, production according to customer demand
Becoming coiled strip to be easy to SMT automatic chip mounting, in the present embodiment, in punching course, reinforcement steel disc need to connect material by fight back in mould to steel band
Producing, after i.e. punching press is cut off, lower mold is by origin-location in steel disc jack-up to material strip, and material strip uses automatic material receptacle to carry out rewinding row
Useless, the hot-setting adhesive glue surface using silica gel single layer protection film (viscosity is 10-15g) to be pasted on reinforcement steel disc during rewinding carries out rolling,
I.e. there iing hot-setting adhesive one side to attach silica gel single layer protection film, on the one hand playing a protective role, on the other hand, moreover it is possible to keep steel disc
Together with material strip, production becomes coiled strip to be easy to client's SMT automatic chip mounting.
This utility model overflows the producing cause of glue with hot-setting adhesive kind, pressing parameter, shape of product and big according to hot-setting adhesive
Little etc., hot-setting adhesive is recessed in reinforcement steel disc 0.15 to 0.3mm, it is possible to resolve hot-setting adhesive overflows glue and causes asking of FPC disabler
Topic.
Claims (5)
1. can solve a reinforcement steel disc for fingerprint recognition FPC of excessive glue, it is characterized in that: described reinforcement steel disc includes that steel disc is originally
Body and hot-setting adhesive, together with hot-setting adhesive is fixedly installed with steel disc body, the outer edge of the outer edge distance steel disc body of hot-setting adhesive
It is 0.15~0.3mm.
The reinforcement steel disc of fingerprint recognition FPC that can solve excessive glue the most according to claim 1, is characterized in that: described steel
Offer fabrication hole on sheet body, the outer edge of the outer edge of the hot-setting adhesive around fabrication hole distance fabrication hole be 0.15~
0.3mm。
3. a reinforcement steel disc material strip, is characterized in that: described material strip includes that more than material strip support part and a row such as right want
Seeking the reinforcement steel disc described in 1 or 2, reinforcement steel disc is arranged in material strip support part.
Reinforcement steel disc material strip the most according to claim 3, is characterized in that: described material strip support part is respectively provided on two sides with
Hole, location, is provided with hole, a location corresponding to each steel disc body.
Reinforcement steel disc material strip the most according to claim 3, is characterized in that: described reinforcement steel disc is provided with two rows.