CN205680696U - The reparation band of photovoltaic cell - Google Patents

The reparation band of photovoltaic cell Download PDF

Info

Publication number
CN205680696U
CN205680696U CN201620346872.8U CN201620346872U CN205680696U CN 205680696 U CN205680696 U CN 205680696U CN 201620346872 U CN201620346872 U CN 201620346872U CN 205680696 U CN205680696 U CN 205680696U
Authority
CN
China
Prior art keywords
layer
photovoltaic cell
reparation
adhesive layer
backboard
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201620346872.8U
Other languages
Chinese (zh)
Inventor
吕瑞瑞
傅冬华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Canadian Solar Inc
Canadian Solar Manufacturing Changshu Inc
Original Assignee
Canadian Solar Manufacturing Changshu Inc
Canadian Solar China Investment Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Canadian Solar Manufacturing Changshu Inc, Canadian Solar China Investment Co Ltd filed Critical Canadian Solar Manufacturing Changshu Inc
Priority to CN201620346872.8U priority Critical patent/CN205680696U/en
Application granted granted Critical
Publication of CN205680696U publication Critical patent/CN205680696U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

This application discloses the reparation band of a kind of photovoltaic cell, comprising: adhesive layer, for fitting in the damaged part of the backboard of photovoltaic cell;Substrate layer, is used for carrying described adhesive layer;Weathering layer, is coated on described substrate layer outer surface for resisting the erosion of environment foreign matter.This reparation band is bonded in the damaged part of the backboard of photovoltaic cell, had both been easy to photovoltaic cell and has used stably in a long term, be unlikely to again to bring big cost to increase.

Description

The reparation band of photovoltaic cell
Technical field
The application relates to photovoltaic cell field, particularly relates to a kind of consumptive material repairing photovoltaic cell.
Background technology
In prior art, photovoltaic cell is by glass, ethylene-vinyl acetate copolymer (Ethylene Vinyl Acetate, EVA), silicon chip, backboard composition, according to glass EVA cell piece EVA backboard construction packages constitute.Its In, backboard is positioned at the outermost layer at the photovoltaic cell back side, is photovoltaic cell important component part, not only acts as the effect of encapsulation, with When also act as guarantee photovoltaic cell do not acted on by ambient influnence, it is ensured that the service life of photovoltaic cell.
The typical structure of backboard is: the tack coat of the weathering layer-base material-internal layer of outer layer.Photovoltaic cell manufacture, transport or Put into and during power station uses, there will be backboard scuffing problem.The method solving at present is:
If 1. scuffing scope is little and does not scratch middle base material and can directly use;
2., if scuffing scope is big or damage base material, need to change backboard.
During realizing prior art, inventor finds that in prior art, at least there are the following problems:
Backboard scratches when processing according to the first solution, and owing to weathering layer has damaged, thus backboard is easily by ring The contaminating erosion such as the moisture in border and reliability when reducing photovoltaic cell Long-Time Service.
Backboard scratches when processing according to second workaround, owing to whole backboard changed by needs, thus improves photovoltaic The cost of battery operation and maintenance.
Accordingly, it is desirable to provide solution when the backboard of a kind of photovoltaic cell is damaged, consequently facilitating photovoltaic cell for a long time may be used Use by ground, be unlikely to again to bring big cost to increase.
Utility model content
The embodiment of the present application provides the reparation band of photovoltaic cell, comprising:
Adhesive layer, for fitting in the damaged part of the backboard of photovoltaic cell;
Substrate layer, is used for carrying described adhesive layer;
Weathering layer, is coated on described substrate layer outer surface for resisting the erosion of environment foreign matter.
Further, described adhesive layer is coated with pressure sensitive adhesive, repairs band and backboard gluing under pressure state in order to improve Knot power.
Further, described reparation band also includes the release layer protecting adhesive layer;Described adhesive layer is positioned at release layer And between substrate layer two-layer.
Further, described release layer is made up of PE material.
Further, described release layer thickness is between 5-25um.
Further, described adhesive layer is made up of polyurethane or acrylate material.
Further, described adhesive layer thickness is between 5-50um.
Further, described substrate layer is made up of material at least one in PET, PBT, PA, PPO.
Further, described substrate layer thickness is between 30-100um.
Further, described weathering layer is made up of material at least one in PVF, PVDF, ECTFE, FEVE, described weathering layer Thickness is between 5-25um.
The reparation band that the embodiment of the present application provides, at least has the advantages that
This reparation band is affixed on the damaged part of the backboard of photovoltaic cell, had both been easy to photovoltaic cell and has used stably in a long term, It is unlikely to again to bring big cost to increase.
Brief description
Accompanying drawing described herein is used for providing further understanding of the present application, constitutes the part of the application, this Shen Schematic description and description please is used for explaining the application, is not intended that the improper restriction to the application.In the accompanying drawings:
The structural representation repairing band of the photovoltaic cell that Fig. 1 provides for the embodiment of the present application.
Detailed description of the invention
Purpose, technical scheme and advantage for making the application are clearer, below in conjunction with the application specific embodiment and Technical scheme is clearly and completely described by corresponding accompanying drawing.Obviously, described embodiment is only the application one Section Example, rather than whole embodiments.Based on the embodiment in the application, those of ordinary skill in the art are not doing The every other embodiment being obtained under the premise of going out creative work, broadly falls into the scope of the application protection.
As it is shown in figure 1, the reparation band 100 of a kind of photovoltaic cell providing for the application.Repair band 100 and can be bonded in light The damaged part of backboard of volt battery so that backboard has the functions such as good electric insulating quality, waterproof damp proof and weather resisteant.
Repair band 100 and include adhesive layer the 1st, substrate layer the 2nd, weathering layer 3.
Adhesive layer 1 fits in the damaged part of the backboard of photovoltaic cell.Adhesive layer 1 and backboard need to possess good bonding Property.In the embodiment of the present application, adhesive layer 1 is made up of polyurethane or acrylate material.Adhesive layer 1 thickness is micro-at 5 micron-50 Between meter.
Further, in order to improve the cohesive force between adhesive layer 1 and backboard, in the another embodiment that the application provides In, adhesive layer 1 is coated with pressure sensitive adhesive, in order to improve reparation band 100 and cohesive force under pressure state for the backboard.Pressure sensitive adhesive is permissible Use acrylic acid series or rubber series, solvent-borne type or latex type adhesive.
Substrate layer 2 is used for carrying adhesive layer 1.Substrate layer 2 is in order to provide the electric insulating quality, waterproof damp proof repaired with 100 Performance.In the embodiment of the present application, substrate layer 2 is by PET (polyethylene terephthalate, poly terephthalic acid second Diester), PBT (polybutylene terephthalate, polybutylene terephthalate (PBT)), PA (polyamide, polyamides Amine), at least one material is made, it is of course also possible to mixed by different materials in PPO (Polyphenylene Oxide, polyphenylene oxide) Conjunction forms.PET, PBT, PA and PPO are current material, here do not repeat.Substrate layer 2 thickness is at 30 microns-100 microns Between.
Weathering layer 3 is coated on described substrate layer 2 outer surface for resisting the erosion of environment.Weathering layer 3 need to possess resistance to always Change, heat resistance, moisture-resistant freeze and the performances such as cold-and-heat resistent circulation.In the embodiment of the present application, weathering layer 3 is by PVF (polyvinyl Fluoride, polyvinyl fluoride), PVDF (Polyvinylidene Fluoride, Kynoar), ECTFE (Ethylene- Chlorotrifluoroethylene copolymer, ethene chlorotrifluoroethylene), FEVE (Fluorine olefin And vinyl ether copolymer resin, the copolymer resins of fluoroolefins and vinyl ethers) at least one material system Become;And PVF, PVDF, ECTFE and FEVE are current material, here do not repeat.Weathering layer 3 thickness is micro-at 5 micron-25 Between meter.
Further, in order to protect adhesive layer 1, adhesive layer 1 is prevented to lose efficacy, in the another embodiment that the application provides, Repair the release layer 4 also including protecting adhesive layer 1 with 100.Adhesive layer 1 is positioned between release layer 4 and substrate layer 2 two-layer. Release layer 4 can be made up of polyethylene (polyethylene, PE).Release layer 4 thickness is between 5 microns-25 microns.
During repairing the use with 100, can first take off release layer 4, then, adhesive layer 1 be fitted in photovoltaic electric The damaged part of the backboard in pond.This reparation band 100 is bonded in the damaged part of the backboard of photovoltaic cell, has both been easy to photovoltaic cell long Phase reliably uses, and is unlikely to again to bring big cost to increase.
The foregoing is only embodiments herein, be not limited to the application.For those skilled in the art For, the application can have various modifications and variations.All any modifications, equivalent made within spirit herein and principle Replacement, improvement etc., within the scope of should be included in claims hereof.

Claims (9)

1. the reparation band of a photovoltaic cell, it is characterised in that include:
Adhesive layer, for fitting in the damaged part of the backboard of photovoltaic cell;
Substrate layer, is used for carrying described adhesive layer;
Weathering layer, is coated on described substrate layer outer surface for resisting the erosion of environment foreign matter.
2. as claimed in claim 1 reparation carries, it is characterised in that: described adhesive layer is coated with pressure sensitive adhesive, in order to improve reparation Band and cohesive force under pressure state for the backboard.
3. as claimed in claim 1 reparation carries, it is characterised in that: described reparation band also includes protecting the release of adhesive layer Layer;
Described adhesive layer is positioned between release layer and substrate layer two-layer.
4. as claimed in claim 3 reparation carries, it is characterised in that described release layer is made up of PE material.
5. as claimed in claim 4 reparation carries, it is characterised in that described release layer thickness is between 5-25um.
6. as claimed in claim 1 reparation carries, it is characterised in that described adhesive layer is by polyurethane or acrylate material system Become.
7. as claimed in claim 1 reparation carries, it is characterised in that described adhesive layer thickness is between 5-50um.
8. as claimed in claim 1 reparation carries, it is characterised in that described substrate layer thickness is between 30-100um.
9. as claimed in claim 1 reparation carries, it is characterised in that described weathering layer thickness is between 5-25um.
CN201620346872.8U 2016-04-22 2016-04-22 The reparation band of photovoltaic cell Expired - Fee Related CN205680696U (en)