CN204373557U - For detecting the fixture impacting sample size and breach - Google Patents
For detecting the fixture impacting sample size and breach Download PDFInfo
- Publication number
- CN204373557U CN204373557U CN201420790650.6U CN201420790650U CN204373557U CN 204373557 U CN204373557 U CN 204373557U CN 201420790650 U CN201420790650 U CN 201420790650U CN 204373557 U CN204373557 U CN 204373557U
- Authority
- CN
- China
- Prior art keywords
- groove
- clamp body
- grooves
- cuboid
- breach
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The fixture for detecting impact sample size and breach providing a kind of reasonable in design, efficiency high of the present utility model.The bottom of clamp body is fixed on horizontal stand; Clamp body is long is 68mm, and wide is 65mm, and height is 10mm; Horizontal director 100mm, wide 80mm, high 5mm; A groove one end open is the cuboid of long 55mm, high 10mm, wide 10mm; No. two groove one end open are the cuboid of long 55mm, high 10mm, wide 7.5mm; No. three groove one end open are the cuboid of long 55mm, high 10mm, wide 5mm; The end face of salient angle flushes with the end face of clamp body, and bottom surface flushes with the bottom surface of clamp body; Salient angle is towards No. two grooves; The xsect of salient angle is isosceles triangle, and its base is fixed in the middle of the sidewall of a groove, and base is 2mm, and the height on base is 2mm, and the angle of drift angle is 45 degree.
Description
Technical field
The utility model relates to a kind of for detecting the fixture impacting sample size and breach.
Background technology
Component in use can be subject to the effect of shock load, and this needs component in use to meet enough toughness.
In engineering, a conventional pendulum impact test measures the ability of material repels shock load and removes Ak with the sectional area F at sample break place, and can obtain impact toughness (impact value) index of material, i.e. ak=Ak/F, its unit is kJ/m
2or J/cm
2.Therefore, impact toughness ak represents the ability of material resistance to deformation and fracture under impact loading.The size of ak value represents the toughness quality of material.
According to GB/T 229-2007 metal material Charpy pendulum impact test method, its principle is placed in by the notched specimen of regulation geometric configuration between testing machine two bearing, and the breach dorsad scope of attack is placed, and once hits sample with pendulum, measures the absorption energy of sample.Its specified standard size impact specimen length is 55mm, and xsect is 10mm × (5 mm, 7.5 mm, 10mm) square-section.Specimen surface roughness R ɑ should be better than 5 μm, except end.
Current employing kind of calliper one impacts the size of sample, and required time at least wants 15 seconds, and efficiency is lower.
Utility model content
The purpose of this utility model is to overcome above shortcomings in prior art, and the fixture for detecting impact sample size and breach providing a kind of reasonable in design, efficiency high.
The technical scheme in the invention for solving the above technical problem is: a kind of for detecting the fixture impacting sample size and breach, it is characterized in that: comprise clamp body and horizontal stand; The bottom of clamp body is fixed on horizontal stand; Clamp body is cuboid, and it is long is 68mm, and wide is 65mm, and height is 10mm; Horizontal stand is cuboid, and length is 100mm, and width is 80mm, is highly 5mm; Clamp body has successively a groove, No. two grooves and No. three grooves, groove, No. two grooves and No. three grooves are arranged side by side, and run through clamp body in the height direction; A groove, No. two grooves are all identical with No. three groove length, highly also all identical; A groove one end open, a groove is cuboid, and length is 55mm, is highly 10mm, and width is 10mm; No. two groove one end open, No. two grooves are cuboid, and length is 55mm, are highly 10mm, and width is 7.5mm; No. three groove one end open, No. three grooves are cuboid, and length is 55mm, are highly 10mm, and width is 5mm; Be fixedly installed salient angle in the middle of the sidewall of a groove, its end face flushes with the end face of clamp body, and bottom surface flushes with the bottom surface of clamp body; Salient angle is towards No. two grooves; The xsect of salient angle is isosceles triangle, and its base is fixed in the middle of the sidewall of a groove, and base is 2mm, and the height on base is 2mm, and the angle of drift angle is 45 degree.
Clamp body described in the utility model and horizontal stand one-body molded.
Clamp body described in the utility model and horizontal stand adopt 304 stainless steels to make.
The utility model compared with prior art, has the following advantages and effect: reasonable in design, and detecting an impact sample required time is 3 seconds, improves the work efficiency of 5 times than original detection mode.
Accompanying drawing explanation
Fig. 1 be the utility model embodiment face structural representation.
Fig. 2 is the left TV structure schematic diagram of the utility model embodiment.
Fig. 3 is the plan structure schematic diagram of the utility model embodiment.
Embodiment
Below in conjunction with accompanying drawing, also by embodiment, the utility model is described in further detail, and following examples are that the utility model is not limited to following examples to explanation of the present utility model.
See Fig. 1 ~ Fig. 3, the utility model embodiment comprises clamp body 1 and horizontal stand 2.
The bottom of clamp body 1 is fixed on horizontal stand 2.Clamp body 1 and horizontal stand 2 one-body molded.Clamp body 1 is cuboid, and it is long is 68mm, and wide is 65mm, and height is 10mm, the size of suitable staff, conveniently takes and uses.Horizontal stand 2 is cuboid, and length is 100mm, and width is 80mm, is highly 5mm, and horizontal stand 2 machining precision must ensure, polishing need be carried out in surface.Fixing horizontal platform 2 is put in order to ensure that sample is placed in same level in the bottom of clamp body 1.
Clamp body 1 has successively a groove 3, No. two grooves 4 and No. three grooves 5, groove 3, No. two grooves 4 and No. three grooves 5 to be arranged side by side, a groove 3, No. two grooves 4 and No. three grooves 5 run through clamp body 1 in the height direction.A groove 3, No. two grooves 4 and No. three grooves 5 are the positions of placing impact specimen.A groove 3, No. two grooves 4 and No. three groove 5 identical length are together, highly also all identical.
Groove 3 one end open, conveniently puts into sample.A groove 31 is cuboid, and length is 55mm, is highly 10mm, and width is 10mm.
No. two groove 4 one end open, conveniently put into sample.No. two grooves 41 are cuboid, and length is 55mm, are highly 10mm, and width is 7.5mm.
No. three groove 5 one end open, conveniently put into sample.No. three grooves 51 are cuboid, and length is 55mm, are highly 10mm, and width is 5mm.
Be fixedly installed salient angle 6 in the middle of the sidewall of a groove 3, its end face flushes with the end face of clamp body 1, and bottom surface flushes with the bottom surface of clamp body 1.Salient angle 6 is towards No. two grooves 4.The xsect of salient angle 6 is isosceles triangle, and its base is fixed in the middle of the sidewall of a groove 3, and base is 2mm, and the height on base is 2mm, and the angle of drift angle is 45 degree.Salient angle 6 is to check Charpy key hole specimen break, is placed on by impact sample in a groove 3, can detects the length of sample, width, height and breach.
Groove 3 can detect that length is 55mm, width is 10mm, be highly the bulk sample of 10mm.Sample is put into a groove 3, if length all meets, then show that sample is qualified.
A groove 3 and No. two grooves 4 being combined, can detection width be the impact sample of 7.5mm.First can detect the length of sample, height and breach by a groove 3, then be detected the width of sample by No. two grooves 4; Also first can detect the length of sample, height and width by No. two grooves 4, a more logical groove 3 detects the breach of sample.
A groove 3 and No. three grooves 5 being combined, can detection width be the impact sample of 5mm.First can detect the length of sample, height and breach by a groove 3, then be detected the width of sample by No. three grooves 5; Also first can detect the length of sample, height and width by No. three grooves 5, a more logical groove 3 detects the breach of sample.
The utility model is inspection size, therefore higher to size tolerance requirements.
Clamp body 1 and horizontal stand 2 adopt 304 stainless steels to make, because the mould of straight carbon steel easily corrodes after contacting with water.
In addition, it should be noted that, the specific embodiment described in this instructions, the shape, institute's title of being named etc. of its parts and components can be different, and the above content described in this instructions is only to the explanation of the utility model structure example.
Claims (3)
1., for detecting the fixture impacting sample size and breach, it is characterized in that: comprise clamp body and horizontal stand; The bottom of clamp body is fixed on horizontal stand; Clamp body is cuboid, and it is long is 68mm, and wide is 65mm, and height is 10mm; Horizontal stand is cuboid, and length is 100mm, and width is 80mm, is highly 5mm; Clamp body has successively a groove, No. two grooves and No. three grooves, groove, No. two grooves and No. three grooves are arranged side by side, and run through clamp body in the height direction; A groove, No. two grooves are all identical with No. three groove length, highly also all identical; A groove one end open, a groove is cuboid, and length is 55mm, is highly 10mm, and width is 10mm; No. two groove one end open, No. two grooves are cuboid, and length is 55mm, are highly 10mm, and width is 7.5mm; No. three groove one end open, No. three grooves are cuboid, and length is 55mm, are highly 10mm, and width is 5mm; Be fixedly installed salient angle in the middle of the sidewall of a groove, its end face flushes with the end face of clamp body, and bottom surface flushes with the bottom surface of clamp body; Salient angle is towards No. two grooves; The xsect of salient angle is isosceles triangle, and its base is fixed in the middle of the sidewall of a groove, and base is 2mm, and the height on base is 2mm, and the angle of drift angle is 45 degree.
2. according to claim 1 for detecting the fixture impacting sample size and breach, it is characterized in that: described clamp body and horizontal stand one-body molded.
3. according to claim 1 and 2 for detecting the fixture impacting sample size and breach, it is characterized in that: described clamp body and horizontal stand adopt 304 stainless steels to make.