CN204303467U - 无缝铜包铝杆生产装置 - Google Patents
无缝铜包铝杆生产装置 Download PDFInfo
- Publication number
- CN204303467U CN204303467U CN201520008487.8U CN201520008487U CN204303467U CN 204303467 U CN204303467 U CN 204303467U CN 201520008487 U CN201520008487 U CN 201520008487U CN 204303467 U CN204303467 U CN 204303467U
- Authority
- CN
- China
- Prior art keywords
- copper
- cover aluminum
- outer tube
- aluminum bar
- copper liquid
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
无缝铜包铝杆生产装置,其熔化炉外壳内置保温层,内装铜液,熔化炉顶部设有加料口,一侧设置铜液出口;铜包铝杆结晶装置的中部设计有结晶器,结晶器的外管内套有内管,内管与外管之间留有间隙均匀的铜液通道,内管底部位于外管中部,内管和外管之间留有的间隙上端留有铜液进口,铜液进口与熔化炉的铜液出口连接,铜液进口与铜液通道连接,在外管的上部包有铜液冷却套,在外管的下部包有铝液冷却套,在结晶器的上端,装有铝杆牵引器,铝杆穿过铝杆牵引器,插入内管中,在结晶器的下部,装有铜包铝杆牵引器,冷却后的铜包铝杆从铜包铝杆牵引器中穿过。利用本实用新型生产的铜包铝杆,外层铜壁厚度均匀,铜和铝无缝结合,使用时电流损失较小,导体质量较高。
Description
技术领域
本实用新型属于金属导电杆技术领域,涉及一种无缝铜包铝杆生产装置。
背景技术
导电铜包铝杆是用铜外壳将铝芯无缝包裹在内的一种导电材料,它是利用电流在导体上流动时的集肤效应,让大部分电流在电阻率较小的导体表面铜层流动,小部分电流在电阻率稍大的导体内部铝芯流动,在尽可能减少导电材料导致的电流损失的情况下,用铝芯替代铜芯降低导线材料的制造成本。
现有技术中,铜包铝导电材料的制造,大部分是在铝芯外部包裹一层铜层,这种结构的导电材料,由于铜层和铝芯无法紧密贴合,电流在流经两种材料的贴合面时,产生的电流损失较大,由于包裹在铝芯上的铜层有螺旋搭接边,表面铜层厚度不均匀,导致电流损失较大。
发明内容
本实用新型的目的是提供一种无缝铜包铝杆生产装置,解决现有技术中铜包铝导电材料存在的铜层和铝芯无法紧密贴合、包裹在铝芯上的铜层有螺旋搭接边,表面铜层厚度不均匀,导致电流损失较大的问题。
本实用新型的技术方案是:无缝铜包铝杆生产装置,由熔化炉和铜包铝杆结晶装置组成;熔化炉外壳内置保温层,内装铜液,熔化炉顶部设有加料口,一侧设置铜液出口;铜包铝杆结晶装置的中部设计有结晶器,结晶器的外管内套有内管,内管与外管之间留有间隙均匀的铜液通道,内管底部位于外管中部,内管和外管之间留有的间隙上端留有铜液进口,铜液进口与熔化炉的铜液出口连接,铜液进口与铜液通道连接,在外管的上部包有铜液冷却套,在外管的下部包有铝液冷却套,在结晶器的上端,装有铝杆牵引器,铝杆穿过铝杆牵引器,插入内管中,在结晶器的下部,装有铜包铝杆牵引器,冷却后的铜包铝杆从铜包铝杆牵引器中穿过。
其工作过程是:首先将熔化炉中熔化的铜液引入结晶器的铜液通道中,在铜液冷却套中通入循环冷却液,使铜液在铜液通道下段凝固成铜管;同时,利用铝杆牵引器将铝杆牵引进入结晶器内管,在此过程中控制铜液冷却套的冷却温度,使结晶器中铜液通道的温度低于铜的凝固点,使内管中的温度高于铝的熔点,当铜液凝固成铜管后,铝杆在内管里融化成铝液,将铜管内腔充满;当铜管经过结晶器外管下部时,包裹在外管外部的铝液冷却器使铜管及铜管中的铝液再次冷却,铝液凝固在铜管中心,与铜管内壁形成无缝结合,铜铝凝固结合后的导电杆由结晶器下部的铜包铝杆牵引器引出。铝杆融化过程中产生的气体,由内管和铝杆接触面的间隙排出,确保铝液在铜管内部凝固时,尽量减少凝固的铝液中出现小气泡;调整铝杆牵引器和铜包铝杆牵引器的牵引速比,使铜管内的铝液均匀填充铜管。
利用本实用新型生产的铜包铝杆,外层铜壁厚度均匀,铜和铝无缝结合,使用时电流损失较小,导体质量较高。
附图说明
图1为本实用新型的结构示意图。
具体实施方式
实施例:如图1所示,无缝铜包铝杆生产装置,由熔化炉2和铜包铝杆结晶装置组成;熔化炉2外壳内置保温层3,内装铜液4,熔化炉顶部设有加料口1,一侧设置铜液出口5;铜包铝杆结晶装置的中部设计有结晶器,结晶器的外管8内套有内管12,内管12与外管8之间留有间隙均匀的铜液通道7,内管底部位于外管中部,内管12和外管8之间留有的间隙上端留有铜液进口6,铜液进口6与熔化炉的铜液出口5连接,铜液进口6与铜液通道7连接,在外管8的上部包有铜液冷却套13,在外管的下部包有铝液冷却套11,在结晶器的上端,装有铝杆牵引器14,铝杆15穿过铝杆牵引器14,插入内管12中,在结晶器的下部,装有铜包铝杆牵引器10,冷却后的铜包铝杆9从铜包铝杆牵引器10中穿过。
Claims (1)
1.无缝铜包铝杆生产装置,其特征在于:由熔化炉(2)和铜包铝杆结晶装置组成;熔化炉(2)外壳内置保温层(3),内装铜液(4),熔化炉顶部设有加料口(1),一侧设置铜液出口(5);铜包铝杆结晶装置的中部设计有结晶器,结晶器的外管(8)内套有内管(12),内管(12)与外管(8)之间留有间隙均匀的铜液通道(7),内管底部位于外管中部,内管(12)和外管(8)之间留有的间隙上端留有铜液进口(6),铜液进口(6)与熔化炉的铜液出口(5)连接,铜液进口(6)与铜液通道(7)连接,在外管(8)的上部包有铜液冷却套(13),在外管的下部包有铝液冷却套(11),在结晶器的上端,装有铝杆牵引器(14),铝杆(15)穿过铝杆牵引器(14),插入内管(12)中,在结晶器的下部,装有铜包铝杆牵引器(10),冷却后的铜包铝杆(9)从铜包铝杆牵引器(10)中穿过。