CN204144337U - Without the unleaded alkali button battery of mercury - Google Patents

Without the unleaded alkali button battery of mercury Download PDF

Info

Publication number
CN204144337U
CN204144337U CN201420682587.4U CN201420682587U CN204144337U CN 204144337 U CN204144337 U CN 204144337U CN 201420682587 U CN201420682587 U CN 201420682587U CN 204144337 U CN204144337 U CN 204144337U
Authority
CN
China
Prior art keywords
negative
current collector
alloy
cover
negative current
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201420682587.4U
Other languages
Chinese (zh)
Inventor
肖秀华
肖雅文
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201420682587.4U priority Critical patent/CN204144337U/en
Application granted granted Critical
Publication of CN204144337U publication Critical patent/CN204144337U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A kind of without the unleaded alkali button battery of mercury, comprise negative cover, negative current collector, O-ring seal, negative zinc cream, barrier film, positive electrode and anode cover, described negative current collector is arranged on the inner side of negative cover, the inner shape of the outer shape of negative current collector, size and negative cover, measure-alike, the outer surface of negative current collector and the inner surface of negative cover are combined closely, and the inner surface of negative current collector contacts with negative zinc cream.This negative current collector adopts the good aluminium of electric conductivity or copper or aluminium alloy or alcu alloy film, on aluminium or copper or aluminium alloy or alcu alloy film surface, is coated with indium or tin or indium alloy or tin alloy coat, makes through punching press.The utility model, without the need to strip, efficiently solves existing technology and there is plurality of heavy metal discharge, can cause the problem of severe contamination and the wasting of resources, be conducive to environmental protection to environment.

Description

Without the unleaded alkali button battery of mercury
Technical field
The utility model relates to field of batteries, especially relates to a kind of without the unleaded alkali button battery of mercury, comprises without mercury unleaded zinc-manganese button cell with without the unleaded silver oxide button cell of mercury.
Background technology
The production technology of existing mercury-free alkali button battery, be adopt plating, chemical plating and strip method directly at battery cathode iron covering integral surface plating indium or zinc-plated or plating indium alloy or zinc-plated alloy, prepare mercury-free alkali button battery negative current collector.Be included in battery cathode iron covering integral surface to carry out electroplating or electroless plating indium or zinc-plated or plating indium alloy or zinc-plated alloy, then the outer surface coating decoating liquid of battery cathode lid removed.Due to the self structure reason of battery cathode iron covering, cause covering power and covering power all poor, easily cause the thickness of coating of negative cover uneven, not fine and close, poor adhesive force, there is pore, even dark recess does not have the defects such as coating, and strip be easy to cause battery cathode lid inside coating be damaged, cause negative zinc cream and negative cover iron substrate contact generation chemical reaction liberation of hydrogen, cause battery inflatable, leakage such as even to be exploded at the safety problem, in addition, these methods have waste water, waste gas, heavy metals emission, particularly there are the heavy metals emissions such as a large amount of chromium ions in strip process, severe contamination and the wasting of resources can be caused to environment.Therefore, be badly in need of a kind of not only environmental protection but also the technical scheme of existing mercury-free alkali button battery potential safety hazard can be overcome.
Utility model content
The utility model provides a kind of without the unleaded alkali button battery of mercury, efficiently solve prior art directly in the defect that the plating of negative pole iron covering integral surface or chemically plating exist for negative current collector, and strip causes coating damaged inside battery cathode lid, cause negative zinc cream and negative cover iron substrate contact generation chemical reaction liberation of hydrogen, the safety problem such as cause that battery inflatable, leakage are even exploded.
The utility model, without the need to strip, efficiently solves existing technology and there is plurality of heavy metal discharge, can cause the problem of severe contamination and the wasting of resources to environment.
For achieving the above object, the utility model is achieved in that
A kind of without the unleaded alkali button battery of mercury, comprise negative cover, negative current collector, O-ring seal, negative zinc cream, barrier film, positive electrode and anode cover, described negative current collector is arranged on the inner side of negative cover, the inner shape of the outer shape of negative current collector, size and negative cover, measure-alike, the outer surface of negative current collector and the inner surface of negative cover are combined closely, and the inner surface of negative current collector contacts with negative zinc cream.This negative current collector adopts the good aluminium of electric conductivity or copper or aluminium alloy or alcu alloy film, on aluminium or copper or aluminium alloy or alcu alloy film surface, is coated with indium or tin or indium alloy or tin alloy coat, makes through punching press.The utility model negative current collector effectively prevents self-discharge of battery liberation of hydrogen, effectively prevent negative zinc cream simultaneously and contacts with negative cover iron chemical reaction liberation of hydrogen occurs.
Compared with prior art, the utility model is provided with a negative current collector between battery cathode lid and negative zinc cream, solve prior art directly at negative pole iron covering integral surface plating indium or zinc-plated or plating indium alloy or zinc-plated alloy, again cathode cover exterior face coating is carried out the method for strip, easily occur coating poor plating and strip be easy to cause battery cathode lid inside coating be damaged, cause negative zinc cream and negative cover iron substrate contact generation chemical reaction liberation of hydrogen, cause battery inflatable, leakage such as even to be exploded at the safety problem, the utility model negative current collector effectively prevents self-discharge of battery liberation of hydrogen, effectively prevent negative zinc cream to contact with negative cover iron chemical reaction liberation of hydrogen occurs simultaneously, overcome the deficiency that prior art exists, improve security performance and the shelf characteric of battery.The utility model, without the need to strip, efficiently solves existing technology and there is plurality of heavy metal discharge, can cause the problem of severe contamination and the wasting of resources, be conducive to environmental protection to environment.
Below in conjunction with drawings and Examples, the utility model is further elaborated.
Accompanying drawing explanation
Fig. 1 is the profile of the utility model embodiment 1.
Fig. 2 is the profile of the utility model embodiment 2.
Embodiment
Execution mode 1
As shown in Figure 1, described in the utility model embodiment without the unleaded alkali button battery of mercury, comprise negative cover 1, negative current collector 2, O-ring seal 3, negative zinc cream 4, barrier film 5, positive electrode 6 and anode cover 7.Described negative zinc cream 4 is without the unleaded calamine cream of mercury, positive electrode 6 is silver oxide or manganese dioxide, the base material aluminium of negative current collector 2 or copper or aluminium alloy or alcu alloy film, on the surface of aluminium or copper or aluminium alloy or alcu alloy film, be coated with indium or tin or indium alloy or tin alloy layers, be combined into one with negative cover 1 after punch forming.Negative current collector 2 base material is the surface of signal bronze or copper tin multicomponent alloy, can not plate indium or not zinc-plated or do not plate indium alloy or not zinc-plated alloy.
This negative current collector 2 is arranged on the inner side of negative cover 1, and the outer surface of negative current collector 2 and the inner surface of negative cover 1 are combined closely, and the inner surface of negative current collector 2 contacts with negative zinc cream 4.This negative current collector 2 effectively prevent self-discharge of battery liberation of hydrogen, effectively prevent negative zinc cream 4 simultaneously and contacts with negative cover iron chemical reaction liberation of hydrogen occurs, the safety problem such as cause that battery inflatable, leakage are even exploded.
Execution mode 2
As shown in Figure 2, described in the utility model embodiment without the unleaded alkali button battery of mercury, comprise negative cover 1, negative current collector 2, O-ring seal 3, negative zinc cream 4, barrier film 5, positive electrode 6 and anode cover 7.Described negative zinc cream 4 is without the unleaded calamine cream of mercury, positive electrode 6 is silver oxide or manganese dioxide, negative cover 1 and negative current collector 2 are integrated, adopt that one side is nickel plating or tin-plated cold rolled steel or stainless steel substrates, another side is coated with the aluminium of indium or tin or indium alloy or tin alloy layers or the specialty metal sheet of copper or aluminium alloy or alcu alloy film, to be coated with in the facing of indium or tin or indium alloy or tin alloy layers, nickel plating or tin-plated cold rolled steel or stainless face outside, negative cover 1 and the negative current collector 2 of integration are made in a punching press.Negative current collector 2 base material is the surface of signal bronze or copper tin multicomponent alloy, can not plate indium or not zinc-plated or do not plate indium alloy or not zinc-plated alloy.
This negative cover 1 and negative current collector 2 are integrated, and negative cover 1 and negative current collector 2 are combined closely for seamless, and the inner surface of negative current collector 2 contacts with negative zinc cream 4.This negative current collector 2 effectively prevent self-discharge of battery liberation of hydrogen, effectively prevent negative zinc cream 4 simultaneously and contacts with negative cover iron chemical reaction liberation of hydrogen occurs, the safety problem such as cause that battery inflatable, leakage are even exploded.
The above, be only preferred embodiment of the present utility model, not in order to limit the utility model, all do within spirit of the present utility model and principle any amendment, equivalent to replace and improvement etc., all should be included within protection range of the present utility model.

Claims (3)

1. one kind without the unleaded alkali button battery of mercury, comprise negative cover, negative current collector, O-ring seal, negative zinc cream, barrier film, positive electrode and anode cover, it is characterized in that: described negative current collector is arranged on the inner side of negative cover, the inner shape of the outer shape of negative current collector, size and negative cover, measure-alike, the outer surface of negative current collector and the inner surface of negative cover are combined closely, and the inner surface of negative current collector contacts with negative zinc cream.
2. according to claim 1 without the unleaded alkali button battery of mercury, it is characterized in that: described negative current collector base material is aluminium or copper or aluminium alloy or alcu alloy film, on aluminium or copper or aluminium alloy or alcu alloy film surface, be coated with indium or tin or indium alloy or tin alloy layers, be combined into one with negative cover after punch forming.
3. according to claim 1 without the unleaded alkali button battery of mercury, it is characterized in that: described negative cover and negative current collector are integrated, adopt that one side is nickel plating or tin-plated cold rolled steel or stainless steel substrates, another side is coated with the aluminium of indium or tin or indium alloy or tin alloy layers or the specialty metal sheet of copper or aluminium alloy or alcu alloy film, to be coated with in the facing of indium or tin or indium alloy or tin alloy layers, nickel plating or tin-plated cold rolled steel or stainless face outside, negative cover and the negative current collector of integration are made in a punching press.
CN201420682587.4U 2014-11-16 2014-11-16 Without the unleaded alkali button battery of mercury Expired - Fee Related CN204144337U (en)