CN204138522U - A kind of vial bottleneck tooth mould movement - Google Patents
A kind of vial bottleneck tooth mould movement Download PDFInfo
- Publication number
- CN204138522U CN204138522U CN201420496683.XU CN201420496683U CN204138522U CN 204138522 U CN204138522 U CN 204138522U CN 201420496683 U CN201420496683 U CN 201420496683U CN 204138522 U CN204138522 U CN 204138522U
- Authority
- CN
- China
- Prior art keywords
- movement
- tooth mould
- stopper slot
- movement body
- bottleneck
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model discloses a kind of vial bottleneck tooth mould movement, the stopper slot circle of the movement body comprising column and the middle part excircle that is located at movement body, the top that described movement body is positioned at stopper slot circle is up-small and down-big cone boss.The utility model solves the large osculum produced the brilliant tooth process processed of boring glass feeding bottle of high borosilicate and occur, large denticle and the uneven problem of bottleneck, improves the good article rate that feeding bottle is produced.
Description
Technical field
The utility model relates generally to full-automatic high-boron-silicon glass feeding bottle tooth equipment.
Background technology
It is the feeding bottle adopting high-boron-silicon glass pipe to fire that high borosilicate crystalline substance bores glass feeding bottle, and it is fired and most importantly in link is tooth processed (making mouth thread) process.Now main exist two kinds of production technique, and one is manual production, and one is machine production.
Because the inefficiency of manual production, machine production has started progressively substituting manual production, becomes the theme that glass feeding bottle is produced.Machine production mainly adopts 18 feeding bottle machines, arranges different duration and degree of heatings to reach different temperature, carry out tooth processed to bottle between its 18 stations.Because namely Glass tubing itself also exists pipe detector for outer diameter error and wall thickness deflection, the degree causing the duration and degree of heating temperature set to be fired each bottle is different, occurs large osculum (mouth external diameter size, tooth external diameter size) and oral area injustice.
Mouthful external diameter is crossed senior general and is caused feeding bottle tooth lid to twist not enter, and mouth external diameter is crossed young pathbreaker and caused feeding bottle tooth lid to be twisted tightly cannot not fixing nipple, and oral area unfairness will cause bottleneck be combined with nipple tight and do not occur milk leakage phenomenon.These are all called functional defect in the industry, occur that these defects are directly scrapped directly causing milk bottle body not use.
These feeding bottles scrapped are definitely large amounts of losses to feeding bottle manufacturer, have both wasted resource, the energy, and have again reduced benefit.And the pipe detector for outer diameter error of high-boron-silicon glass pipe and wall thickness deflection are unavoidably, so just can only improve from feeding bottle production unit, and this improvement is extremely urgent.
Summary of the invention
Goal of the invention: for above-mentioned Problems existing and defect, a kind of vial bottleneck of the utility model tooth mould movement, solve the large osculum produced the brilliant tooth process processed of boring glass feeding bottle of high borosilicate and occur, large denticle and the uneven problem of bottleneck, improve the good article rate that feeding bottle is produced.
Technical scheme: to achieve the above object of the invention, the utility model is by the following technical solutions: a kind of vial bottleneck tooth mould movement, the stopper slot circle of the movement body comprising column and the middle part excircle that is located at movement body, the top that described movement body is positioned at stopper slot circle is up-small and down-big cone boss.
Improve further such scheme, described stopper slot circle is provided with right angle groove along movement body, and the outer side wall of this groove is provided with pitch angle.
As preferably, the diameter difference of the top and bottom of the cone boss on described movement body top is 1mm.
Further, the excircle of described cone boss is provided with at least one tangent plane.
Beneficial effect: compared with prior art, the utility model has the following advantages: 1, traditional machine core adopts right cylinder boss, and does not adopt cone boss, when glass tube external diameter is less than normal, when wall thickness is partially thin, causes movement and bottle mutually to be conflicted, make movement directly destroy bottle; And adopt modified version movement to adopt cone boss, after movement leading portion can be made to enter bottle, bottle being burnt soft position swells, and carries out tooth processed smoothly; 2, traditional machine core and bottleneck end face adopt planar design, utilize the distance controlling mouth external diameter size of mould and movement, adopt the compression that spring pulls mould to carry out bottleneck frit, when pipe external diameter is bigger than normal or wall thickness partially thick after, melt because frit does not burn, make spring tension press not in place not, occur large mouth.Modified version movement adopts pitch angle design, while mould is compressed frit under the drive of spring tension, unnecessary frit is along pitch angle to downward-extension, utilize when mould is compressed to a certain degree frit the pitch angle of movement itself to allow it receive limit to put together, allow mould be well on donsole to feeding bottle; 3, the straight-line groove design of modified version movement, is the reinforcement to pitch angle design.Frit is after putting together through dies compress and receipts limit, pitch angle, and bottleneck lower rim enters straight-line groove position, carries out spacing.A mouthful external diameter size is strictly controlled according to groove outward flange diameter.
Embodiment
Fig. 1 is the structural representation of bottleneck tooth mould movement described in the utility model;
Fig. 2 is the sectional view of bottleneck tooth mould movement described in the utility model;
Fig. 3 is the partial enlarged drawing at A place in Fig. 2.
Wherein, movement body 1, stopper slot circle 2, right angle groove 3, pitch angle 4, tangent plane 5.
Embodiment
Below in conjunction with the drawings and specific embodiments, illustrate the utility model further.These embodiments should be understood and be only not used in restriction scope of the present utility model for illustration of the utility model, after having read the utility model, the amendment of those skilled in the art to the various equivalent form of value of the present utility model has all fallen within the application's claims limited range.
As described in Fig. 1 ~ 3, a kind of vial bottleneck tooth mould movement, the stopper slot circle of the movement body comprising column and the middle part excircle that is located at movement body, the top that described movement body is positioned at stopper slot circle is up-small and down-big cone boss.Improve further such scheme, described stopper slot circle is provided with right angle groove along movement body, and the outer side wall of this groove is provided with pitch angle.As preferably, the diameter difference of the top and bottom of the cone boss on described movement body top is 1mm.Further, the excircle of described cone boss is provided with at least one tangent plane.
Use raw material 6000 to adjust when to stablize every day with 18 feeding bottle machines, after using modified version movement, substandard products quantity decreases 972 every day.Sold finished product price statistics according to single month, average price is 3.2 yuan/.After using modified version movement, the odd-numbered day improves corporate income 3110.4 yuan, can improve company's benefit every year and reach 1119744 yuan.So after use modified version movement, the yield rate of production plant is significantly improved, and company's benefit is also obviously increased.
Modified version movement specification (illustrating): suppose that the mouth external diameter that we will make feeding bottle is produced with 2.5mm wall thickness glass-tube, finish dimensional requires: 36.5 ± 0.3mm, silk tooth external diameter 39.5 ± 0.3mm, oral area wall thickness is 2.5mm, so movement design elements drawing is: 1, cone boss size is decided to be: lower end diameter 30.5mm, upper end diameter 29.5mm, boss height 21.4mm(is in actual production process, bottleneck understands slight expansion after having fired, generally can be greater than setting size 1mm, so boss lower end size design key element is: mouth external diameter-mouth wall thickness x2-0.5mm, so boss lower end diameter is of a size of 36.5-2.5x2-1=30.5mm, boss upper end 1mm less of lower end, is set to 29.5mm, and height raises Distance positioning 21.4mm according to pincers platform, when ensureing station revolution, movement upper end and bottleneck lower end enter with detach procedure in do not contact with each other cause bottleneck to be out of shape).2, straight-line groove size: recess width 2.6mm, degree of depth 0.6mm, i.e. outside diameter 35.7mm, (after cone boss lower end external diameter determination internal diameter of the bottleneck, oral area wall thickness is 2.5mm as requested, so recess width is mouth wall thickness, namely recess width is 2.5mm, considers the factors such as the actual wall thickness deflection of Glass tubing, increase 0.1mm thickness to supplement as reserved, be 2.6mm.After depth of groove considers to put together in receipts limit, pitch angle, frit is upwards filled a tooth and is entered oral area grinding downwards, and showing that groove rises the degree of depth according to actual experience data is 0.6mm).3, pitch angle size: outside diameter 40mm, inner edge external diameter 35.7mm(is external diameter outside groove), the mouth external diameter size setting that outside height 0.8mm(pitch angle, diameter limits according to second pincers platform, generally about 1mm larger than mouth external diameter.Pitch angle tilts to and ensures that the straight-line groove degree of depth is 0.6mm position.So determine pitch angle size according to this type of product size.) according to these 3 design considerations, add movement and core base coordinating size, draw the complete drawing (see photo) of modified version movement.
Modified version movement is succeeded in developing in May, 2013 and comes into operation.According to the Data Comparison before and after the use modified version movement that workshop provides, can find out that modified version movement is in use respond well.
Cartridge types | Statistical magnitude | Large mouth | Denticle | Oral area is uneven | Fraction defective |
Traditional machine core | 3000 | 365 | 140 | 162 | 22.2% |
Improve movement | 3000 | 92 | 36 | 70 | 6% |
During statistic data, the equipment that is is added up in stably manufactured process after completing self-heating debugging.According to data presentation, equally in the production process of 3000 raw materials, occur that the quantity of large mouth drops to 92 from 365, occurrence rate reduces 9%; Occur that the quantity of denticle is reduced to 36 from 140, occurrence rate reduces 4%; Occur that the quantity of dipped ring drops to 70 from 162, occurrence rate reduces 3%.The accumulative yield that improves reaches 16.2%.
Claims (4)
1. a vial bottleneck tooth mould movement, is characterized in that: the stopper slot circle of the movement body comprising column and the middle part excircle that is located at movement body, the top that described movement body is positioned at stopper slot circle is up-small and down-big cone boss.
2. vial bottleneck tooth mould movement according to claim 1, is characterized in that: described stopper slot circle is provided with right angle groove along movement body, and the outer side wall of this groove is provided with pitch angle.
3. vial bottleneck tooth mould movement according to claim 2, is characterized in that: the diameter difference of the top and bottom of the cone boss on described movement body top is 1mm.
4. vial bottleneck tooth mould movement according to claim 3, is characterized in that: the excircle of described cone boss is provided with at least one tangent plane.