CN204010533U - Labeling - Google Patents

Labeling Download PDF

Info

Publication number
CN204010533U
CN204010533U CN201420222292.9U CN201420222292U CN204010533U CN 204010533 U CN204010533 U CN 204010533U CN 201420222292 U CN201420222292 U CN 201420222292U CN 204010533 U CN204010533 U CN 204010533U
Authority
CN
China
Prior art keywords
hot melt
melt adhesive
labeling
adhesive layer
basalis
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201420222292.9U
Other languages
Chinese (zh)
Inventor
肖颖
田东文
周淑宝
龚云
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Publishing and Printing College
University of Shanghai for Science and Technology
Original Assignee
Shanghai Publishing and Printing College
University of Shanghai for Science and Technology
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Publishing and Printing College, University of Shanghai for Science and Technology filed Critical Shanghai Publishing and Printing College
Priority to CN201420222292.9U priority Critical patent/CN204010533U/en
Application granted granted Critical
Publication of CN204010533U publication Critical patent/CN204010533U/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The utility model provides a kind of labeling, for affixing to object, object is indicated, and it is characterized in that, comprising: basalis; And understand the hot melt adhesive layer that produces viscosity after being coated in basalis surface heating, this hot melt adhesive layer thickness is dwindled to center position gradually by all edges.Labeling of the present utility model adopts hot melt adhesive layer to replace the existing viscous layers such as non-drying glue layer, there is no at normal temperatures viscosity, so do not need to use the base stock of isolation viscous layer, therefore the labeling of three layers and above structure can be reduced to double-layer structure, thereby avoid the waste because using base stock to cause.In addition, due to hot melt adhesive layer thickness by week along dwindling gradually to center position, not only guaranteed the fastness that labeling is pasted but also the waste that can avoid hot melt adhesive too much to cause.

Description

Labeling
Technical field
The utility model relates to a kind of labeling, belongs to packaging field.
Background technology
Existing labeling need to be isolated with base stock the viscosity of labeling before affixing on object conventionally; as adhesive label; it just can use the viscosity of labeling after base stock being taken off when pasting, and this kind of labeling can consume base stock, and base stock conventionally can be dropped and causes waste after being taken off.
Utility model content
The utility model carries out in order to solve above-mentioned problem, and object is to provide a kind of labeling that can not need base stock.
The utility model to achieve these goals, has adopted following structure:
The utility model provides a kind of labeling, for affixing to object, object is indicated, and it is characterized in that, comprising: basalis; And understand the hot melt adhesive layer that produces viscosity after being coated in basalis surface heating, this hot melt adhesive layer thickness is dwindled to center position gradually by all edges.
In addition, in labeling of the present utility model, can also there is such feature: wherein, hot melt adhesive layer is that fusing point is 70~84 ℃ of hot melt adhesive layers that viscosity is 25~35Pa.s.
In addition, in labeling of the present utility model, can also there is such feature, also comprise: be opened in the hollow area that in hot melt adhesive layer, the relative hot melt adhesive layer of heart shape dwindles in proportion, this hollow area size accounts for hot melt adhesive layer area 1/64~1/4.
In addition, in labeling of the present utility model, can also there is such feature: wherein, basalis is paper.
In addition, in labeling of the present utility model, can also there is such feature: wherein, basalis is film.
Utility model effect and effect
According to labeling of the present utility model, because adopt hot melt adhesive layer to replace the existing viscous layers such as non-drying glue layer, there is no at normal temperatures viscosity, so do not need to use the base stock of isolation viscous layer, therefore the labeling of three layers and above structure can be reduced to double-layer structure, thereby avoid the waste because using base stock to cause.
In addition, because hot melt adhesive layer thickness is dwindled to center position gradually by all edges, so hot melt adhesive layer is thicker on all edges, and after heating and melting, stickum is more; Thinner in inside, after heating and melting, stickum is less.Because week is along needing viscosity large, so the many fastnesses that can guarantee that labeling is pasted of stickum when labeling is pasted; And the inner viscosity needing is little, so the waste that stickum can avoid hot melt adhesive too much to cause less.
Accompanying drawing explanation
Fig. 1 is the labeling that relates to of the utility model structural representation in an embodiment;
Fig. 2 is the labeling that relates to of the utility model side schematic view in an embodiment.
Embodiment
Referring to accompanying drawing, the related labeling of the utility model is elaborated.
Fig. 1 is the labeling that relates to of the utility model structural representation in an embodiment.
Fig. 2 is the labeling that relates to of the utility model side schematic view in an embodiment.
As depicted in figs. 1 and 2, labeling has basalis 1, hot melt adhesive layer 2 and hollow area 3.
Basalis 1 is paper.Hot melt adhesive layer 2 is coated in basalis 1 surface, after heating, can produce viscosity.Hot melt adhesive layer 2 for fusing point be 75 ℃ of hot melt adhesive layers that viscosity is 30Pa.s, its thickness by week along dwindling gradually to center position.
Hollow area 3 is opened in the center of hot melt adhesive layer 2, is shaped as relative hot melt adhesive layer 2 and dwindles in proportion, and size accounts for 1/16 of hot melt adhesive layer 2 areas.
Use procedure: when needs affix on object by labeling, the hot melt adhesive layer of this labeling 2 can be heated within the scope of the melt temperature of this hot melt adhesive, so that this hot melt adhesive becomes molten state rapidly and produces viscosity, now the labeling that produces viscosity is affixed on object, after hot melt adhesive is cooling, this labeling just can closely be sticked together with this object.
Embodiment effect and effect
The labeling related according to the present embodiment, because adopt hot melt adhesive layer to replace the existing viscous layers such as non-drying glue layer, there is no at normal temperatures viscosity, so do not need to use the base stock of isolation viscous layer, therefore the labeling of three layers and above structure can be reduced to double-layer structure, thereby avoid the waste because using base stock to cause.
In addition, because hot melt adhesive layer thickness is dwindled to center position gradually by all edges, so hot melt adhesive layer is thicker on all edges, and after heating and melting, stickum is more; Thinner in inside, after heating and melting, stickum is less.Because week is along needing viscosity large, so the many fastnesses that can guarantee that labeling is pasted of stickum when labeling is pasted; And the inner viscosity needing is little, so the waste that stickum can avoid hot melt adhesive too much to cause less.
In addition, because hot melt adhesive layer heating and melting again, so can repair the not good labeling of stickup, thus the utilization rate of labeling improved; And can remove the labeling of hot melt adhesive layer under molten condition from object, and can be on object residual stickup vestige.
In addition, owing to offering hollow area at hot melt adhesive layer center, so center do not have hot melt adhesive layer, there is no stickum after heating and melting.Because center does not need viscosity, do not affect the fastness that labeling is pasted yet, so center does not have stickum, can avoid the waste that causes hot melt adhesive too much to cause.
Certainly, the labeling that the utility model relates to is not merely defined in the structure in above embodiment.According to using needs, the hot melt adhesive melting range of the utility model hot melt adhesive layer can be selected arbitrarily between 70~84 ℃, and range of viscosities can be selected arbitrarily between 25~35Pa.s; Hollow area size accounts for the ratio of hot melt adhesive layer area and can between 1/64~1/4, select arbitrarily; Basalis can also be film.

Claims (4)

1. a labeling, for affixing to object, indicates object, it is characterized in that, comprising:
Basalis;
After being coated in described basalis surface heating, understand the hot melt adhesive layer that produces viscosity, this hot melt adhesive layer thickness is dwindled to center position gradually by all edges; And
Be opened in the hollow area that in described hot melt adhesive layer, the relatively described hot melt adhesive layer of heart shape dwindles in proportion, this hollow area accounts for described hot melt adhesive layer area 1/64~1/4.
2. labeling according to claim 1, is characterized in that:
Wherein, described hot melt adhesive layer is that fusing point is 70~84 ℃ of hot melt adhesive layers that viscosity is 25~35Pa.s.
3. labeling according to claim 1, is characterized in that:
Wherein, described basalis is paper.
4. labeling according to claim 1, is characterized in that:
Wherein, described basalis is film.
CN201420222292.9U 2014-05-04 2014-05-04 Labeling Expired - Fee Related CN204010533U (en)