CN203882089U - 一种掩膜版 - Google Patents

一种掩膜版 Download PDF

Info

Publication number
CN203882089U
CN203882089U CN201420142375.7U CN201420142375U CN203882089U CN 203882089 U CN203882089 U CN 203882089U CN 201420142375 U CN201420142375 U CN 201420142375U CN 203882089 U CN203882089 U CN 203882089U
Authority
CN
China
Prior art keywords
mask plate
reflectance coating
metal
tinsel
half tone
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN201420142375.7U
Other languages
English (en)
Inventor
张家清
盛科
黄守银
黄秋蓉
王海宏
焦峰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nanjing CEC Panda FPD Technology Co Ltd
Original Assignee
Nanjing CEC Panda LCD Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nanjing CEC Panda LCD Technology Co Ltd filed Critical Nanjing CEC Panda LCD Technology Co Ltd
Priority to CN201420142375.7U priority Critical patent/CN203882089U/zh
Application granted granted Critical
Publication of CN203882089U publication Critical patent/CN203882089U/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

本实用新型提供一种掩膜版,该掩膜版包括金属丝网版和粘贴于所述的金属丝网版下面的遮光金属片;在所述的金属丝网版上设有用于反射紫外光的反射膜或反射金属片,所述的反射膜或反射金属片和所述的遮光金属片分别位于金属丝网版的两侧。本实用新型通过在掩膜版远离玻璃基板的一侧设置反射膜或反射金属片,可以反射掉遮光金属片的胶水上的紫外光,避免了胶水的老化带来的金属脱落翘曲损坏液晶面板的问题,提高了显示器件的良率和品质。

Description

一种掩膜版
技术领域
本实用新型涉及液晶显示器制造领域,尤其涉及一种掩膜版。 
背景技术
液晶面板包括彩膜基板、阵列基板以及位于两者间的液晶组成。在液晶面板的制造过程中,彩膜基板或是阵列基板上涂布一圈封框胶,使用液晶滴下装置在封框胶围成的区域内滴下适量的液晶,在真空环境中将另一枚基板与之贴合,使用紫外光照射和热硬化使封框胶硬化固定,防止彩膜基板和阵列基板因受外力而发生偏移错位,而引起对位精度的下降,影响显示。 
在用紫外光固化封框胶的工程中,为防止紫外光照射液晶面板的显示区,需要用掩膜版对显示区进行遮光,掩模版只在对应封框胶图形的区域开口,图1为常用的掩模板的平面示意图。掩模版100是由金属丝网版101和粘贴于金属丝网版101下面的遮光金属片102构成,遮光金属一般可以是不锈钢、铬、铝等金属。图2为图1中A-A处的剖视图。图3为使用现有技术掩膜版紫外光固化封框胶示意图。在工程中,为了防止紫外光斜射入显示区,掩模版一般和贴合的基板距离仅有几毫米,并且由于丝网的厚度较大,遮光金属片是做在靠近基板一侧。胶水长时间暴露在紫外光的照射下,发生光老化和热老化,并且紫外光也会在金属片表面反射或吸收,产生的热被胶水吸收,加速胶水老化,当胶水涂布较薄或老化到黏着力不足以抵消遮光金属片的重力和内部应力时,遮光金属片就会发生脱落或翘曲变形,由于掩模版和玻璃基板距离很近,一旦翘曲,就会刮伤玻璃基板导致液晶显示器件制造良率下降和品质恶化。 
实用新型内容
为解决上述问题,本实用新型提供一种具有反射紫外光的反射膜或反射金属片的掩膜版,该掩膜版可以反射掉遮光金属片的胶水上的紫外光,避免了胶水的老化带来的金属脱落翘曲损坏液晶面板的问题,提高了显示器件的良率和品质。 
本实用新型提供一种掩膜版,该掩膜版包括金属丝网版和粘贴于所述的金属丝网版下面的遮光金属片;在所述的金属丝网版上设有用于反射紫外光的反射膜或反射金属片,所述的反射膜或反射金属片和所述的遮光金属片分别位于金属丝网版的两侧。所述的反射膜或反射金属片尺寸比遮光金属片小,反射膜或反射金属片与遮光金属片相邻两边的间距为500um至2000um,所述的反射膜或反射金属片用胶水粘在所述的金属丝网版上,所述反射膜可以是涂覆有紫外光反射层的聚对苯二甲酸乙二醇酯膜,反射金属片可以采用不锈钢、铬、铝等金属。 
本实用新型通过提供一种具有反射紫外光的反射膜或反射金属片的掩膜版,可以反射掉遮光金属片的胶水上的紫外光,避免了胶水的老化带来的金属脱落翘曲损坏液晶面板的问题,提高了显示器件的良率和品质。 
附图说明
图1为现有技术掩膜版的俯视图; 
图2为图1中A-A处的剖视图; 
图3为使用现有技术掩膜版紫外光固化封框胶示意图; 
图4为本实用新型掩膜版的俯视图; 
图5为图3中B-B处的剖视图; 
图6为使用本实用新型掩膜版封框胶固化示意图; 
具体实施方式
下面结合附图和具体实施例,进一步阐明本实用新型,应理解这些实施例仅用于说明本实用新型而不用于限制本实用新型的范围,在阅读了本发明之后,本领域技术人员对本实用新型的各种等价形式的修改均落于本申请所附权利要求所限定的范围。 
图3为使用现有技术掩膜版紫外光固化封框胶示意图,液晶面板制造过程中,下基板201上涂布一圈封框胶204,使用液晶滴下装置在封框胶204围成的区域内滴下适量的液晶203,在真空环境中将上基板201与下基板201贴合,使用紫外光固化封框胶204,为防止紫外光照射液晶面板的显示区,需要使用掩膜版100的遮光金属102对显示区进行遮光,掩模版100只在对应封框胶204图形 的区域开口。紫外光固化封框胶一般有两种方式,一种是彩膜基板在上侧,阵列基板在下侧;一种是阵列基板在上侧,彩膜基板在下侧。 
图4和图5分别为本实用新型提供的掩膜版的俯视图和剖视图,如图所示,该掩膜版100’包括金属丝网版101和通过胶水103黏贴于金属丝网版101靠近上基板201一侧的遮光金属片102;在金属丝网版101远离上基板201的一侧设有用于反射紫外光的反射膜或反射金属片104,即所述的反射膜或反射金属片104和所述的遮光金属片102分别位于金属丝网版101的两侧。所述的反射膜或反射金属片104用胶水103粘在所述的金属丝网版101上,所述的反射膜或反射金属片104尺寸比遮光金属片102小,反射膜或反射金属片104与遮光金属片102相邻两边的间距为500um至2000um,所述反射膜可以是涂覆有紫外光反射层的聚对苯二甲酸乙二醇酯膜,反射金属片104可以采用不锈钢、铬、铝等金属。图6为使用本实用新型掩膜版封框胶固化示意图。通过在掩膜版上增加反射膜或反射金属片可以反射掉照在下侧遮光金属片的胶水上的紫外光,避免了胶水的老化带来的金属脱落翘曲损坏玻璃基板的问题,提高了显示器件的良率和品质。 
本实用新型提供一种具有反射紫外光的反射膜或反射金属片的掩膜版,该掩膜版可以反射掉遮光金属片的胶水上的紫外光,避免了胶水的老化带来的金属脱落翘曲损坏液晶面板的问题,提高了显示器件的良率和品质。 

Claims (4)

1.一种掩膜版,包括金属丝网版和粘贴于所述的金属丝网版下面的遮光金属片,其特征在于:在所述的金属丝网版上设有用于反射紫外光的反射膜或反射金属片,所述的反射膜或反射金属片和所述的遮光金属片分别位于金属丝网版的两侧。 
2.根据权利要求1所述的掩膜版,其特征在于:所述的反射膜或反射金属片尺寸比遮光金属片小,反射膜或反射金属片与遮光金属片相邻两边的间距为500um至2000um。 
3.根据权利要求1所述的掩膜版,其特征在于:所述的反射膜或反射金属片用胶水粘在所述的金属丝网版上。 
4.根据权利要求1所述的掩膜版,其特征在于:所述反射膜可以是涂覆有紫外光反射层的聚对苯二甲酸乙二醇酯膜。 
CN201420142375.7U 2014-03-26 2014-03-26 一种掩膜版 Expired - Lifetime CN203882089U (zh)