CN203827389U - 一种新型手机后盖合体结构 - Google Patents
一种新型手机后盖合体结构 Download PDFInfo
- Publication number
- CN203827389U CN203827389U CN201420111038.1U CN201420111038U CN203827389U CN 203827389 U CN203827389 U CN 203827389U CN 201420111038 U CN201420111038 U CN 201420111038U CN 203827389 U CN203827389 U CN 203827389U
- Authority
- CN
- China
- Prior art keywords
- plastic cement
- mobile phone
- rear cover
- injection
- metal main
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
本实用新型提出一种新型手机后盖合体结构,包括金属主盖,和与金属主盖注塑结合在一起的塑胶副件;金属主盖在与塑胶副件相对应处形成有多个蚀刻纳米孔,塑胶副件形成有通过注塑成型方法匹配嵌入蚀刻纳米孔内的纳米凸起。如此,本实用新型突破传统手机后盖金属件与塑胶件胶合或直接注塑在一起的构造形式,用腐蚀性液体对金属主盖的相应处进行腐蚀,形成多个纳米级尺寸的蚀刻纳米孔,再用注塑成型工艺将塑胶副件与金属主盖注塑成型在一起,使金属主盖与塑胶副件牢固地结合在一起,且在金属主盖和塑胶副件都很薄的情况下,依然可达到牢固的结合强度,与现有技术相比,本实用新型的强度高,厚薄加工性强,加工效率高,成本低,实用性强。
Description
技术领域
本实用新型涉及手机部件领域,具体涉及一种新型手机后盖合体结构。
背景技术
为了满足使用、工艺以及装配上的要求,金属手机后盖一般需要与塑胶件结合,目前市场上普遍采用的结合方法是胶合和注塑成型等。但是在实际使用过程中,采用前述结合方法的手机后盖经常出现开裂甚至塑胶件脱落的情况,严重影响的人们的正常使用。而且为了满足各部件本身及结合整体的强度要求,采用前述结合方法的手机后盖不易过薄,厚薄加工性差,整体实用性受到了一定的限制。
鉴于此,本案发明人对上述问题进行深入研究,遂有本案产生。
实用新型内容
本实用新型的目的在于提供一种强度高,厚薄加工性强,加工效率高,成本低,实用性强的新型手机后盖合体结构。
为了达到上述目的,本实用新型采用这样的技术方案:
一种新型手机后盖合体结构,包括金属主盖,和与金属主盖注塑结合在一起的塑胶副件;所述金属主盖在与所述塑胶副件相对应处形成有多个蚀刻纳米孔,所述塑胶副件形成有通过注塑成型方法匹配嵌入所述蚀刻纳米孔内的纳米凸起。
上述金属主盖在与上述塑胶副件相对应处布满上述蚀刻纳米孔。
上述蚀刻纳米孔的直径为20-30nm。
采用上述技术方案后,本实用新型的新型手机后盖合体结构,突破传统手机后盖金属件与塑胶件胶合或直接注塑在一起的构造形式,用腐蚀性液体对金属主盖的相应处进行腐蚀,形成多个纳米级尺寸的蚀刻纳米孔,再用注塑成型工艺将塑胶副件与金属主盖注塑成型在一起,使塑胶副件在液态时流入蚀刻纳米孔内,凝固后即形成匹配嵌入蚀刻纳米孔的纳米凸起,纳米凸起与蚀刻纳米孔这种“根深蒂固”的结合,再加上注塑工艺的粘结力,使金属主盖与塑胶副件牢固地结合在一起,且在金属主盖和塑胶副件都很薄的情况下,依然可达到牢固的结合强度,与现有技术相比,本实用新型的新型手机后盖合体结构,其强度高,厚薄加工性强,加工效率高,成本低,实用性强。
附图说明
图1为本实用新型的结构示意图;
图2为本实用新型的分解结构示意图;
图3为本实用新型的局部分解剖视示意图。
图中:
1-金属主盖 11-蚀刻纳米孔
2-塑胶副件 21-纳米凸起
具体实施方式
为了进一步解释本实用新型的技术方案,下面通过具体实施例进行详细阐述。
本实用新型的一种新型手机后盖合体结构,如图1-3所示,包括金属主盖1和塑胶副件2。
塑胶副件2与金属主盖1注塑结合在一起;金属主盖1在与塑胶副件2相对应处形成有多个蚀刻纳米孔11,塑胶副件2形成有通过注塑成型方法匹配嵌入蚀刻纳米孔11内的纳米凸起21。在实际中,采用纳米成型技术(NMT),用腐蚀性液体对金属主盖1的相应处进行腐蚀,形成多个纳米级尺寸的蚀刻纳米孔11,具体步骤可以是这样的,(1)将冲压加工完成的金属主盖1放入碱液中,浸泡约一分钟进行脱脂;(2)将金属主盖1浸泡在酸液中,进行中和;(3)将金属主盖1放入腐蚀性液体中浸泡,使金属主盖1相应表面处形成多个蚀刻纳米孔11;(4)将金属主盖1放入清水中进行冲洗,然后进行干燥处理。然后再用注塑成型工艺将塑胶副件2与金属主盖1注塑成型在一起,使塑胶副件2在液态时流入蚀刻纳米孔11内,凝固后即形成匹配嵌入蚀刻纳米孔11内的纳米凸起21,纳米凸起21与蚀刻纳米孔11这种“根深蒂固”的结合,再加上注塑工艺的粘结力,使金属主盖1与塑胶副件2牢固地结合在一起,且在金属主盖1和塑胶副件2都很薄的情况下,依然可达到牢固的结合强度。
为了确保金属主盖1与塑胶副件2的结合强度,优选地,金属主盖1在与塑胶副件2相对应处布满蚀刻纳米孔11。
优选地,蚀刻纳米孔11的直径为20-30nm。
本实用新型的新型手机后盖合体结构,蚀刻纳米孔的具体尺寸、形状、数量和分布形式等可根据实际要求进行调整和设计;金属主盖和塑胶副件优选为现有的铝合金的金属主盖和树脂的塑胶副件的结构形式,具体材料和结构形式也可根据实际要求进行调整和设计。
本实用新型的产品形式并非限于本案图示和实施例,任何人对其进行类似思路的适当变化或修饰,皆应视为不脱离本实用新型的专利范畴。
Claims (3)
1.一种新型手机后盖合体结构,其特征在于:包括金属主盖,和与金属主盖注塑结合在一起的塑胶副件;所述金属主盖在与所述塑胶副件相对应处形成有多个蚀刻纳米孔,所述塑胶副件形成有通过注塑成型方法匹配嵌入所述蚀刻纳米孔内的纳米凸起。
2.根据权利要求1所述的一种新型手机后盖合体结构,其特征在于:上述金属主盖在与上述塑胶副件相对应处布满上述蚀刻纳米孔。
3.根据权利要求1或2所述的一种新型手机后盖合体结构,其特征在于:上述蚀刻纳米孔的直径为20-30nm。