CN203697236U - 保温冒口 - Google Patents
保温冒口 Download PDFInfo
- Publication number
- CN203697236U CN203697236U CN201320794752.0U CN201320794752U CN203697236U CN 203697236 U CN203697236 U CN 203697236U CN 201320794752 U CN201320794752 U CN 201320794752U CN 203697236 U CN203697236 U CN 203697236U
- Authority
- CN
- China
- Prior art keywords
- layer
- insulation layer
- shaped body
- column
- insulated feeder
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种保温冒口,包括柱状体和圆弧状体,所述柱状体与所述圆弧状体通过螺纹连接,所述柱状体底端设有凹槽,所述凹槽内固定有螺母,所述圆弧状体上设有与所述螺母相对应的螺丝,所述柱状体和所述圆弧状体均由涂料层、隔热层、填充层和保温层构成,所述隔热层、填充层和保温层的厚度比为1:2:2,所述隔热层内添加有莫来石颗粒,所述填充层为石棉层,所述保温层为膨胀珍珠岩、火山灰、蛭石、稻壳和稻壳灰中的一种。本实用新型可以根据需要调节冒口进口的形状,同时可以根据需要调节形状,适用范围广、补缩效率高、铸造工艺出品率高,同时设有涂层,可以很好的避免保温冒口表面的物质剥落。
Description
技术领域
本实用新型涉及一种铸件,特别是涉及一种保温冒口。
背景技术
目前, 在电熔锆刚玉砖制造企业使用的冒口都为方形冒口,所述的方形冒口包括冒口本体,冒口本体顶端设置的冒口进口为方形,冒口本体内部的冒口腔体横截面为方形。使用时将方形冒口置于砖材铸件上方,可为砖材铸件提供补缩液料。由于方形冒口进口较大,冒口腔体的保温效果较差,冒口腔体内的降温梯度较大,会导致砖材缩孔和液料使用率低,影响砖材铸件的质量。
实用新型内容
本实用新型所要解决的技术问题是提供一种保温冒口,可以根据需要调节冒口进口的形状,同时可以根据需要调节形状,适用范围广、补缩效率高、铸造工艺出品率高。
为解决上述技术问题,本实用新型所采取的技术方案如下:保温冒口,包括柱状体和圆弧状体,所述柱状体与所述圆弧状体通过螺纹连接,所述柱状体底端设有凹槽,所述凹槽内固定有螺母,所述圆弧状体上设有与所述螺母相对应的螺丝,所述柱状体和所述圆弧状体均由涂料层、隔热层、填充层和保温层构成,所述隔热层、填充层和保温层的厚度比为1:2:2,所述隔热层内添加有莫来石颗粒,所述填充层为石棉层,所述保温层为膨胀珍珠岩、火山灰、蛭石、稻壳和稻壳灰中的一种。
作为优选,所述涂料层为耐火涂料层。
作为优选,所述隔热层为轻质隔热层。
本实用新型可以根据需要调节冒口进口的形状,同时可以根据需要调节形状,适用范围广、补缩效率高、铸造工艺出品率高,同时设有涂层,可以很好的避免保温冒口表面的物质剥落。本实用新型耐火度高.保溫性能好.對鑄件產生效果是:1.補縮.2.去渣.3.保溫性能好.4.透气性強.5.使用分便.節省鋼水。
附图说明
图1为本实用新型的结构示意图;
图2为本实用新型柱状体的结构示意图;
图3为本实用新型圆弧状体的结构示意图。
具体实施方式
为使本实用新型实现的技术手段、创作特征、达成目的与功效易于明白了解,下面结合具体实施方式,进一步阐述本实用新型。
参照图1-3,本具体实施方式采用以下技术方案:保温冒口,包括柱状体1和圆弧状体2,所述柱状体1与所述圆弧状体2通过螺纹连接,所述柱状体1底端设有凹槽,所述凹槽内固定有螺母7,所述圆弧状体2上设有与所述螺母7相对应的螺丝8,所述柱状体1和所述圆弧状体2均由涂料层3、隔热层4、填充层5和保温层6构成,所述隔热层4、填充层5和保温层6的厚度比为1:2:2,所述隔热层4内添加有莫来石颗粒,所述填充层5为石棉层,所述保温层6为膨胀珍珠岩、火山灰、蛭石、稻壳和稻壳灰中的一种。
值得注意的是,所述涂料层3为耐火涂料层。
此外,所述隔热层4为轻质隔热层。
本实用新型可以根据需要调节冒口进口的形状,同时可以根据需要调节形状,适用范围广、补缩效率高、铸造工艺出品率高,同时设有涂层,可以很好的避免保温冒口表面的物质剥落。
以上显示和描述了本实用新型的基本原理和主要特征和本实用新型的优点。本行业的技术人员应该了解,本实用新型不受上述实施例的限制,上述实施例和说明书中描述的只是说明本实用新型的原理,在不脱离本实用新型精神和范围的前提下,本实用新型还会有各种变化和改进,这些变化和改进都落入要求保护的本实用新型范围内。本实用新型要求保护范围由所附的权利要求书及其等效物界定。
Claims (3)
1. 保温冒口,其特征在于,包括柱状体(1)和圆弧状体(2),所述柱状体(1)与所述圆弧状体(2)通过螺纹连接,所述柱状体(1)底端设有凹槽,所述凹槽内固定有螺母(7),所述圆弧状体(2)上设有与所述螺母(7)相对应的螺丝(8),所述柱状体(1)和所述圆弧状体(2)均由涂料层(3)、隔热层(4)、填充层(5)和保温层(6)构成,所述隔热层(4)、填充层(5)和保温层(6)的厚度比为1:2:2,所述隔热层(4)内添加有莫来石颗粒,所述填充层(5)为石棉层,所述保温层(6)为膨胀珍珠岩、火山灰、蛭石、稻壳和稻壳灰中的一种。
2. 根据权利要求1所述的保温冒口,其特征在于,所述涂料层(3)为耐火涂料层。
3.根据权利要求1所述的保温冒口,其特征在于,所述隔热层(4)为轻质隔热层。