CN203683682U - Titanium bar electrode for water treatment - Google Patents
Titanium bar electrode for water treatment Download PDFInfo
- Publication number
- CN203683682U CN203683682U CN201320811317.4U CN201320811317U CN203683682U CN 203683682 U CN203683682 U CN 203683682U CN 201320811317 U CN201320811317 U CN 201320811317U CN 203683682 U CN203683682 U CN 203683682U
- Authority
- CN
- China
- Prior art keywords
- assembly
- groove
- bar electrode
- component
- water treatment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
The utility model relates to a titanium bar electrode for water treatment. The titanium bar electrode comprises a first component with a thread and a second component with a first groove, wherein the first component is fixedly connected with the second component; a second groove is formed in the connecting part of the first component and the second component; the second groove is internally provided with a sealing ring. By connecting the first component to a power supply wire and soaking the second component into saline water, after being powered on, the titanium bar electrode can sterilize and disinfect water through generated chlorine.
Description
Technical field
The utility model relates to a kind of titanium bar electrode for water treatment.
Background technology
In electrochemical industry (as chlorine industry), generally use graphite electrode material and lead alloy material, in addition also has the ferroelectric utmost point etc., its advantage is that cost is low, but current density is little, and work-ing life is short, and because of consumption of electrode, there is a large amount of electrode compositions to stay in product, increased aftertreatment technology, and then increased cost.In order to promote electrochemical application more widely, meet the requirement using, recently develop various new electrode materials, but mostly be chemical cell electrode and electrode for capacitors, and be applied to electrode materials in field of Environment Protection few.
Utility model content
The utility model provides a kind of titanium bar electrode for water treatment, to solve the problem that existing electrode materials current density is little, the life-span is short and aftertreatment cost is high.
For solving the problems of the technologies described above, the utility model provides a kind of titanium bar electrode for water treatment, comprise screwed the first assembly, the second assembly with the first groove, described the first assembly is fixedly connected with the second assembly, the junction of described the first assembly and the second assembly forms the second groove, in described the second groove, is provided with sealing-ring.
Preferably, described the first assembly and the second assembly all adopt pure titanium material to make.
Preferably, described the first assembly and the second assembly be externally coated with rhodium iridium oxide.
Compared with prior art, the titanium bar electrode for water treatment that the utility model provides, comprise screwed the first assembly, the second assembly with the first groove, described the first assembly is fixedly connected with the second assembly, the junction of described the first assembly and the second assembly forms the second groove, in described the second groove, is provided with sealing-ring.The utility model is by described the first assembly is connected to supply lead, and the second assembly is immersed in salt solution, and after energising, the chlorine of generation is to the water sterilization that carries out disinfection.
Brief description of the drawings
Fig. 1 is the perspective view of the titanium bar electrode for water treatment of the utility model one embodiment;
Fig. 2 is the front view of the titanium bar electrode for water treatment of the utility model one embodiment;
Fig. 3 is the A portion enlarged view of Fig. 2.
In figure: 10-the first assembly, 11-screw thread, 20-the second assembly, 21-the first groove, 30-the second groove, 31-sealing-ring.
Embodiment
For making above-mentioned purpose of the present utility model, feature and advantage can be more clear understandable, below in conjunction with accompanying drawing, embodiment of the present utility model is described in detail.It should be noted that, the utility model accompanying drawing all adopts the form of simplification and all uses non-ratio accurately, only in order to convenient, the object of aid illustration the utility model embodiment lucidly.
The titanium bar electrode for water treatment that the utility model provides, as shown in Figures 1 to 3, comprise and be threaded the first assembly 10 of 11, the second assembly 20 with the first groove 21, described the first assembly 10 is fixedly connected with the second assembly 20, the junction of described the first assembly 10 and the second assembly 20 forms the second groove 30, in described the second groove 30, be provided with sealing-ring 31, particularly, in described the first assembly 10 exposures and air, for with carry out fastening with the mating parts (not shown) matching with described screw thread 11, particularly, described mating parts is supply lead; Described the second assembly 20 welds with titanium blade by the first groove 21, forms electrode slice; Described sealing-ring 31 plays sealing function, prevents that salt solution from infiltrating into supply lead one end, causes danger.The utility model is by described the first assembly 10 is connected to supply lead, and the second assembly 20 is immersed in salt solution, and after energising, the chlorine of generation is to the water sterilization that carries out disinfection, and then keeps the clean of water.
Preferably, described the first assembly 10 and the second assembly 20 all adopt pure titanium material to make.Because pure titanium material erosion resistance is extremely strong, the good stability in electrolytic solution (salt solution), compared to graphite electrode material and lead alloy material, there is current density large, long service life, and electrodeless consumption, without follow-up treatment process, thereby greatly reduce production cost.
Preferably, described the first assembly 10 and the second assembly 20 be externally coated with rhodium iridium oxide.Because metal rhodium, iridium have good erosion resistance and electroconductibility, and there is good electrocatalysis effect.
In sum, the titanium bar electrode for water treatment that the utility model provides, comprise and be threaded the first assembly 10 of 11, the second assembly 20 with the first groove 21, described the first assembly 10 is connected with the second assembly 20 rotary types, the junction of described the first assembly 10 and the second assembly 20 forms the second groove 30, in described the second groove 30, is provided with sealing-ring 31.The utility model is by described the first assembly 10 is connected to supply lead, and the second assembly 20 is immersed in salt solution, and after energising, the chlorine of generation is to the water sterilization that carries out disinfection, and then keeps the clean of water.
Obviously, those skilled in the art can carry out various changes and modification and not depart from spirit and scope of the present utility model utility model.Like this, if these amendments of the present utility model and within modification belongs to the scope of the utility model claim and equivalent technologies thereof, the utility model is also intended to including these changes and modification.
Claims (3)
1. the titanium bar electrode for water treatment, it is characterized in that, comprise screwed the first assembly, the second assembly with the first groove, described the first assembly is fixedly connected with the second assembly, the junction of described the first assembly and the second assembly forms the second groove, in described the second groove, is provided with sealing-ring.
2. the titanium bar electrode for water treatment as claimed in claim 1, is characterized in that, described the first assembly and the second assembly all adopt pure titanium material to make.
3. the titanium bar electrode for water treatment as claimed in claim 1, is characterized in that, described the first assembly and the second assembly be externally coated with rhodium iridium oxide.