CN203622850U - Battery shell mould - Google Patents
Battery shell mould Download PDFInfo
- Publication number
- CN203622850U CN203622850U CN201320822251.9U CN201320822251U CN203622850U CN 203622850 U CN203622850 U CN 203622850U CN 201320822251 U CN201320822251 U CN 201320822251U CN 203622850 U CN203622850 U CN 203622850U
- Authority
- CN
- China
- Prior art keywords
- drag hook
- plate
- mould
- bullet piece
- front mould
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
The utility model discloses a battery shell mould which comprises a plate A (2), a push plate (3), a fixing plate (4) and a front mould elastic block (6), wherein the plate A (2) is provided with a groove (21) in which the front mould elastic block (6) is positioned; the push plate (3) is provided with a drag hook passing hole (32). The battery shell mould further comprises a demoulding mechanism (7), wherein the demoulding mechanism (7) comprises a first drag hook (71) and a second drag hook (72), wherein the first drag hook (71) is fixedly connected to the front mould elastic block (6); one end of the second drag hook (72) is fixedly connected to the fixing plate (4); the other end of the second drag hook (72) passes through the drag hook passing hole (32) to be tightly buckled with the first drag hook (71) at a mould assembling state; when the front mould elastic block (6) partially exits from the groove (21) under the action of an acting force of the second drag hook (72) to the first drag hook (71) at a mould opening state, the first drag hook (71) is completely separated away from the second drag hook (72), so that a battery shell can be demoulded when the front mould elastic block (6) is invalid.
Description
Technical field
The application relates to field of batteries, is specifically related to a kind of battery case mould.
Background technology
The stripping means of present most of battery case moulds has two kinds conventionally, and one is the ejecting push plate demoulding, and another kind is that front mould bullet piece ejects the demoulding.
The ejecting push plate demoulding is applicable to little, the highly higher battery case mould of draw taper.And some battery moulds will be used the front mould bullet piece ejection demoulding.
The application for a patent for invention that application number 201210404028.2 is announced, name is called " a kind of battery case mould ", and wherein A plate is provided with the mounting groove coordinating with bullet piece, and bullet piece can partly eject mounting groove in the time of die sinking.This stripping means is that front mould bullet piece ejects the demoulding.
Front mould bullet piece ejects the demoulding and refers to after die sinking, and front mould bullet piece skids off A plate certain distance under the active force of spring.Front mould bullet piece skids off A plate and is prone to front mould bullet piece Problem of Failure, that is: when spring fatigue, front mould bullet piece cannot be ejected or spring eject not up time, and front mould bullet piece is stuck, and causes product not take off mould.
Summary of the invention
The problem that while inefficacy for the front mould bullet piece of battery case mould, product cannot the demoulding, the application provides a kind of battery case mould, comprises A plate, push pedal, fixed head and front mould bullet piece, and push pedal is between A plate and fixed head; A plate is provided with groove, and front mould bullet piece is positioned at groove; Also comprise mould emptier, mould emptier comprises the first drag hook and the second drag hook; Push pedal is provided with drag hook perforation;
The first drag hook is bolted on front mould bullet piece;
Second drag hook one end is connected with fixed head, and under matched moulds state, the second drag hook other end links closely with the first drag hook through drag hook perforation;
Under die opening state, when the second drag hook makes front mould bullet piece part exit groove to the active force of the first drag hook, the first drag hook and the second drag hook depart from completely.
In one embodiment, front mould bullet piece is provided with the accommodating position of drag hook, and the first drag hook is positioned at the accommodating position of drag hook side and is provided with screens or button bit, and the second drag hook upper end is placed in the accommodating position of drag hook, and is provided with the button bit or the screens that coordinate with the first drag hook.
In one embodiment, the first drag hook is provided with boss, and the second drag hook comprises the second drag hook plate, and the second drag hook plate upper end is provided with groove.
In one embodiment, the second drag hook also comprises the second drag hook briquetting, and the second drag hook briquetting and fixed head are spirally connected.
In one embodiment, the second drag hook plate lower end is provided with container cavity, and the second drag hook plate lower end is held between the second drag hook briquetting and fixed head.
In one embodiment, the second drag hook also comprises the second drag hook spring, and the second drag hook spring fitting is in container cavity.
The application's beneficial effect is: the battery case mould that the application provides has the first drag hook and the second drag hook; The first drag hook is fixed in front mould bullet piece, one end of the second drag hook is fixed on fixed head, when matched moulds, the second drag hook other end links closely with the first drag hook through drag hook perforation, under die opening state, when front mould bullet piece lost efficacy, the second drag hook makes front mould bullet piece part exit A plate groove to the active force of the first drag hook, has prevented that product cannot the demoulding.
Accompanying drawing explanation
Fig. 1 is battery case die structure dwg;
Fig. 2 is front mould bullet block structural diagram;
Fig. 3 is the first hook structure figure;
Fig. 4 is the second hook structure figure;
Fig. 5 is the second drag hook side view;
Fig. 6 is battery case mould mold-opening structure figure for the first time;
Fig. 7 is battery case mould mold-opening structure figure for the second time;
Fig. 8 is battery case mould mold-opening structure figure for the third time;
Fig. 9 is battery case mould mould-matching structure figure for the first time;
Figure 10 is battery case mould mould-matching structure figure for the second time;
Figure 11 is battery case mould mould-matching structure figure for the third time.
The specific embodiment
By reference to the accompanying drawings the present invention is described in further detail below by the specific embodiment.
Please refer to Fig. 1, in the embodiment of the present application, battery case mould comprises panel 1, A plate 2, push pedal 3, fixed head 4, base plate 5, front mould bullet piece 6 and mould emptier 7.
Annexation between panel 1, A plate 2, push pedal 3, fixed head 4, base plate 5 and front mould bullet piece 6 in the present embodiment is that those skilled in the art are known, does not repeat.
A plate 2 is provided with groove 21, and groove 21 is trapezium structure.Push pedal 3 is provided with the second die cavity 31, and fixed head 4 is provided with the first die cavity 41, and the cavity forming between front mould bullet piece 6 and groove 21 is called the 3rd die cavity 22, the first die cavities 41, the second die cavity 31 and the 3rd die cavity 22 respectively about mold center's axial symmetry and communicate.
Front mould bullet piece 6 adopts right-angled trapezium design, and front mould bullet piece 6 is installed in groove 21, and the inclined-plane of front mould bullet piece 6 is adjacent with the inclined-plane of groove 21.Front mould bullet piece 6 comprises the accommodating position 64 of front mould bullet piece spring 61, spring guide pillar 62, front mould bullet piece limited block 63 and drag hook, as shown in Figure 2.Spring guide pillar 62 one end are fixed on panel 1, are called stiff end, and the other end, through front mould bullet piece spring 61, is called free end; Front mould bullet piece spring 61 is installed on front mould bullet piece 6, and its one end is connected with the stiff end of spring guide pillar 62, and front mould bullet piece spring 61 ejects front mould bullet piece 6 for part.Front mould bullet piece limited block 63 is installed on A plate 2, specifically with fixed screw, front mould bullet piece limited block 63 and A plate 2 are locked, front mould bullet piece limited block 63 for front mould bullet piece 6 parts when skidding off in groove 21, spacing to front mould bullet piece 6.
Mould emptier 7 comprises the first drag hook 71; as shown in Figure 3; the first drag hook 71 is positioned at the accommodating position of drag hook side and is provided with screens or button bit; in the present embodiment; the first drag hook 71 is provided with screens; be provided with boss 711, boss 711 is provided with screw perforation 7111 above, bore a hole and 7111 boss 711 and front mould bullet piece 6 is locked by screw.
Mould emptier 7 also comprises the second drag hook 72; as shown in Figure 4 and Figure 5; the second drag hook 72 can be installed on fixed head 4 and also can be installed in push pedal 3; but; in the time that the second drag hook 72 is installed in push pedal 3, when front mould bullet piece 6 lost efficacy, easily make front mould bullet piece 6 and push pedal 3 simultaneously in the same way motion cause the product cannot the demoulding; therefore, the present embodiment adopts the second drag hook 72 to be installed on fixed head 4.
The second drag hook 72 comprises that the second drag hook plate 721, the second drag hook briquetting 722 and the second drag hook spring 723, the second drag hook plate 721 upper ends are provided with button bit or screens, and in the present embodiment, the second drag hook plate 721 upper ends are provided with groove 7211; The lower end of the second drag hook plate 721 is provided with container cavity 7212, the second drag hook springs 723 and is installed in container cavity 7212; The second drag hook briquetting 722 is rectangular shape, and be provided with screw perforation 7221 above, the second drag hook briquetting 722 is bolted on fixed head 4 together with the second drag hook plate 721, specifically: the lower end of the second drag hook plate 721 is held between the second drag hook briquetting 722 and fixed head 4, screw is bolted on fixed head 4 the second drag hook plate 721 and the second drag hook briquetting 722 through screw perforation 7221, under the effect of the second drag hook spring 723, the second drag hook plate 721 can move left and right between the second drag hook briquetting 722 and fixed head 4.
Battery case mould also comprises that mold insert 8 and purt chew 9; The upper end of mold insert 8 is successively through the first die cavity 41, the second die cavity 31 and the 3rd die cavity 22, chews 9 lower end in contact with purt, and the lower end of mold insert 8 is fixed on base plate 5.
Battery case mould also comprises guide pillar 10, and one end of guide pillar 10 is fixed on base plate 5, and the other end of guide pillar 10 is successively through the corresponding guide pillar perforation arranging on push pedal 3, A plate 2 and panel 1.
Battery case mould also comprises push pedal limited block 11, and push pedal limited block 11 is provided with accommodating position 111, and accommodating position 111 can be concave groove, can be also cavity.One end of push pedal limited block 11 is screwed on fixed head 4, is called stiff end.One end of push pedal 3 is provided with boss 33, and boss 33 can be free to slide in accommodating position 111, in the time of the upper end in contact of boss 33 and push pedal limited block 11, and the distance that restriction push pedal 3 and fixed head 4 are opened.
Battery case mould also comprises A plate limited block (not occurring in figure), the distance that A plate limited block is opened for limiting A plate 2 and push pedal 3.
Battery case mould is in the time of matched moulds state, and panel 1, A plate 2, push pedal 3, fixed head 4 and base plate 5 stack gradually, and the first drag hook 71 links closely mutually with the second drag hook 72.
The battery case mould of describing based on the present embodiment, the die sinking mode of the battery case mould of specific descriptions the present embodiment.
1. die sinking for the first time (the auxiliary front mould bullet piece of drag hook and spring ejects)
As shown in Figure 6, when mould is opened, front mould bullet piece 6 part under the active force of front mould bullet piece spring 61 and the first drag hook 71 and the second drag hook 72 skids off A plate 2, and then drives product section to skid off A plate 2.
Front mould bullet piece 6 easily causes the product cannot the demoulding while inefficacy, the present embodiment adopt the first drag hook 71, the second drag hook 72 and front mould bullet piece spring 61 together auxiliary front mould bullet piece 6 skid off A plate 2.When mould is opened, because the first drag hook 71 and the second drag hook 72 are in the state of linking closely, the active force of the second drag hook 72 to the first drag hook 71 and the active force of front mould bullet piece spring 61, front mould bullet piece 6 is to the direction motion of push pedal 3, because front mould bullet piece 6 moves along the bevel direction of groove 21, the first drag hook 71 is also along with front mould bullet piece 6 is to diagonal crossing, and the second drag hook 72 is vertical direction motion always, when the first drag hook 71 moves to certain distance, in the groove 7211 that boss 711 arranges from the second drag hook plate 721, deviate from, realize the first drag hook 71 and the second drag hook 72 departs from.When front mould bullet piece 6 is spacing by front mould bullet piece limited block 63, the first drag hook 71 and the second drag hook 72 depart from completely.
2. die sinking for the second time
In the time of die sinking for the first time, front mould bullet piece 6 is by front mould bullet piece spring 61, the first drag hook 71 and the auxiliary A plate 2 that ejects of the second drag hook 72, in the time that front mould bullet piece 6 is spacing by front mould bullet piece limited block 63, the first drag hook 71 and the second drag hook 72 depart from completely, now, push pedal 3, fixed head 4, base plate 5, the second drag hook 72 continue to move downward together with mold insert 8 and product, until spacing out between A plate 2 and push pedal 3 equals setpoint distance, wherein, setpoint distance refers to the distance that the A plate limited block (not shown) between A plate 2 and push pedal 3 limits, as shown in Figure 7.
3. die sinking for the third time (product taking-up)
After die sinking for the second time, base plate 5, fixed head 4, the second drag hook 72 continues to move downward together with mold insert 8, the drag hook perforation 32 that the upper end of the second drag hook 72 arranges from push pedal 3, deviate from, simultaneously, because the upper port of mold insert 8 is less than the lower port of product, when die sinking for the third time, product is stayed above push pedal 3, mold insert 8 is deviate from and is rested in the second die cavity 31 that push pedal 3 arranges from product, in the time of push pedal 3 boss 33 of one end setting and the upper end in contact of push pedal limited block 11, illustrate that the distance that push pedal 3 and fixed head 4 pull open equals the distance that push pedal limited block 11 limits, product and mold insert 8 depart from completely, as shown in Figure 8.
The battery case mould of describing based on the present embodiment, the clamping system of the battery case mould of specific descriptions the present embodiment.
1. matched moulds (A plate and push pedal are affixed) for the first time
When matched moulds, panel 1 moves downward together with A plate 2 for the first time, until front mould bullet piece 6 is attached in push pedal 3, front mould bullet piece 6 resets, as shown in Figure 9.
2. matched moulds for the second time
Continue matched moulds, the perforation 33 that the upper end of the second drag hook 72 arranges through push pedal 3, arrives the accommodating position 64 of drag hook that front mould bullet piece 6 arranges, the first drag hook 71 and the second drag hook 72 are collided, under the effect of clamp force, impel the second drag hook 72 to slide to mold center, as shown in figure 10.
3. matched moulds (push pedal and fixed head are affixed) for the second time
Continue matched moulds, the second drag hook 72 is got back to original position under the active force of the second drag hook spring 723, and the first drag hook 71 and the second drag hook 72 link closely, and matched moulds completes, as shown in figure 11.
Above content is in conjunction with concrete embodiment further description made for the present invention, can not assert that specific embodiment of the invention is confined to these explanations.For general technical staff of the technical field of the invention, without departing from the inventive concept of the premise, can also make some simple deduction or replace.
Claims (6)
1. a battery case mould, comprise A plate (2), push pedal (3), fixed head (4) and front mould bullet piece (6), described push pedal (3) is positioned between described A plate (2) and fixed head (4), described A plate (2) is provided with groove (21), described front mould bullet piece (6) is positioned at described groove (21), it is characterized in that, also comprise mould emptier (7), described mould emptier (7) comprises the first drag hook (71) and the second drag hook (72); Described push pedal (3) is provided with drag hook perforation (32);
Described the first drag hook (71) is fixed on described front mould bullet piece (6);
Described the second drag hook (72) one end is connected with described fixed head (4), under matched moulds state, described the second drag hook (72) other end links closely through described drag hook perforation (32) and described the first drag hook (71);
Under die opening state, when described the second drag hook (72) makes described front mould bullet piece (6) part exit described groove (21) to the active force of described the first drag hook (71), described the first drag hook (71) departs from completely with the second drag hook (72).
2. battery case mould as claimed in claim 1, it is characterized in that, described front mould bullet piece (6) is provided with the accommodating position of drag hook (64), described the first drag hook (71) is positioned at the accommodating position of described drag hook (64) side and is provided with screens or button bit, described the second drag hook (72) upper end is placed in the accommodating position of described drag hook (64), and is provided with the button bit or the screens that coordinate with described the first drag hook (71).
3. battery case mould as claimed in claim 2, it is characterized in that, described the first drag hook (71) is provided with boss (711), described the second drag hook (72) comprises the second drag hook plate (721), and described the second drag hook plate (721) upper end is provided with groove (7211).
4. battery case mould as claimed in claim 3, is characterized in that, described the second drag hook (72) also comprises the second drag hook briquetting (722), and described the second drag hook briquetting (722) is spirally connected with described fixed head (4).
5. battery case mould as claimed in claim 4, it is characterized in that, described the second drag hook plate (721) lower end is provided with container cavity (7212), and described the second drag hook plate (721) lower end is held between described the second drag hook briquetting (722) and described fixed head (4).
6. battery case mould as claimed in claim 5, it is characterized in that, described the second drag hook (72) also comprises the second drag hook spring (723), and described the second drag hook spring (723) is positioned in described container cavity (7212).