CN203474920U - 一种铝电解槽并联预热装置 - Google Patents
一种铝电解槽并联预热装置 Download PDFInfo
- Publication number
- CN203474920U CN203474920U CN201320609900.7U CN201320609900U CN203474920U CN 203474920 U CN203474920 U CN 203474920U CN 201320609900 U CN201320609900 U CN 201320609900U CN 203474920 U CN203474920 U CN 203474920U
- Authority
- CN
- China
- Prior art keywords
- bus bar
- plate
- bus
- electrolysis
- short
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
一种铝电解槽并联预热装置,以解决现有采用分流片的电解槽预热方式,每次只能预热一个电解槽,预热效率较低,在预热时,还需向分流片吹压缩空气,成本较高,同时,分流片的发热属于无效损耗,增加了电解槽的预热电耗,造成能源浪费的问题。依次设置三个电解槽,相邻两电解槽中,上游电解槽阴极母线板通过立柱母线与下游电解槽阳极母线板相连,立柱母线的两侧设置短路母线板,短路母线板与立柱母线之间设置绝缘板,短路母线板与下游电解槽阴极母线板相连,上游电解槽的阳极母线板通过连接母线与短路母线板或下游电解槽阴极母线板相连接。本实用新型用于铝电解生产。
Description
技术领域
本实用新型涉及一种电解槽预热装置,具体涉及一种铝电解槽的并联预热装置。
背景技术
一般在铝电解车间中,一个电解系列有上百台电解槽,数十万安培的大电流串联通过每台电解槽。电解槽的初始通电状态,国际上都称为预热preheat,国内称为焙烧。一台刚通电的电解槽,槽内衬是常温,电阻大,槽电压高,会有一个较高的冲击电压,并且会快速的升温。为了避免高冲击电压和快速升温对槽内衬的不利影响和损害,通常给刚通电预热的电解槽加装分流片,分流片与电解槽想并联。分流片用薄钢板制作,连接在预热电解槽的阳极母线和阴极母线之间,让大约一半的电流通过分流片,以降低通过电解槽的电流,来降低电解槽的冲击电压和升温速度。在预热时,钢分流片上通过大电流,发热严重,通常都烧得发红,为避免烧断分流片,要吹压缩空气来冷却分流片。同时,分流片的发热属于无效损耗,增加了电解槽的预热电耗。
发明内容
本实用新型的目的在于:提供一种铝电解槽并联预热装置,以解决现有采用分流片的电解槽预热方式,预热效率较低,在预热时,还需向分流片吹压缩空气,同时,分流片的发热属于无效损耗,增加了电解槽的预热电耗。
本实用新型的方案如下:一种铝电解槽并联预热装置,包括连续设置的三个电解槽,相邻两个电解槽中,上游电解槽阴极母线板通过立柱母线与下游电解槽阳极母线板相连,立柱母线的两侧分别设置一个短路母线板,且短路母线板与立柱母线之间设置绝缘板,短路母线板与下游电解槽阴极母线板相连,上游电解槽的阳极母线板通过连接母线与短路母线板或下游电解槽阴极母线板相连接。
所述连接母线包括上母线块、四根软母线和下母线块,所述四根软母线的一端分别与上母线块相连,四跟软母线的另一端分别连接有一个下母线块,上母线块与上游电解槽阳极母线板相连,四个下母线块分别连接在两个短路母线板的两侧。
本实用新型与现有技术相比,主要优点是:
1、本实用新型采用连接母线将相邻两电解槽中上游电解槽的阳极母线板与短路母线板或下游电解槽阴极母线板相连接,使依次的三个电解槽中,两端的电解槽并联,中间的电解槽相当于断路,在三个电解槽所组成机构的两端施加预热电压后,两端的两个电解槽同时预热,增加预热效率,同时,无需使用分流板,避免了向分流板吹压缩空气和分流片上产生的无效电耗,降低预热成本,节约能源;
2、四根软母线分别通过下母线块与两个短路母线板的两侧相连,使上游电解槽阳极母线板与下游电解槽阴极母线板的连接及导电效果更好。
附图说明
图1是本实用新型的主视结构示意图;图2是图1中相连两电解槽之间的立柱母线和连接母线处的局部放大图;图3是图2的俯视图;图4是连接母线的主视结构示意图;图5是图4的俯视结构示意图;图6是立柱母线的主视结构示意图;图7是图6的俯视图;图8是图6的右视图;图9是本实用新型的原理图。
具体实施方式
参照附图,一种铝电解槽并联预热装置,依次设置三个电解槽9,相邻两电解槽9中,上游电解槽阴极母线板1通过立柱母线2与下游电解槽阳极母线板6相连,立柱母线2的两侧分别设置一个短路母线板4,且短路母线板4与立柱母线2之间设置绝缘板3,短路母线板4与下游电解槽阴极母线板5相连,上游电解槽的阳极母线板8通过连接母线7与短路母线板4或下游电解槽阴极母线板5相连接,由于每个电解槽9都相当于一个电源,中间的电解槽9相当于断路,两端的两个电解槽9相并联,系列电流(一个电解系列为多个电解槽串联组成,系列电流即电解系列中通入的电流)通过并联的两个电解槽9,所述两端的两个电解槽9各通过系列电流的一半,从而实现两端的两个电解槽9各以额定电流(指系列电流)的一半进行预热。所述连接母线7包括上母线块71、四根软母线72和下母线块73,所述四根软母线72的一端分别与上母线块71相连,四跟软母线72的另一端分别连接有一个下母线块73,上母线块71与上游电解槽阳极母线板8相连,四个下母线块73分别连接在两个短路母线板4的两侧。
预热结束后,取下连接母线7,所述两端的两个电解槽9即可进行正常的电解生产。
Claims (2)
1.一种铝电解槽并联预热装置,包括连续设置的三个电解槽(9),相邻两个电解槽(9)中,上游电解槽阴极母线板(1)通过立柱母线(2)与下游电解槽阳极母线板(6)相连,立柱母线(2)的两侧分别设置一个短路母线板(4),且短路母线板(4)与立柱母线(2)之间设置绝缘板(3),短路母线板(4)与下游电解槽阴极母线板(5)相连,其特征在于:上游电解槽的阳极母线板(8)通过连接母线(7)与短路母线板(4)或下游电解槽阴极母线板(5)相连接。
2.根据权利要求1所述一种铝电解槽并联预热装置,其特征在于:所述连接母线(7)包括上母线块(71)、四根软母线(72)和下母线块(73),所述四根软母线(72)的一端分别与上母线块(71)相连,四跟软母线(72)的另一端分别连接有一个下母线块(73),上母线块(71)与上游电解槽阳极母线板(8)相连,四个下母线块(73)分别连接在两个短路母线板(4)的两侧。