CN203438555U - Device for adhering adhesive piece to tire lining - Google Patents

Device for adhering adhesive piece to tire lining Download PDF

Info

Publication number
CN203438555U
CN203438555U CN201320393288.4U CN201320393288U CN203438555U CN 203438555 U CN203438555 U CN 203438555U CN 201320393288 U CN201320393288 U CN 201320393288U CN 203438555 U CN203438555 U CN 203438555U
Authority
CN
China
Prior art keywords
film
dancer rools
adhesive piece
adhering
laminating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn - After Issue
Application number
CN201320393288.4U
Other languages
Chinese (zh)
Inventor
满彦林
范钱龙
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu General Science Technology Co Ltd
Original Assignee
Jiangsu General Science Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangsu General Science Technology Co Ltd filed Critical Jiangsu General Science Technology Co Ltd
Priority to CN201320393288.4U priority Critical patent/CN203438555U/en
Application granted granted Critical
Publication of CN203438555U publication Critical patent/CN203438555U/en
Anticipated expiration legal-status Critical
Withdrawn - After Issue legal-status Critical Current

Abstract

The utility model relates to a device for adhering a adhesive piece to a tire lining. The device for adhering the adhesive piece to the tire lining is mounted on original cutting equipment, and is characterized by comprising adhesive piece cutters, regulating roll sets and an adhering press roll, wherein two adhesive piece cutters are mounted on a cutter rest of the original cutting equipment, and are positioned on the outer sides of two side trimming cutters respectively; the adhesive piece cutters are connected with a control switch through connecting wires; the adhesive piece cutters are matched with the trimming cutters of the original cutting equipment to cut a part of a rubber edge cut from a transitional-layer adhesive piece as an adhering adhesive piece; two regulating roll sets are arranged on the two sides of a receiving roll bed of the original cutting equipment respectively; the regulating roll sets are used for overturning the adhering adhesive piece cut by the cutters above the cut transitional-layer adhesive piece; the adhering press roll is mounted on the receiving roll bed; the adhering press roll is used for adhering the adhering adhesive piece which is overturned in place to the transitional-layer adhesive piece by pressing. The device for adhering the adhesive piece to the tire lining can be used for directly adhering the adhesive piece during production of the lining, thereby reducing the reject ratio caused by bubbles in a tire bead and improving the quality of the tire.

Description

Tire liner gluing sheet device
Technical field
The utility model relates to a kind of tire liner gluing sheet device, specifically a kind of to the device that has the green tyres of mass defect (as tyre bead starved) to carry out the transformation of inner liner gluing sheet after some sulfuration, belongs to tire production manufacturing technology field.
Background technology
In prior art, tire liner production process is as follows: first by extruder and calender, backing powder formula sizing material is made to the smooth transition layer film of regulation section thickness, then by cutting apparatus, transition zone film is carried out to cutting edge, transition zone film is cut into Rack, then fit when producing inner liner formula film.But in actual production, there is tyre bead starved problem in some green tyres, current method is when moulding, directly on the wear-resisting glue in sidewall, to add gluing sheet to solve after sulfuration, and this kind of solution is owing to being cold subsides, easily there is tyre bead bubble phenomenon, and increased operation and cost.Existing inner liner production equipment cannot directly carry out film laminating when producing.
Summary of the invention
The purpose of this utility model is to overcome the deficiencies in the prior art, a kind of tire liner gluing sheet device is provided, it is simple in structure, directly be installed on former cutting apparatus, can when producing, inner liner directly add gluing sheet, solve some fetus because inner liner defect causes there is the problem of mass defect after sulfuration, reduce the fraction defective of tyre bead bubble, improve the quality of tire.
The technical scheme providing according to the utility model: tire liner gluing sheet device, it is installed on former cutting apparatus, it is characterized in that: comprise Film cutter, dancer rools group and laminating pressure roller, described Film cutter has two, two Film cutters are arranged on the cutoff knife rack of former cutting apparatus, lay respectively at the outside of both sides edge iron, Film cutter connects gauge tap by connecting line, Film cutter is for coordinating with the edge iron of former cutting apparatus, and a part of glue sideline judge that transition zone film is cut cuts as laminating film; Described dancer rools group has two groups, and what two groups of dancer rools groups were separately positioned on former cutting apparatus accesses roller bed both sides, and dancer rools group turn to the transition zone film top cutting for the laminating film that cutting knife is cut; Described laminating pressure roller is arranged on and accesses on roller bed, and laminating pressure roller attaches to transition zone film for the laminating film that upset is put in place.
As further improvement of the utility model, described dancer rools group comprises the first dancer rools, the second dancer rools and the 3rd dancer rools setting gradually along transition zone film transport direction, described the first dancer rools is for rising and guide to the second dancer rools by laminating film, described the second dancer rools for by laminating film to 90 ° of transition zone film direction upsets and guide to the 3rd dancer rools, described the 3rd dancer rools is for overturning the continuation of laminating film 90 ° and guide to paster pressure roller.
compared with prior art, advantage is the utility model:the utility model is simple in structure, directly be installed on former cutting apparatus, do not change existing equipment agent structure, can when producing, inner liner directly add gluing sheet, solve some fetus because inner liner defect causes there is the problem of mass defect after sulfuration, reduce the fraction defective of tyre bead bubble, improve the quality of tire.
Accompanying drawing explanation
Fig. 1 is the structural representation of existing cutting apparatus.
Fig. 2 is the structural representation of the utility model embodiment.
Description of reference numerals: 1-cutoff knife rack, 2-edge iron, 3-glue limit, 4-access roller bed, 5-transition zone film, 6-connecting line, 7-Film cutter, 8-laminating film, 9-the first dancer rools, 10-the second dancer rools, 11-the 3rd dancer rools, the 12-pressure roller of fitting.
The specific embodiment
Below in conjunction with concrete drawings and Examples, the utility model is described in further detail.
As shown in the figure: the inner liner gluing sheet device in embodiment is installed on former cutting apparatus, mainly by Film cutter 7, dancer rools group and laminating pressure roller 12, formed, described Film cutter 7 has two, two Film cutters 7 are arranged on the cutoff knife rack 1 of former cutting apparatus, lay respectively at the outside of both sides edge iron 2, Film cutter 7 connects gauge tap by connecting line 6, Film cutter 7 coordinates for the edge iron 2 with former cutting apparatus, and a part of glue limit 3 that transition zone film 5 is cut cuts as laminating film 8; Described dancer rools group has two groups, and what two groups of dancer rools groups were separately positioned on former cutting apparatus accesses roller bed 4 both sides, and dancer rools group turn to for the laminating film 8 that cutting knife is cut transition zone film 5 tops that cut; Described laminating pressure roller 12 is arranged on and accesses on roller bed 4, and laminating pressure roller 12 attaches to transition zone film 5 for the laminating film 8 that upset is put in place.
In the utility model, described dancer rools group is mainly comprised of the first dancer rools 9, the second dancer rools 10 and the 3rd dancer rools 11, the first dancer rools 9, the second dancer rools 10 and the 3rd dancer rools 11 set gradually along transition zone film 5 throughput directions, described the first dancer rools 9 is for rising laminating film 8 guide to the second dancer rools 10, described the second dancer rools 10 for by laminating film 8 to 90 ° of transition zone film 5 directions upsets and guide to the 3rd dancer rools 11, described the 3rd dancer rools 11 is for continuing laminating film 8 to overturn 90 ° and guide to paster pressure roller.
The outside of the utility model original edge iron 2 on the cutoff knife rack 1 of former cutting apparatus respectively increases a paster limit cutter, another part glue limit 3 that a part of glue limit 3 of cutting on transition zone film 5 is cut as laminating film 8(is normally returned), then by some dancer rools groups and the pressure roller accessing on roller bed 4, the laminating film 8 cutting is fitted on transition zone film 5.Facts have proved, this film laminating type has not only successfully solved tyre bead starved phenomenon, and has stopped the problem of the cold subsides generation of moulding tyre bead bubble, compares moulding manual assembly and has improved production efficiency, has reduced cost, has improved the quality of tire.

Claims (2)

1. tire liner gluing sheet device, it is installed on former cutting apparatus, it is characterized in that: comprise Film cutter (7), dancer rools group and laminating pressure roller (12), described Film cutter (7) has two, two Film cutters (7) are arranged on the cutoff knife rack (1) of former cutting apparatus, lay respectively at the outside of both sides edge iron (2), Film cutter (7) connects gauge tap by connecting line (6), Film cutter (7) coordinates for the edge iron with former cutting apparatus (2), a part of glue limit (3) that transition zone film (5) is cut cuts as laminating film (8), described dancer rools group has two groups, and what two groups of dancer rools groups were separately positioned on former cutting apparatus accesses roller bed (4) both sides, and dancer rools group turn to transition zone film (5) top cutting for the laminating film (8) that cutting knife is cut, described laminating pressure roller (12) is arranged on and accesses roller bed (4) above, and laminating pressure roller (12) attaches to transition zone film (5) for the laminating film (8) that upset is put in place.
2. tire liner gluing sheet device as claimed in claim 1, it is characterized in that: described dancer rools group comprises the first dancer rools (9) setting gradually along transition zone film (5) throughput direction, the second dancer rools (10) and the 3rd dancer rools (11), described the first dancer rools (9) rises and guides to the second dancer rools (10) for the film (8) of fitting, described the second dancer rools (10) for the film (8) of fitting to 90 ° of transition zone film (5) direction upsets and guide to the 3rd dancer rools (11), described the 3rd dancer rools (11) continues 90 ° of upsets and guides to paster pressure roller for the film (8) of fitting.
CN201320393288.4U 2013-07-02 2013-07-02 Device for adhering adhesive piece to tire lining Withdrawn - After Issue CN203438555U (en)