CN203414391U - Comprehensive power grid material corrosion environment simulator - Google Patents
Comprehensive power grid material corrosion environment simulator Download PDFInfo
- Publication number
- CN203414391U CN203414391U CN201320402127.7U CN201320402127U CN203414391U CN 203414391 U CN203414391 U CN 203414391U CN 201320402127 U CN201320402127 U CN 201320402127U CN 203414391 U CN203414391 U CN 203414391U
- Authority
- CN
- China
- Prior art keywords
- device box
- box body
- corrosion
- porous plate
- environment simulator
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
The utility model relates to a comprehensive power grid material corrosion environment simulator. The simulator comprises a multi-component gas connection device and a device box body, wherein the multi-component gas connection device and the device box body are connected through a pipe provided with a flow meter; an air exhausting valve and a box body pressure meter are mounted at the top of the device box body; a water inlet valve is mounted on the left side wall of the device box body; a water exhausting valve is mounted at the bottom of the right side wall of the device box body; an acid rain generator, an ultraviolet irradiator and an acid mist generator are mounted at the top in the device box body; the top of the device box body is downwardly hung with a corrosion test piece; a porous plate is mounted under the corrosion test piece, and is provided with a stray current generation device and a test box; a multi-component water solution is injected into the device box body under the porous plate; and a corrosion test block hung under the porous plate is dipped in the multi-component water solution. The comprehensive power grid material corrosion environment simulator realizes the corrosion simulation acceleration experiment of power grid materials and coating layers in various complex environments.
Description
Technical field
The utility model belongs to the environmental test technical field of electric power material corrosion resistance, particularly a kind of comprehensive electrical network material corrosion environment simulator.
Background technology
Existing corrosion accelerated test case is generally all based under single salt air corrosion gas condition or the corrosion accelerated test of carrying out under soil environment on the market at present, mainly for single metal testing plate, test, can not meet the environmental simulation test of comprehensive electrical network material corrosion.
Summary of the invention
The purpose of this utility model is to overcome the deficiencies in the prior art, and a kind of comprehensive electrical network material corrosion environment simulator is provided.
The utility model solves its technical matters and takes following technical scheme to realize:
A kind of comprehensive electrical network material corrosion environment simulator, it is characterized in that: comprise multicomponent gas coupling arrangement and device box, multicomponent gas coupling arrangement is connected by the pipeline of flowmeter is installed with device box, on the pipeline being communicated with box house of installing in device box top left outside, vent valve is installed, in device box top right outside, tank pressure instrument is installed, on the pipeline being communicated with box house of installing in device box left side wall bottom, water intaking valve is installed, on the pipeline being communicated with box house of installing in device box right side wall bottom, draining valve is installed, top in device box is provided with acid rain generator from left to right successively, ultraviolet irradiation device and acid mist generator, top in device box is also hung with corrosion coupon downwards, the horizontal perforated panel affixed with device box sidewall is installed below corrosion coupon, at porous plate upper surface, lay respectively stray current generating means and bottom is the chamber of porous, in device box below porous plate, be injected with polycomponent aqueous solution, in polycomponent aqueous solution immersed with the corrosion test block of hanging below porous plate.
And described multicomponent gas coupling arrangement Wei San installs valvular connecting pipe in road.
And described bottom is the interior corrosion test material of placing of the chamber of porous.
And the liquid level of the polycomponent aqueous solution of injecting in described device box is below porous plate plane.
And the position of the corrosion coupon that hang downwards at described top in device box is below described acid rain generator, ultraviolet irradiation device and acid mist generator.
Advantage of the present utility model and good effect are
The utility model is realized electrical network material and coating at marine atmosphere eroded environment; Seawater (configuration, natural) corrosion environment; Rainwater corrosion environment; The drying and watering cycle corrosion environment of seawater Tidal zone; Marine climate corrosion simulation environment; The corrosion simulated environment of soil (salt content, water cut); Stray current corrosion simulated environment, corrosion simulated accelerated test under the environment such as high temperature ultraviolet irradiation Aging simulation corrosion environment.
Accompanying drawing explanation
Fig. 1 is the utility model device one-piece construction schematic diagram.
Embodiment
Below in conjunction with accompanying drawing, the utility model embodiment is further described, following examples are descriptive, are not determinate, can not limit protection domain of the present utility model with this.
A kind of comprehensive electrical network material corrosion environment simulator, as shown in Figure 1, comprise multicomponent gas coupling arrangement 1 and device box 4, multicomponent gas coupling arrangement is connected by the pipeline of flowmeter 2 is installed with device box, on the pipeline being communicated with box house of installing in device box top left outside, vent valve 3 is installed, in device box top right outside, tank pressure instrument 9 is installed, on the pipeline being communicated with box house of installing in device box left side wall bottom, water intaking valve 16 is installed, on the pipeline being communicated with box house of installing in device box right side wall bottom, draining valve 12 is installed, top in device box is provided with acid rain generator 5 from left to right successively, ultraviolet irradiation device 7 and acid mist generator 8, top in device box is also hung with corrosion coupon 6 downwards, the horizontal perforated panel 11 affixed with device box sidewall is installed below corrosion coupon, at porous plate upper surface, lay respectively stray current generating means 15 and bottom is the chamber 10 of porous, in device box below porous plate, be injected with polycomponent aqueous solution 13, in polycomponent aqueous solution immersed with the corrosion test block 14 of hanging on porous plate.
In concrete enforcement of the present utility model, described multicomponent gas coupling arrangement Wei San installs valvular connecting pipe in road.
In concrete enforcement of the present utility model, described bottom is the interior corrosion test material of placing of the chamber of porous.
In concrete enforcement of the present utility model, the liquid level of the polycomponent aqueous solution of injecting in described device box is below porous plate plane.
In concrete enforcement of the present utility model, the position of the corrosion coupon that hang downwards at described top in device box is below described acid rain generator, ultraviolet irradiation device and acid mist generator.
The utility model can be as required realized drying and watering cycle corrosion environment, marine climate corrosion simulation environment, soil corrosion simulated environment, the stray current corrosion simulated environment of marine atmosphere eroded environment, corrosive environment of sea water, rainwater corrosion environment, seawater Tidal zone, the simulated acceleration test of high temperature ultraviolet irradiation Aging simulation corrosion environment to electrical network material and coating.
Claims (5)
1. a comprehensive electrical network material corrosion environment simulator, it is characterized in that: comprise multicomponent gas coupling arrangement and device box, multicomponent gas coupling arrangement is connected by the pipeline of flowmeter is installed with device box, on the pipeline being communicated with box house of installing in device box top left outside, vent valve is installed, in device box top right outside, tank pressure instrument is installed, on the pipeline being communicated with box house of installing in device box left side wall bottom, water intaking valve is installed, on the pipeline being communicated with box house of installing in device box right side wall bottom, draining valve is installed, top in device box is provided with acid rain generator from left to right successively, ultraviolet irradiation device and acid mist generator, top in device box is also hung with corrosion coupon downwards, the horizontal perforated panel affixed with device box sidewall is installed below corrosion coupon, at porous plate upper surface, lay respectively stray current generating means and bottom is the chamber of porous, in device box below porous plate, be injected with polycomponent aqueous solution, in polycomponent aqueous solution immersed with the corrosion test block of hanging below porous plate.
2. comprehensive electrical network material corrosion environment simulator according to claim 1, is characterized in that: described multicomponent gas coupling arrangement Wei San installs valvular connecting pipe in road.
3. comprehensive electrical network material corrosion environment simulator according to claim 1, is characterized in that: described bottom is the interior corrosion test material of placing of the chamber of porous.
4. comprehensive electrical network material corrosion environment simulator according to claim 1, is characterized in that: the liquid level of the polycomponent aqueous solution of injecting in described device box is below porous plate plane.
5. comprehensive electrical network material corrosion environment simulator according to claim 1, is characterized in that: the position of the corrosion coupon that hang downwards at described top in device box is below described acid rain generator, ultraviolet irradiation device and acid mist generator.