CN203304546U - 一种连铸中间包钢水加热装置 - Google Patents
一种连铸中间包钢水加热装置 Download PDFInfo
- Publication number
- CN203304546U CN203304546U CN2012205338580U CN201220533858U CN203304546U CN 203304546 U CN203304546 U CN 203304546U CN 2012205338580 U CN2012205338580 U CN 2012205338580U CN 201220533858 U CN201220533858 U CN 201220533858U CN 203304546 U CN203304546 U CN 203304546U
- Authority
- CN
- China
- Prior art keywords
- blocking wall
- retaining wall
- continuous casting
- hollow structure
- zone
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种连铸中间包钢水加热装置,涉及冶金行业炼钢生产,由直流电源,阴极、阳极、上挡墙、下挡墙、前挡墙,底吹氩孔、水口,集电板构成。阴极采用等离子枪,设在包顶,阳极为导电镁碳砖,位于包底。洼流区和加热区之间有上挡墙,呈低空结构,上挡墙和加热点之间设下挡墙,呈半壁上空结构,加热区和分流区之间设前挡墙,呈半壁侧空结构,加热点和下挡墙之间有底吹氧孔。本实用新型设备简单、操作方便、实用可靠、近似恒温浇注。
Description
技术领域
本实用新型属于冶金行业炼钢生产领域,具体的说是一种连铸中间包内加热钢水装置。
背景技术
连铸的钢水温度是保证连铸机正常生产的重要因素之一,连铸中间包钢水温度过高会导致铸坯的柱状晶过于发达,内部裂纹粗大,易造成拉漏溢钢等事故,温度过低则钢水流动性差,易堵死水口o目前,多采取出钢温度宁高勿低的办法,这样就加重了炼钢炉的热负荷,使钢的质量恶化,炉龄降低。世界上较先进的生产技术是采用直流等离子加热法,昭59-107755和昭61-95755公开了两种中间包钢水的加热法,两种方式都采用交流等离子枪进行加热,中间包周围设备较多,可利用空间小,实际生产中带来许多不便,等离子弧不稳,热效率不高。昭57-115674和昭54-168780是两种中间包钢水感应加热法,设备复杂,热效率低。
发明内容
为了克服现有技术中的不足,提供一种加热装置,以控制中间包内钢水的过热度,实现近似恒温浇注。
本实用新型解决其技术问题所采用的技术方案是:一种连铸中间包内加热钢水装置,由直流电源、阴极、阳极、上挡墙、下挡墙、前挡墙、底吹氩孔、水口、集电板构成的连铸中间包钢水加热装置,其特征在于:阴极采用等离子枪或石墨电极或中空石墨电极,置于中间包的顶部;阳极采用导电镁碳砖或用钢板包裹的镁碳砖的结构;在注流区和加热区之间有上挡墙,呈半壁底空结构,上挡墙和加热点之间有下挡墙,呈半壁上空结构,加热区和分流区之间有前挡墙,前挡墙呈半壁侧空结构;底吹氩孔为单孔或排在一条直线上的多孔构成,位于加热点和下挡墙之间。
本实用新型的有益效果:本实用新型设备简单、操作方便、实用可靠。可在连铸过程中加热钢水,准确控制中间包内钢水的过热度,实现近似恒温浇注。
附图说明
下面结合附图和实施例对本实用新型进一步说明。
图1是本实用新型主视剖面图。
图2是本实用新型只有下挡墙的主视剖面图。
图中 1.直流电源,2.阴极,3.钢包,4.中间包,5.上挡墙,6.下挡墙,7.底吹氩孔,8.水口,9.导电镁碳砖,10.集电板,11.前挡墙,12.包盖,13.结晶器。
具体实施方式
在图中,一种连铸中间包内加热钢水装置,直流电源1由变压器、整流器组成,整流方式为6脉、12脉、18脉和24脉。阴极2使用直流等离子枪、电渣和电弧三种方式加热,即等离子加热、电渣加热和电弧加热。阴极2一般装在一个可上下移动和旋转的机构上进行操作,位于包盖12中部,石墨电极作阴极时还可以中心开孔并通氩气以稳定电弧。阳极回路由导电镁碳砖9或用钢板包裹的镁碳砖和集电板10组成。导电镁碳砖9装在中间包底部,或装在中间包侧壁,其一端与钢水接触导电,另一端与集电板10相连,集电板10经电缆与直流电源1相连。导电镁碳砖9其特点是在常温和温度达1600℃范围内电阻率基本接近,都是电的良导体,也就是说中间包在冷状态下也能正常导电形成回路。水口8设在前挡墙11一侧。中间包4是加热钢水容器。直流电源1、阴极2、钢液、阳极导电镁碳砖9、集电板10构成回路。钢水经钢包3注入中间包4的注流区,从上挡墙5下部流出,经下挡墙6上部流到加热区,通过阴极2加热和底吹氩搅拌后,流经前挡墙11进入分流区,然后从水口8流入结晶器13铸成连铸坯。
实施例1:图l给出四流弧型连铸中间包钢水加热装置。连铸中间包4分为注流区、加热区和分流区,中间包的包盖12中部设有阴极2,阴极2使用直径70mm钨阴极等离子枪。阳极在分流区侧壁,用导电镁碳砖9和集电板10构成,注流区和加热区之间设有上挡墙5,上挡墙5为下空结构,和加热点之间有半壁下挡墙6,加热区和分流区之间有侧空结构的前挡墙11,下挡墙6和加热点之间有底吹氩孔7。直流电源变压器容量l250KVA、整流器采用两组三相桥并联12脉动整流,直流电压200V,直流电流5500A。
实施例2:图2适用于双流水平连铸中间包钢水加热装置。阴极2使用Φ150mm中空石墨电极,中间包内只设下挡墙6和底吹氩孔7,其它同实施例1。
实施例3:双流水平连铸中间包钢水加热装置,阴极2使用150*150mm铸坯进行电渣加热,其它同实施例1。
Claims (2)
1.一种由直流电源、阴极、阳极、上挡墙、下挡墙、前挡墙、底吹氩孔、水口、集电板构成的连铸中间包钢水加热装置,其特征在于:阴极采用等离子枪或石墨电极或中空石墨电极,置于中间包的顶部;阳极采用导电镁碳砖或用钢板包裹的镁碳砖的结构;在注流区和加热区之间有上挡墙,呈半壁底空结构,上挡墙和加热点之间有下挡墙,呈半壁上空结构,加热区和分流区之间有前挡墙,前挡墙呈半壁侧空结构;底吹氩孔为单孔或排在一条直线上的多孔构成,位于加热点和下挡墙之间。
2.根据权利要求l所述的连铸中间包钢水加热装置,其特征在于:中间包内只设下挡墙、底吹氩孔。