CN202852218U - 一种耐腐蚀玻璃钢管道 - Google Patents
一种耐腐蚀玻璃钢管道 Download PDFInfo
- Publication number
- CN202852218U CN202852218U CN 201220535387 CN201220535387U CN202852218U CN 202852218 U CN202852218 U CN 202852218U CN 201220535387 CN201220535387 CN 201220535387 CN 201220535387 U CN201220535387 U CN 201220535387U CN 202852218 U CN202852218 U CN 202852218U
- Authority
- CN
- China
- Prior art keywords
- corrosion
- layer
- reinforced plastic
- thermal insulation
- resisting
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种耐腐蚀玻璃钢管道,包括基管、复合层以及玻璃钢套管,基管为厚度40~50mm的钢管,其内壁衬有一层耐腐蚀陶瓷层,而复合层夹在基管以及玻璃钢套管之间,通过热熔胶粘接,包括保温层以及耐腐蚀层,保温层紧贴基管,而耐腐蚀层则贴合在保温层外壁上与玻璃钢套管粘合,所述保温层采用聚氨酯保温材料发泡填充制成,而耐腐蚀层则由树脂与氯丁橡胶通过物理方式均匀混合制成。本实用新型工艺简单,加工方便,耐腐蚀能力优秀。
Description
技术领域
本实用新型涉及管道输送技术,具体为一种耐腐蚀玻璃钢管道。
背景技术
在现代工业作业领域中,经常需要对一些流质进行远距离输送。现有的输送管道通常都是采用普通的钢管、铸铁管或者复合管作为基管,并在基管外层缠绕保温防护材料,然后在保温材料的基础上再用铁皮等物覆盖。然而,这种输送管道存在的问题在于:整个管道的刚性和硬度都很差,外覆铁皮很容易在环境以及外力作用下腐蚀、变形甚至穿孔,导致其管道性能下降,使用寿命,仅仅能维持在三个月到一年,严重影响管道的正常输送,以至于影响到正常的工业装配生产。
实用新型内容
本实用新型所解决的技术问题在于提供一种耐腐蚀玻璃钢管道,以解决上述背景技术中的缺点。
本实用新型所解决的技术问题采用以下技术方案来实现:
一种耐腐蚀玻璃钢管道,包括基管、复合层以及玻璃钢套管,其中,基管为钢管,厚度为40~50mm,其内壁衬有一层耐腐蚀陶瓷层,而复合层夹在基管以及玻璃钢套管之间,通过热熔胶粘接,包括保温层以及耐腐蚀层,保温层紧贴基管,而耐腐蚀层则贴合在保温层外壁上与玻璃钢套管粘合,所述保温层采用聚氨酯保温材料发泡填充制成,而耐腐蚀层则由树脂与氯丁橡胶通过物理方式均匀混合制成。
在本实用新型中,所述复合层中耐腐蚀层的厚度为15mm~25mm,而保温层厚度为60mm~100mm。
在本实用新型中,所述耐腐蚀层中应优选采用不饱和聚酯树脂,且树脂的含量比按重量配比为25%~32%。
有益效果:本实用新型具有耐磨、耐热、耐腐蚀等众多优点,且其内部填料层分布均匀、密度低,可有效减少复合管道重量,在保证保温性能的同时易于运输安装,且由于采用玻璃钢套管套装,使得管道本身在外力作用下损坏的可能性大大降低,可有效延长整个管道的使用寿命。
附图说明
图1 为本实用新型较佳实施例的示意图。
具体实施方式
为了使本实用新型实现的技术手段、创作特征、达成目的与功效易于明白了解,下面结合具体图示,进一步阐述本实用新型。
参见图1的一种耐腐蚀玻璃钢管道的较佳实施例,在本实施例中,包括基管4、复合层以及玻璃钢套管1,其中,基管4为厚度40mm的钢管,其内壁衬有一层耐腐蚀陶瓷层5,复合层位于基管4以及玻璃钢套管1之间,包括保温层3以及耐腐蚀层2,保温层3采用聚氨酯保温材料发泡填充制成紧贴基管4的外表面,而耐腐蚀层则由树脂与氯丁橡胶通过物理方式均匀混合制成贴合在玻璃钢套管1的内表面。
在本实施例中,所述复合层中耐腐蚀层2的厚度为20mm,而保温层3厚度为60mm。
以上显示和描述了本实用新型的基本原理、主要特征和本实用新型的优点。本行业的技术人员应该了解,本实用新型不受上述实施例的限制,上述实施例和说明书中描述的只是说明本实用新型的原理,在不脱离本实用新型精神和范围的前提下,本实用新型还会有各种变化和改进,这些变化和改进都落入要求保护的本实用新型范围内。本实用新型要求保护范围由所附的权利要求书及其等效物界定。
Claims (3)
1.一种耐腐蚀玻璃钢管道,包括基管、复合层以及玻璃钢套管,其特征在于,基管为厚度40~50mm的钢管,其内壁衬有一层耐腐蚀陶瓷层,而复合层夹在基管以及玻璃钢套管之间,通过热熔胶粘接,包括保温层以及耐腐蚀层,保温层紧贴基管,而耐腐蚀层则贴合在保温层外壁上与玻璃钢套管粘合,所述保温层采用聚氨酯保温材料发泡填充制成,而耐腐蚀层则由树脂与氯丁橡胶通过物理方式均匀混合制成。
2.根据权利要求1所述的一种耐腐蚀玻璃钢管道,其特征在于,所述复合层中耐腐蚀层的厚度为15mm~25mm,而保温层厚度为60mm~100mm。
3.根据权利要求1所述的一种耐腐蚀玻璃钢管道,其特征在于,所述耐腐蚀层为不饱和聚酯树脂,且树脂的含量比按重量配比为25%~32%。