CN202805777U - 一种双色烂花绒 - Google Patents
一种双色烂花绒 Download PDFInfo
- Publication number
- CN202805777U CN202805777U CN 201220343921 CN201220343921U CN202805777U CN 202805777 U CN202805777 U CN 202805777U CN 201220343921 CN201220343921 CN 201220343921 CN 201220343921 U CN201220343921 U CN 201220343921U CN 202805777 U CN202805777 U CN 202805777U
- Authority
- CN
- China
- Prior art keywords
- layer
- etched
- coating layer
- double
- grey cloth
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种双色烂花绒,包括平置的坯布层,坯布层的顶面固定有由坯布进行单面抓绒起毛形成的绒毛层,坯布层的顶面还固定有第一涂料层,绒毛层的每根绒毛都贯穿第一涂料层,且每根绒毛都覆盖有第二涂料层,第二涂料层与第一涂料层连接,且第二涂料层厚度小于第一涂料层厚度,绒毛层设有至少一个由罗拉印花形成的凹陷,坯布层的底面还固定有第三涂料层。所述凹陷在绒毛层顶面的截面形状为花瓣形。所述凹陷的数量为两个以上。所述各凹陷的深度沿着坯布层的延伸方向递减或递加。本双色烂花绒,其印花的花型图案立体性强,还有效保持了绒布本身的柔软性和手感舒适性,色彩牢固度强,不易褪色,且设计合理,结构简单。
Description
技术领域
本实用新型涉及一种布料,具体涉及一种双色烂花绒。
背景技术
随着科技进步和人们居住水平的日益提高,人们对布面家具的面料及花纹要求日渐提升,这便对此类面料的印染企业提出了新的技术突破指标。
在面料的选择上,易于清洗、柔软、手感舒适性等要求,尤其是家具类外包材料选择的首要考虑,其次面料的成本也是家具制造商所考虑的重点。经过繁杂的筛选,涤纶超细纤维绒布面料便成为其中一类应用较多的外包材料,为人们带来了极为舒适的触感。
超细纤维用途很广:用它作的织物,经砂洗、磨绒等高级整理后,表面形成一层类似桃皮茸毛的外观,并极为膨松、柔软、滑爽。
但目前市场上家具外包绒布产品,其色彩牢固度差,手感也较硬,颜色单调,花型图案立体性差。
实用新型内容
本实用新型的目的在于提供一种双色烂花绒,其印花的花型图案立体性强,还有效保持了绒布本身的柔软性和手感舒适性,且设计合理,结构简单。
为实现上述目的,本实用新型的技术方案是设计一种双色烂花绒,包括平置的坯布层,坯布层的顶面固定有由坯布进行单面抓绒起毛形成的绒毛层,坯布层的顶面还固定有第一涂料层,绒毛层的每根绒毛都贯穿第一涂料层,且每根绒毛都覆盖有第二涂料层,第二涂料层与第一涂料层连接,且第二涂料层厚度小于第一涂料层厚度,绒毛层设有至少一个由罗拉印花形成的凹陷,坯布层的底面还固定有第三涂料层。
优选的,所述各绒毛覆盖的第二涂料层厚度相同。
优选的,所述各绒毛覆盖的第二涂料层厚度沿着坯布层的延伸方向递减或递加。
优选的,所述凹陷在绒毛层顶面的截面形状为多边形。
优选的,所述凹陷在绒毛层顶面的截面形状为矩形。
优选的,所述凹陷在绒毛层顶面的截面形状为圆形。
优选的,所述凹陷在绒毛层顶面的截面形状为花瓣形。
优选的,所述凹陷的数量为两个以上。
优选的,所述各凹陷的深度相同。
优选的,所述各凹陷的深度沿着坯布层的延伸方向递减或递加。
由于烂花后形成的花型图案(由各个凹陷组成)与原印花的深浅过渡的花型图案(由各第二涂料层组成)相复合,且透视性地呈现了底面坯布层的原色,极大地提高了涤纶超细纤维绒布面料的印花立体感程度,且有效保持了绒布本身的柔软性和手感舒适性。
本实用新型的优点和有益效果在于:提供一种双色烂花绒,其印花的花型图案立体性强,还有效保持了绒布本身的柔软性和手感舒适性,色彩牢固度强,不易褪色,且设计合理,结构简单。
附图说明
图1是本实用新型的示意图。
具体实施方式
下面结合附图和实施例,对本实用新型的具体实施方式作进一步描述。以下实施例仅用于更加清楚地说明本实用新型的技术方案,而不能以此来限制本实用新型的保护范围。
本实用新型具体实施的技术方案是:
一种双色烂花绒,包括平置的坯布层1,坯布层1的顶面固定有由坯布进行单面抓绒起毛形成的绒毛层2,坯布层1的顶面还固定有第一涂料层3,绒毛层2的每根绒毛4都贯穿第一涂料层3,且每根绒毛4都覆盖有第二涂料层5,第二涂料层5与第一涂料层3连接,且第二涂料层5厚度小于第一涂料层3厚度,绒毛层2设有两个以上由罗拉印花形成的凹陷6,坯布层1的底面还固定有第三涂料层7。所述各绒毛4覆盖的第二涂料层5厚度相同。所述凹陷6在绒毛层2顶面的截面形状为花瓣形。所述各凹陷6的深度相同。
以上所述仅是本实用新型的优选实施方式,应当指出,对于本技术领域的普通技术人员来说,在不脱离本实用新型技术原理的前提下,还可以做出若干改进和润饰,这些改进和润饰也应视为本实用新型的保护范围。
Claims (9)
1.一种双色烂花绒,其特征在于,包括平置的坯布层,坯布层的顶面固定有由坯布进行单面抓绒起毛形成的绒毛层,坯布层的顶面还固定有第一涂料层,绒毛层的每根绒毛都贯穿第一涂料层,且每根绒毛都覆盖有第二涂料层,第二涂料层与第一涂料层连接,且第二涂料层厚度小于第一涂料层厚度,绒毛层设有至少一个由罗拉印花形成的凹陷,坯布层的底面还固定有第三涂料层。
2.根据权利要求1所述的双色烂花绒,其特征在于,所述各绒毛覆盖的第二涂料层厚度相同。
3.根据权利要求1所述的双色烂花绒,其特征在于,所述各绒毛覆盖的第二涂料层厚度沿着坯布层的延伸方向递减或递加。
4.根据权利要求1所述的双色烂花绒,其特征在于,所述凹陷在绒毛层顶面的截面形状为多边形。
5.根据权利要求1所述的双色烂花绒,其特征在于,所述凹陷在绒毛层顶面的截面形状为矩形。
6.根据权利要求1所述的双色烂花绒,其特征在于,所述凹陷在绒毛层顶面的截面形状为圆形。
7.根据权利要求1所述的双色烂花绒,其特征在于,所述凹陷的数量为两个以上。
8.根据权利要求7所述的双色烂花绒,其特征在于,所述各凹陷的深度相同。
9.根据权利要求7所述的双色烂花绒,其特征在于,所述各凹陷的深度沿着坯布层的延伸方向递减或递加。